• Title/Summary/Keyword: Beeswax-treated Hanji

Search Result 12, Processing Time 0.016 seconds

Characteristics of Beeswax-treated Hanji Aged by Closed and Ventilated Chamber (밀폐 및 배기조건에서 열화된 밀랍지의 열화특성 분석)

  • Kang, Yeong Seok;Yang, Eun Jeong
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.44 no.6
    • /
    • pp.9-14
    • /
    • 2012
  • Currently a variety of efforts to conserve and restore the injured the Annal of the Joseon Dynasty are continued and many studies about the aging pathway of the beeswax-treated volume have being progressed. In this study, two chambers were set up to assess the influence of VOCs(Volatile Organic Compounds) generated in process of beeswax deterioration. One chamber was closed and the other was continuously ventilated in order to remove the VOCs. In results, the acid compounds of beeswax-treated Hanjis aged in closed chamber was more than that aged in ventilated chamber. The folding endurance of beeswax-treated Hanjis aged in closed chamber was lower than that aged in ventilated chamber. Accumulated acid compounds of beeswax-treated Hanji in closed chamber may cause accelerated aging and strength decrease. In conclusion, accumulated acid compounds can accelerate the aging of beeswax-treated Hanji and cause the severe deterioration of inside of beeswax-treated volume. Therefore, to preserve more safely beeswax-treated volumes of the Annals of the Joseon Dynasty, it is essential that VOCs emitted from beeswax-treated volume are ventilated.

Effect of Wet Cleaning on the Property of Aged Duplicated Beeswax-Treated Paper (열화된 밀랍지 시제품의 습식크리닝 처리효과 분석)

  • Choi, Kyoung-Hwa;Park, Ji-Hee
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.42 no.4
    • /
    • pp.25-32
    • /
    • 2010
  • The beeswax-treated volumes of the Annals of Joseon Dynasty, designated as a UNESCO's Memories of the World, have been more seriously damaged than the untreated ones. As a continuous effort to develop the optimal conservation techniques for the damaged beeswax-treated volumes of the Annals, this study examines the effectiveness of wet cleaning on the conservation of the beeswax-treated paper. To do this, wet cleaning is performed on the duplicated beeswax-treated paper and the Hanji that are aged at $105^{\circ}C$ for 30 days using distilled water of $24^{\circ}C$ and $50^{\circ}C$. As results, it is observed that pH of the both the beeswax-treated paper and the Hanji increase, indicating the removal of the acid of the aged paper samples through wet cleaning. After the wet cleaning, however, the physical properties and viscosity of the Hanji decrease, while those of the beeswax-treated paper increase. It is also found that wet cleaning contributes to enhancement of most optical properties of the Hanji, but not for those of the beeswax-treated paper except for the $b^*$ value. Analyses of UV absorbance of cleaning water demonstrate that both the beeswax-treated paper and the Hanji have typical spectra of chromophore compounds of cellulose.

Evaluation of Dewaxing and Strengthening Treatments for Stabilization of Aged Beeswax-treated Hanji (열화 밀랍지의 탈랍 및 강도보강 처리 안정성 평가)

  • Jeong, Hye Young;Go, In Hee;Nam, Hyun Ju;Choi, Kyoung Hwa
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.45 no.6
    • /
    • pp.10-16
    • /
    • 2013
  • This study aims to carry out the final evaluation on the deterioration stability of dewaxing and strengthening treatments devised to conserve and restore the beeswax-treated volumes of the Annals of the Joseon Dynasty. Thus, this study artificially deteriorated dewaxed Hanji, strengthened Hanji and beeswax-treated Hanji with optimized processing conditions applied, and comparatively analyzed the deterioration characteristics of each kind of Hanji. As a result of this study, it turned out that there was the loss of physical strength and the value of $L^*$ was increased and the values of $a^*$ and $b^*$ were decreased from removing beeswax after dewaxing by supercritical fluid extraction (SFE). Also deteriorated strength during dewaxing was reinforced by strengthening treatment with methylcellulose and it showed higher strength than beeswax-treated Hanji. From the evaluation on deterioration stability after dewaxing and strengthening, it turned out that deterioration stability of strengthened Hanji is the superior. Therefore, it is presumed that conservation of aged beeswax-treated Hanji can be improved and extended when dewaxing and strengthening are applied under optimum conditions.

Effect of Humid Cycling Accelerated Aging on Deterioration of Duplicated Beeswax-Treated Volume (밀랍본 시제품의 습식 순환인공열화 특성분석)

  • Choi, Kyoung-Hwa;Park, Ji-Hee;Jeong, Hye-Young;Seo, Jin-Ho
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.42 no.4
    • /
    • pp.15-24
    • /
    • 2010
  • Many efforts to understand the deterioration processes of the beeswax-treated volume of "The Annals of Joseon Dynasty" have been made. However, most previous studies have focused on individual sample sheet of the beeswax-treated paper but not book volume format. In this study, humid cycling accelerated aging for duplicated beeswax-treated book volume and Hanji book volume were carried out to examine differences in the deterioration of different parts of each volume as well as between the two book volumes during the aging. As results, it is found that the deterioration rate for the beeswax-treated volume is higher than that for the Hanji book volume. Different parts in each volume show different magnitude of deterioration. In particular, outer sides in both beeswax-treated and Hanji book volumes, which are directly exposed to the air, are deteriorated more seriously than inner sides. It is also observed that inner sides are considerably deteriorated during the aging, implying that inner deterioration may have different mechanisms from outer deterioration.

Effect of Dewaxing Ratio of Beeswax-treated Hanji by Heat and Pressure Method on Aging Behavior of Dewaxed Hanji (가온 가압법에 의한 밀랍도포한지의 탈랍율이 탈랍지의 열화 거동에 미치는 영향)

  • Cho, Byoung-Uk;Choi, Do-Chim;Jo, Byoung-Muk
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.44 no.3
    • /
    • pp.15-21
    • /
    • 2012
  • The optimum dewaxing ratio in dewaxing treatment by the heat and pressure method was investigated by considering aging stability of dewaxed Hanji. Commercial Hanji was coated with beeswax and thermally aged at $150^{\circ}C$ for 24 hours. Then it was dewaxed using the laboratory sheet press equipped with hot plates on both top and bottom sides. Dewaxing ratio was controlled by pressing temperature and time. Four type of dewaxed Hanji samples with different dewaxing ratio were prepared and thermally aged at $150^{\circ}C$. Then the aging stability of dewaxed Hanji samples was evaluated in terms of optical and strength properties. It was found that the aging stability of dewaxed Hanji was superior with higher dewaxing ratio. The result concluded that, in the aspect of aging stability, the coated beeswax in beeswax-treated Hanji shall be completely removed if the coated wax would be dewaxed.

Optimal Organic Solvent Extraction Method for Dewaxing of Beeswax-treated Hanji (밀랍도포한지의 탈랍을 위한 최적 유기용매 추출기법 탐색)

  • Choi, Do-Chim;Choi, Eun-Yeon;Jo, Byoung-Muk;Cho, Byoung-Uk
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.44 no.6
    • /
    • pp.50-57
    • /
    • 2012
  • In this study, the beeswax extraction methods using organic solvents were examined to develop a optimal dewaxing technology for beeswax-treated Hanji. Thermally-aged beeswax-treated Hanji was dewaxed using four types of extraction methods including dipping, Soxhlet extraction, ultrasonic washing and shaking methods. Then, the aging stability of the dewaxed Hanji was evaluated in terms of variations in paper strength and in the color of the printed area with muk. The experimental results suggested that the dewaxing methods allowing solvent to flow during extraction showed superior extraction efficiency. The dipping method in which the organic solvent does not flow showed the slowest extraction rate of beeswax compared to three other methods. In terms of variations in tensile strength and folding endurance, however, no obvious differences in the aging stability were observed amongst these four extraction methods. Regarding the aging stability in terms of the color of the printed area with muk, Soxhlet extraction method showed the best performance of dewaxing.

A Study on Growth of Aspergillus versicolor and Penicillium polonicum within the beeswax treated paper (밀랍지 내에서의 Aspergillus versicolor와 Penicillium polonicum의 생장 특성 연구)

  • Park, Ji-Hee;Choi, Kyoung-Hwa;Seo, Jin-Ho
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.42 no.2
    • /
    • pp.20-26
    • /
    • 2010
  • Paper composed mainly of organic materials and they can be used as nutrient by microorganisms. Therefore microorganisms are damaging the important documents and works of art irreversibly. Previous research reported that mycelium or spores of the fungi were observed on the wax of the volumes of King Sejong especially were heavily deteriorated by fungi. Fungal strains isolated from the annals of Joseon dynasty were identified as Biscogniauxia atropunctata, Aspergillus versicolor, Penicillium polonicum, Ceriporia lacerata, Irpex lacteus. Especially Aspergillus and Penicillium are able to grow on the substrates having a 7-8% moisture content, which is much lower than the general storage condition (RH55-60%) of the paper cultural properties. Moreover, they are known as fungi cause paper deterioration and discoloration. In this study, we selected Aspergillus versicolor and Penicillium polonicum among five strains, then biological aging has been executed for 30 days. The growth of Aspergillus versicolor and Penicillium polonicum in wax was lower than wax treated paper and Hanji. The growth of them in beeswax treated paper and Hanji both were excellent.

Characteristics of Reinforced Dewaxed Hanji after Aging (강도보강 처리 탈랍지의 특성)

  • Kim, Kang-Jae;Lee, Min-Hyung;Eom, Tae-Jin
    • Proceedings of the Korea Technical Association of the Pulp and Paper Industry Conference
    • /
    • 2011.04a
    • /
    • pp.73-79
    • /
    • 2011
  • The annals of Joseon Dynasty has been known as one of the UNESCO's Memory of the World Heritage. Some of the annals of Joseon Dynasty was composed with wax coated book. Especially the waxed book have been severely damaged by various reason. To find out the safety preservation method of the annals of Joseon Dynasty waxed book, the characteristics of reinforced dewaxed Hanji was evaluated in this paper. From strength properties of MC treated dewaxed Hanji after dewaxing with different method, dewaxing ratio was been high, polymer treated dew axed Hanji showed a better strength. As the aging time, polymer layer on dewaxed Hanji was became brittle and cracked.

  • PDF

Studies on Conservation of the Beeswax-treated Annals of Joseon Dynasty (조선왕조실록 밀랍본 보존을 위한 연구)

  • Jeong, Hye Young;Choi, Kyoung Hwa;Lee, Kye Shik;Jo, Byoung-Muk
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.44 no.6
    • /
    • pp.70-78
    • /
    • 2012
  • The Annals of Joseon Dynasty, which recorded governmental affairs for 472 years (AD 1392-1863) during the Joseon dynasty is an representative paper cultural heritage in Korea. Being recognised their authenticity and values they were designated as the No 151 national treasure of Korea in 1973 and registered as 'The Memories of the World' by UNESCO in 1997. Unusually, some volumes of the Annals were treated by beeswax for the permanent preservation. However, the examinations on the deterioration of the beeswax-treated volumes had been exposed the serious damage than the untreated volumes. In particular, the larger amount of beeswax were worst in deterioration condition. In order to solve these problems, NRICH(National Research Institute of Cultural Heritage) of Korea launched the investigation study for the conservation of beeswax-treated volumes of the Annals. Now then, the five study areas have been set up; 1) to understand the damaged condition of the Annals; 2) to analyse the raw materials and production techniques; 3) to test the degradation degree using the duplication samples for understanding the aging factors and mechanism; 4) to develop the conservation techniques through dewaxing and thereafter strengthening the base paper of Hanji; 5) to develop the long-term storage technique using inert gases. On the basis of outcomes from this study, NRICH will plan to establish the systematic conservation and management plan for the beeswax-treated volumes of the Annals in future.

The Analysis of the Oxidation Index of Korea Traditional Paper(Hanji) Which Is Used as the Rrestoration Paper of the Waxed Volume in the Annals of Joseon Dynasty (조선왕조실록 밀랍본 복원용지로서 전통한지의 oxidation index 분석)

  • Seo, Jin-Ho;Jeong, So-Young;Jeong, Seon-Hwa
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.40 no.1
    • /
    • pp.55-61
    • /
    • 2008
  • The annals of Joseon Dynasty is the most valuable resource containing the record of Korean history and has been known as one of the UNESCO's Memory of the World Register. In some period, wax-treated paper was used in the annals of Joseon Dynasty to prevent the damage from pests. But, wax-treated volumes were discolored to brown, white or black, and partially cracked by the stiffened wax. It means that wax-treated volumes were damaged by the hardening and oxidizing of wax. The wax is considered as the first reason in damages on the wax-treated volume. Therefore, in this study we analysed the oxidation index of Korea traditional paper(Hanji) which is used as the restoration paper of the waxed volume in the annals of Joseon Dynasty by using FT-IR. As the analysis of FT-IR, the traditional two-layed stamping paper (Hanji sample F), which was treated by starch in its surface, was shown the most stable state after the accelerated ageing test.