• 제목/요약/키워드: Adhesive systems

검색결과 257건 처리시간 0.023초

The effect of different adhesive system applications on push-out bond strengths of glass fiber posts

  • Kivanc, Bagdagul Helvacioglu;Arisu, Hacer Deniz;Uctasli, Mine Betul;Okay, Tufan Can
    • The Journal of Advanced Prosthodontics
    • /
    • 제5권3호
    • /
    • pp.305-311
    • /
    • 2013
  • PURPOSE. Over the past years, the adhesion of fiber posts luted with simplified adhesive systems has been a matter of great interest. The aim of this study was to assess the post retentive potential of a self-adhesive resin cement using different adhesive systems to compare the push-out bond strengths of fiber posts. MATERIALS AND METHODS. The post spaces of 56 mandibular premolar roots were prepared and divided into 4 experimental groups and further divided into 2 subgroups according to testing time (n=7). The fiber posts (Rely X Fiber Post) were luted with a self-adhesive resin cement (RelyX Unicem) and one of the following adhesive systems: no adhesive, a total-etch adhesive resin (Single Bond), a two-step self-etch adhesive resin (Clearfil SE Bond) and a one-step self-etch adhesive resin (Clearfil S3 Bond). Each root was cut horizontally, and 1.5 mm thick six root segments were prepared. Push-out tests were performed after one week or three months (0.5 mm/min). Statistical analysis were performed with three-way ANOVA (${\alpha}$=.05). RESULTS. Cervical root segments showed higher bond strength values than middle segments. Adhesive application increased the bond strength. For one week group, the total-etch adhesive resin Single Bond showed higher bond strength than the self-adhesive resin cement RelyX Unicem applied without adhesive resin at middle region. For 3 months group, the two-step self-etch adhesive resin Clearfil SE Bond showed the highest bond strength for both regions. Regarding the time considered, Clearfil SE Bond 3 months group showed higher bond strength values than one week group. CONCLUSION. Using the adhesive resins in combination with the self-adhesive resin cement improves the bond strengths. The bond strength values of two-step self-etch adhesive resin Clearfil SE Bond improved as time passes.

미세-전단 결합 강도 시험을 이용한 상아질 접착제와 수복용 복합 레진의 호환성에 관한 연구 (IN VITRO MICRO-SHEAR BOND STRENGTH OF FIVE COMPOSITE RESINS TO DENTIN WITH FIVE DIFFERENT DENTIN ADHESIVES)

  • 정진호;노병덕
    • Restorative Dentistry and Endodontics
    • /
    • 제29권4호
    • /
    • pp.353-364
    • /
    • 2004
  • The purpose of this study was to compare and to evaluate the combination use of 5 kinds of dentin adhesive systems and 5 kinds of composite resins using micro-shear bond test. Five adhesive systems (Prime & Bond NT (PBN). Onecoat bond (OC), Excite (EX), Syntac (SY), Clearfil SE bond (CS)) and five composite resins (Spectrum (SP), Synergy Compact (SC), Tetric Ceram (TC), Clearfil AP-X (CA), Z100 (Z1)) were used for this study ($5{\;}{\times}{\;}5{\;}={\;}25group$, n =14/group). The slices of horizontally sectioned human tooth were bonded with each bonding system and each composite resin, and tested by a micro-shear bond strength test. These results were analyzed statistically. The mean micro-shear bond strength of dentin adhesive systems were in order of CS (22.642 MPa), SY (18.368 MPa), EX (14.599 MPa). OC (13.702 MPa). PBN (12.762 MPa). The mean bond strength of self-etching primer system group (CS, SY) in dentin was higher than that of self-priming adhesive system groups (PBN, EX, OC) significantly (P<0.05). The mean bond strength of composite resins was in order of SP (19.008 MPa), CA (17.532 MPa). SC (15.787 MPa), TC (15.068 MPa). Z1 (14.678 MPa). Micro-shear bond strength of SP was stronger than those of other composite resins significantly (P < 0.05). And those of TC and Z1 were weaker than other composite resins significantly (P < 0.05). No difference was found in micro-shear bond strength of composite resin in self-etching primer adhesive system groups (CS, SY) statistically. However, there was significant difference of micro-shear bond strength of composite resin groups in self-priming adhesive systems group (PBN, EX, OC). The combination of composite resin and dentin adhesive system recommended by manufacturer did not represent positive correlation. It didn't seem to be a significant factor.

신발 접착제 도포 시스템을 위한 CAD 기반 로봇 오프라인 프로그래밍 (CAD Based Robot Off-line Programming for Shoe Adhesive Application System)

  • 윤중선;차동혁;김진영
    • 제어로봇시스템학회논문지
    • /
    • 제10권7호
    • /
    • pp.643-648
    • /
    • 2004
  • Most of shoes manufacturing processes are not yet automated, which puts restrictions on the increase of productivity. Among them, adhesive application processes particularly are holding the most workers and working hours. In addition, its working conditions are very poor due to the toxicity of adhesive agents. In case of automating adhesive application processes by using robots, the robot teaching by playback is difficult to produce high productivity because the kinds of shoes to be taught mount up to several thousands. Therefore, it is essential to generate the robot working paths automatically according to the kind, the size, and the right and left of shoes, and also to teach them to the robot automatically. This study deals with automated adhesive spraying to shoe outsoles and uppers by using a robot, and develops the program to generate three-dimensional robot working paths off-line based on CAD data. First, the three-dimensional data of an outsole outline or an upper profiling line are extracted from the two-dimensional CAD drawing file or the three-dimensional scanner. Next, based on the extracted data and the nozzle conditions for adhesive spraying, a robot working path is generated automatically. This research work is the core in automating adhesive spraying processes, and will do much for increasing productivity of shoes manufacturing.

Microleakage and characteristics of resin-tooth tissues interface of a self-etch and an etch-and-rinse adhesive systems

  • Xuan Vinh Tran;Khanh Quang Tran
    • Restorative Dentistry and Endodontics
    • /
    • 제46권2호
    • /
    • pp.30.1-30.13
    • /
    • 2021
  • Objectives: This study was conducted to compare the microleakage and characteristics of the resin-tooth tissue interface between self-etch and etch-and-rinse adhesive systems after 48 hours and 3 months. Materials and Methods: 40 extracted premolar teeth were randomly divided into 2 groups: 1-step self-etch adhesive system - OptibondTM All-In-One, and 2-step etch-and-rinse adhesive system - AdperTM Single Bond 2. Both groups were subjected to 500 thermocycles (5℃-55℃) before scanning electron microscope (SEM) analysis or microleakage trial at 48-hour and 3-month time periods. Results: SEM images showed the hybrid layer thickness, diameter, and length of resin tags of the self-etch adhesive (0.42 ± 0.14 ㎛; 1.49 ± 0.45 ㎛; 16.35 ± 14.26 ㎛) were smaller than those of the etch-and-rinse adhesive (4.39 ± 1.52 ㎛; 3.49 ± 1 ㎛; 52.81 ± 35.81 ㎛). In dentin, the microleakage scores of the 2 adhesives were not different in both time periods (48 hours/3 months). However, the microleakage score of etch-and-rinse adhesive increased significantly after 3 months (0.8 ± 0.63 and 1.9 ± 0.88, p < 0.05). Conclusions: The self-etch adhesive exhibited better long-term sealing ability in dentin when compared to that of the etch-and-rinse adhesive. The greater hybrid layer thickness and dimensions of resin tags did not guarantee reliable, long-lasting sealing in the bonding area.

Adhesive systems applied to dentin substrate under electric current: systematic review

  • Carolina Menezes Maciel;Tatiane Cristina Vieira Souto;Barbara de Almeida Pinto;Lais Regiane Silva-Concilio;Kusai Baroudi;Rafael Pino Vitti
    • Restorative Dentistry and Endodontics
    • /
    • 제46권4호
    • /
    • pp.55.1-55.9
    • /
    • 2021
  • Objectives: The purpose of this systematic review was to collect and discuss the technique of adhesive systems application on dentin substrate under electric current. Materials and Methods: The first search strategy was based on data available at PubMed, LILACS, Scielo, Scopus, and Cochrane Library, using a combination of descriptors such as "dentin bond agents OR adhesive system AND electric current OR electrobond" or "dentin bonding agents OR dentin bonding agent application OR adhesive system AND electric current OR electrobond", with no limit regarding the publication year. The second search strategy was based on the articles' references found previously. An additional search strategy was applied that concerned the proposed theme in the SBU-UNICAMP (Unicamp's Library System Institutional Repository). Results: Twelve studies published between 2006 and 2020 were found. The analyses of the selected studies showed that the use of electric current during adhesive systems application on dentin, whether conventional or self-conditioning, increases resinous monomer infiltration in the dentin substrate, which improves the hybridization processes and the bond strength of the restorative material to dentin. Conclusions: Despite the favorable results related to the use of this technique, there is still no specific protocol for the application of adhesive systems under electric current.

Au-Ag-Cu-Pd합금과 복합레진간의 접착결합강도에 관한 연구 (A STUDY ON THE ADHESIVE BOND STRENGTH OF COMPOSITE RESIN TO Au-Ag-Cu-Pd ALLOY)

  • 설영훈;정창모;전영찬
    • 대한치과보철학회지
    • /
    • 제32권3호
    • /
    • pp.378-395
    • /
    • 1994
  • The purpose of this study was to investigate the effect of various metal surface treatments and adhesive systems on the flexural bond strength of composite resin to Au-Ag-Cu-Pd alloy. The specimens were divided into nine groups by the combinations of surface treatment methods and adhesive systems. The types of surface treatment in this study were alumina blasting only, alumina blasting-Sn plating, alumina blasting-heating and three kinds of adhesive system used in this study were Silicoater system(Heraeus Kulzer GmbH,Germany), Superbond C & B(Sun Medical Co.,Ltd.,Japan) and Cesead opaque primer(Kurary Co.,Ltd.,Japan). After surface treatments and adhesive systems were applied, each specimen was built up with Dentacolor composite resin (Heraeus Kulzer GmbH,Germany). Four-point flexural bond strength was measured by Instron universal testing machine (Model 4301,U.S.A.) and modes of failure were observed by SEM(JEOL,SSM-840A,Japan). The obtained results were as follows: 1. The group that was bonded with Superbond C & B after alumina blasting-heating shelved the highest bond strength with significant difference among the groups, except the group with Cesead opaque primer after alumina blasting-Sn plating(P<0.05). 2. In the groups bonded with Cesead opaque primer, there was significant difference only in the bond strength between the alumina blasting-Sn plating group and alumina blasting group, where the former showed a higher bond strength(P<0.05). 3. In the groups bonded with Silicoater system, there were no significant differences in bond strength regardless of the surface treatment method(P<0.05). 4. In SEM evaluation, the groups of high bond strength, especially bonded with Superbond C & B after alumina blasting-heating and Cesead opaque primer after alumina blasting-Sn plating, revealed mainly cohesive-adhesive failure, whereas the others showed the tendency of adhesive failure.

  • PDF

시멘트제법에 대한 우레탄 접착제의 품질 특성에 관한 연구 (The Study on the Quality Characteristic of Urethane Adhesive on the Cementing Process)

  • 양대용;김운섭;이종석;김영채;김형진;문세기
    • 산업경영시스템학회지
    • /
    • 제19권38호
    • /
    • pp.105-115
    • /
    • 1996
  • According to the manual of shoemaking, the urethane adhesive for dress shoe applicable to the cementing process in KS G 3116 has been steadily developed. The evaluation test result of urethane adhesive, which is a mathematical model of men's shoe on shoemaking, is presented. Also, the quality test result of urethane adhesive, which is a list of experiment for field application and a model of assembling component in each unit process is introduced.

  • PDF

Antibacterial effect of self-etching adhesive systems on Streptococcus mutans

  • Kim, Seung-Ryong;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • 제39권1호
    • /
    • pp.32-38
    • /
    • 2014
  • Objectives: In this study, we evaluated the antibacterial activity of self-etching adhesive systems against Streptococcus mutans using the agar diffusion method. Materials and Methods: Three 2-step systems, Clearfil SE Bond (SE, Kuraray), Contax (CT, DMG), and Unifil Bond (UnB, GC), and three 1-step systems, Easy Bond (EB, 3M ESPE), U-Bond (UB, Vericom), and All Bond SE (AB, BISCO) were used. 0.12% chlorhexidine (CHX, Bukwang) and 37% phosphoric acid gel (PA, Vericom) were used as positive controls. Results: The antibacterial activity of CHX and PA was stronger than that of the other groups, except SE. After light activation, the inhibition zone was reduced in the case of all 2-step systems except CT. However, all 1-step systems did not exhibit any inhibition zone upon the light activation. Conclusions: SE may be better than CT or UnB among the 2-step systems with respect to antibacterial activity, however, 1-step systems do not exhibit any antibacterial activity after light curing.

치아 맹출 유무에 대한 자가부식 접착제에 의한 교정용 부착장치의 접착강도 (Effects of conventional and self-etching adhesive systems on bond strength of orthodontic attachments bonded to erupted and unerupted teeth)

  • Nur, Metin;Uysal, Tancan;Yesilyurt, Cemal;Bayram, Mehmet
    • 대한치과교정학회지
    • /
    • 제40권4호
    • /
    • pp.267-275
    • /
    • 2010
  • 이번 연구의 목적은 맹출 또는 미맹출된 치아에 교정용 버튼을 부착 후 자가부식 접착제(self-etching adhesive)의 사용 유무에 대한 전단결합강도(shear bond strength)와 탈락모드를 비교하고자 함이다. 각각 84개의 맹출 또는 미맹출된 제3대구치를 사용하였다. 각각 치아의 협측면을 다음의 부착시스템 그룹으로 할당하였다. A, 기존방식: 1, Transbond XT (3M Unitek); 2, Prime & Bond NT (Dentsply/Caulk); 3, Single Bond (3M ESPE); B, 자가부식 접착제; 4, Clearfil SE Bond (Kuraray); 5, Transbond Plus (3M Unitek); 6, Clearfil S3 (Kuraray); 7, G Bond (GC). 부착물의 전단강도와 접착제 잔류지수를 측정하였으며 결과값은 ANOVA와 independent t-test 및 chi-square 검증을 통해 분석되었다. 맹출 또는 미맹출된 치아의 전단결합강도를 비교하였을 때 Clearfil SE와 G Bond에서 유의한 차이가 관찰되었다. Single Bond를 제외한 모든 접착시스템에서 맹출보다는 미맹출 치아면에서 높은 접착강도가 관찰되었다. 기존 접착제를 사용하는 경우 맹출 또는 미맹출 치아에 대한 접착강도에는 차이가 없을 수 있다. 그러나 임상의사는 사용 전에 self-etching system의 종류를 고려할 필요가 있다.

혼성층의 두께가 three-step과 self-etching 상아질 접착제의 미세인장결합강도에 미치는 효과 (THE EFFECT OF HYBRID LAYER THICKNESS ON MICROTENSILE BOND STRENGTH OF THREE-STEP AND SELF-ETCHING DENTIN ADHESIVE SYSTEMS)

  • 이혜정;박정길;허복
    • Restorative Dentistry and Endodontics
    • /
    • 제28권6호
    • /
    • pp.491-497
    • /
    • 2003
  • The purpose of this study was to evaluate the correlation between hybrid layer thickness and bond strength using confocal laser scanning microscope and microtensile bond strength test of two adhesive systems. The dentin surface of human molars. sectioned to remove the enamel from the occlusal surface. Either Scotchbond Multi-Purpose(3M Dental Product, St. Paul, MN, U.S.A) or Clearfil SE Bond (Kuraray, Osaka, Japan) was bonded to the surface. and covered with resin-composite. The resin-bonded teeth were serially sliced perpendicular to the adhesive interface to measure the hybrid layer thickness by confocal laser scanning microscope. The specimen were trimmed to give a bonded cross-sectional surface area of $1\textrm{mm}^2$, then the micro-tensile bone test was performed at a cross head speed of 1.0 mm/min. All fractured surfaces were also observed by stereomicroscope. There was no significant differences in bond strengths the materials(p>0.05). However. the hybrid layers of three-step dentin adhesive system, SM, had significantly thicker than self-etching adhesive system. CS(p<0.05). Pearson's correlation coefficient showed no correlation between hybrid layer thickness and bond strengths(p>0.05). Bond strengths of dentin adhesive systems were not dependent on the thickness of hybrid layer.