• Title/Summary/Keyword: Austenitic Stainless Steels

Search Result 167, Processing Time 0.031 seconds

Comparison of Welding Characteristics of Austenitic 304 Stainless Steel and SM45C Using a Continuous Wave Nd:YAG Laser (오스테나이트계 스테인리스강과 SM45C의 연속파형 Nd:YAG 레이저 용접특성비교)

  • 유영태;오용석;노경보;임기건
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • v.12 no.3
    • /
    • pp.58-67
    • /
    • 2003
  • Welding characteristics of austienite 304 stainless and SM45C using a continuous wave Nd:YAG laser n experimentally investigated Laser beam welding is increasingly being used in welding of structural steels. The laser welding process is one of the most advanced manufacturing technologies owing to its high speed and deep penetration. The thermal cycles associated with laser welding are generally much Inter than those involved in conventional welding processes, leading to a rather small weld zone. Experiments are performed for 304 stainless steel plates changing several process parameter such as laser power, welding speed, shielding gas flow rate, presence of surface pollution, with fixed or variable gap and misalignment between the similar and dissimilar and plates, etc. The Nd:YAG laser welding process is one of the most advanced manufacturing technologies owing to its high speed and penetration. This paper describes the weld ability of SM45C carbon steel for machine structural use by Nd:YAG laser. The follow conclusions can be drawn that laser power and welding speed have a pronounced effect on size and shape of the fusion zone. Increase in welding speed resulted in an increase in weld depth/aspect ratio and hence a decrease in the fusion zone size. The penetration depth increased with the increase in laser power.

Effect of Thermal Cycle and Stress on the Intergranular Corrosion in 316 Stainless Steel (316 스테인리스강의 입계부식에 미치는 열사이클과 응력의 영향)

  • Jung, Byong-Ho;Kim, Moo-Gil
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.30 no.6
    • /
    • pp.709-715
    • /
    • 2006
  • The effects of thermal cycle condition and applied stress on the intergranular corrosion in austenitic 316 type stainless steels were investigated. Specimens were solution-treated at 1100$^{\circ}C$ for one hour and then sensitized in the temperature range of $500{\sim}800^{\circ}C$ by holding $2{\sim}300s$ with a various applied stresses of $0{\sim}8kg/mm^2$. Degree of sensitization. DOS %, was measured through polarization curve by electrochemical DL-EPR test. Microstructural observations were also conducted DOS % increased with an increase of sensitization temperature and/or holding time. Increase of applied stress resulted in increase of DOS % and more corroded surface because of acceleration of intergranular corrosion and fine grain size due to the stress. Cr depleted zone near grain boundary was observed. The amount of depletion was profounded with an increase of sensitization temperature, holding time and applied stress. $M_{23}C_6$ carbides were precipitated discontinuously at grain boundary. However, its amount was relatively small in the thermal cycle condition of 800$^{\circ}C$, 300sec and 4kg/mm$^2$.

Electrochemical Characteristics of Superaustenitic Stainless Steel with Temperature in Sea Water (슈퍼오스테나이트 스테인리스강의 해수환경에서 온도에 따른 전기화학적 특성)

  • Hwang, Hyun-Kyu;Kim, Seong-Jong
    • Corrosion Science and Technology
    • /
    • v.20 no.6
    • /
    • pp.391-402
    • /
    • 2021
  • In this investigation, the electrochemical characteristics of superaustenitic and general austenitic stainless steels were compared by conducting potentiodynamic polarization experiment with varying temperatures in natural seawater solution. From the result of the potentiodynamic polarization experiment, the corrosion rate of UNS S31603 was found to be 17 times faster than that of UNS N08367 under the most severe corrosion conditions. The relationship between the corrosion rate by maximum damage depth and the corrosion rate by the corrosion current density was expressed as α value for each stainless steel. The α value of UNS S31603 under all temperature conditions was higher than that of UNS N08367 under similar conditions. This means that UNS S31603 is more prone to localized corrosion than UNS N08367. UNS S31603 expressed pitting type damages under all temperature conditions as shown by SEM analysis results. The pitting damage rapidly grew at the relatively poor grain boundaries. Damage on UNS N08367 was not clearly represented at 30 ℃ and 60 ℃, and slight intergranular corrosion damage was observed on the entire surface at 90 ℃.

Low Temperature Plasma Nitriding Process of AISI 304L Austenitic Stainless Steels for Improving Surface Hardness and Corrosion Resistance (내식성 및 표면경도 향상을 위한 AISI 304L 스테인리스강의 저온 플라즈마질화 프로세스)

  • Lee, In-Sup
    • Korean Journal of Metals and Materials
    • /
    • v.47 no.10
    • /
    • pp.629-634
    • /
    • 2009
  • The effects of processing parameters on the surface properties of the hardened layers processed by the low temperature plasma nitrocarburizing and the low temperature two-step plama treatment (carburizing+nitriding) were investigated. The nitrogen-enriched expanded austenite structure (${\gamma}_N$) or S phase was formed on all of the treated surface. The surface hardness reached up to 1200 $HV_{0.025}$, which is about 5 times higher than that of untreated sample (250 $HV_{0.1}$). The thickness of hardened layer of the low temperature plasma nitrocarburized layer treated at $400^{\circ}C$ for 40 hour was only $15{\mu}m$, while the layer thicknesss in the two-step plama treatment for the 30 hour treatment increased up to about $30{\mu}m$. The surface thickness and hardness increased with increasing treatment temperature and time. In addition, the corrosion resistance was enhanced than untreated samples due to a high concentration of N on the surface. However, higher treatment temperature and longer treatment time resulted in the formation of $Cr_2N$ precipitates, which causes the degradation of corrosion resistance.

Effects on Machining on Surface Residual Stress of SA 508 and Austenitic Stainless Steel (SA508 탄소강 및 오스테나이트 스테인리스강의 표면잔류응력에 미치는 기계가공효과)

  • Lee, Kyoung-Soo;Lee, Seong-Ho;Park, Chi-Yong;Yang, Jun-Seok;Lee, Jeong-Geun;Park, Jai-Hak
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.35 no.5
    • /
    • pp.543-547
    • /
    • 2011
  • Primary water stress corrosion cracking has occurred in dissimilar weld areas in nuclear power plants. Residual stress is a driving force in the crack. Residual stress may be generated by weld or surface machining. Residual stress due to surface machining depends on the machining method, e.g., milling, grinding, or EDM. The stress is usually distributed on or near the surface of the material. We present the measured residual stress for machining on SA 508 and austenitic stainless steels such as TP304 and F316. The residual stress can be tensile or compressive depending on the machining method. The depth and the magnitude of the residual stress depend on the material and the machining method.

Effect of Cobalt Contents on the Biocompatibility and Corrosion Properties of Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N Alloy (Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N계 초내식성 스테인리스강의 생체적합성 및 부식특성에 미치는 Co함량의 영향)

  • Jang, Soon Geun;Yoo, Young Ran;Nam, Hee Soo;Shim, Gyu Tae;Kim, Jung Gu;Kim, Young Sik
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.4
    • /
    • pp.209-216
    • /
    • 2008
  • Super austenitic stainless steels shows the high PRE (Pitting Resistance Equivalent) number and the good corrosion resistance. This work controlled the Co contents in Fe-31Cr-1.7Mo-27Ni-0.25N alloys to elucidate the effect of cobalt contents on the biocompatibility and corrosion resistance. Increasing Co contents, the hardness of the annealed alloys tends to be reduced. In aged alloys, cobalt decreased the increments of hardness by aging treatment. Cobalt decreased the critical pitting temperature (CPT) in 6% $FeCl_3$ + 1% HCl solution, but improved the anodic polarization behavior in Hanks' balanced salt solution and artificial saliva solution. Repassivation rate in artificial body solutions was improved by increasing cobalt contents, but didn't show the linear relationship to PRE number of the alloys. The experimental alloys showed the non-cytotoxicity because of its high corrosion resistance.

Analysis of CTOD Tests on Steels for Liquefied Hydrogen Storage Systems Using Hydrogen Charging Apparatus (수소 장입 장치를 활용한 액체수소 저장시스템 강재의 CTOD 시험 분석)

  • Ki-Young Sung;Jeong-Hyeon Kim;Jung-Hee Lee;Jung-Won Lee
    • Journal of the Korean Society of Industry Convergence
    • /
    • v.26 no.5
    • /
    • pp.875-884
    • /
    • 2023
  • Hydrogen infiltration into metals has been reported to induce alterations in their mechanical properties under load. In this study, we conducted CTOD (Crack Tip Opening Displacement) tests on steel specimens designed for use in liquid hydrogen storage systems. Electrochemical hydrogen charging was performed using both FCC series austenitic stainless steel and BCC series structural steel specimens, while CTOD testing was carried out using a 500kN-class material testing machine. Results indicate a notable divergence in behavior: SS400 test samples exhibited a higher susceptibility to failure compared to austenitic stainless steel counterparts, whereas SUS 316L test samples displayed minimal changes in displacement and maximum load due to hydrogen charging. However, SEM (Scanning Electron Microscopy) analysis results presented challenges in clearly explaining the mechanical degradation phenomenon in the tested materials. This study's resultant database holds significant promise for enhancing the safety design of liquid hydrogen storage systems, providing invaluable insights into the performance of various steel alloys under the influence of hydrogen embrittlement.

Creep Behavior of High Temperature Prestrain in Austenitic 25Cr-20Ni Stainless Steels (오스테나이트계 25Cr-20Ni 스테인리스강의 고온예변형에 의한 크리프 거동)

  • Park, In-Duck;Nam, Ki-Woo;Ahn, Seok-Hwan
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.35-40
    • /
    • 2002
  • In the present study, we examined the influence of prestrain on creep strength of Class M alloy(STS310S) and Class A(STS310J1TB) alloys containing precipitates. Prestrain was given by prior creep at a higher stress than the following creep stresses. Creep behaviour before and after stress change and creep rate of pre-strianed specimens were compared with that of virgin specimens. Pre-straining produced the strain region where the strain rate was lower than that of a virgin specimen both for STS310J1TB and STS310S steels. The reason for this phenomenon was ascribable to the viscous motion of dislocations, the interaction between dislocations and precipitates in a STS310J1TB steel, and the interaction of dislocations with sub-boundaries in a STS310S steel which has the higher dislocation density and smaller subgrain size resulted from pre-straining at higher stress.

  • PDF

Deformation behavior of the Fe-18Cr-14Mn-4Ni-0.9N high nitrogen steel under different strain rate conditions (Fe-18Cr-14Mn-4Ni-0.9N 고질소 내식강의 고온 석출과 변형률 속도에 따른 변형특성 연구)

  • Nam, S.M.;Kim, Y.S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2006.05a
    • /
    • pp.421-424
    • /
    • 2006
  • High nitrogen steels (HNS) exhibit both high strength and ductility during tensile deformation. In the present study the Fe-18Cr-14Mn-4Ni-0.9N high nitrogen steel was heat treated at $1000^{\circ}C$ and $1100^{\circ}C$ to produce $Cr_2N$ precipitates in austenite matrix and full austenite microstructures, respectively. Tensile tests of the heat treated specimens were performed at two different strain rates of 0.05/sec and 0.00005/sec. Each tensile curve of the specimens could be well characterized by the the modified Ludwik equation. Plastic deformation of the steel was adequately represented by the four parameters of the modified Ludwik equation. At 0.05/s strain rate, the specimen with the $Cr_2N$ precipitate exhibited higher strength than the full austenite specimen, while the full austenite specimen showed better mechanical properties at 0.00005/s strain rate. It was found that the $Cr_2N$ precipitates influences deformation behavior of the high nitrogen steel significantly.

  • PDF

Effect of Room Temperature Prestrain on Creep Life of Austenitic 25Cr-20Ni Stainless Steels (오스테나이트계 25Cr-20Ni 스테인리스강의 실온예변형이 크리프 수명에 미치는 영향)

  • Park, In-Duck;Ahn, Seok-Hwan;Nam, Ki-Woo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.28 no.4
    • /
    • pp.453-459
    • /
    • 2004
  • 25Cr-20Ni series strainless steels have an excellent high temperature strength high oxidation and high corrosion resistance. However, further improvement can be expected of creep strength by work hardening prior creep. In the present study, the effect of prestraining at room temperature on the creep behavior of a Class M(STS310S) and a Class A(STS310J1TB) alloy containing precipitates have been examined. Prestaining was carried out at room temperature and range of prestrain was 0.5-2.5 % at STS310J1TB and 2.0-7.0% at STS310S. Creep behavior and creep rate of pre-strained specimens were compared with that of virgin specimens. Room temperature prestraining produced the creep life that is longer than that of a virgin specimen both for STS310J1TB and STS310S when creep test was carried out at the temperature lower than recrystallization temperature. The reason for this improvement of creep life was ascribable to the interaction between dislocations and precipitates in addition to the dislocation-dislocation interaction in STS310J1TB and the dislocation-dislocation interaction in STS310S. The beneficial effect of prestraining in STS310J1TB was larger than that of STS310S.