• 제목/요약/키워드: All-bond 2

검색결과 795건 처리시간 0.032초

탄산가스 레이저 조사가 법랑질 표면구조와 치면열구 전색재의 결합강도에 미치는 효과 (THE EFFECT OF $CO_2$ LASER IRRADIATION ON ENAMEL SURFACE AND THE BOND STRENGTH OF SEALANT MATERIAL)

  • 윤동식;김용기;김종수
    • 대한소아치과학회지
    • /
    • 제25권4호
    • /
    • pp.761-771
    • /
    • 1998
  • In this study, attempt has been made to evaluate the effect of $CO_2$ laser irradiation on enamel surface structure and the bond strength of sealant material. Conventional acid etching was used as a control technic for comparison. The results obtained from this experiment were as follows; 1. The highest mean shear bond strength value was observed in samples of Group I (acid-etching) with the statistical significance(p<.05) between all the other groups. 2. The shear bond strength in Group IV was the lowest among laser etching groups. but there were no significant difference between them(p>.05). 3. Scanning electron microscopic observation showed that the rough and irregular surface was created by $CO_2$ laser treatment with the formation of numerous pores, micro-cracks, and small bubble-like inclusion. Increasing the energy density induced localized surface melt with a thin smooth glaze-like appearance. 4. In acid-etched control specimen cohesive failure predominated, whereas adhesive failure was the main mode in laser-treated group. Based upon the above-mentioned results, it can be assumed that the $CO_2$ laser is not an adequate substitute for the acid-etch technique in enamel preconditioning. More studies are required to explore the effective condition of laser irradiation which could attain the better bond strength of restorative materials.

  • PDF

The effect of a desensitizer and $CO_2$ laser irradiation on bond performance between eroded dentin and resin composite

  • Ding, Meng;Shin, Sang-Wan;Kim, Min-Soo;Ryu, Jae-Jun;Lee, Jeong-Yol
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권3호
    • /
    • pp.165-170
    • /
    • 2014
  • PURPOSE. This study was aimed to evaluate effect of the desensitizing pretreatments on the micro-tensile bond strengths (${\mu}TBS$) to eroded dentin and sound dentin. MATERIALS AND METHODS. Forty-two extracted molars were prepared to form a flat dentin surface, and then they were divided into two groups. Group I was stored in distilled water while group II was subjected to a pH cycling. Each group was then subdivided into three subgroups according to desensitizing pretreatment used: a) pretreatment with desensitizer (Gluma); b) pretreatment with $CO_2$ Laser (Ultra Dream Pluse); c) without any pretreatment. All prepared surfaces were bonded with Single Bond 2 and built up with resin composite (Filtek Z250). The micro-tensile bond test was performed. Fracture modes were evaluated by stereomicroscopy. Pretreated surfaces and bonded interfaces were characterized by scanning electron microscope (SEM). The data obtained was analyzed by two-way ANOVA (${\alpha}$=0.05). RESULTS. For both sound and eroded dentin, samples treated with desensitizer showed the greatest ${\mu}TBS$, followed by samples without any treatment. And samples treated with $CO_2$ laser showed the lowest ${\mu}TBS$. SEM study indicated that teeth with eroded dentin appeared prone to debonding, as demonstrated by existence of large gaps between adhesive layers and dentin. CONCLUSION. Pretreatment with Gluma increased the ${\mu}TBS$ of Single Bond 2 for eroded and sound teeth. $CO_2$ laser irradiation weakened bond performance for sound teeth but had no effect on eroded teeth.

도재의 부식정도에 따른 접합강도에 관한 실험적 연구 (AN EXPERIMENTAL STUDY ON BOND STRENGTH OF ETCHED PORCELAIN)

  • 조경;이호용
    • 대한치과보철학회지
    • /
    • 제24권1호
    • /
    • pp.177-189
    • /
    • 1986
  • To investigate the bond strength of etched porcelain, porcelain specimens were etched by 5% hydrofluoric acid during the time of 2.5 min., 5 min., 7.5 min., and 10 min. at $23^{\circ}C$ and observed by SEM. Also, electrolytically etched metal was observed by SEM. Etched porcelain specimens were treated or were not treated with Silane coupling agent and bonded to etched metals with Comspan and Panavia. The bonded specimens were stored in water at $37^{\circ}C$. 24 hours after bonding, the bond strengths were measured. There were four groups of 25 specimens each. Group 1 was bonded with Panavia. Group 2 was bonded with Panavia after treated with Silane coupling agent. Group 3 was bonded with Comspan, Group 4 was bonded with Comspan after treated with Silane coupling agent. The results were as follows: 1. he etched porcelains were obviously observed by SEM. 2. The dendritic arms were observed in etched metal by SEM. 3. The bond strength in relation to the increase of etching time increased and an analysis of variance shows significantly different at the 0.01 level in all groups. 4. The bond strength of Silane coupling agent treated groups were higher than the untreated. 5. The ratios of increase of the bond strengths of Silane coupling agent treated groups in relation to the increase of etching of etching time were lower than the untreated. 6. The bond strength of the groups used Comspan were higher than Panavia.

  • PDF

리튬디실리케이트 세라믹과 표면처리방법에 따른 라미네이트 베니어의 전단결합강도 비교 (Comparison of Shear Bonding Strength of Laminate Veneer by Lithium Disilicate Ceramics and Surface Treatment Methods)

  • 박상준;정인성
    • 대한치과기공학회지
    • /
    • 제41권3호
    • /
    • pp.177-185
    • /
    • 2019
  • Purpose: This study was to investigate the effect of three different surface treatments on the shear bond strength of lithium disilicate ceramics to enamel. Methods: Totally 60 lithium disilicate ceramic disc specimens were fabricated with IPS e.max press (Ivoclar Vivadent, Schaan, Liechtenstein) and Mazic Claro (Vericom, Korea). 30 specimens in each lithium disilicate ceramic were assigned to 3 groups of the each following surface treatment: 1) $50{\mu}m$ airborne particle abrasion+silane, 2) 9.5% hydroflouric acid etching (HF)+silane, 3) $50{\mu}m$ airborne particle abrasion+9.5% HF+silane. Lithium disilicate ceramic surfaces after surface treatments were AFM examined. The shear bond strength was measured in a universal testing machine at 0.5mm/min crosshead speed. All data were analyzed using a two-way ANOVA and Tukey's test(${\alpha}=0.05$). Results: The mean surface roughness of lithium disilicate ceramics ranged from $0.178{\mu}m$ to $0.441{\mu}m$. The mean shear bond strengths ranged from $23.81{\pm}2.78MPa$ to $33.99{\pm}4.85MPa$. Conclusion: 1. Mazic Claro showed higher shear bond strength than IPS e.max press at 3 different surface treatments, and no statistically significant was observed. 2. The shear bond strength of IPS e.max press was strongly enhanced as surface treated with $50{\mu}m$ airborne particle abrasion and 9.5% hydroflouric acid etching. And there was no statistical significance at the shear bond strength of Mazic Claro with surface treatments.

치질에 대한 상아질 접착제의 접합도에 관한 연구 (A STUDY ON THE ADAPTATION OF DENTIN BONDING AGENTS TO TOOTH STRUCTURE)

  • 박성택;조영곤;황호길
    • Restorative Dentistry and Endodontics
    • /
    • 제20권2호
    • /
    • pp.732-743
    • /
    • 1995
  • The purpose of this study was to evaluate the adaptation of light cured dentin bonding agents to tooth structure by measuring contraction gaps on interfaces between cavity wall and composite resin under SEM study. In this study, class V cavities with cementum margin were prepared on the buccal surfaces of 15 extracted human premolar teeth and teeth were randomly assigned 3 groups of 5 teeth each. The cavities were filled with three dentin bonding agents and two composite resins were investigated for this study: three dentin bonding agents; Scotchbond 2, Scotchbond Multi-Purpose. All-Bond 2, two composite resins; Silux Pius, Z-100. Group 1 : Scotchbond 2 + Silux Plus Group 2 : Scotchbond Multi~Purpose + Z-100 Group 3 : All-Bond 2 + Z-100 The restored teeth were stored in 100% relative humidity at $37^{\circ}C$ for 7 days. And then, the roots of the teeth were removed with the tapered fissure bur and the remaining crowns were sectioned occlusogingivally through the center of restorations. Adaptation at tooth-restoration interface was assesed occlusally, gingivally, and axially by scanning electron microscope. The results were as follows : 1. In Group 1, the adaptation to dentinal wall of Scotchbond 2 was poor, but the adaptation to enamel wall of Scotchbond 2 was excellent. 2. In Group 2, the adaptation to occlusal was axial wall and gingival wall of Scotchbond Multi-Purpose was excellent. Especially in axially wall, the dentin bonding agents infiltrated into dentinal tubules and there was excellent adaptation to dentinal wall. 3. In Group 3, the adaptation to occlusal wall and axial wall of All-Bond 2 was excellent. But in gingival wall, there was gap formation between composite resin and dentin bonding agent.

  • PDF

다양한 산처리 방법이 lithium Disilicate 도재와 복합레진간의 전단결합강도에 미치는 영향 (Effects of Various Acid Etching Methods on the Shear Bond Strength between Iithium Disilicate Ceramic and Composite Resin)

  • 강대현;복원미;송진원;송광엽;안승근
    • 구강회복응용과학지
    • /
    • 제22권2호
    • /
    • pp.149-159
    • /
    • 2006
  • Statement of problem. Porcelain repair mainly involves replacement with composite resin, but the bond strength between composite resin and all-ceramic coping materials has not been studies extensively. Purpose. The objective of this study was to investigate the influence of composite resin and ceramic etching pattern on shear bond strength of Empress2 ceramic and observe the change of microstructure of ceramic according to etching methods. Material and methods. Eighty-five cylinder shape ceramic specimens (diameter 5mm, IPS Empress 2 core materials) embeded by acrylic resin were used for this study. The ceramic were specimens divided into sixteen experimental groups with 5 specimens in each group and were etched with phosphoric acid(37%, 65%) & hydrofluoric acid (4%, 9%) according to different etching times(30s, 60s, 120s 180s). All etched ceramic surfaces were examined morphologically using SEM(scanning electron microscopy). Etched surfaces of ceramic specimens were coated with silane (Monobond-S) & adhesive(Heliobond) and built up composite resin using Teflon mold. Accomplished specimens were tested under shear loading until fracture on universal testing machine at a crosshead speed 1mm/min; the maximum load at fracture(kg) was recorded. Shear bond strength data were analyzed with one way ANOVA and Duncan tests.(P<.05) Results. Maximum shear bond strength was $30.07{\pm}2.41(kg)$ when the ceramic was etched with 4% hydrofluoric acid at 120s. No significant difference was found between phosphoric etchant group and control group with respect to shear bond strength. Conclusion. Empress 2 ceramic surface was not etched by phosphoric acid, but etched by hydrofluoric acid.

착색지르코니아 코어와 전장 도재 사이의 전단결합강도에 관한 연구 (A study on the shear bond strengths of veneering ceramics to the colored zirconia core)

  • 강선녀;조욱;전영찬;정창모;윤미정
    • 대한치과보철학회지
    • /
    • 제47권3호
    • /
    • pp.312-319
    • /
    • 2009
  • 연구목적: 지르코니아-도재 수복물에 있어 상부도재와 코어 사이의 결합 실패가 종종 보고되어 왔으며 특히 착색지르코니아 코어는 기존의 백색 지르코니아보다 상부 도재와의 결합력이 약하다고 보고된 바 있다. 이 연구의 목적은 착색 지르코니아 코어 위의 상부도재를 적층식과 열가압식으로 제작하여 그 전단결합강도를 알아보고, 이를 전통적인 금속-도재간 결합강도와 비교하여 그 임상적 안정성을 평가하는 것이다. 연구 재료 및 방법: 금속도재군 (MC)을 대조군으로 하였다. 전통적인 금속도재군 (MC)과 지르코니아 코어를 사용한 두가지 군 (ZB, ZP)에 대하여 각 시스템별로 10개씩, 총 30개의 시편을 제작했다. CAD/CAM을 이용해 직경 12 mm, 높이 2.8 mm의 원판형 지르코니아 코어 (Katana zirconia)를 제작하고, 그 상부에 직경 2.8 mm, 높이 3 mm의 도재를 축성했다. ZB군은 CZR을 이용하여 적층법으로 상부도재를 제작했으며 ZP군은 NobelRondo Press ingot를 열가압하여 제작했다. Shear bond test machine (R&B Inc. Daejeon, Korea)을 이용하여 분당 0.50 mm의 속도로 파절이 일어날 때까지 전단력을 가하여 최대적용력 (N)을 측정하여 전단결합강도를 계산하고, 일원배치 분산분석을 사용하여 유의수준 5%에서 검정하였다. 파절양상을 알아보기 위하여 전자주사현미경을 통해 파절단면을 관찰했다. 결과: 평균 전단강도 (SD)는 MC 대조군 29.14 (2.26); ZB 29.48 (2.30); ZP 29.51 (2.32) 이었다. 실험군과 대조군 사이에 유의한 차이는 없었다. 모든 실험군에서 접착성 실패와 응집성 실패가 혼재된 양상을 보였으며, 응집성 실패가 우세했다. 결론: 1. 착색지르코니아 코어와 상부도재들 간의 전단결합강도는 금속 도재간 전단결합강도와 유의한 차이가 없었다. 2. 착색지르코니아 코어의 상부도재를 제작하는 방식에 있어 적층법과 열가압법 간의 전단결합강도에 유의한 차이는 없었다 (P > .05). 3. 파절양상은 응집성 파절이 우세한 가운데 접착성 파절과 응집성 파절이 혼재되어 나타났다.

열순환이 상아질 접착제의 결합 내구성에 미치는 영향 (THE EFFECT OF THERMOCYCLING ON THE DURABILITY OF DENTIN ADHESIVE SYSTEMS)

  • 문영훈;김종률;최경규;박상진
    • Restorative Dentistry and Endodontics
    • /
    • 제32권3호
    • /
    • pp.222-235
    • /
    • 2007
  • 이 논문의 목적은 열순환이 4종 상아질 접착 시스템의 결합 내구성에 미치는 영향을 측정한 것이다. 제3대구치의 상아질층을 노출시킨 후, 무작위로 8개군으로 나눈다: 3단계 산부식 시스템 (Scotchbond Multi-Purpose Plus; SM, All Bond-2 ; AB), 2 단계 산부식 시스템 (Single Bond; SB, One Step plus, OS), 2단계 자가부식 시스템 (Clearfil SE Bond; SE, AdheSE; AD), 1 단계 자가부식 시스템 (Promp L-Pop ; PL, Xeno III; XE). 8개 군에 각 상아질 접착제를 제조사의 지시에 따라 도포하고 복합레진 (Z250)을 적층한 후, 광조사한다. $37^{\circ}C$ 증류수에서 24시간 보관한 후, 각 군마다 정해진 프로그램으로 0, 1000, 2000회 열순환한 후, 저속 diamond saw로 $1\times1mm$ 막대형 시편을 제작한다. Universal testing machine (EZ-test; Shimadzu, Japan)으로 미세인장 결합강도를 측정하였고, 유의수준 0.05 level에서 ANOVA / Duncan's test로 통계분석 하였다. 상아질측 파단면과 접착계면에 대한 주사전자현미경 관찰을 시행하였다. 이 연구의 결과는 다음과 같다; 1. 3단계 상아질 접착제의 결합강도는 열순환 전후에 통계학적으로 유의한 변화를 나타내지 않았다. 2단계 산부식형 상아질 접착제의 결합강도는 열순환 처리에 의하여 유의하게 감소되었다. 2. 2단계 자가부식형 접착제 (SE)의 결합강도가 가장 높았고, 1단계 자가부식 접착제 (PL, XE)는 실험군 중 가장 낮은 결합강도를 보였다. 3. 모든 접착제는 주로 접착성 파괴가 발생하였고, 열순환에 의하여 산부식형 접착제는 접착성 파괴가, 1단계 자가부식형 접착제에서는 혼합형 파괴가 증가하는 경향을 나타내었다. 이상의 결과로, 상아질 접착제의 접착단계/과정이 결합내구성에 영향을 미침을 알 수 있었다. 따라서 접착과정의 단순화가 반드시 접착에 효과적이라고 할 수 없다.

Self-Priming Adhesives를 침투시킨 탈회 상아질의 인장강도 (Tensile Strengths of Demineralized Dentin derived from Self-Priming Adhesives)

  • 이혜윤;윤미란;이린;이정;이광원
    • 구강회복응용과학지
    • /
    • 제22권2호
    • /
    • pp.181-191
    • /
    • 2006
  • The objectives of this study were to evaluate the tensile strength of resin-infiltrated demineralized dentin according to the demineralization time, and to evaluate the tensile strength of hybrid layer that is formed by infiltrating different priming adhesives or primer/adhesive into demineralizd dentin matrix. Seventy five hour-glass shaped dentin specimens were prepared in mid-coronal dentin from extracted human molars. Thirty specimens were distributed into three groups according to demineralization time - 2 hours, 4 hours and 8 hours. Each specimen was placed in primer/adhesive of All-Bond 2 for 5 hours of infiltration. Another forty-five specimens of them were demineralized in 37% phosphoric acid for 4 hours. They were randomly assigned to three experimental groups - AB, SB and OS - to designate All-Bond 2, Single Bond and One-Step. Each specimen was placed in one of three different adhesives for 5 hours of infiltration. The specimens were visible light-cured for 5 minutes, and then stored for 24 hours in distilled water at $37^{\circ}C$. After that, microtensile bond strength for each specimen was measured, and the fractured surfaces were then observed by SEM. The data were statistically analysed by one-way ANOVA and Tukey's multiple comparison test and Bonferroni's multiple comparison test. The results were as follows; 1. Tensile strength of the group demineralized for 4 hours was significantly higher than that of groups demineralized for 2 hours and 8 hours (P < .01). 3. Tensile strength of the AB group was significantly higher than that of the SB group and OS group (P < .01).

Pull-out bond strength of a self-adhesive resin cement to NaOCl-treated root dentin: effect of antioxidizing agents

  • Khoroushi, Maryam;Kachuei, Marzieh
    • Restorative Dentistry and Endodontics
    • /
    • 제39권2호
    • /
    • pp.95-103
    • /
    • 2014
  • Objectives: This study evaluated the effect of three antioxidizing agents on pullout bond strengths of dentin treated with sodium hypochlorite. Materials and Methods: Root canals of 75 single-rooted human teeth were prepared. Fifteen teeth were irrigated with normal saline for a negative control group, and the remaining 60 teeth (groups 2 - 5) with 2.5% NaOCl. The teeth in group 2 served as a positive control. Prior to post cementation, the root canals in groups 3 - 5 were irrigated with three antioxidizing agents including 10% rosmarinic acid (RA, Baridge essence), 10% hesperidin (HPN, Sigma), and 10% sodium ascorbate hydrogel (SA, AppliChem). Seventy-five spreaders (#55, taper .02, Produits Dentaires S.A) were coated with silica and silanized with the Rocatec system and ceramic bond. All the prepared spreaders were cemented with a self-adhesive resin cement (Bifix SE, Voco Gmbh) in the prepared canals. After storage in distilled water (24 h/$37^{\circ}C$), the spreaders were pulled out in a universal testing machine at a crosshead speed of 1.0 mm/min. Pull-out strength values were analyzed by one-way ANOVA and Tukey's HSD test (${\alpha}$ = 0.05). Results: There were significant differences between study groups (p = 0.016). The highest pullout strength was related to the SA group. The lowest strength was obtained in the positive control group. Conclusions: Irrigation with NaOCl during canal preparation decreased bond strength of resin cement to root dentin. Amongst the antioxidants tested, SA had superior results in reversing the diminishing effect of NaOCl irrigation on the bond strength to root dentin.