• Title/Summary/Keyword: All Solid State.

Search Result 390, Processing Time 0.022 seconds

Fabrication and Characterization of $La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_{3-\delta}$ Oxygen Permeation Membranes Prepared with Different Powders ($La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_{3-\delta}$ 산소 투과 분리막의 제조 및 특성)

  • Lim, Kyoung-Tae;Lee, Kee-Sung;Han, In-Sub;Seo, Doo-Won;Hong, Kee-Seog;Bai, Kang;Woo, Sang-Kuk;Cho, Tong-Lae
    • Journal of the Korean Ceramic Society
    • /
    • v.38 no.10
    • /
    • pp.886-893
    • /
    • 2001
  • We synthesized $La_{0.6}Sr_{0.4}Co_{0.2}Fe_{0.8}O_{3-\delta}$ powders by coprecipitation, citration and solid-state reactions. The oxygen permeation membranes were fabricated by cold isostatic pressing of the synthesized powders, followed by sintering in air. All powders and membranes consist of perovskite phases. The coprecipitated powders showed the highest surface area ($7.5m^2/g$) but strontium deficiency was found during washing and filtering in the process. The membrane with lower relative density was fabricated by citration method. On the other hand, solid state reacted powders had high relative density (95%), and mechanical properties showed superior properties. Especially, the composition of the solid-state reacted powders was relatively well-controlled.

  • PDF

Physical Properties of the Nonstoichiometric Perovskite $Dy_{1-x}Sr_xCoO_{3-y}$ System

  • 정수경;김민규;김규홍;여철현
    • Bulletin of the Korean Chemical Society
    • /
    • v.17 no.9
    • /
    • pp.794-798
    • /
    • 1996
  • Solid solutions of the nonstoichiometric Dy1-xSrxCoO3-y system with the compositions of x=0.00, 0.25, 0.50, 0.75, and 1.00 have been synthesized by the solid state reaction at 1000 ℃ under atmospheric air pressure. The crystallographic structures of the solid solutions are analyzed by the powder X-ray diffraction patterns at room temperature. The analyses assign the compositions of x=0.00 and 0.25 to the orthorhombic system with space group of Pbnm/D2h16, the compositions of x=0.50 and 0.75 to the tetragonal system like a typical SrCoO2.86, and the composition of x=l.00 or SrCoO2.50 to the brownmillerite type system with space group of I**a. The reduced lattice volumes increase with x value due to the larger radius of Sr2+ ion than that of Dy3+ ion. The mole ratio of Co4+ ion to total Co ion with mixed valence state between Co3+ and Co4+ ions at B sites or τ value has been determined by an iodometric titration. All the samples except for the DyCoO3 compound show the mixed valnce state and thus the composition of x=0.50 has the maximum τ value in the system. The oxygen vacancies increasing with x value are randomly distributed over the crystal lattice except for the composition of x=l.00 which have the ordering of the oxygen vacancies. The nonstoichiometric chemical formulas of the Dy1-xSrxCo3+1-τCo4+τO3-(x-τ)/2 system are formulated from the x, τ, and y values. The electrical conductivity in the temperature range of 100 to 900 K increases with τ value linearly because of positive holes of the Co4+ ions in π* band as a conducting carrier. The activation energy of the x=0.50 as Ea=0.17 eV is minimum among other compouds. Broad and high order transition due to the overlap between σ* and π* bands broadened by the thermal activation is observed near 1000 K and shows a low temperature-semiconducting behavior. Magnetic properties following the Currie-Weiss law show the low to high spin transition in the cobaltate perovskite. Especially, the composition of x=0.75 presents weak ferromagnetic behavior due to the Co3+-O2--Co4+ indirect superexchange interaction.

Effects of Eu3+ and Tb3+ Activator Ions on the Properties of SrSnO3 Phosphors (Eu3+와 Tb3+ 활성제 이온이 SrSnO3 형광체의 특성에 미치는 영향)

  • Kim, Jung Dae;Cho, Shinho
    • Korean Journal of Materials Research
    • /
    • v.24 no.9
    • /
    • pp.469-473
    • /
    • 2014
  • $SrSnO_3$ phosphor powders were synthesized with two different contents of activator ions $Eu^{3+}$ and $Tb^{3+}$ using the solid-state reaction method. The structural, morphological, and optical properties of the phosphors were investigated using X-ray diffractometry, field-emission scanning electron microscopy, and fluorescence spectrophotometry, respectively. All the phosphors showed a cubic structure, irrespective of the type and the content ratio of activator ions. For $Eu^{3+}$-doped $SrSnO_3$ phosphors, the intensity of the 620 nm red emission spectrum resulting from the $^5D_0{\rightarrow}^7F_2$ transition of $Eu^{3+}$ was stronger than that of the 595 nm orange emission signal due to the $^5D_0{\rightarrow}^7F_1$ transition in the range 0.01-0.05 mol of $Eu^{3+}$, but the ratio of the intensity was reversed in the range 0.10-0.20 mol of $Eu^{3+}$. The variation in the emission intensity indicates that the site symmetry of the $Eu^{3+}$ ions around the host crystal was changed from non-inversion symmetry to inversion. For the $Tb^{3+}$-doped $SrSnO_3$ phosphors under excitation at 281 nm, one strong green emission band at 550 nm and several weak bands were observed. These results suggest that the optimum red and green emission signals can be realized when the activator ion content for $Eu^{3+}$- or $Tb^{3+}$-doped $SrSnO_3$ phosphors is 0.20 mol and 0.15 mol, respectively.

Synthesis and Photoluminescence Properties of Red Phosphors Gd1-xAl3(BO3)4:Eux3+ (적색 형광체 Gd1-xAl3(BO3)4:Eux3+의 합성과 발광 특성)

  • Cho, Shin-Ho;Cho, Seon-Woog
    • Korean Journal of Materials Research
    • /
    • v.22 no.3
    • /
    • pp.145-149
    • /
    • 2012
  • Red phosphors of $Gd_{1-x}Al_3(BO_3)_4:{Eu_x}^{3+}$ were synthesized by using the solid-state reaction method. The phase structure and morphology of the phosphors were measured using X-ray diffraction (XRD) and field emission-scanning electron microscopy (FE-SEM), respectively. The optical properties of $GdAl_3(BO_3)_4:Eu^{3+}$ phosphors with concentrations of $Eu^{3+}$ ions of 0, 0.05, 0.10, 0.15, and 0.20 mol were investigated at room temperature. The crystals were hexagonal with a rhombohedral lattice. The excitation spectra of all the phosphors, irrespective of the $Eu^{3+}$ concentrations, were composed of a broad band centered at 265 nm and a narrow band having peak at 274 nm. As for the emission spectra, the peak wavelength was 613 nm under a 274 nm ultraviolet excitation. The intensity ratio of the red emission transition ($^5D_0{\rightarrow}^7F_2$) to orange ($^5D_0{\rightarrow}^7F_1$) shows that the $Eu^{3+}$ ions occupy sites of no inversion symmetry in the host. In conclusion, the optimum doping concentration of $Eu^{3+}$ ions for preparing $GdAl_3(BO_3)_4:Eu^{3+}$ phosphors was found to be 0.15 mol.

Photoluminescence Properties of CaNb2O6:RE3+ (RE= Sm, Eu) Phosphors (CaNb2O6:RE3+ (RE= Sm, Eu) 형광체의 광학 특성)

  • Joeng, Woon Hwan;Cho, Shinho
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.27 no.7
    • /
    • pp.477-482
    • /
    • 2014
  • $CaNb_2O_6:RE^{3+}$ (RE=Sm or Eu) phosphor powders were prepared with different contents of activator ions by using solid-state reaction method. The X-ray diffraction patterns exhibited that the phosphors synthesized with different activator ions showed an orthorhombic system with a main (131) diffraction peak. The maximum size of the grain particles, determined from the measurement of scanning electron microscopy, was observed at 0.05 mol of $Eu^{3+}$ ions and at 0.01 mol of $Sm^{3+}$. As for the $Eu^{3+}$-doped phosphor powders, the excitation spectra were composed of a broad band peaked at 278 nm and several weak bands in the range of 350~500 nm, and the highest red emission spectrum was observed at 0.15 mol of $Eu^{3+}$ ions. As for the $Sm^{3+}$-activated phosphor powders, three strong emission bands under excitation at 273 nm were observed at 570, 612, and 659 nm, respectively. The intensities of all the emission bands approached maxima for 0.05 mol of $Sm^{3+}$ ions. The optical properties show that the $Eu^{3+}$- or $Sm^{3+}$-doped $CaNb_2O_6$ powders are promising red-orange emitting phosphor powders applicable to full-color photonic devices.

Characterization of the Material Properties of 0.68Pb ($Mg_{1}$3/$Nb_{2}$3/)$O_3$-0.32PbT$iO_3$ Single Crystals Grown by the Solid-State-Crystal-Growth Method (고상단결정법으로 성장시킨 0.68Pb ($Mg_{1}$3/$Nb_{2}$3/)$O_3$-0.32PbT$iO_3$ 압전단결정의 물성평가)

  • 이상한;노용래
    • The Journal of the Acoustical Society of Korea
    • /
    • v.23 no.2
    • /
    • pp.103-108
    • /
    • 2004
  • In this paper, all the materials constants of the PMN-32%PT single crystals grown by the solid state crystal growth method were measured by the resonance method. PMN-PT crystals of tetragonal symmetry have six elastic constants, three piezoelectric constants and two dielectric constants for their independent material constants. These materials constants were extracted from six sets of crystal samples of each different geometry to have different vibration modes respectively. Measured results showed that the crystal has larger electromechanical coupling factor k/sub 33/ (∼86%) and piezoelectric constant d/sub 33/ (∼1200pC/N) than conventional piezoceramics. Validity of the measurement was confirmed through comparison of the results with the impedance spectrum from finite element analysis of the samples and the results measured with a commercial do meter.

Synthesis of CoTiOx and Its Catalytic Activity in Continuous Wet TCE Oxidation (CoTiOx의 합성 및 연속 습식 TCE 산화반응에서의 촉매활성)

  • Kim, Moon-Hyeon
    • Journal of Environmental Science International
    • /
    • v.16 no.12
    • /
    • pp.1431-1437
    • /
    • 2007
  • Cobalt titanates($CoTiO_x$), such as $CoTiO_3$ and $Co_2TiO_4$, have been synthesized via a solid-state reaction and characterized using X-ray diffraction(XRD) and X-ray photoelectron spectroscopic(XPS) measurement techniques, prior to being used for continuous wet trichloroethylene(TCE) oxidation at $36^{\circ}C$, to support our earlier chemical structure model for Co species in 5 wt% $CoO_x/TiO_2$(fresh) and(spent) catalysts. Each XRD pattern for the synthesized $CoTiO_3$ and $Co_2TiO_4$ was very close to those obtained from the respective standard XRD data files. The two $CoTiO_x$ samples gave Co 2p XPS spectra consisting of very strong main peaks for Co $2p_{3/2}$ and $2p_{1/2}$ with corresponding satellite structures at higher binding energies. The Co $2p_{3/2}$ main structure appeared at 781.3 eV for the $CoTiO_3$, and it was indicated at 781.1 eV with the $Co_2TiO_4$. Not only could these binding energy values be very similar to that exhibited for the 5 wt% $CoO_x/TiO_2$(fresh), but the spin-orbit splitting(${\Delta}E$) had also no noticeable difference between the cobalt titanates and a sample of the fresh catalyst. Neither of all the $CoTiO_x$ samples were active for the wet TCE oxidation, as expected, but a sample of pure $Co_3O_4$ had a good activity for this reaction. The earlier proposed model for the surface $CoO_x$ species existing with the fresh and spent catalysts is very consistent with the XPS characterization and activity measurements for the cobalt titanates.

Priority-Based Hybrid File Storage Management System Using Logical Volume Manager (논리 볼륨 매니저를 이용한 파일 우선순위 기반의 하이브리드 저장장치 관리 시스템)

  • Choi, Hoonha;Kim, Hyeunjee;No, Jaechun
    • Journal of the Institute of Electronics and Information Engineers
    • /
    • v.53 no.12
    • /
    • pp.94-102
    • /
    • 2016
  • Recently, the I/O performance of a single node is rapidly improving due to the advent of high-performance SSD. As a result, the next-generation storage platform based on SSD has received a great deal of attention and such storage platforms are increasingly adopted to commodity servers or data centers that look for the high-bandwidth computation and I/O. However, building all SSD-based storage platform may not be cost-effective because the price per storage capacity is very high as compared to that of HDD. In this paper. we propose a hybrid file management solution, called HyPLVM(Hybrid Priority Logical Volume Manager), which combines the strength of SSD with the desirable aspects of low-price, high-storage capacity HDD. HyPLVM prioritizes the files and directories to be accessed by users, in order to determine the target storage device (SSD/HDD) in which files are allocated, while mitigating the cost of building storage platforms.

Characterization of $YBa_2Cu_3O_{7-x}F_y$ Superconducting Materials Made by a Sol-Gel Process (졸-겔법으로 제조한 $YBa_2Cu_3O_{7-x}F_y$ 초전도물질의 특성분석)

  • 김봉흡;강형부;김현택
    • The Transactions of the Korean Institute of Electrical Engineers
    • /
    • v.41 no.5
    • /
    • pp.525-532
    • /
    • 1992
  • Fluorine-doped YBaS12TCuS13TOS17-xTFS1yT superconducting materials with y varing two orders of magnitude form 0.02 to 2.0 have been prepared by a sol-gel process by using metal nitrate salts, sodium hydroxide and sodium fluoride. Fluorine contents have been measured using an ion-selective electrode. All fluorine doped as reactant were found to be present in the resulted samples. From the observation of XRD it has been concluded that the samples with y 0.2 formed simply the single phase of perovskite structure, whereas those with y 0.5 yielded together some compounds such as BaFS12T, YFS13T and CuO in the resulted samples. The observation of solid state S019TF NMR has been carried out in order to check whether fluorine was actually incorporated into the lattice sites, and the experimental results revealed that the mole ratio of fluorine incorporated into the lattice sites of YBaS12TCuS13TOS17-xT was approximately 0.2 per mole of the compound. Also electrical resistivity measurement indicated that onset transition temperature has the tendency to increase slightly with increasing y in the dilute region as y 0.2.

  • PDF

Synthesis and Photoluminescence Properties of Dy3+- and Eu3+-codoped CaMoO4 Phosphors (Dy3+와 Eu3+ 이온이 동시 도핑된 CaMoO4 형광체의 합성과 발광 특성)

  • Kim, Junhan;Cho, Shinho
    • Journal of the Korean institute of surface engineering
    • /
    • v.48 no.3
    • /
    • pp.82-86
    • /
    • 2015
  • $Dy^{3+}$- and $Eu^{3+}$-codoped $CaMoO_4$ Phosphors were synthesized by using the solid-state reaction method. The crystal structure, morphology, and optical properties of the resulting phosphor particles were investigated by using the X-ray diffraction, field-emission scanning electron microscopy, and photoluminescence spectroscopy. XRD patterns exhibited that all the synthesized phosphors showed a tetragonal system with a main (112) diffraction peak, irrespective of the content of $Eu^{3+}$ ions. As the content of $Eu^{3+}$ ions increased, the grains showed a tendency to agglomerate. The excitation spectra of the synthesized powders were composed of one strong broad band centered at 305 nm in the range of 220 - 350 nm and several weak peaks in the range of 350 - 500 nm resulting from the 4f transitions of activator ions. Upon ultraviolet excitation at 305 nm, the yellow emission line due to the $^4F_{9/2}{\rightarrow}^6H_{13/2}$ transition of $Dy^{3+}$ ions and the main red emission spectrum resulting from the $^5D_0{\rightarrow}^7F_2$ transition of $Eu^{3+}$ ions were observed. With the increase of the content of $Eu^{3+}$, the intensity of the yellow emission band gradually decreased while that of the red emission increased. These results indicated that the emission intensities of yellow and red emissions could be modulated by changing the content of the $Dy^{3+}$ and $Eu^{3+}$ ions incorporated into the host crystal.