• Title/Summary/Keyword: Al-Mg coating

Search Result 108, Processing Time 0.023 seconds

Phase-Field Modelling of Zinc Dendrite Growth in ZnAlMg Coatings

  • Mikel Bengoetxea Aristondo;Kais Ammar;Samuel Forest;Vincent Maurel;Houssem Eddine Chaieb;Jean-Michel Mataigne
    • Corrosion Science and Technology
    • /
    • v.23 no.2
    • /
    • pp.93-103
    • /
    • 2024
  • In the present work, a phase-field model for dendritic solidification is applied to hot-dip ZnAlMg coatings to elucidate the morphology of zinc dendrites and the solute segregation leading to the formation of eutectics. These aspects define the microstructure that conditions the corrosion resistance and the mechanical behaviour of the coating. Along with modelling phase transformation and solute diffusion, the implemented model is partially coupled with the tracking of crystal orientation in solid grains, thus allowing the effects of surface tension anisotropy to be considered in multi-dendrite simulations. For this purpose, the composition of a hot-dip ZnAlMg coating is assimilated to a dilute pseudo-binary system. 1D and 2D simulations of isothermal solidification are performed in a finite element solver by introducing nuclei as initial conditions. The results are qualitatively consistent with existing analytical solutions for growth velocity and concentration profiles, but the spatial domain of the simulations is limited by the required mesh refinement.

Microstructure and Corrosion Properties of Plasma Electrolytic Oxide Coatings on AZ31 Magnesium Matrix Composite (플라즈마 전해 산화 처리한 AZ31 및 Al18B4O33w/AZ31 마그네슘 복합재료 피막의 미세구조 및 부식특성)

  • Cheon, Jinho;Park, Yongho;Park, Ikmin
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.3
    • /
    • pp.270-274
    • /
    • 2011
  • Plasma electrolytic oxidation (PEO) treatment was performed on squeeze cast AZ31 alloy and $Al_{18}B_4O_{33}w/AZ31$ composite. Scanning electron microscope (SEM) was employed to characterize the surface morphology and cross-section microstructure of the coating. The phase structures of the PEO coating were analyzed by X-ray diffraction (XRD). The corrosion resistance of the PEO coating was evaluated by electrochemical method. The results showed that the $Al_{18}B_4O_{33}$ whisker on the surface of the composite was decomposed and $MgAl_2O_4$ was formed in the PEO coating layer of $Al_{18}B_4O_{33}w/AZ31$ composite during PEO treatment. As a result, the electrochemical corrosion potential of the PEO coated $Al_{18}B_4O_{33}w/AZ31$ composite was increased compared with that of AZ31 alloy.

Effect of Mg content and heat treatment on the corrosion resistance of Al-Mg coating (Al-Mg 코팅의 내식성에 미치는 Mg 함량 및 열처리의 영향)

  • Gang, Jae-Uk;Park, Jun-Mu;Yun, Yong-Seop;Lee, Myeong-Hun
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2015.11a
    • /
    • pp.144-144
    • /
    • 2015
  • 본 연구에서는 PVD법 중의 하나인 스퍼터링(sputtering) 기술을 이용하여 향상된 희생양극(sacrificial anode)적 특성을 가지는 고내식 Al-Mg 막을 제작함은 물론 그 제작 조건에 따른 표면의 몰포로지, 성분 분포, 결정구조 등의 변화를 해석하였다. 또한 표면 및 단면에 대한 염수분무 노출시험을 통해 Mg 성분의 첨가에 따른 막의 내식특성을 평가하였다. 이상의 재료특성 분석 및 내식성 평가 결과간 연구-고찰을 통해 제작 조건과 막의 내식성에 대한 종합적인 연관성을 해석하였으며 이를 통해 최적의 Al-Mg 제작에 대한 기초적인 설계 조건을 제시하고자 하였다.

  • PDF

Characteristics of Conversion Coating of AZ31 Magnesium Alloy Formed in Chromium-Free Cerium-Based Solution (크롬 프리 세륨 용액에 의한 AZ31 마그네슘 합금의 화성 피막에 대한 특성 평가)

  • Kim, Myung Hwan;Lee, Dong Uk;Kwag, Sam-Tag;Moon, Myung-Jun
    • Journal of the Korean institute of surface engineering
    • /
    • v.49 no.1
    • /
    • pp.62-68
    • /
    • 2016
  • A chromium-free Ce-based conversion coating formed by immersion in a solution containing cerium chloride and nitric acid on AZ31 magnesium alloy has been studied. The effects of acid pickling on the morphology and the corrosion resistance of the cerium conversion coating were investigated. The corrosion resistance of the conversion coating prepared on AZ31 Mg alloy after organic acid pickling was better than that of inorganic acid pickling. The morphology of the conversion-coated layer was observed using optical microscope and SEM. Results show that the conversion coatings are relatively uniform and continuous, with thickness 1.0 to $1.1{\mu}m$. The main elements of the conversion coating of AZ31 Mg alloy are Mg, O, Al, Ce and Zn by EDS analysis. The electrochemical polarization results showed that the Ce-based conversion coating could reduce the corrosion activity of the AZ31 Mg alloy substrates in the presence of chloride ions.

Preparation of $LaAlO_3$ thin Films by Sol-gel Method (Sol-gel 방법에 의한 $LaAlO_3$ 박막의 제조)

  • Kim, H.J.;Kim, B.J.;Lee, H.G.;Hong, G.W.
    • Progress in Superconductivity
    • /
    • v.9 no.1
    • /
    • pp.85-90
    • /
    • 2007
  • Lanthanum aluminate($LaAlO_3$) film has been prepared on single crystal and metal substrates by dip coating method. Lanthanum acetate and aluminum were prepared via ligand exchange starting from lanthanum nitrate hexahydrate and aluminum nitrate hexahydrate in acetate glacial acetic acid solution after being refluxed. Coating solution was obtained by diluting the gel with methanol and 2-methoxyethanol to adjust the total cation concentration to 0.67 M. Precursor coated film was prepared by dip-coating with a speed of 25 mm/min on various substrates such as $LaAlO_3$ (001), MgO(001), $SrTiO_3$(001) single crystal, LMO/MgO/Ni-alloy. Thin films have been obtained by heat treating the precursor film at various temperatures from $600^{\circ}C{\sim}900^{\circ}C$ and various heating rate from $0.83^{\circ}C/min{\sim}1.25^{\circ}C/min$ under $Ar/O_2$ mixture containing 1000ppm oxygen. The films have been characterized by scanning electronic microscopy (SEM) and X-ray diffraction (XRD). XRD analysis for the prepared film showed that $LaAlO_3$ thin films with a preferred orientation of (100) plane parallel to substrate surface were obtained at $800^{\circ}C(1.11\;^{\circ}C/min)$ on LMO/MgO/Ni-alloy substrate, but the intensity decreased with the increase of heat treatment temperature.

  • PDF

Performance of Hot-dip Zn-6%Al-3%Mg Alloy Coated Steel Sheet as Automotive Body Material

  • Shimizu, Takeshi;Asada, Hiroshi;Morikawa, Shigeru
    • Corrosion Science and Technology
    • /
    • v.9 no.2
    • /
    • pp.74-80
    • /
    • 2010
  • For the purpose of applying a hot-dip Zn-6mass%Al-3mass%Mg alloy coated steel sheet (ZAM) to automotive body materials, a laboratory study of the general properties required for inner and outer panels of automotive bodies was performed. Even with only light coating weight, ZAM showed an excellent corrosion resistance in terms of both cosmetic and perforation corrosion compared to the currently used materials for automotive bodies, GI70 and GA45. In our study, it was confirmed that ZAM exhibits as good as or better properties than GI70 in terms of spot weldability and press formability. Furthermore, since the same corrosion resistance can be achieved with less coating weight by applying ZAM, laser weldability is better than GI and GA.

Preparation and Characteristics of Ceramic Composite Powders Coated with $Al_2O_3$ : (II) Composite Powders of $Al_2O_3$-$TiO_2$ ($Al_2O_3$ 로 피복시킨 세라믹 복합분체의 제조 및 특성 : (II) $Al_2O_3$-$TiO_2$ 복합분체)

  • 현상훈;정형구
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.4
    • /
    • pp.338-346
    • /
    • 1991
  • The alumina-titania composite powders coated with Al2O3 were prepared by the method of hydrolysis-deposition of mixed aluminium salt solution of Al2(SO)4-Al(NO3)3-Urea. The effects of coating-process parameters on the characteristics of coated composite powders were also investigated. As the content of TiO2 dispersed in deionized water increased, the coated composite powders were found to be more uniform in size and unagglomerated. When TiO2 powders were coated for 30 min, the optimum TiO2 content in the coating process was 400 mg/ι. The size of TiO2 particle was increased approximately from 0.7${\mu}{\textrm}{m}$ to 1.0${\mu}{\textrm}{m}$ through coating of Al2O3. The IEP of coated composite powders was pH=8.3 identical to the value of aluminium hydroxides and the zeta-potential showed nearly similar values each other. When heat treating coated composite powders at 130$0^{\circ}C$, only two phases of TiO2(rutile) and Al2TiO5 were observed. These results showed that the suface of TiO2 could be uniformly coated with the aluminium hydroxide.

  • PDF

Effect of Al and Mg Contents on Wettability and Reactivity of Molten Zn-Al-Mg Alloys on Steel Sheets Covered with MnO and SiO2 Layers

  • Huh, Joo-Youl;Hwang, Min-Je;Shim, Seung-Woo;Kim, Tae-Chul;Kim, Jong-Sang
    • Metals and materials international
    • /
    • v.24 no.6
    • /
    • pp.1241-1248
    • /
    • 2018
  • The reactive wetting behaviors of molten Zn-Al-Mg alloys on MnO- and amorphous (a-) $SiO_2$-covered steel sheets were investigated by the sessile drop method, as a function of the Al and Mg contents in the alloys. The sessile drop tests were carried out at $460^{\circ}C$ and the variation in the contact angles (${\theta}_c$) of alloys containing 0.2-2.5 wt% Al and 0-3.0 wt% Mg was monitored for 20 s. For all the alloys, the MnO-covered steel substrate exhibited reactive wetting whereas the $a-SiO_2$-covered steel exhibited nonreactive, nonwetting (${\theta}_c>90^{\circ}$) behavior. The MnO layer was rapidly removed by Al and Mg contained in the alloys. The wetting of the MnO-covered steel sheet significantly improved upon increasing the Mg content but decreased upon increasing the Al content, indicating that the surface tension of the alloy droplet is the main factor controlling its wettability. Although the reactions of Al and Mg in molten alloys with the $a-SiO_2$ layer were found to be sluggish, the wettability of Zn-Al-Mg alloys on the $a-SiO_2$ layer improved upon increasing the Al and Mg contents. These results suggest that the wetting of advanced high-strength steel sheets, the surface oxide layer of which consists of a mixture of MnO and $SiO_2$, with Zn-Al-Mg alloys could be most effectively improved by increasing the Mg content of the alloys.

Influence of Corrosion Products on Corrosion Resistance of Al-Mg Coating Films (Al-Mg 코팅막의 부식특성에 대한 부식생성물의 영향)

  • Lee, Seung-Hyo;Kim, Hye-Min;Im, Gyeong-Min;Yun, Yong-Seop;Jeong, Jae-In;Yang, Ji-Hun;Lee, Myeong-Hun
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2012.11a
    • /
    • pp.190-190
    • /
    • 2012
  • 여기서는 5% NaCl 염수분무 환경에 노출된 Al-Mg 다층 코팅막의 부식 거동이 부식생성물 분석을 통하여 평가되었다. 동일 두께의 코팅막이라고 할지라도 Al과 Mg의 코팅층을 다층으로 할수록 내식성이 우수한 경향으로 나타났다. 이때 SEM, EDS 및 XRD 평가 기법을 통하여, 내식성에 기여하는 주요 부식생성물은 수산화알루미늄($Al(OH)_3$)이 지배적인 것으로 확인 되었다. 코팅막이 다층인 경우 차폐(barrier) 특성을 가진 수산화알루미늄이 상대적으로 치밀하게 표면을 피복됨으로써 내식성을 오래도록 유지해 주는 것으로 사료된다.

  • PDF

An Experimental Study to Secure Electromagnetic Pulse Shielding Performance of Concrete Coated by an Arc Metal Spraying Process (아크 금속 용사 공법에 의해 코팅된 콘크리트의 전자기파 차폐 성능 확보를 위한 실험적 연구)

  • Jang, Jong-Min;Jeong, Hwa-Rang;Lee, Han-Seung
    • Journal of the Korea Institute of Building Construction
    • /
    • v.21 no.6
    • /
    • pp.519-527
    • /
    • 2021
  • In this study, an electromagnetic pulse shielding effect was obtained by applying the arc metal spraying method to the ordinary concrete. For this study, to evaluate the electrical properties in the thickness of the metal sprayed coating, 8 types of metals(Cu, CuAl, CuNi, CuZn, Al, Zn, ZnAl, AlMg) were sprayed as coatings with a thickness of 100, 200 and 500㎛. The electrical conductivity on the surface was measured with a 4-pin probe, and an electromagnetic wave shielding effect test was performed according to KS. Based on the test results, 200 ㎛ was proposed as an optimal metal coating thickness for electromagnetic pulse shielding, and it was thermally sprayed on a 300×300×100mm concrete specimen to analyze the electromagnetic wave shielding performance. However, in the area of adhesion strength, the maximum was 1.11MPa, which was found to be less than 74% of the target performance.