0.015% C-1.5% Mn-0~0.5% Mo 강의 어닐링과정에서 미세조직과 집합조직의 변화 (Changes in Microstructure and Texture during Annealing of 0.015% C-1.5% Mn-0~0.5% Mo Steels)

  • 정우창
    • 열처리공학회지
    • /
    • 제24권5호
    • /
    • pp.251-261
    • /
    • 2011
  • The changes in microstructure and texture during annealing were examined in a series of 0.015% C-1.5% Mn cold-rolled sheet steels with 0~0.5% Mo. Orientation distribution function data were calculated from the (110), (200), (211) pole figures determined on the rolled plane of cold-rolled and annealed steel sheets. Regardless of Mo content and annealing conditions, martensite volume fraction was less than 1.0%, not affecting the texture evolution. Textural change at the cooling stage after heating at $820^{\circ}C$ for 67 sec was not observed. Increasing the Mo content and annealing temperature markedly strengthened the intensities of ${\gamma}$-fiber texture, resulting in the increase in $r_m$ value. The desirable texture evolution for deep drawability in the 0.5% Mo steel may be mainly caused by the grain refining effect of Mo carbide in the hot-rolled steel sheet.

Impact Tensile Properties and Intergranular Fracture Behavior with Strain Rate Variations of Al-M g-X (X = Cr,Si) Alloy

  • Chang-Suk Han;Min-Gyu Chun;Sung-Soon Park;Seung-In Lim
    • 한국재료학회지
    • /
    • 제34권7호
    • /
    • pp.330-340
    • /
    • 2024
  • Al-Mg-Si alloys are light weight and have excellent corrosion resistance, and are attracting attention as a liner material for high-pressure hydrogen containers in hydrogen fuel cell vehicles. Because it has excellent plastic hardening properties, it is also applied to car body panel materials, but it is moderate in strength, so research to improve the strength by adding Si-rich or Cu is in progress. So far, the authors have conducted research on the intergranular fracture of alloys with excessive Si addition from the macroscopic mechanical point of view, such as specimen shape. To evaluate their impact tensile properties, the split-Hopkinson bar impact test was performed using thin plate specimens of coarse and fine grain alloys of Al-Mg-X (X = Cr,Si) alloy. The effect of the shape of the specimen on the characteristics was studied through finite element method (FEM) analysis. As a result, it was found that the intergranular fracture of the alloy with excessive Si depended on the specimen width (W)/grain size (d), which can be expressed by the specimen size and grain size. As W/d decreases, the intergranular fracture transforms into a transgranular fracture. As the strain rate increases, the fracture elongation decreases, and the fracture surface of the intergranular fracture becomes more brittle. It was confirmed that intergranular fracture occurred in the high strain rate region even in materials with small grain sizes.

One-step Forming 방법을 이용한 차체 판넬 성형해석에 관한 연구 (A Study of auto-body panel correction of forming analysis that use One-step Forming method)

  • 정동원;황재신
    • 한국정밀공학회지
    • /
    • 제22권2호
    • /
    • pp.89-97
    • /
    • 2005
  • Thin plate correction of forming process that it is nowadays smile change of simple contact surface as it becomes possible that forecast dictionary numerically exactly to analyze comparative big comp displacement real industry spot problems between complicated and abnormal curved line shapes and thin plate and die more reliable and need many efforts yet economical analysis method is required and develops this efficient algorithm. This research analyzes correction of forming and examined possibility and validity of spot application using One-Step Finite Element Method. Its application is being increased especially in the automotive industrial area for the cost reduction, weight saving, and improvement of strength.

광 삼각법 측정 알고리즘을 이용한 자동차 도어 간격 측정 및 보정에 관한 연구 (A study on measurement and compensation of automobile door gap using optical triangulation algorithm)

  • 강동성;이정우;고강호;김태민;박규백;박정래;김지훈;최두선;임동욱
    • Design & Manufacturing
    • /
    • 제14권1호
    • /
    • pp.8-14
    • /
    • 2020
  • In general, auto parts production assembly line is assembled and produced by automatic mounting by an automated robot. In such a production site, quality problems such as misalignment of parts (doors, trunks, roofs, etc.) to be assembled with the vehicle body or collision between assembly robots and components are often caused. In order to solve such a problem, the quality of parts is manually inspected by using mechanical jig devices outside the automated production line. Automotive inspection technology is the most commonly used field of vision, which includes surface inspection such as mounting hole spacing and defect detection, body panel dents and bends. It is used for guiding, providing location information to the robot controller to adjust the robot's path to improve process productivity and manufacturing flexibility. The most difficult weighing and measuring technology is to calibrate the surface analysis and position and characteristics between parts by storing images of the part to be measured that enters the camera's field of view mounted on the side or top of the part. The problem of the machine vision device applied to the automobile production line is that the lighting conditions inside the factory are severely changed due to various weather changes such as morning-evening, rainy days and sunny days through the exterior window of the assembly production plant. In addition, since the material of the vehicle body parts is a steel sheet, the reflection of light is very severe, which causes a problem in that the quality of the captured image is greatly changed even with a small light change. In this study, the distance between the car body and the door part and the door are acquired by the measuring device combining the laser slit light source and the LED pattern light source. The result is transferred to the joint robot for assembling parts at the optimum position between parts, and the assembly is done at the optimal position by changing the angle and step.

자동차 조립공정 작업의 실시간 모니터링을 위한 UWB 기반 공구위치 추적 시스템 개발 (The Development of Tool Position Tracking system Based on UWB for Automotive Assembly Process)

  • 정승현
    • 한국산학기술학회논문지
    • /
    • 제20권8호
    • /
    • pp.657-661
    • /
    • 2019
  • 자동차 산업은 전 세계적으로 매출액이 1조 달러가 넘고 1천만 명 이상을 고용하고 있는 세계최대 제조업으로서, 약 2만 여개의 부품으로 완성되는 복합적 성격의 대표적인 산업이며 자동차 조립공정은 도장된 차체에 약 3천여 종의 내장, 계기판, 시트, 유리, 엔진, 트랜스미션, 차축 등의 유닛(Unit)을 조립하는 노동집약적 공정으로, 타 공정에 비해 자동화 비율이 가장 낮은 특징을 가지고 있다. 또한, 현재의 자동차 조립공정은 작업자의 조립작업에 대한 실시간 모니터링이 이루어지고 있지 못한 실정으로, 작업자의 작업 공구위치 측정시스템의 도입을 통해 공구의 위치를 실시간으로 파악하고 분석하여 일관된 작업 순서를 지시하면서 작업의 누락 및 가감을 체크한다면, 자동차 제조공정에서 발생할 수 있는 불량을 사전에 차단하여 조립공정의 생산성 및 품질향상을 이룰 수 있다. 따라서 본 논문에서는 작업자의 작업공구 위치 측정 시스템의 도입을 통해 일관된 작업 순서를 지시하면서 작업의 누락 및 가감을 체크하고, 제조공정에서 발생할 수 있는 조립불량을 사전에 차단하여 조립공정의 생산성 및 품질향상을 이룰 수 있는 실시간 공구 위치추적 시스템의 구성을 위하여 UWB(Ultra Wide Band) 무선측위를 활용한 공구의 실시간 위치추적시스템을 개발하고 그 효용성을 증명하고자 한다.

저항 점용접에 의한 실러 패치워크 적용 판재 프레스 성형 연구 (A Study for Stamping of Patchwork with Resistance Spot Weld)

  • 이경민;정찬영;송일종
    • 한국산학기술학회논문지
    • /
    • 제19권8호
    • /
    • pp.25-31
    • /
    • 2018
  • 본 연구에서는 카울 모듈의 성형 시 최적 설계 공정을 유한요소해석을 통해 도출하는 방안을 제시하였다. 소재 인장시험 및 성형성 평가와 같은 기계적 물성 평가를 통해 성형 해석의 주름 및 크랙 발생을 사전에 파악하고 이를 개선하기 위한 공정 설계 변경을 통해 최적 설계 방안을 도출하였다. 또한 제진성 향상이 필요한 카울 로워 패널에 패치워크를 적용을 통해 카울 모듈의 강성 증대 및 제진 특성 향상을 고유진동수 측정 시험과 해석을 통해 확인하였다. 해석 결과, 실러 패치워크 기술 적용에 따른 1차 고유진동수가 향상됨을 알 수 있었고, 이는 강성 및 제진특성 증대와 관련있다고 볼 수 있다. 실러 패치워크 적용 시 공정수 감소를 위해 성형 전 로워 패널 블랭크에 패치워크 블랭크를 점용접으로 접합시켜 성형하므로, 성형 후 패치워크 패널의 위치가 점용접 조건에 따라 달라진다. 이를 위해 점용접 위치에 따른 성형 해석을 실시하여 결과를 바탕으로 최적 공정 설계를 도출하였다. 스탬핑 공법을 이용한 타부품의 적용을 위해 성형 해석 기법을 구축하여 다양한 제품 설계에 도움이 될 것으로 판단된다.

자동차 에어백의 제어부품 불량에 의한 고장현상 및 후방 추돌에 관련된 에어백 미전개에 대한 사례 연구 (Study of Examples for Air Bag Non-deployment Including Rear Collision and Failure Phenomenon by Damage of Control Parts in Vehicle Air Bag)

  • 이일권;김영규;문학훈
    • 한국가스학회지
    • /
    • 제16권6호
    • /
    • pp.102-106
    • /
    • 2012
  • 이 논문의 목적은 현장에서 발생되는 자동차 에어백 시스템의 고장사례를 모아 분석하고 연구하는 것이다. 첫 번째 사례에서는 에어백 시스템의 클럭 스프링과 에어 백 모듈 사이 배선 핀의 납땜부가 이탈되어, 배선 접촉불량에 의해 핀이 흔들릴 때마다 에어백의 작동불량 현상이 발생되는 것을 확인하였다. 두 번째 사례에서는 에어백 컴퓨터 내부의 단품 소자의 손상으로 인해 에어백 작동불량 현상이 발생된 것을 확인하였다. 세 번째 사례에서는 조수석 시트 벨트 프리텐셔너(pre-tensioner)의 내부 핀과 저항을 연결해 주는 납땜부 이탈로 인해 에어백 경고등이 점등된 것을 확인하였다. 네 번째 사례에서는 승용자동차가 화물자동차의 후면을 추돌하였을 때 때 범퍼는 상대편 차량보다 낮아 아래로 끼어들게 된다. 이 때 사고의 충격은 차량의 프레임부분에 전달되지 않기 때문에 충격센서가 설치된 프레임부분에 충격이 적게 전달되어 에어백이 작동하지 않은 것을 확인하였다.