• 제목/요약/키워드: Activated hwangtoh concrete

검색결과 12건 처리시간 0.018초

활성황토를 사용한 콘크리트의 염소이온 침투 저항성에 관한 실험적 연구 (Experimental Study on the Resistance of Chloride Infiltration of Concrete Using Activated Hwangtoh Admixture)

  • 이강우;장종호;최희용;구자술;황혜주;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 가을 학술발표회 논문집
    • /
    • pp.781-786
    • /
    • 2001
  • The Salt attack is one of the primary factors that cause the deterioration of durability in steel reinforced concrete structure. And to depreciate the deterioration from the Salt attack in concrete structure, pozzolanic materials are used widely in recent years. In this study, experiments about the resistance of chloride infiltration of concrete according to the replacement rations of Activated Hwangtoh and various pozzolanic materials(silica fume, fly ash, blast furnace slag and non Activated/Activated Hwangtoh) are performed and the results of this study were shown as follows; 1) As the replacement ratios of Activated Hwangtoh were getting higher, the strength of concrete was increased and in case of various pozzolanic materials, strength of Activated Hwangtoh in specimen was better than that of fly ash, blast furnace slag and non Activated Hwangtoh. 2) As the replacement ratios of Activated Hwangtoh were getting higher, the resistance of chloride infiltration of concrete was increased and in case of various pozzolanic materials, silica fume is better than any other pozzolanic materials and Activated Hwangtoh was better than that of fly ash, blast furnace slag and non Activated Hwangtoh.

  • PDF

활성 황토 콘크리트 보의 전단 및 부착 강도 (Shear and Bond Strength of Activated Hwangtoh Concrete Beam)

  • 이남곤;박홍근;황혜주
    • 콘크리트학회논문집
    • /
    • 제22권5호
    • /
    • pp.685-694
    • /
    • 2010
  • 지금까지 환경 친화적 재료로서 황토에 관한 연구는 포틀랜드 시멘트를 부분적 대체하거나, 완전 대체하는 연구로 진행되어 왔다. 기존의 대부분의 연구에서는 압축강도, 건조수축, 크리프 등 황토 콘크리트의 역학적 성질에 초점이 맞춰졌다. 이 연구에서는 황토 콘크리트로 제작된 보 실험체의 전단강도를 실험하였다. 또한 황토 콘크리트에 정착된 인장 철근의 부착강도를 실험하였다. 이번 실험에서 시멘트를 20% 대체하는 활성 황토와 시멘트를 100% 대체하는 활성 황토를 사용한 콘크리트가 사용되었다. 실험 결과, 시멘트 20% 대체 활성 황토와 무시멘트 활성 황토 콘크리트 보의 전단 강도는 일반 포틀랜드 시멘트 콘크리트 보와 동등하였다. 반면에, 무시멘트 활성 황토 콘크리트의 부착 강도는 일반 포틀랜드 시멘트 콘크리트보다 작았다.

활성 황토 콘크리트 보의 휨 성능 (Flexural Performance of Activated Hwangtoh Concrete Beam)

  • 이남곤;황혜주;박홍근
    • 콘크리트학회논문집
    • /
    • 제22권4호
    • /
    • pp.567-574
    • /
    • 2010
  • 지금까지 환경 친화적 재료로서 황토에 관한 연구는 포틀랜드 시멘트를 부분적 대체하거나, 완전 대체하는 연구로 진행되어 왔다. 기존의 대부분의 연구에서는 압축강도, 건조수축, 크리프 등 황토 콘크리트의 역학적 성질에 초점이 맞춰졌다. 이 연구에서는 황토 콘크리트로 제작된 보 실험체의 휨 성능을 실험하였다. 이번 실험에서는 시멘트를 20% 대체하는 활성 황토를 사용한 콘크리트와 시멘트를 100% 대체하는 활성 황토 콘크리트가 사용되었다. 단순보 실험은 2점 정적 재하 하중으로 실험하였다. 휨 강도, 균열 모멘트, 처짐, 연성도 등의 결과를 일반 포틀랜드 시멘트 콘크리트로 제작된 보의 실험 결과와 비교하였다.

혼화재 종류 및 활성황토 대체율별 콘크리트의 공학적 특성에 관한 실험적 연구 (Experimental Study on the Properties of Concrete by the Kinds of Admixture and the Replacement Ratios of Activated Hwangtoh)

  • 최희용;김무한;김문한;황혜주;최성우
    • 콘크리트학회논문집
    • /
    • 제13권2호
    • /
    • pp.123-129
    • /
    • 2001
  • 본 연구에서는 천연재료인 황토의 활용성을 넓히기 위해, 황토를 혼화재로 사용한 경우 혼화재 종류 및 황토 대체율에 따른 콘크리트의 기초물성을 비교.검토하였다. 연구 결과, 황토를 사용할 경우 유동성은 다소 저하하는 것으로 나타났으며, 혼화재를 대체하지 않은 콘크리트에 비해 공기량도 다소 저하하는 것으로 나타나, 고성능 감수제의 선택성 및 AE제의 사용에 의한 공기량 보정이 필요할 것으로 판단된다. 황토와 시멘트간의 포졸란반응에 의한 강도발현성상을 검토한 결과, 황토를 콘크리트용 혼화재로서 사용하기 위해서는 가열에 의한 활성화공정이 필요한 것으로 나타났으며, 활성황토를 콘크리트용 혼화재료로 사용할 경우 활발한 포졸란반응에 의해 압축 강도 발현이 플레인콘크리트보다 높게 나타나, 건설 신재료로서의 황토의 개발이 가능할 것으로 사료된다. 활성황토의 대체율에 따른 콘크리트의 특성은 대체율이 증가할수록 강도발현수준이 높게 나타났으나, 대체율 30%의 경우 무혼입에 비해 강도가 저하하는 것으로 나타나, 활성황토의 적정 대체율에 대한 보다 심도 있는 연구가 필요할 것으로 사료되며, 본 연구의 범위에서 활성황토의 적정 대체율의 범위는 10~20%내외에 존재할 것으로 사료된다.

Mechanical Properties of Hwangtoh-Based Alkali-Activated Concrete

  • Yang, Keun-Hyeok;Hwang, Hey-Zoo;Lee, Seol
    • Architectural research
    • /
    • 제11권1호
    • /
    • pp.25-33
    • /
    • 2009
  • This study presents the testing of 15 hwangtoh-based cementless concrete mixes to explore the significance and limitations of the development of eco-friendly concrete without carbon dioxide emissions while maintaining various beneficial effects. Hwangtoh, which is a kind of kaolin, was incorporated with inorganic materials, such as calcium hydroxide, to produce a cement-less binder. The main variables investigated were the water-to-binder ratio and fine aggregate-to-total aggregate ratio to ascertain the reliable mixing design of hwangtoh-based cementless concrete. The variation of slump with elapsed time was recorded in fresh concrete specimens. Mechanical properties of hardened concrete were also measured: including compressive strength gain, splitting tensile strength, moduli of rupture and elasticity, stress-strain relationship, and bond resistance. In addition, mechanical properties of hwangtoh-based cement-less concrete were compared with those of ordinary portland cement (OPC) concrete and predictions obtained from the design equations specified in ACI 318-05 and CEB-FIP for OPC concrete, wherever possible. Test results show that the mechanical properties of hwangtoh-based concrete were significantly influenced by the water-to-binder ratio and to less extend by fine aggregate-to-total aggregate ratio. The moduli of rupture and elasticity of hwangtoh-based concrete were generally lower than those of OPC concrete. In addition, the stress-strain and bond stress-slip relationships measured from hwangtoh-based concrete showed little agreement with the design model specified in CEB-FIP. However, the measured moduli of rupture and elasticity, and bond strength were higher than those given in ACI 318-05 and CEB-FIP. Overall, the test results suggest that the hwangtoh-based concrete shows highly effective performance and great potential as an environmental-friendly building material.

화학적 침해를 받은 알칼리활성 황토콘크리트의 응력-변형률 관계 (Stress-Strain Relationship of Alkali-Activated Hwangtoh Concrete under Chemical Attack)

  • 문주현;양근혁
    • 한국건축시공학회지
    • /
    • 제14권2호
    • /
    • pp.170-176
    • /
    • 2014
  • 본 연구에서는 알칼리활성 황토콘크리트의 응력-변형률 관계에 대한 화학적 침식의 영향을 평가하였다. 배합의 주요변수는 물-결합재비와 공기량이다. 알칼리활성 황토콘크리트의 응력-변형률 관계는 재령 28일 이후 침지일이 0, 7, 28, 56 및 91일일 때 측정하였다. 실험결과를 기반하여, 화학적 침식하에서 감소된 알칼리활성 황토콘크리트의 압축강도 모델이 제시되었다. 또한, 화학적 침식하에서 알칼리활성 황토콘크리트의 응력-변형률 관계는 공기량과 화학용액에 침지된 일수에 현저한 영향을 받았는데, 침지일수에서 탄성계수의 저하는 동일한 압축강도 저하비율에 비해 더 컸다. 결과적으로 CEB-FIP 기준의 예측모델은 화학적 침식하에서 측정된 응력-변형률 관계와 잘 일치하지 않았다.

PVA 섬유보강 황토 콘크리트에 대한 GFRP 보강근의 부착성능에 관한 실험적 연구 (An Experimental Study on the Bond Characteristic of GFRP Bars in PVA Fiber Reinforced Activated Hwangtoh Concrete)

  • 박미래;김승훈
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제21권1호
    • /
    • pp.134-141
    • /
    • 2017
  • 시멘트 생산 과정에서 생성되는 이산화탄소 배출량을 감소시키기 위하여 시멘트를 대체할 수 있는 건축 재료 개발에 많은 연구가 진행되어왔다. 시멘트 대체재로 사용될 수 있는 활성 황토는 $850^{\circ}C$에서 소성 과정을 거쳐 제작된다. Poly-Vinyl Alcohol(PVA) 섬유와 GFRP 보강근은 활성 황토 콘크리트의 균열 문제를 해결하기 위하여 사용된다. 본 논문은 PVA 섬유 보강 활성 황토 콘크리트에 대하여 인발 하중에 따른 GFRP 보강근의 부착 성능을 평가하기 위한 실험 연구를 나타내고 있다. 실험 결과, 황토가 치환된 PVA 보강 및 무보강 실험체들의 평균 부착 응력 계수가 2.27~2.48로 나타났으며, 부착 응력 계수가 PVA 섬유 보강 유무 및 황토 치환율에 크게 영향을 받지 않는 것으로 나타났다. 그리고 부착 길이가 길어질수록 부착 강도는 저하되었다.

알칼리활성 천연황토 결합제 개발을 위한 기초연구 (Preliminary Study for the Development of Alkali Activated Natural Hwangtoh Binder)

  • 김백중;김준환;이종구;강경인
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2010년도 춘계 학술대회 제22권1호
    • /
    • pp.389-390
    • /
    • 2010
  • 본 연구는 콘크리트 결합재로 사용되는 시멘트의 대체재 개발을 위해 천연황토에 수산화나트륨(NaOH) 수용액과 액상 규산나트륨($Na_2SiO_3$)을 혼합한 후 $60^{\circ}C$에서 알칼리 활성화하여 경화시켜 강도 발현 양상을 분석한 천연황토 콘트리트 결합재 개발을 위한 기초연구이다.

  • PDF

재생 PET섬유가 혼입된 황토 콘크리트 보의 휨 거동 (Flexural Behavior of Hwangtoh Concrete Beams with Recycled PET Fiber)

  • 김성배;남진원;이나현;김장호;최홍식
    • 콘크리트학회논문집
    • /
    • 제20권5호
    • /
    • pp.619-626
    • /
    • 2008
  • 환경문제에 대한 높은 관심으로 친환경 콘크리트의 개발을 위해 많은 연구가 수행되어지고 있으며, 특히 콘크리트 배합 시 시멘트 사용량을 줄이기 위한 노력이 계속되고 있다. 시멘트 사용량을 줄이기 위한 방법으로 고로슬래그, 플라이애쉬, 메타카올린 등 포졸란반응재료들이 혼화재료로 많이 사용되고 있다. 우리나라 전역에 널리 매장되어 있는 황토는 친환경 재료로서 황토를 활성화시킨 활성황토는 포졸란반응을 하는 메타카올린계의 일종으로 콘크리트의 혼화재료로 활용성이 증가하고 있다. 또한 재생 PET섬유는 폐 PET병을 재활용하여 만든 친환경재료로서 콘크리트에 혼입되어 미세균열을 제어하는 역할을 한다. 하지만 보강섬유를 혼입한 콘크리트에 대한 연구는 아직도 미비한 실정이고 활성황토를 혼화재로 사용한 철근 황토 콘크리트의 경우 활성황토 혼화재의 포졸란반응과 보강섬유의 보강 효과가 복합적으로 나타날 것으로 판단된다. 따라서 본 연구에서는 에너지 절약 차원에서의 친환경 재료인 활성황토와 재생 PET 섬유를 혼입한 철근콘크리트 보의 거동 특성을 확인하기 위하여 재생 PET섬유를 혼입한 철근 황토콘크리트 보 시험체를 제작하여 휨 거동을 수행하였다.

Durability and mechanical performance in activated hwangtoh-based composite for NOx reduction

  • Kim, Hyeok-Jung;Park, Jang-Hyun;Yoon, Yong-Sik;Kwon, Seung-Jun
    • Advances in concrete construction
    • /
    • 제11권4호
    • /
    • pp.307-314
    • /
    • 2021
  • Activated hwangtoh (ACT) is a natural resource abundant in South Korea, approximately 15.0% of soil. It is an efficient mineral admixture that has activated pozzolanic properties through high-temperature heating and rapid cooling. The purpose of this study is to improve a curb mixture that can reduce NOx outside and investigate durability performance. To this end, mortar curb specimens were manufactured by replacing OPC with ACT. The ACT substitution ratios of 0.0, 10.0, and 25.0% were considered, and mechanical and durability tests on the curb specimens were conducted at 28 and 91 days of age. Steam curing was carried out for three days for the production of curbs, which was very effective to strength development at early ages. The reduction in strength at early ages could be compensated through this process, and no significant performance degradation was evaluated in the tests on chloride attack, carbonation, and freezing and thawing. The mortar curb with an ACT of 10.0~25.0% replacement ratio exhibited clear NOx reduction through photocatalytic (TiO2) treatment. This is due to the increase in physical absorption through surface absorption and the photocatalyst-containing TiO2 coating. In this study, the reasonable range of the ACT replacement ratio for NOx reduction was quantitatively evaluated through a comprehensive analysis of each test.