• Title/Summary/Keyword: Aluminium Alloy 6061

Search Result 25, Processing Time 0.022 seconds

A6061-T6과 A5052-H32재의 이종 마찰교반용접시 핀 형상이 기계적 강도에 미치는 영향에 관한 연구 (A Study on the Effect that Pin Shape on Mechanical Strength in Dissimilar Friction Stir Welding A6061-T6 and A5052-H32)

  • 박희상;최원두;고준빈;이영호;신기석;김인철;최만용
    • 한국생산제조학회지
    • /
    • 제18권3호
    • /
    • pp.270-278
    • /
    • 2009
  • Friction stir welding is a relatively new solid state joining process. A6061-T6 and A5052-H32 aluminium alloy has gathered wide acceptance in the fabrication of light weight structures requiring a high strength to weight ratio and good corrosion resistance. This friction stir process uses a non-consumable tool to generate frictional heat in the abutting surfaces. The welding parameters such as tool rotational speed, welding speed, etc., and tool pin profile play a major role in deciding FSP zone formation in A6061-T6 and A5052-H32 aluminium alloy. Three different tool pin profiles have been used to fabricate the dissimilar butt joints. The formation of friction stir processed zone has been analysed macroscopically. Tensile properties of the joints have been evaluated and correlated with the friction stir processed zone formation.

  • PDF

P/M법과 유도가열 공정변수가 6061 알루미늄 합금의 미세기공과 기계적 성질에 미치는 영향 (Effect of Process Parameters of P/M and Induction Heating on the Cell Morphology and Mechanical Properties of 6061 Aluminum Alloy)

  • 강충길;윤성원
    • 한국정밀공학회지
    • /
    • 제20권6호
    • /
    • pp.222-229
    • /
    • 2003
  • The purpose of this study is to evaluate the mechanical properties of 6061 Al foams, which were fabricated by P/M and multi-step induction heating method, and to build the database, which is needed for computer aided modeling or foam components design. Aluminium foams, consisting of solid aluminium and large quantities of porosities, is widely used in automotive, aerospace, naval as well as functional applications because of its high stiffness at very low density, high impact energy absorption, heat and fire resistance, and greater thermal stability than any organic material. In this study, 6061 Al foams were fabricated for variation of fraction of porosities (%) according to porosities (%)-final heating temperature ( $T_{a3}$) curves. Mechanical properties such as compressive strength, energy absorption capacity, and efficiency were investigated to evaluate the feasibility of foams as crash energy absorbing components. Moreover, effect of the surface skin thickness on plateau stress and strain sensitivity of the 6061 Al foams with low porosities (%) were studied.d.

알루미늄 합금 6061에서 와이어 진동부가에 의한 와이어 컷 방전가공에 따른 표면 거칠기 특성 (I) (Characteristics of Surface Roughness Based on Wire Vibration and Wire-cut Electric Discharge Machining of Aluminum Alloy 6061 (I))

  • 류청원;최성대
    • 한국기계가공학회지
    • /
    • 제14권2호
    • /
    • pp.59-66
    • /
    • 2015
  • The production of high value-added products requires efficient processing and this constant demand for complex shape processing has led to the need for hybrid processing. In this study, the surface characteristics of hybrid machining, which combines wire-cut E.D.M and vibration, are examined. The selected experimental parameters are verticality, waveform, amplitude, peak current and frequency. The experimental results provide a guideline for selecting reasonable machining parameters. Surface roughness was improved by increasing the amplitude of the vibration.

Mechanical and Electrical Properties of Aluminium Alloy by Cryorolling Process

  • Wangkasem, P.;Rojananan, S.
    • International Journal of Advanced Culture Technology
    • /
    • 제3권1호
    • /
    • pp.46-51
    • /
    • 2015
  • The mechanical and electrical properties of aluminium alloy 6061 are reported in this present work. Aluminium alloys were homogenized at $550^{\circ}C$, for 5 hours and cooled in the furnace. The different thickness reductions of 60-90% on homogenized aluminium alloy plates were achieved by cryo-rolling. Later, the as rolled samples were aged by solution treatment at the temperatures of $520^{\circ}C$ for 1 hour, water quenched; subsequently aged at $160^{\circ}C$ for 8-24 hours and partial aged (not solution treatment) at $160^{\circ}C$ for 8- 24 hours. Mechanical and electrical properties of samples were investigated. The experimental result showed that the microhardness of cryo-rolled samples were increase with increasing the percentage of the thickness reduction. Moreover, the microhardness of cryo-rolled, aged by solution treatment samples were higher than those of the cryo-rolled and cryo-rolled, partial aged samples. The cryo-rolled alloys subjected to full aged at $160^{\circ}C$ for 24 hours exhibited the hardness of 125 HV and electrical conductivity values was 45.76 %IACS and the cryo-rolled alloys subjected to partial aged at $160^{\circ}C$ for 20 hours exhibited the hardness of 67 HV and electrical conductivity values was 49.67 %IACS.

SiC 휘스커 보강 Al 6061 복합재료의 피로균열진전 특성에 관한 기초 연구 (The Basic Study on Fatigue Crack Growth Behavior of SiC Whisker Reinforced Aluminium 6061 Composite Material)

  • 권재도;안정주;김상태
    • 대한기계학회논문집
    • /
    • 제18권9호
    • /
    • pp.2374-2385
    • /
    • 1994
  • SiCw/Al composite material is especially attractive because of their superior specific strength, specific stiffness, corrosion fatigue resistance, creep resistance, and wear resistance compared with the corresponding wrought Al alloy. In this study, Fatigue crack growth behavior and fatigue crack path morphology(FCPM) of SiC whisker reinforced Al 6061 alloy with 25% SiC volume fraction and Al 6061 allay were performed. Result of the fatigue crack growth test sgiwed that fatigue crack growth rate of SiCw/Al 6061 composite was slower than that of Al 6061 matrix therefore it was confirmed that Sic whisker have a excellent fatigue resistance. And Al 6061 matrix had only FCPM perpendicular to loading direction. On the other hand SiCw/Al 6061 composite had three types in fatigue crack path morphology. First type is that both sides FCPM of artificial notch are perpendicular to loading direction. Second type is that a FCPM in artifical notch has slant angle to loading direction and the other side FCPM is perpendicular to loading direction. Third type is that both sides FCPM of notch have slant angle to loading direction. It was considered that this kinds of phenomena were due to non-uniform distribution of SiC whisker and confirmed by SEM observation for fracture mechanism study.

알루미늄 합금 접합부의 부식 특성 연구 (A study on the corrosion characteristics of GMA and FS welded Aluminium alloy)

  • 윤병현;노중석;김홍주;장웅성
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.293-295
    • /
    • 2004
  • For the evaluation of corrosion resistance, Al 6061-T6 alloy was welded by Friction Sti. Welding(FSW) and Gas Metal Arc Welding(GMAW) evaluated by Tafel method and immersion test. The Tafel and immersion test results indicated that GMA weld was severely attacked compared with those of friction stir weld. It may be mainly due to the galvanic corrosion mechanism act on the CMA weld.

  • PDF

SHPB를 이용한 구조용 AL합금재의 동적거동 특성 시험에 관한 연구 (Dynamic Behavior Characteristic Test of Structural Aluminium Alloy Materials using SHPB)

  • 허신;김동성;구정서;강흥식;홍성인;정동택
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2001년도 춘계학술대회논문집A
    • /
    • pp.419-423
    • /
    • 2001
  • It is important to know the mechanical properties of the materials under dynamic load. The mechanical properties of most materials are influenced to some extent by strain rate. One of the reliable test device for determining the mechanical properties of materials at high strain rate is Split Hopkinson Pressure bar. In this paper, we conducted the mechanical properties test for the aluminium alloy 6063 and 6061 using the SHPB device.

  • PDF

알루미늄합금 6061-T6의 마찰교반용접 조건에 따른 기계적특성 및 용접부 조직평가 (Mechanical Characteristics and Microstructure on Friction Stir Welded Joints with 6061-T6 Aluminium Alloy)

  • 장석기;박종식
    • 대한기계학회논문집A
    • /
    • 제33권7호
    • /
    • pp.693-699
    • /
    • 2009
  • This paper shows mechanical properties and behaviors of macro- and micro-structures on friction stir welded specimen with 6061-T6 aluminum alloy plate. It apparently results in defect-free weld zone jointed at welding conditions like the traverse speed of 267mm/min, tool rotation speed of 2500rpm, pin inserted depth of 4.5mm and tilting angle of $2^{\circ}$ with tool dimensions such as tool pin diameter of 5mm, shoulder diameter of 15mm and pin length of 4.5mm. The tensile stress ${\sigma}_T=228MPa$ and the yield point ${\sigma}Y=141MPa$ are obtained at the condition of traverse speed of 267mm/min and tool rotation speed of 2500rpm. With the constant rotation speed, the higher traverse speed become, the higher tensile stress and yielding point become. Vickers hardness for welding zone profile were also presented.

3차원 적층 제조 공정(DED) 기반 Al-6061+Al-12Si 합금 조합 실험 (Combinatorial Experiment for Al-6061 and Al-12Si alloy Based on Directed Energy Deposition (DED) Process)

  • 전서연;박수원;송용욱;박지원;박현영;이보람;최현주
    • 한국분말재료학회지
    • /
    • 제30권6호
    • /
    • pp.463-469
    • /
    • 2023
  • Aluminum alloys, known for their high strength-to-weight ratios and impressive electrical and thermal conductivities, are extensively used in numerous engineering sectors, such as aerospace, automotive, and construction. Recently, significant efforts have been made to develop novel aluminum alloys specifically tailored for additive manufacturing. These new alloys aim to provide an optimal balance between mechanical properties and thermal/electrical conductivities. In this study, nine combinatorial samples with various alloy compositions were fabricated using direct energy deposition (DED) additive manufacturing by adjusting the feeding speeds of Al6061 alloy and Al-12Si alloy powders. The effects of the alloying elements on the microstructure, electrical conductivity, and hardness were investigated. Generally, as the Si and Cu contents decreased, electrical conductivity increased and hardness decreased, exhibiting trade-off characteristics. However, electrical conductivity and hardness showed an optimal combination when the Si content was adjusted to below 4.5 wt%, which can sufficiently suppress the grain boundary segregation of the α-Si precipitates, and the Cu content was controlled to induce the formation of Al2Cu precipitates.

레이저 여기 표면파의 음향비선형성을 이용한 Al6061 합금의 소성변형 평가 (Assessment of Plastic Deformation in Al6061 Alloy using Acoustic Nonlinearity of Laser-Generated Surface Wave)

  • 김정석;남태형;최성호;장경영
    • 비파괴검사학회지
    • /
    • 제32권1호
    • /
    • pp.20-26
    • /
    • 2012
  • 본 연구의 목적은 비접촉식 레이저 여기 표면파의 비선형성 계측을 통하여 소성 변형된 알루미늄 합금의 소성변형을 평가하고자 하는 데 있다. 슬릿마스크와 고출력 펄스 레이저를 통한 선배열 레이저빔을 이용하여 협대역의 표면파를 발생 시켰으며, 표면파의 음향 비선형 특성을 이용하기 위하여 슬릿 마스크의 열림 폭과 간격을 변화시킴으로써 레이저 여기 표면파의 주파수 특성을 제어하였다. 스트로크 제어를 통한 인장시험을 통하여 단계별 인장 소성변형 정도를 달리하는 시험편을 제작하였다. 실험결과 인장 소성 변형율이 커짐에 따라 음향 비선형 파라미터는 증가하였으며, 경도 및 EBSD 측정결과 손상의 정도와 매우 밀접한 관계를 보였다. 결과적으로 본 연구에서의 레이저 여기 표면파의 비선형 평가기법은 알루미늄 합금의 소성변형 평가에 매우 유용할 것으로 판단된다.