• 제목/요약/키워드: Alumina coated zirconia powder

검색결과 3건 처리시간 0.017초

가수분해법에 의한 알루미나 코팅 지르코니아 분말의 제조 (Preparation of Alumina Coated Zirconia Powder by Hydrolysis of Aluminum Butoxide)

  • 이종국;김윤수;김환
    • 한국세라믹학회지
    • /
    • 제32권12호
    • /
    • pp.1401-1407
    • /
    • 1995
  • Zirconia powder coated with alumina was prepared by hydrolysis of alumina butoxide. The coated powder was obtained by a hydrolysis reaction between the adsorbed water on the surface of zirconia particles and aluminum sec-butoxide. Amorphous aluminum hydroxide was uniformly coated on the surface of zirconia particles with the thickness of about 30 nm. The shape and distribution of aluminum hydroxide was varied with an existence of surfactant. The coated layer of aluminum hydroxide consists of the fine particle size, and the zirconia powder coated by alumina hydroxide have the large specific surface area of 120 $m^2$/g, compared with that of starting zirconia powder.

  • PDF

지르코니아 인성강화 알루미나 분체의 제조 및 소결 (Preparation and Sintering of Zirconia-Toughnened Alumina Powder)

  • 이전;최상욱;한기성;김승태
    • 한국세라믹학회지
    • /
    • 제29권3호
    • /
    • pp.167-176
    • /
    • 1992
  • Zirconia-toughnened alumina(ZTA) powders that were uniformly coated with zirconia and yttria on the surface of alumina particles were prepared in order to inhibit the grain growth of alumina. Alumina particles were ultrasonically dispersed in the ethanol solution of Zr-n-propoxide, and then the Zr-alkoxide was hydrolyzed. Hydrated zironia as thin film was stabilized to tetragonal crystalline form by doping yttria as a stabilizer. The prepared ZTA powders had the good sinterability even at the lower temperature. As a result, the sintered bodies showed the enhanced fracture toughness compared with pure alumina. The relative density and fracture toughness(KIC) of the ZTA bodies sintered at 1550$^{\circ}C$ were 98% and 5 MPa$.$m1/2 respectively.

  • PDF

생체 유리와 소다 유리침투에 따른 알루미나 세라믹의 굴곡 강도 및 PBS에서의 표면 생성물 연구 (Bending strength of alumina coated with bioglass and soda lime glass and the precipitation on the surface of coated alumina in PBS)

  • 유재양
    • 대한치과기공학회지
    • /
    • 제30권2호
    • /
    • pp.39-45
    • /
    • 2008
  • Titanium and its alloys are widely used as dental implants materials because of their excellent mechanical properties. However, the alumina and zirconia ceramics are preferred to use as the substitute of Ti implants because there is a problems in esthetics and biocompatibility in Ti implant. The the glass infiltrated alumina ceramics are studied to increase the toughness and biocompatibility. The 45S5 and soda-lime glass powder was mixed with ethanol at ratio of 1:1 and brushed on the surface of alumina. Then it was heat treated in the electric furnace at $1400^{\circ}C$ from 30 min. to 5 hours. The glass powder was controlled from 200 to $350{\mu}m$ using ball milling. After heat treatment, the glass infiltrated specimen was tested in universal testing machine to measure the bending strength. The surface microstructure of each specimen was observed with SEM. The biocompatibility of 45S5 and soda-lime glass coated alumina was investigated using PBS at $36.5^{\circ}C$ incubator. The specimen was immersed in PBS for 3, 5, 7, 10 days. After that, the surface morphology was investigated with SEM. As the results of experiment, the 45S5 bioglass infiltrated alumina show the increase of bending strength according to the increasing of heat treatment time from 30 min. to 5 hours at $1400^{\circ}C$ Finally the 1370N bending strength of alumina increased to 1958N at 5 hours heat treatment, which shows 1.4 times higher. In contrast to this, the soda lime glass infiltrated alumina ceramics shows the convex curve according to heat treatment time. Thus it shows maximum bending strength of 1820N at 1 hour heat treatment of $1400^{\circ}C$ It gives 1.3 times higher. However, the bending strength of soda lime glass infiltrated alumina is decreasing with increasing heat treatment time after 1 hour. The precipitation on the surface of 45S5 glass infiltrated alumina was revealed as a sodium phosphate ($Na_{6}P_{6}O_{24}6H_{2}O$) and the amount of precipitation is increasing with increasing of immersion time in PBS. In contrast to this, there is no precipitation are observed on the surface of soda lime glass infiltrated alumina. This implies that 45S5 glass infiltrated alumina brings more biocompatible when it is implanted in human body.

  • PDF