The bond performance of glass fibre reinforced polymer (GFRP) bars and that of steel bars embedded in Alkali Activated Cement (AAC) concrete are analysed and compared using pull-out specimens. The bond failure modes, the average bond strength and the free end bond stress-slip curves are used for comparison. Tepfers' concrete ring model is used to further analyse the splitting failure in ribbed steel bar and GFRP bar specimens. The angle the bond forces make with the bar axis was calculated and used for comparing bond behaviour of ribbed steel bar and GFRP bars in AAC concrete. The results showed that bond failure mode plays a significant role in the comparison of the average bond stress of the specimens at failure. In case of pull-out failure mode, specimens with ribbed steel bars showed a higher bond strength while specimens with GFRP bars showed a higher bond stress in case of splitting failure mode. Comparison of the bond stress-slip curves of ribbed steel bars and GFRP bars depicted that the constant bond stress region at the peak is much smaller in case of GFRP bars than ribbed steel bars indicating a basic bond mechanism difference in GFRP and ribbed steel bars.
The lap splice lengths of deformed steel reinforcing bars and GFRP bars were experimentally compared using beam specimens. The purpose was to evaluate the length required of the GFRP bar to develop strength at least equivalent to the conventional steel reinforcing bar. The main test variable was the lap splice length: 10, 20, 30 $d_b$ for the deformed steel bars and 20, 30, 40 $d_b$ for the GFRP bars. Two different types of GFRP bars were tested: (1) one with spiral-type deformation and (2) plain round bars. Elastic modulus was about 1/5 of the steel bars while the tensile strength was about 690 MPa for the GFRP bars. Nominal diameter of the GFRP bars and steel bars was 12.7 and 13 mm, respectively. Normal strength concrete (28-day $f_{cu}$ = 30 MPa) was used. For the conventional steel bars (SD400 grade), strength over 400 MPa in tension was developed using the lap splice length of 20 and 30 $f_{cu}$. Only $87\%$ of the nominal yield strength was reached with the lap splice length of 10 $d_b$. For the spiral-type deformed GFRP bars with $40-d_b$ lap splice length, 440 MPa in tension was determined. The maximum tensile strength developed of the GFRP bars with smaller lap splice lengths decreased. The plain GFRP bar was not effective in developing the tensile strength even with $40-d_b$ lap splice length. Development of the cracks on beam surface was clearly visible for the beams reinforced with the GFRP bars. Mid-span deflections, however, were significantly smaller than the comparable beams with conventional steel bars indicating potential ductility problem.
곡류의 기능성 소재를 바탕으로 칼로리가 낮고 조직감이 우수한 편의식 형태의 아침대용식 제품을 개발하기 위하여 9가지 곡물(옥수수, 통밀, 멥쌀, 흑미, 현미, 수수, 발아현미, 검은콩, 율무)을 이용하여 선식형과 퍼핑형 씨리얼바 2종류를 제조하여 수분함량, 색도, 조직감 등의 품질변화를 측정하였다. 씨리얼바의 제조는 9가지의 곡류 배합${\to}$부재료의 크림화${\to}$반죽${\to}$성형틀에 투입${\to}$굽기${\to}$냉각${\to}$견과류 토핑의 단계로 이루어졌다. 수분함량은 선식형 씨리얼바가 $9.4\%$, 퍼핑형 씨리얼바가 $10.1\%$였으며 색도 측정 결과 L값은 퍼핑형이 선식형보다 높았으며 a값은 프락토올리고당을 첨가한 선식형의 씨리얼바가 가장 강했으며 b값은 시료간에 유의적 차이를 보이지 않았다. 조직감에 있어 경도는 선식형보다 퍼핑형이 더 컸으며 선식형 씨리얼바의 경우에 프럭토올리고당을 첨가한 군이 가장 경도가 높았다. 관능검사 결과 전반적인 바람직성에 있어서 퍼핑형 씨리얼바가 선식형 씨리얼바보다 높은 기호도를 나타내었다.
Generally significant reinforcement is used for nuclear power plant structures and may cause potential problems when concrete is poured. In particular pouring concrete into structural member joint area is more difficult than other areas since the joint area is very congested due to hooked bars, embedded plates, and other reinforcements. The purpose of this study is to solve the problem by applying high-strength(ASTM A615 Gr. 75/80) bars. In addition large-sized(#14 & #18) headed deformed bar could be used as alternative of standard hooked bars to relieve the congestion to some extent. In order to apply headed deformed bars to nuclear power plant structures effectively, the large-sized diameter bars and the high-strength bars shall be used as thick as clear cover thickness 1". Therefore, test results were obtained by taking bar size, yield strength, and clear cover thickness as variables.
Kim, Taehyun;Lee, Myung Gyoon;Sheth, Kartik;Gadotti, Dimitri
천문학회보
/
제39권1호
/
pp.38.2-38.2
/
2014
Radial light profiles of bars are known to be related to the morphology of their host galaxies in a way that bars in early type disk galaxies show flat radial light profile, while bars in late type disk galaxies show exponential profile. To quantify how flat or steep bar profiles are, we have performed detailed two-dimensional decompositions on 3.6 micron images for 144 barred galaxies from the Spitzer Survey of Stellar Structure in Galaxies (S4G), and then modeled bar profiles with Sersic functions. We find that bars in classical bulge, higher bulge-to-total (B/T) galaxies are flatter than bars in bulgeless, lower B/T galaxies. In particular, we find that the presence of a bulge almost always guarantees that the bar is flat. Conversely, bulgeless galaxies, mostly have bars with steep profiles. This implies that the light profile of bars may be a dynamical age indicator of bars. We also find that the shape of bars are boxy and do not change with B/T. This indicates that as galaxies evolve, bars change their light profile while keeping their outermost shape boxy.
The lap splice lengths of deformed steel reinforcing bars and GFRP bars with two different to surface type were experimentally compared using beam specimens. The purpose was to evaluate the length required of the GFRP bar to develop strength equivalent to the conventional steel reinforcing bar. The main test variable was the lap splice length. Two different GFRP bar surfaces were tested: (1) spiral-type GFRP bars and (2) sand coated GFRP bars. For the conventional steel bars (SD400 grade), strength over 400 MPa in tension was reached using the lap splice length of $30d_b$. Splice failure was observed in the specimen with the lap splice length of $20d_b$. For the spiral-type and sand coated GFRP bars, the tensile strength developed in the GFRP bars decreased with decreasing splice lengths. Development of the cracks on beam surfaces was clearly visible for the beams reinforced with the GFRP bars. Mid-span deflections, however, were significantly smaller than the comparable beams with conventional steel bars indicating potential ductility problem.
해안선의 횡방향 표사이동에 대하여 장시간 관측된 자료를 이용하여 연안사주와 관련된 제반 특성들을 해석하였다. 전체적으로, 발생된 내부 연안사주는 시간이 지남에 따라 외해쪽으로 이동하다가 임의의 위치에서 외부 연안사주를 형성하게 된다. 이와 같이 외부 연안사주가 형성된 후, 내부 연안사주는 반대로 시간에 따라 해안선 쪽으로 진행하면서 동시에 많은 양의 표사가 해안선과 외부 연안사주방향으로 이동 소멸되어 외부 연안사주가 다시 내부 연안사주로 변화되는 과정을 거친다. 또한 외부 연안사주의 존재여부에 따라 내부 연안사주의 계절적인 변화특성이 매우 다르게 나타났다.
The aims of this study are to investigate rib geometries of reinforcing bars commercially available in Korea, Japan and USA, and evaluate bond performance using beam-end test specimens. Measurement of rib geometries of the bars include nominal area, average distance of rib, height of rib and an angle of rib perpendicular to bar axis. The result of this study show that rib height of Korean reinforcement bars are much less than those of Japan and USA resulting in the lowest value of relative rib area. Average bond strength of Korean D25 deformed bars is known as 9 % less than that of bars produced in USA. Bond strength depends primarily on the relative rib area. Bond strength of the high relative rib area bars produced in USA show 18% higher than that of bars produced in Korea.
International Journal of Concrete Structures and Materials
/
제2권2호
/
pp.99-105
/
2008
Southern exposure test specimens were used to evaluate corrosion performance of epoxy-coated reinforcing bars in chloride contaminated concrete by electrochemical impedance spectroscopy method. The test specimens with conventional bars, epoxy-coated bars and corrosion inhibitors were subjected 48 weekly cycles of ponding with sodium chloride solution and drying. The polarization resistance obtained from the Nyquist plot was the key parameter to characterize the degree of reinforcement corrosion. The impedance spectra of specimens with epoxy-coated bars are mainly governed by the arc of the interfacial film and the resistance against the charge transfer through the coating is an order of magnitude higher than that of the reference steel bars. Test results show good performance of epoxy-coated bars, although the coatings had holes simulating partial damage, and the effectiveness of corrosion-inhibiting additives. The corrosion rate obtained from the impedance spectroscopy method is equivalent to those determined by the linear polarization method for estimating the rate of corrosion of reinforcing steel in concrete structures.
콩의 흑색뿌리썩음병을 일으키는 Cylindrocladium crotalariae은 감자한천배지와 콩의 조직을 함유한 한천 배지를 서로 다르게 Water potential를 조절하여 이 병원균을 접종한 결과 균사신장과 대형분생포자형성은 -14bars에서 좋았고 $30^{\circ}C$에서는 -100bars $25^{\circ}C$에서는 -80bars $20^{\circ}C$에서는 -64bars에서 균사신장이 중지되었으며 포자형성도 -64bars에서 중지되었다. 자낭각과 미소균핵형성은 소금을 첨가하지 않은 -1.4나 -3.0bars에서 잘 되었고 이 균에 대한 포자발아율은 -1.4bars에서 -20bars의 모든 Water potential에서 똑 같이 좋았고 -20bars에서 Water potential이 낮아지므로 발아율이 떨어지다가 -60bars에서 억제되었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.