• Title/Summary/Keyword: Base Metal Zone

Search Result 341, Processing Time 0.021 seconds

Effect of Hot-stamping Heat Treatment on Microstructure and Hardness in TWB Laser Joints of Al-Si-coated Boron Steel and Zn-coated DP Steel (Al-Si 도금된 보론강과 Zn 도금된 DP강의 TWB 레이저 용접부 미세조직과 경도에 미치는 핫 스탬핑 열처리의 영향)

  • Jung, Byung-Hun;Kong, Jong-Pan;Kang, Chung-Yun
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.3
    • /
    • pp.224-232
    • /
    • 2012
  • In this study, the effect of hot-stamping heat treatment on the microstructure and hardness of TWB(Tailor Welded Blank) laser joints in Al-Si-coated boron steel and Zn-coated DP(Dual Phase)590 steel was investigated. In the TWB joints without heat treatment, hardness profiles showed local hardness deviation near the fusion zone. However, there was no hardness deviation in the heat treated specimen and its hardness was higher than that of the one without the heat treatment, due to a fully martensite microstructure. In the TWB joints of both the boron and DP steels, the maximum hardnesses were observed at the HAZ(Heat Affected Zone) near the base metal, and the hardness decreased gradually to the base metal. In the heat treated joints, the hardnesses of the HAZ and the base metal of the boron steel side were similar to the maximum hardness of the weld, while those of the HAZ and the base metal of the DP steel side were higher than the maximum hardness.

Measurement of Mmechanical Properties in Weld Zone of Nuclear Material using an Instrumented Indentation Technique (계장형 압입시험법에 의한 원자력 구조재료 용접 물성치 측정)

  • Song, Kee-Nam;Ro, Dong-Seong
    • Journal of Welding and Joining
    • /
    • v.30 no.3
    • /
    • pp.51-56
    • /
    • 2012
  • Different microstructures in the weld zone of a metal structure including a fusion zone and heat affected zone are formed as compared to the base material. Thus, the mechanical properties in the weld zone are different from those in the base material. As the basic data for reliably understanding the structural characteristics of welded nuclear material, the mechanical properties in the weld zone and base material for a Zircaloy-4 strap and Hastelloy${(R)}$-X alloy strap are measured using an instrumented indentation technique (IIT) in this study.

Effect of Welding Condition and Roller on Weldability of Al Coated Steel Sheet using Plasma Arc Welding (박판 알루미늄 도금강판의 플라즈마 용접성에 미치는 용접조건 및 롤러의 영향)

  • Lee, Tae-Woo;Park, Cheol-Ho;Kang, Nam-Hyun;Kim, Myung-Duk
    • Journal of Welding and Joining
    • /
    • v.30 no.2
    • /
    • pp.54-58
    • /
    • 2012
  • Al-coated steel sheets with excellent heat and corrosion resistance are widely used in various applications. In welding of thin plate, some defects such as unmelted zone and metal-through occur easily in the beginning and ending of welding line. In the study, the welding defects in Al-coated steel sheets were investigated with respect to plasma arc current, height between Cu block and base metals, and using a roller to align the height of the base metal. Full penetration and voids free welds were obtained with a plasma arc current 52A and weld speed 2.3m/min. An unmelted zone increased and Ericshen rate decreased as the height between Cu block and base metal increased from 0 to 0.6mm. Using a roller moving ahead of the plasma arc, the length of unmelted zone decreased from 1.7mm to 0.5mm.

A Characteristic of microstructural evolution, microhardness and tensile properties in CrMoV rotor steel weldment experienced by the cyclic thermal aging heat treatment (CrMoV강 용접부의 주기적 열시효처리에 따른 미세조직, 미세경도 및 인장강도 특성)

  • Kim, G.S.;Koh, J.H.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.12 no.4
    • /
    • pp.303-312
    • /
    • 1999
  • An investigation of the CrMoV rotor steel weldment which experienced by cyclic thermal aging heat treatment and as-received condition was performed. This evaluation was carried out to confirm whether this type of weldment is appropriate for the service environment in terms of microstructural examinations, microhardness measurements and tensile tests. The cyclic thermal aging heat treatment, containing continuous heating and cooling thermal cycle was programmed to simulate the real rotor service condition. The heat treatment was performed for 40 cycles(5920hrs). The results indicated that the weldment was composed of 4 different regions such as heat affected zone of the base metal, butter weld(initial weld), full thickness weld(final weld) and the base metal. The double welding process was applied to eliminate the susceptibility of reheat cracking at heat affected zone of base metal. The grain refinement at the HAZ due to the welding process could reduce the possibility of cracking susceptibility, but its tensile properties was appeared to be low due to the weld metal in as-received condition. The benefit effect, grain refinement was extended with carbides coarsening during the cyclic thermal aging heat treatment. However the poor mechanical properties of the weldment was more degraded as undergoing the heat treatment.

  • PDF

A Study on the Corner Crack Propagation by Plane Bending Fatigue in Butt Welded Joints of Steel (平面굽힘 疲勞荷重 에 의한 鋼熔接部 의 모서리균열 傳파特性)

  • 김영식;조상명
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.6 no.3
    • /
    • pp.232-238
    • /
    • 1982
  • The behavior of corner crack propagation by unidirectional plane bending fatigue was investigated in the butt welded joints of SS41 and SM50 steel plates including an edge through-thickness notch. The properties of fatigue crack propagation were inspected in the weld metal, heat-affected zone, and base metal of the welded joints. Main results obtained are as follows; (1) When a plate with an edge through-thickness notch is loaded by plane bending fatigue in indirection, the 2 variant corner cracks on the upper and lower edge of the plate are initiated and propagated respectively from the notch. (2) In case of a specimen containing a corner crack, it is more reasonable to estimate the crack propagation rate by area of fracture surface than by crack surface length. (3) The rate of fatigue crack propagation becomes faster in the following order; weld metal, heat-affected zone, and base metal. (4) The specimen including reinforcement shape is rapidly failed throughout bond due to effect of its shape when the repeated load exceeds a certain cycle.

Evaluation of Electrochemical and Mechanical Characteristics in MIG Welding Parts of Dissimilar Al Alloys for Ship (선박용 이종 알루미늄 합금 미그 용접부의 기계적 및 전기화학적 특성 평가)

  • Woo, Yong-Bin;Kim, Seong-Jong
    • Journal of the Korean institute of surface engineering
    • /
    • v.42 no.1
    • /
    • pp.34-40
    • /
    • 2009
  • In the study, it was carried out dissimilar metal welding on materials for Al ship. The electrochemical and mechanical characteristics evaluated for specimen welded by ROBOT. The hardness of welding zone is lower than those of heat affected zone and base metal. At the result of tensile test, the specimen welded with ER5183 welding material presented excellent property compared with ER5556. The polarization trend for the base metal and welding metal showed the effects of concentration polarization due to oxygen reduction and activation polarization due to hydrogen generation. At the Tafel experiments result, the corrosion density in welded with ER5183 welding material presented the lowest value.

The Effect of Weld Metal Copper Content on HAZ Cracking in Austenitic Stainless Steel welded with Al-brass

  • Lee, H.W.;Lee, J.S.;Choe, W.H.
    • Proceedings of the KWS Conference
    • /
    • 2005.06a
    • /
    • pp.152-154
    • /
    • 2005
  • Austenitic stainless steel has good weldability but is sensitive to hot cracking such as solidification crack and liquation crack. In this study, the specimens of dissimilar metals made between austenitic stainless steel and Al-brass were welded by GTAW process using four different filler metals. Cracks were detected in the heat-affected zone of the stainless steel when welded with CuAl, CuSn and NiCu filler metals, but no cracks were detected a Ni filler metal was used. The cracks propagated along the grain boundary in the heat affected zone near the fusion line to base metal of 316L stainless steel. The cracks were located inside the weld bead with very fine hairline crack. All cracks initiated at the fusion line and moved forward in the base metal. From energy dispersion spectroscopy (EDS), Cu peak was detected only in the crack-opening area.

  • PDF

A study on the fatigue crack growth characteristics of weldments of A5083-0 Al-alloy by plane bending fatigue (A5083-0 알루미늄 합금재의 용접부위의 평면 굽힘 피로에 의한 피로균열성장 특성에 관한 연구)

  • 김원녕;김기준;임종문
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.10 no.1
    • /
    • pp.65-73
    • /
    • 1986
  • Surface fatigue crack propagation tests by plane bending fatigue were conducted on the welding specimens of an aluminium alloy, A5083-0, having an edge through thickness notch to study the fatigue crack growth characteristics. Moreover, the experiments were performed in order to clarify the fatigue crack initiation and growth. The properties of fatigue crack growth were quantitatively inspected in welded metal, heat-affected zone and base metal of the welding specimens. The main results obtained are summarized as follows: 1. It is found that the hardness distributions of A5083-0 aluminium alloy weldments are quite different with those of steel material weldments, so that the hardness distribution becomes lower in the following order: base metal, heat-affected zone and weld metal. 2. It is observed that the grain size of this specimen weldment appears to be almost equal to the base metal, when TIC welding method is adopted. 3. In a surface fatigue crack initiation and growth, the fatigue crack does not begin by opening-closing mechanism until hardening is saturated at the crack tip. 4. The fatigue crack growth characteristics of A5083-0 alluminium alloy weldments can be concluded.$${\frac{da}{dn}}=C({\Delta}K)^n=3.8{\times}10^{-9}{({\frac}{1}{2}{\Delta}S_t{\sqrt{{\pi}a}})}^{2.4}$$

  • PDF

Creep and creep crack growth behaviors for base, weld, and heat affected zone in a grade 91 weldment

  • Kim, Woo-Gon;Sah, Injin;Kim, Seon-Jin;Lee, Hyeong-Yeon;Kim, Eung-Seon
    • Nuclear Engineering and Technology
    • /
    • v.53 no.2
    • /
    • pp.572-582
    • /
    • 2021
  • This study investigated the creep and creep crack growth (CCG) behavior of the base metal (BM), weld metal (WM), and heat affected zone (HAZ) in a Gr. 91 weldment, which was made by a shield metal arc weld process. A series of tensile, creep, and CCG tests were performed for the BM, WM, and HAZ at 550 ℃. Creep behavior of the BM, WM, and HAZ was analyzed in terms of various creep laws; Norton's power-law, Monkman-Grant relation and damage tolerance factor (λ), and their constants were determined. In addition, each CCGR law for the BM, WM, and HAZ was proposed and compared in terms of a C*-fracture parameter. The WM and HAZ revealed faster creep rate, lower rupture ductility, and faster CCGRs than the BM, but they showed a similar behavior in the creep and CCG. The CCGRs obtained in the present study exhibited a marginal difference when compared with those of RCC-MRx of currently elevated design code in France. A creep crack path in the HAZ plane progressed towards a weak fine-grained HAZ adjacent to the BM.

Electrochemical Evaluation of Corrosion Property of Welded Zone of Seawater Pipe by DC Shielded Metal Arc Welding with Types of Electrodes (선박 해수배관에서 용접봉의 종류에 따라 직류 아크 용접한 용접부위의 부식특성에 관한 전기화학적 평가)

  • Lee, Sung-Yul;Lee, Kyu-Hwan;Won, Chang-Uk;Na, Shane;Yoon, Young-Gon;Lee, Myeong-Hoon;Kim, Yun-Hae;Moon, Kyung-Man;Kim, Jin-Gyeong
    • Journal of Ocean Engineering and Technology
    • /
    • v.27 no.3
    • /
    • pp.79-84
    • /
    • 2013
  • The seawater pipes in the engine rooms of ships are surrounded by severely corrosive environments caused by fast flowing seawater containing chloride ions, high conductivity, etc. Therefore, it has been reported that seawater leakage often occurs at a seawater pipe because of local corrosion. In addition, the leakage area is usually welded using shielded metal arc welding with various electrodes. In this study, when seawater pipes were welded with four types of electrodes(E4311, E4301, E4313, and E4316), the difference between the corrosion resistance values in their welding zones was investigated using an electrochemical method. Although the corrosion potential of a weld metal zone welded with the E4316 electrode showed the lowest value compared to the other electrodes, its corrosion resistance exhibited the best value compared to the other electrodes. In addition, a heat affected zone welded with the E4316 electrode also appeared to have the best corrosion resistance among the electrodes. Furthermore, the corrosion resistance of the weld metal zone and heat affected zone exhibited relatively better properties than that of the base metal zone in all of the cases welded with the four types of electrodes. Furthermore, the hardness values of all the weld metal zones were higher than the base metal zone.