• Title/Summary/Keyword: Al(Fe-Cu) system

Search Result 85, Processing Time 0.024 seconds

Crystallization and Magnetic Properties of Non-Equilibrium Al(Fe-Cu) Alloy Powders Produced by Rod Milling and Chemical Leaching (Rod Milling과 Chemical Leaching에 의해 제작된 비평형 Al(Fe-Cu) 합금 분말의 결정화 및 자기적 특성)

  • Kim Hyun-Goo
    • Journal of Powder Materials
    • /
    • v.11 no.6 s.47
    • /
    • pp.486-492
    • /
    • 2004
  • We report the crystallization and magnetic properties of non-equilibrium $Al_{0.6}(Fe_{x}Cu_{1-x})_{0.4}(x=0.25, 0.50, 0.75)$ alloy powders produced by rod-milling as well as by new chemical leaching. X-ray diffractometry, transmission electron microscopy, differential scanning calorimetry and vibrating sample magnetometry were used to characterize the as-milled and leached specimens. After 400 h or 500 h milling, only the broad peaks of nano bcc crystalline phases were detected in the XRD patterns. The crystallite size, the peak and the crystallization temperatures increased with increasing Fe. After being annealed at $600{^\circ}C$ for 1 h for as-milled alloy powders, the peaks of bcc $AlCu_{4}\;and\;Al_{13}Cu_{4}Fe_{3}\;for\;x=0.25,\;bcc\;AlCu_{4}\;and\;Al_{5}Fe_{2}\;for\;x=0.50,\;and\;Al_{5}Fe_{2},\;and\;Al_{0.5}Fe_{0.5}\;for\;x=0.75$ are observed. After being annealed at $500{^\circ}\;and\;600{^\circ}C$for 1 h for leached specimens, these non-equi-librium phases transformed into fcc Cu and $CuFe_{2}O_{4}$phases for the x=0.25 specimen, and into bcc ${\alpha}-Fe,\;fcc\;Cu,\;and\;CuFe_{2}O_{4}$ phases for both the x=0.50 and the x=0.75 specimens. The saturation magnetization decreased with increasing milling time for $Al_{0.6}(Fe_{x}Cu_{1-x})_{0.4}$ alloy powders. On cooling the leached specimens from $800{\~}850^{\circ}C$,\;the magnetization first sharply increase at about $491.4{\circ}C,\;745{\circ}C,\;and\;750.0{\circ}C$ for x=0.25, x=0.50, and x=0.75 specimens, repectively.

Magnetic Properties of Ultrafine grained Fe-Al-Nb-B-(Cu) Alloys. (Fe-Al-Nb-B-(Cu)계 초미세결정합금의 자기적 특성)

  • 박진영;서수정;김규진;김광윤;노태환
    • Journal of the Korean Magnetics Society
    • /
    • v.6 no.4
    • /
    • pp.218-224
    • /
    • 1996
  • The magnetic properties and crystallization behaviors of $Fe_{83-x}Al_{x}Nb_{5}B_{12}(X=1~5at%)$ alloys were investigated. The $Fe_{80}Al_{3}Nb_{5}B_{12}$ alloy was developed a very good soft magnetic material with ultra-fine grain structure in Fe-Al-Nb-B system alloys. When 1 at% of Cu was added in Fe-Al-Nb-B alloy, the soft magnetic properties were found to improve significantly through the reduction of the grain size upto about 6~7 nm at $450^{\circ}C$. The magnetic properties of the $Fe_{79}Al_{3}Nb_{5}B_{12}Cu_{1}$ alloy were as follows : ${\mu}_{eff}(1\;kHz)=26,000,\;B_{10}=1.45\;T,\;H_{c}=25\;mOe,\;P_{c}(100\;kHz,\;0.2\;T)=55\;W/kg$, respectively.

  • PDF

The Optical properties of Fe2O3/Na3AlF6/Fe2O3/Cu, Al, Cr Multi Layered Thin Film depending on the Optical Thickness (Fe2O3/Na3AlF6/Fe2O3/Cu, Al, Cr 다층박막의 광학적 두께에 따른 광학특성)

  • Kim, Jun-Sik;Jang, Gang-Jae;Jang, Gun-Eik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.21 no.7
    • /
    • pp.665-668
    • /
    • 2008
  • Multi-layered thin films of $Fe_2O_3/Na_3AlF_6/Fe_2O_3/Cu$, Cr, Al were deposited on glass substrate by evaporation process. As high and low refractive index material, $Fe_2O_3$ and $Na_3AlF_6$ were selected and additionally Cu, Al and Cr were chosen as mid reflective layer respectively. Optical properties including reflectance were systematically studied depending on optical thickness of $Na_3AlF_6$ especially $0.25{\lambda}$ and $0.5{\lambda}$. In order to expect the experimental result, the simulation program, the Essential Macleod Program(EMP) was adopted and compared with the experimental data. Based on the results taken by spectrophotometer at viewing angle $45^{\circ}C$, the $Fe_2O_3/Na_3AlF_6/Fe_2O_3/Cu$ show the colour rage between red and orange in $0.25{\lambda}$ and green and pupple in $0.5{\lambda}$ respectively. When the Al was used as mid reflective layers in $Fe_2O_3/Na_3AlF_6/Fe_2O_3$ system, typical yellow colour and mixed colour between green and pupple were appeared in $0.25{\lambda}$ and $0.5{\lambda}$ of $Na_3AlF_6$ respectively. As compared the experimental result to simulation data, it was found out that the experimental data is relatively well matched with the EMP simulation data.

Microstructural Change and Magnetic Properties of Nanocrystalline Fe-Si-B-Nb-Cu Based Alloys Containing Minor Elements

  • Nam, Seul-Ki;Moon, Sun-Gyu;Sohn, Keun Yong;Park, Won-Wook
    • Journal of Magnetics
    • /
    • v.19 no.4
    • /
    • pp.327-332
    • /
    • 2014
  • The effect of minor element additions (Ca, Al) on microstructural change and magnetic properties of Fe-Nb-Cu-Si-B alloy has been investigated, in this paper. The Fe-Si-B-Nb-Cu(-Ca-Al) alloys were prepared by arc melting in argon gas atmosphere. The alloy ribbons were fabricated by melt-spinning, and heat-treated under a nitrogen atmosphere at $520-570^{\circ}C$ for 1 h. The soft magnetic properties of the ribbon core were analyzed using the AC B-H meter. A differential scanning calorimetry (DSC) was used to examine the crystallization behavior of the amorphous alloy ribbon. The microstructure was observed by X-ray diffraction (XRD), transmission electron microscope (TEM) and scanning electron microscope (SEM). The addition of Ca increased the electrical resistivity to reduce the eddy current loss. And the addition of Al decreased the intrinsic magnetocrystalline anisotropy $K_1$ resulting in the increased permeability. The reduction in the size of the ${\alpha}$-Fe precipitates was observed in the alloys containing of Ca and Al. Based on the results, it can be concluded that the additions of Ca and Al notably improved the soft magnetic properties such as permeability, coercivity and core loss in the Fe-Nb-Cu-Si-B base nanocrystalline alloys.

Behavior of Intermetallic Compound Formation in Al-25Nb system and (Al,X)-25Nb (X= Cr, Cu, Fe, Mn) systems by Mechanical Alloying Method (A1-25Nb계와 (A1,X)-25Nb계 (X = Cr, Cu, Fe, Mn)의 기계적 합금화에 의한 금속간 화합물의 형성 거동에 관한 연구)

  • Choi, Jae-Woong;Kang, Sung-Goon
    • Korean Journal of Materials Research
    • /
    • v.11 no.9
    • /
    • pp.733-739
    • /
    • 2001
  • In Al-25Nb binary system, it was observed only formation of $D0_{22}$ $Al_3Nb$ intermetallic compound after 5hr milling but it was not observed formation of meta stable phase like L1$_2$ phase. In this state, $D0_{22}$ $Al_3Nb$ fabricated had nano sized grain of approximately 20nm. Ternary systems, transition metals such as Cr, Cu, Fe, Mn were added 6~12at.% as substitution of Al, showed formation of $D0_{22}$ $Al_3Nb$ like Al-25Nb binary system. In Al- l2Cu-25Nb system, it was observed that broad XRD pattern like amorphization of Al and not observed formation of $D0_{22}$ $Al_3Nb$ after 5hr milling. But there was mixed phase of a lot of amorphous Al and little $D0_{22}$ $Al_3Nb$ through TEM. In the states of unalloyed, 5~7hr milling time, those showed exothermic reaction at 35$0^{\circ}C$, which was formation of $D0_{22}$ $Al_3Nb$ like Al-25Nb binary system. With increasing milling time to 10hr, $D0_{22}$ $Al_3Nb$ was transformed to mixed phase of amorphous and nanocryatlline, having approximately 10nm grain but the meta stable $Al_3Nb$ was not fabricated by adding transition metals.

  • PDF

Properties and Casting Capabilities of Al-Fe-Zn-Cu Alloys for High Conductivity Parts (고전도성 부품용 Al-Fe-Zn-Cu합금의 물성 및 주조성)

  • Yun, Ho-Seob;Kim, Jeong-Min;Park, Joon-Sik;Kim, Ki-Tae;Ko, Se-Hyun
    • Journal of Korea Foundry Society
    • /
    • v.33 no.6
    • /
    • pp.242-247
    • /
    • 2013
  • The most widely utilized commercial, aluminum-casting alloys are based on an aluminum-silicon system due to its excellent casting, and good mechanical, properties. Unfortunately, these Al-Si based alloys are inherently poor energy conductors; compared to pure aluminum, because of their high silicon content. This means that they are not suitable for applications demanding high eletrical or thermal conductivity. Therefore, efforts are currently being made to develop new, highly-conductive aluminum-casting alloys containing no silicon. In this research, a number of properties; including potential for castability, were investigated for a number of Al-Fe-Zn-Cu alloys with varying Cu content. As the copper content was increased, the tensile strength of Al-Fe-Zn-Cu alloy tended to increase gradually, while the electrical conductivity was slightly reduced. Fluidity was found to be lower in high-Cu alloys, and susceptibility to hot-cracking was generally high in all the alloys investigated.

Mechanical Aalloying Behavior of $Al_3$Hf 및 $Al_3$Ta Intermetallic Compounds by SPEX Mill and the Effect of Ternary Additions on the Formation of $Ll_2$ Phase (SPEX mill을 이용한 $Al_3$Hf 및 $Al_3$Ta 금속간화합물의 기계적합금화 거동과 $Ll_2$상형성에 미치는 제 3 원소 첨가의 영향)

  • Lee, Seong-Hun;Choe, Jong-Hyeon;Kim, Jun-Gi;Kim, Seon-Jin
    • Korean Journal of Materials Research
    • /
    • v.10 no.8
    • /
    • pp.569-574
    • /
    • 2000
  • To improve the ductility of $Al_3Hf$ and $Al_3Ta$ intermetallic compounds, which are the potential temperature structural materials, the mechanical alloying behaviour and the effect of ternary additions on the $Ll_2$ phase formation were investigated. During the mechanical alloying by the SPEX mill, the $Ll_2$ $Al_3Hf$ intermetallic compound was formed after 6 hours of milling in AL-25%Hf system. In AL-25%Ta system, however, only the $D0_{22}$ $Al_3Ta$ intermetallic compound was formed until 30 hours of milling and the $Ll_2$ phase was not observed. In AL-12.5%M-25%Ta(M=Cu, Zn, Mn, Fe, Ni) systems, the additions of Cu and Zn had no effect on the $D0_{22}$ structure of the binary $Al_3Hf$ and the additions of Mn, Fe and Ni produced the amorphous phase. Therefore it was considered that these ternary additions could not overcome the energy difference between $Ll_2$ and $D0_{22}$ structures in the $Al_3Hf$ intermetallic compound. In AL-12.5%M-25%Hf(M=Cu, Zn, Mn, Fe, Ni)systems, the additions of Cu and Zn did not affect the $Ll_2$ structure of the binary $Al_3Hf$ but the additions of oMn, Fe and Ni produced the amorphous phase as they did in AL-12.5%M-25%Ta systems. Therefore, it was considered that the Ni, Mn and Fe additions promote the formation of amorphous phase in $Al_3X$ intermetallic compounds.

  • PDF

Effect of Ca and Al Additions on the Magnetic Properties of Nanocrytalline Fe-Si-B-Nb-Cu Alloy Powder Cores

  • Moon, Sun Gyu;Kim, Ji Seung;Sohn, Keun Yong;Park, Won-Wook
    • Journal of Magnetics
    • /
    • v.21 no.2
    • /
    • pp.192-196
    • /
    • 2016
  • The Fe-Si-B-Nb-Cu alloys containing Ca and Al were rapidly solidified to thin ribbons by melt-spinning. The ribbons were ball-milled to make powders, and then mixed with 1 wt.% water glass and 1.5 wt.% lubricant. The mixed powders were burn-off, and then compacted to form toroidal-shaped cores, which were heat treated to crystallize the nano-grain structure and to remove residual stress of material. The characteristics of the powder cores were analyzed using a differential scanning calorimetry (DSC) and a B-H meter. The microstructures were observed using transmission electron microscope (TEM). The optimized soft magnetic properties (${\mu}_i$ and $P_{cv}$) of the powder cores were obtained from the Ca and Al containing alloys after annealing at $530^{\circ}C$ for 1 h. The core loss of Fe-Si-B-Nb-Cu-based powder cores was reduced by the addition of Ca element, and the initial permeability increased due to the addition of Al element.

MAGNETORESISTANCE OF NiFeCo/Cu/NiFeCo/FeMn MULTILAYERED THIN FILMS WITH LOW SATURATION FIELD

  • Bae, S.T.;Min, K.I.;Shin, K.H.;Kim, J.Y.
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.570-574
    • /
    • 1995
  • Magnetoresistance of NiFeCo/Cu/NiFeCo/FeMn uncoupled exchange biased sandwiches has been studied. The magnetoresistance change ratio, ${\Delta}R/R_{s}$ showed 4.1 % at a saturation field as low as 11 Oe in $Si/Ti(50\;{\AA})/NiFeCo(70\;{\AA})/Cu(23\;{\AA})/NiFeCo(70\;{\AA})/FeMn(150\;{\AA})/Cu(50\;{\AA})$ spin valve structure. In this system, the magnetoresistance was affected by interlayer material and thickness. When Ti and Cu were used as the interlayer material in this structure, maximum magnetoresistance change ratio were 0.32 % and 4.1 %, respectively. 6.1 % MR ratio was obtained in $Si/Ti(50\;{\AA})/NiFeCo(70\;{\AA})/Cu(15\;{\AA})/NiFeCo(70\;{\AA})/FeMn(150\;{\AA})/Cu(50\;{\AA})$ spin valve structure. The magnetoresistance change ratio decreased monotonically as the interlayer thickness increased. It was found that the exchange bias field exerted by FeMn layer to the adjacent NiFeCo layer was ~25 Oe, far smaller than that reported in NiFe/Cu/NiFe/FeMn spin valve structure(Dieny et. al., ~400 Oe). The relationship between the film texture and exchange anisotropy ha been examined for spin valve structures with Ti, Cu, or non-buffer layer.

  • PDF

A Microscopic Study on Treatment Mechanism of Acid Mine Drainage by Porous Zeolite-slag Ceramics Packed in a Column Reactor System (컬럼반응조 내 충진된 다공성 zeolite-slag 세라믹에 의한 산성광산배수의 처리기작에 대한 미세분석 연구)

  • Yim, Soo-Bin
    • Journal of Korean Society of Water Science and Technology
    • /
    • v.26 no.6
    • /
    • pp.13-26
    • /
    • 2018
  • This research was conducted to elucidate the removal mechanism of heavy metals and sulfate ion from acid mine drainage(AMD) by porous zeolite-slag ceramics (ZS ceramics) packed in a column reactor system. The average removal efficiencies of heavy metals and sulfate ion from AMD by the 1:3(Z:S) porous ZS ceramics in the column reactor under the HRT condition of 24 hours were Al 97.5%, As 98.8%, Cd 86.1%, Cu 96.2%, Fe 99.7%, Mn 64.1%, Pb 97.2%, Zn 66.7%, and $SO_4{^{2-}}$ 76.0% during 121 days of operation time. The XRD analysis showed that the ferric iron from AMD could be removed by adsorption and/or ion-exchange on the porous ZS ceramics. In addition it was known that Al, As, Cu, Mn, and Zn could adsorb or coprecipitate on the surface of Fe precipitates such as schwertmannite, ferrihydrite, or goethite. The EDS analysis revealed that Al, Fe, and Mn, which were of relatively high concentration in the AMD, would be adsorbed and/or ion-exchanged on the porous ZS ceramics and also exhibited that Al, Cu, Fe, Mn, and Zn could be precipitated as the form of metal hydroxide or sulfate and adsorbed or coprecipitated on the surface of Fe precipitates. The microscopic results on the porous ZS ceramics and precipitated sludge in a column reactor system suggested that the heavy metals and sulfate ion from AMD would be eliminated by the multiple mechanisms of coprecipitation, adsorption, ion-exchange as well as precipitation.