무연계 0.94(Na0.5K0.5NbO3-0.06Ba(Ti0.9Sn0.1)O3 세라믹의 상전이 거동과 압전 특성 (Phase Transitional Behavior and Piezoelectric Properties of 0.94(Na0.5K0.5NbO3-0.06Ba(Ti0.9Sn0.1)O3 Lead-free Ceramics)

  • 차유정;남산;정영훈;이영진;백종후
    • 한국전기전자재료학회논문지
    • /
    • 제22권9호
    • /
    • pp.766-771
    • /
    • 2009
  • Lead-free $0.94(Na_{0.5}K_{0.5})NbO_3$-0.06Ba$(Ti_{0.9}Sn_{0.1})O_3$ [0.94NKN-0.06BTS] ceramics doped with 1 mol% $MnO_2$ were synthesized by a conventional solid state method. The phase transitional behavior and piezoelectric properties of the ceramics sintered at various temperatures were investigated. The 0.94NKN-0.06BTS ceramics sintered at $1050^{\circ}C$, having morphotropic phase boundary of orthorhombic and tetragonal phases, exhibited a microstructure with abnormal grain growth. A diffused phase transition behavior for all the specimens was verified as high degree of diffuseness (${\gamma}$) values from 1.45 to 1.79. A high piezoelectric constant of $d_{33}=256$ pC/N and a satisfactory electromechanical coupling factor of $k_p=42%$ were obtained for the relatively dense 0.94NKN-0.06BTS ceramics sintered at $1050^{\circ}C$.

Crystallization and Electrical Properties of $Ba_2TiSi_2O_8$ Glass-Ceramics from $K_2O-BaO-TiO_2-SiO_2$ System

  • Chae, Su-Jin;Lee, Hoi-Kwan;Kang, Won-Ho
    • 한국반도체및디스플레이장비학회:학술대회논문집
    • /
    • 한국반도체및디스플레이장비학회 2006년도 추계학술대회 발표 논문집
    • /
    • pp.110-114
    • /
    • 2006
  • Dielectric properties of glass-ceramics with fresnoite(Ba2TiSi208) crystals have been investigated in xK20-(33.3-x)BaO-16.7TiO2-50SiO2 ($0{\leq}x{\leq}20mol%$) glasses. The glassy nature was analyzed by differential thermal analyses and glass-ceramics was variable and control table by the processing parameters like time and temperature. Dielectric constant was measured over a temperature from 125K to 425k at frequencies form 100Hz to 1MHz, and laid in the range 16-10. Piezoelectric constant d33 was measured using a YE2703A d33meter and changed from 5.9 to 4.8pCN-1 with x contents. The spontaneous polarization Ps estimated from the hysteresis at ${\pm}1.2kV$ was ${\sim}0.3\;{\mu}C/cm2$ at room temperature.

  • PDF

(Ba,Sr)TiO3계 세라믹스의 PTCR 특성에 미치는 Sb2O3의 영향 (Effects of Sb2O3 on the PTCR Properties of (Ba,Sr)TiO3-based Ceramics)

  • 이호원;김영민;어순철;김일호
    • 한국재료학회지
    • /
    • 제14권2호
    • /
    • pp.115-120
    • /
    • 2004
  • Perovskite barium-strontium titanate, $(Ba, Sr)TiO_3$ was prepared and effects of $Sb_2$O$_3$ additives on its PTCR properties were investigated. $The (Ba,Sr)TiO_3$ with 0.05~0.25 mol% $Sb_2$$O_3$ showed semiconducting PTCR behavior and anomalous grain growth was also observed when it was sintered above $1330^{\circ}C$. It was considered that charge compensation by doping 8b203 as well as abnormal grain growth by sintering lead to resistivity reduction from insulating to semiconducting transition.

Nb+5첨가된 반도성 BaTiO3세라믹스에서 MoO3의 영향과 주파수 특성 (Effect of MoO3 Addition and Their Frequency Characteristics in Nb+5 doped Semiconductive BaTiO3 Ceramics)

  • 윤상옥;정형진;윤기현
    • 한국세라믹학회지
    • /
    • 제24권1호
    • /
    • pp.63-69
    • /
    • 1987
  • Effect of MoO3 additiion on the semiconductive BaTiO3 ceramics doped with 0.2 mole% Nb2O5 and their frequency characteristics have been investigated on the view of intergranular barrier layer model through the observation of changes in their electrical properties. The resistivity increases with the increase of MoO3 addition, but the capacitance, the frequency dependence of capacitance and the effect of positive temperature coefficient of resistivity (PTCR) decrease. It is explained by the possible increase in the thickness of potential barrier due to the formation of insulating layer and thus decrease in the degree of energy band bending. Both the PTCR effect and resistivity decrease with the increase of frequency due to the possible elimination of barrier layer at the grain boundary.

  • PDF

$(Ba,Ca)(TiZr)O_3$ 세라믹을 적용한 적층 칩 커패시터의 전기적 특성 (The Electric Properties of Multilayer Ceramic Capacitors with $(Ba,Ca)(TiZr)O_3$ Ceramics)

  • 윤종락;여동훈;이현용;이석원
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제55권1호
    • /
    • pp.1-5
    • /
    • 2006
  • The effect of A/B moi ratios and sintering temperatures on dielectric properties and microstructure of $(Ba_{0.93}Ca_{0.07})_m(Ti_{0.82}Zr_{0.18})O_3$ ceramics were investigated. The dielectric constant decreased with increasing the A/B mol ratio. However, the dielectric loss is improved. As the dielectric properties of A/B mol ratio with m = 1.009 at sintered temperature $1260^{\circ}C$, we obtained dielectric constant 12,800, dielectric loss $3.5\%$ and Y5V temperature characteristics. Highly reliable Ni-MLCCs, 1.6mm$(length){\time}0.8mm(width){\time}0.8mm$(height) with capacitance of 1.23 ${\mu}F$ and 야ssipation loss of $5.2\%$ were obtained employing dielectric material composed of $(Ba_{0.93}Ca_{0.07})_{1.009}(Ti_{0.82}Zr_{0.18})O_3$ - $MnO_2\;0.2wt\%-Y_2O_3\;0.18wt\%,\;-\;SO_2\;0.15wt\%-(Ba_{0.4}Ca_{0.6})SiO_3\;1wt\%$.

Structure and Microwave Dielectric Characteristics of Ba6-3x(Sm1-yNdy)8+2x(Ti0.95Sn0.05)18O54 Ceramics as a Function Of Sintering Time

  • Li, Yi;Chen, Xiang Ming
    • 한국세라믹학회지
    • /
    • 제40권4호
    • /
    • pp.360-364
    • /
    • 2003
  • Effects of sintering time upon the structures and microwave dielectric characteristics of co-substituted $Ba_{6-3x}$/S $m_{8+}$2x/ $Ti_{18}$ $O_{54}$ ceramics (x=2/3) were investigated. Prolonged sintering had significant effects upon the qf value and temperature coefficient, and a high Qf value (10,600 GHz) was obtained in the present ceramics combined with high-$\varepsilon$ (80) and near-zero temperature coefficient.t..

$BaTiO_3$의 강유전-상유전 상전이에 미치는 A($Cu_{1/3}Nb_{2/3}$)$O_3$ (A=Pb, Ba 및 Sr)의 영향 (Influences of A($Cu_{1/3}Nb_{2/3}$)$O_3$(A=Pb, Ba and Sr) on the Ferroelectric Paraelectric Phase Transition of $BaTiO_3$ Ceramics)

  • 박휴범;김정;김시중
    • 한국세라믹학회지
    • /
    • 제28권12호
    • /
    • pp.969-974
    • /
    • 1991
  • The influences of A(Cu1/3Nb2/3)O3(A=Pb, Ba and Sr) on the ferroelectric-paraelectric phase transition of BaTiO3 ceramics has been investigated. The tetragonality of crystal structure decreased with increasing A(Cu1/3Nb2/3)O3 content at room temperature. A linear correlation between Curie point and the tetragonality of lattice was not observed. In all three systems the variation of Curie point with the mole fraction showed similar tendency that the Curie point decreased at lower mole fraction but gradually increased in the region of higher mole fractions, Diffuse phase transitions were observed at higher mole fractions. The variation of Curie points could be explained by internal stress and Jahn-Teller distortion of BO6 due to Cu2+, and it was thought that the diffuse character of phase transition was caused by compositional fluctuation.

  • PDF

O-3형 BaTiO3-폴리머 복합체의 계면기공율 변화에 따른 유전 및 압전특성 (Effects of Interface Porosity on Dielectric and Piezoelectric Properties of BaTiO3-Polymer Composites of O-3 Type Connectivity)

  • 이형규;김호기
    • 한국세라믹학회지
    • /
    • 제26권5호
    • /
    • pp.617-624
    • /
    • 1989
  • Piezoelectric composites of O-3 connectivity were prepared by thermosetting barium titanate-phenolic resin composite under various cruing pressure. Among three kinds of pore in O-3 type ceramic-polymer composite, such as matrix pores, particle pores, and ceramic-polymer interface pores, the effect of interface porosity on the dielectric and piezoelectric constant was investigated. In pure barium titanate ceramics, the porosity factor of dielectric and piezoelectric constants were 5.7 and 5.0, respectively. However, in BaTiO3-polymer composite, the interface porosity factor of the piezoelectric constant was greater than that of the dielectric constant, interface porosity factor b in d33 was 9.8 and in r 4.6. On the other, piezoelectric voltage constant g33 was independent of the porosity of barium titanate ceramics. But in composite system, the piezoelectric voltage constant g33 was decreased with interface porosity.

  • PDF

BaTiO$_3$ 세라믹의 마이크로파 소성 및 전기적 특성 (Microwave Sintering Behavior and Electrical Properties of BaTiO$_3$ Ceramics)

  • 배강;김호기
    • 한국세라믹학회지
    • /
    • 제35권11호
    • /
    • pp.1203-1211
    • /
    • 1998
  • 적외선 광온도계(IR optical thermometer)와 PID 온도조절기에 의해 소성온도와 시간을 정밀하게 조절할 수 있는 마이크로파 소성장치를 사용하여 BaTiO3 시편을 소성하였다. 또한 마이크로파 소성중에 광섬유 온도계(optical fiber thermoneter)로 시편의 내부온도를 측정하여 같은 조건에서의 일반소성에 의한 시편과 소성특성을 비교한 결과, 소성시간에 따른 빠른 입성장속도과 큰 결정립경을 가졌으며, 온도에 따른 유전성질의 변화는 20~16$0^{\circ}C$의 측정범위에서 같은 경향을 보였다.

  • PDF