• Title/Summary/Keyword: Admixture Analysis

Search Result 180, Processing Time 0.021 seconds

Optimized Mixing Design of Carbon-Capturing and Sequestering Activated Blast-Furnace Slag Mortar by Response Surface Analysis (반응표면분석법에 의한 탄소포집 활성 고로슬래그 모르타르의 최적배합 도출에 관한 연구)

  • Jang, Bong Jin;Park, Cheol woo;Kim, Seung Won;Ju, Min Kwan;Park, Ki Tae;Lee, Sang Yoon
    • International Journal of Highway Engineering
    • /
    • v.15 no.6
    • /
    • pp.69-78
    • /
    • 2013
  • PURPOSES : In this study blast furnace slag, an industrial byproduct, was used with an activating chemicals, $Ca(OH)_2$ and $Na_2SiO_3$ for carbon capture and sequestration as well as strength development. METHODS : This paper presents the optimized mixing design of Carbon-Capturing and Sequestering Activated Blast-Furnace Slag Mortar. Design of experiments in order to the optimized mixing design was applied and commercial program (MINITAB) was used. Statistical analysis was used to Box-Behnken (B-B) method in response surface analysis. RESULTS : The influencing factors of experimental are water ratio, Chemical admixture ratio and Curing temperature. In the results of response surface analysis, to obtain goal performance, the optimized mixing design for Carbon-Capturing and Sequestering Activated Blast-Furnace Slag Mortar were water ratio 40%, Chemical admixture ratio 58.78% and Curing temperature of $60^{\circ}C$. CONCLUSIONS : Compared with previous studies of this experiment is to some extent the optimal combination is expected to be reliable.

Analysis of the influence of combined use of ferronickel slag fine powder and admixture on VR sewage pipe strength development (페로니켈슬래그 미분말 및 혼화재의 복합사용이 VR 하수관 강도발현에 미치는 영향분석)

  • Nam, Sang-Koo;Chung, Tae-Jun;Jo, Seol-Ah;Yoo, Jeong-Hwan;Park, Sang-Soon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.3
    • /
    • pp.214-221
    • /
    • 2018
  • In this paper, the effects of ferronickel slag powder and admixture on the strength of VR sewer pipe were analyzed. the substitution rate was tested as a variable, and the strength development was studied through the flexural strength, compressive strength and using SEM microscopic analysis. bending strength, compressive strength results and micro analysis using SEM showed the correlation in each case. the substitution rates were 20% and 30% relative to the mass of the OPC respectively, and were substituted according to a constant ratio of ferronickel slag fine powder and mixture. when the substitution ratio was 20%, the strength development was excellent. also, bending strength and compressive strength were the best when the ferronickel slag fine powder, quicklime, gypsum and calcium chloride were used as the admixture, dense microstructural patterns appeared. the possibility of progressive strength development is shown after 28 days.

Applicability analysis of carbondioxide conversion capture materials produced by desulfurization gypsum for cement admixture (시멘트 혼합재로서 정유사 탈황석고를 활용하여 제조한 탄산화물의 적용성 분석)

  • Hye-Jin Yu;Young-Jun Lee;Sung-Kwan Seo;Yong-Sik Chu;Woo-Sung Yum
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.33 no.2
    • /
    • pp.54-60
    • /
    • 2023
  • In this study, microstructure and basic property analysis of DG (Desulfurization gypsum) and CCMs (Carbondioxide conversion capture materials) made by reacting CO2 with DG were conducted to analyze applicability as a cement admixture. The main crystalline phases of DG were CaO and CaSO4, and CCMs were CaSO4, CaCO3, Ca(OH)2 and CaSO4·H2O. As a result of particle size analysis, the difference in average particle sizes between the two materials was about 7 ㎛. No major heavy metals were detected in the CCMs, and as a result o f TGA, the CO2 decomposition of CCMs was more than twice as high as that of DG. Therefore, it was judged that CCMs could be used as a cement admixture through optimization of manufacturing conditions. As a results of measuring the strength behavior of DG and CCMs mixture ratios, the long-term strength of CCMs-mixed mortar was higher, and this is due to the filler effect of CaCO3 in CCMs.

A Study on the Properties of Microbial Cementation Soil for Engineering Applicability (미생물 고결토의 공학적 특성 연구)

  • Oh, Jong-Shin;Hwang, Soung-Won;Kang, Hee-Bog;Kang, Keon-Soo;Kim, Jong-Ryeol
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2008.03a
    • /
    • pp.1332-1343
    • /
    • 2008
  • The purpose of this study was to investigate the feasibility of using sedimentation calcium carbonate production based on microorganism activities in the strength manifestation of various soil conditions including ground. For analysis and comparison of microbial cementation soil's strength, unconfined compression test was executed by each content of soil(S), water(W), microorganism(B), microorganism and deposit (BF), microorganism, admixture and deposit(BCF) at specimen. The result, the strength of SB(soil+microorganism) and SBF(soil+microorganism+deposit) increased about 8%, 15% than SW(soil+water). Also, initial strength increased. But the strength of SBC(soil+microorganism+admixture) and SBCF(soil+microorganism+deposit+admixture) increased about 71%, 115% than SW(soil+water). The results of the SEM analysis, leading to the formation of an adhesive substance layers at the surface and resulting in firm particle configuration. The XRD examination of the sediment resulting from the reaction between the microorganism and the deposit control agent confirmed the presence of a type of calcium carbonate ($CaCo_3$) vaterite, which affects soil strength formation, as well as sodium silicate, silicides and so forth. This indicates that microorganism plays an important role in the production of carbonate ($CaCo_3$), sodium silicate and silicides. It affects to revelation of ground strength.

  • PDF

Analytical Estimation of the Performance of Marine Concrete with Mineral Admixture (광물질 혼화재를 혼합한 해양 콘크리트의 해석적 성능 평가)

  • Lee, Bang-Yeon;Kwon, Seung-Jun;Kang, Su-Tae
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.4
    • /
    • pp.301-306
    • /
    • 2015
  • For the purpose of developing high performance marine concrete with improved crack resistance and durability, this analytical study aimed to estimate strength, hydration heat characteristics, and chloride attack resistance of concrete with mineral admixture. Ground granulated furnace slag and fly ash were considered for mineral admixture. The replacement of ground granulated furnace slag and fly ash considered in the analysis was in the range of 0~70% and 0~40 %, respectively. The analysis results indicated that both ground granulated furnace slag and fly ash decreased compressive strength, and the effect of adding ground granulated furnace slag on mitigation of hydration heat was limited whereas fly ash had an noticeable influence on it. It was also found that the replacement with ground granulated furnace slag enhanced the chloride attack resistance but fly ash deteriorated the resistance. From the analytical studies, It could be expected that a ternary blended cement composition with proper amount of ground granulated furnace slag and fly ash might be effective to control crack resistance as well as chloride attack resistance of marine concrete.

Experimental Study on the Properties of Concrete by the Kinds of Admixture and the Replacement Ratios of Activated Hwangtoh (혼화재 종류 및 활성황토 대체율별 콘크리트의 공학적 특성에 관한 실험적 연구)

  • 최희용;김무한;김문한;황혜주;최성우
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.2
    • /
    • pp.123-129
    • /
    • 2001
  • Pozzolan is to improve the strength and the durability of concrete as a result of the pozzolanic reaction, Broadly speaking, pozzolanic materials can be artificial materials, such as slica fume and fly ash, and natural material, such as rice husk ash, clay, volcanic ash, clayish pozzolan. Hwangtoh is a mineral which belongs to a group of matakaolin, especially halloysite, and the main elements is SiO$_2$, Al$_2$O$_3$, Fe$_2$O$_3$. The purpose of this study is to examine the application of Hwangtoh for the concrete admixtures, the composition of this study is shown as follows. Chapter I is analysis for properties of concrete as the kinds of admixture, and Chapter H is analysis for properties of concrete as the replacement ratio of activated Hwangtoh. As a result of this study, Hwangtoh is found to have high practical use as pozzolanic material, and the pertinent range of replacement ratios of Hwangtoh on cement are 10∼20 %.

Utilization of waste fine tailing as cement mineral admixture (폐광미 미립분의 시멘트 혼화재로의 활용)

  • An, Yang-Jin;Yu, Seung-Wan;Mun, Kyoung-Ju;Park, Won-Chun;Soh, Yang-Seob
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2005.05b
    • /
    • pp.381-384
    • /
    • 2005
  • The purpose of this study reutilization of waste fine tailing (FT) as admixture for cement and concrete. Various admixtures were made of Fine tailings and 2 Types of OPC, fly-ash and blast furnace slag. Cement mortars and concrete with FT are tested for fluidity and compressive strength. Also, the hydration reactivity of cement mortar with FT was examined by XRD and SEM morphology analysis. This work showed that the waste fine tailing could be effectively utilized as replacement materials of cement without any decrease in the strength if we can control the blaine of materials like cement, blast furnace slag and fly ash.

  • PDF

A Fluidity Experiment of Pre-Mix Cement for Dispersibility Improvement of Mineral Admixture (광물질 혼화재의 분산성 향상을 위한 프리믹스 시멘트의 유동성 실험)

  • Han, Cheon-Goo;Lee, Hai-Ill;Noh, Sang-Kyun;Kim, Ki-Hoon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.2
    • /
    • pp.90-96
    • /
    • 2009
  • The high rising building construction makes increasing the requirement of high strength concrete. Especially, the workability analysis is related with dispersion of admixture such as SF for improving strength and FA, BS for reducing construction cost and improving durability of Ultra High Strength Concrete which has over 100 MPa of compressive strength is very important. Precisely, decreases dispersion because of lumping situation of each admixture and it causes the workability of admixture is decreased. Therefore, the workability of cement paste is tested for analyze effects of pre-mixed cement for solving those problems with it to this research. The summary of the results are like below. First of all, OBS is increasing workability more than OFS. This result causes that the glassy surface of BS in the OBS is increasing workability and the absorption of admixture of FA in the OFS is decreasing workability. In the case of mixing methods, pre-mixing method is increasing workability more than normal one. This result shows that the normal mixing method is bad dispersion of binders. The other side, the pre-mixing method is good. Furthermore, depending on the mixing time, according to the increasing mixing time such as 30, 60, and 120 seconds, the dispersion of binders and workability turns better.

  • PDF

Quantitative Assessment of Infrared Analysis of Concrete Admixtures

  • Casale, Anthony J. III;Doukakis, Johanna;Najm, Husam;Davis, Kimberly
    • International Journal of Concrete Structures and Materials
    • /
    • v.7 no.3
    • /
    • pp.203-214
    • /
    • 2013
  • This study investigates quantitative methods for assessment of infrared analysis of concrete admixtures using correlation coefficients by performing IR scans following the ASTM C494/C494M-11 specifications. In order to achieve this goal, numerous IR scans were performed on specimens supplied by the manufacturer from different batches to ensure uniformity and equivalency. These scans were then analyzed to create correlation coefficients for each admixture. The correlation coefficients were used to quantitatively evaluate and interpret IR Scans of job samples. The study focused on 23 most commonly used concrete admixtures by the New Jersey Department of Transportation (NJDOT). They include air-entrainers, accelerators, retarders, water reducers, and other combinations of these admixtures. Their correlation coefficients were established by analyzing a total of 12 scans of each admixture from three different batches supplied by the manufacturer at different time intervals. In order to validate the obtained correlation coefficients and establish a target correlation, job samples were tested and compared to the obtained correlations. The study also evaluated the effects of drying time and using different types of KBr on correlation coefficients.

Estimation and Analysis of Slump Loss in Ready Mixed Concrete (레드믹스트 콘크리트의 슬럼프손실량(損失量)의 추정(推定) 및 슬펌프손실(損失)에 영향을 미치는 요인분석(要因分析))

  • Moon, Han Young;Choi, Jae Jin
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.6 no.2
    • /
    • pp.23-34
    • /
    • 1986
  • Multiple regression equation was derived for estimation of slump loss in ready mixed concrete and usefulness of the equation was verfied by field test. Factors affecting slump loss were examined and analyzed for transport distance and transport time of ready mixed concrete. The analysis showed that wait and discharge time of ready mixed concrete in job site caused difficulty in the slump control. To determine the influence of the other factors such as mix proportion, temperature of concrete, and dosage of admixture, experimental tests were performed. Generally, there was no significant difference in slump loss according to cement content and initial slump level. For one retarder, more slump loss was found, but difference according to dosage of admixture was not recognized.

  • PDF