AZ31 판재에서 소둔처리가 상온성형성에 미치는 영향 (Effect of Annealing Treatment on Cold Formability of AZ31 Sheets)

  • 황범규;이영선;문영훈;김대용
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.395-398
    • /
    • 2009
  • The purpose of this paper is to investigate the effect of annealing treatment on cold formability of magnesium alloy sheet AZ31. The AZ31 sheets with three different thickness (1.0t, 1.6t, 2.0t) were annealed at three different temperatures ($345^{\circ}C$, $400^{\circ}C$ and $450^{\circ}C$). The mechanical properties and microstructure evolution of the annealed AZ31 were examined as well as limit dome height (LDH) and compared with those of as received one. The cold formability was enhanced but the strength was deteriorated by the annealing treatment.

  • PDF

AZ31 합금 부풀림 성형의 최적화 연구 (A study on optimization of AZ31 alloy sheet by blow forming)

  • 김승돈;권용남;이영선;김병민;이정환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.67-69
    • /
    • 2006
  • Since magnesium alloy has a limited formability at room temperature, forming should be carried out at the elevated temperature. If the initial grain size is small, superplasticity could be expected over $400^{\circ}C$. Using superplastic behavior, blow forming can be used to overcome the low formability of Mg alloys. In the present study, the optimization of blow forming of AZ31 alloy at the elevated temperature was investigated. Finite element simulation was carried out and verified with the blow forming experiments.

  • PDF

변형률속도 효과를 고려한 AZ31B 판재의 온간 성형한계도 예측 - II (Prediction of the Forming Limit Diagram for AZ31B Sheet at Elevated Temperatures Considering the Strain-rate Effect - II)

  • 최선철;김헌영;김형종
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.285-288
    • /
    • 2009
  • The purpose of this study is to predict the forming limit diagram (FLD) of strain-rate sensitive materials on the basis of the Marciniak and Kuczynski (M-K) theory. The strain-rate effect is taken into consideration in such a way that the stress-strain curves for various strain-rates are inputted into the formulation as point data, not as curve-fitted models such as power function. Tensile tests and R-value tests were carried out at several levels of temperature and strain-rate from $25^{\circ}C$ to $300^{\circ}C$ and 0.16 to 0.00016/s, respectively to obtain the mechanical properties of AZ31B magnesium alloy sheet. The FLD of this material was experimentally obtained by limit dome height tests with the punch velocity of 0.1 and 1.0 mm/s at $250^{\circ}C$. The M-K theory-based FLD predicted using Yld2000-2d yield criterion was compared with the experimental results.

  • PDF

마그네슘 판재의 고온 물성치 실험 (Experiments for Material Properties of Magnesium Metal Sheet at Elevated Temperatures)

  • 최의근;이상욱
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.378-381
    • /
    • 2009
  • In this study, the repetitive loading-unloading tensile tests with AZ31B magnesium sheet metal have been conducted under various elevated temperatures to check out how the Young's moduli of the sheets evolve during the plastic deformation. The loading-unloading tests have been carried out at every 1% of strain increment. With the tested results, some damage parameters of magnesium sheets based on the Lemaitre's continuum damage theory could be calculated at room temperature, $100^{\circ}C$, $150^{\circ}C$, $200^{\circ}C$ and $250^{\circ}C$. It has been shown that the critical damage parameters obtained in all temperature conditions are within the range of 0.12 to 0.18.

  • PDF

마그네슘 합금 판재의 온간 V-굽힘에서 소재의 변형 및 보토밍 공정의 효과 분석 (Study on the Deformation Characteristics of AZ31B Sheets in V-bending and Effect of Bottoming Process)

  • 김현우;유제형;이창환
    • 소성∙가공
    • /
    • 제27권3호
    • /
    • pp.139-144
    • /
    • 2018
  • Many studies have been conducted on the process of forming magnesium alloy sheets to reduce the body weights of vehicles. Magnesium has a lower specific gravity than steel and also has a higher specific strength. Mg alloy sheets have low formability and a lot of springback due to their limited ductility and low young's modulus. As the temperature increases, the yield strength of the material decreases. Warm forming increases the formability and minimizes the springback of a material by heating it and the die to reduce the required load at forming. In this study, the temperature of the AZ31B sheet was controlled in order to reduce springback and increase formability. However, as the temperature increased, the deformation characteristics of the material changed and the radius of curvature of the material increased. The load and springback amount required for forming were analyzed according to the temperature and the bottoming force in the bending deformation.

난연성 AZ31-xCa 마그네슘합금의 열간압연 특성 (Hot Rolling Properties of Non-combustible AZ31-xCa Magnesium Alloys)

  • 임창동;유봉선;이진수;김완철
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2004년도 제5회 압연심포지엄 신 시장 개척을 위한 압연기술
    • /
    • pp.55-62
    • /
    • 2004
  • In this study, the effects of Ca content and processing variables on hot rolling properties of gravity cast AZ31-xCa alloys were evaluated systematically. The number and length of side crack were decreased with increasing preheating temperature and decreasing reduction ratio per pass and Ca content. The UTS and YS were not strongly dependent on the Ca content but the elongation decreased with increasing Ca content. The decrease of elongation in Ca containing alloys was least when the sheets were fabricated under preheating temperature of $400^{\circ}C$ and reduction ratio per pass of $15\%$. The sheets had the sound external features with little side cracks by homogenization of gravity cast AZ31-xCa alloys before hot rolling. In the cases of AZ31-xCa alloys containing under $1wt.\%$ Ca, the annealed sheets after homogenization and hot rolling had the similar tensile properties to those of AZ31 sheet.

  • PDF

마그네슘 판재성형을 위한 인장 및 압축실험을 통한 기계적 물성 평가 (Evaluation of Mechanical Properties for Magnesium Sheet Forming by Tension and Compression Tests)

  • 오세웅;추동균;이준희;강충길
    • 소성∙가공
    • /
    • 제14권7호
    • /
    • pp.635-641
    • /
    • 2005
  • The crystal structure of magnesium was hexagonal close-packed (HCP), so its formability was poor at room temperature. But formability was improved in high temperature with increasing of the slip planes. Purpose of this paper was to know about the mechanical properties of magnesium alloy (AZ31B), before warm and hot forming process. The mechanical properties were defined by the tension and compression tests in various temperature and strain-rate. As the temperature was increased, yield·ultimate strength, K-value, work hardening exponent (n) and anisotropy factor (R) were decreased. But strain rate sensitivity (m) was increased. As strain-rate increased, yield·ultimate strength, K-value, and work hardening exponent (n) were increased. Also, microstructures of grains fined away at high strain-rate. These results would be used in simulations and manufacturing factor fer warm and hot forming process.

마그네슘 합금 판재의 구성식 개발: 스프링백에의 응용 (Modeling Constitutive Behavior of Mg Alloy Sheets for the Prediction of Sheet Springback)

  • 이명규;김성준;김헌영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.67-69
    • /
    • 2007
  • Unusual mechanical constitutive behavior of magnesium alloy sheets has been implemented into the finite element program ABAQUS via user material subroutine. For the verification purpose, the springback of AZ31B magnesium alloy sheet was measured using the unconstrained cylindrical bending test of Numisheet'2002. In addition to the developed constitutive models, the other two models based on isotropic constitutive equations with tensile and compressive properties were also considered. Preliminary comparisons have been made between simulated results by the finite element analysis and corresponding experiments and the newly proposed model showed enhanced prediction capability in springback prediction.

  • PDF

마그네슘 판재를 위한 온도 의존형 C-H/V 구성 모델에 관한 연구 (The Temperature Dependent C-H/V Constitutive Modeling for Magnesium Alloy Sheet)

  • 박종현;이종길;김헌영
    • 소성∙가공
    • /
    • 제21권4호
    • /
    • pp.221-227
    • /
    • 2012
  • The automotive and electronic industries have seriously considered the use of magnesium alloys because of their excellent properties such as strength to weight ratio, EMI shielding capability, etc. However, it is difficult to form magnesium alloys at room temperature because of the mechanical deformation related to twinning. Hence, magnesium alloys are normally formed at elevated temperatures. In this study, a temperature dependent constitutive model, the C-H/V model, for the magnesium alloy AZ31B sheet is proposed. A hardening law based on nonlinear kinematic and H/V(Hollomon/Voce) hardening model is used to properly characterize the Bauschinger effect and the stabilization of the flow stress. Material parameters were determined from a series of uni-axial cyclic experiments(C-T-C) with the temperature ranging between 150 and $250^{\circ}C$. The developed models are fit to experimental data and a comparison is made.

인장 및 압축실험을 통한 마그네슘 합금의 고온 물성 평가 (Estimation of Mechanical Properties of Mg Alloy at High Temperature by Tension and Compression Tests)

  • 오세웅;추동균;이준희;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.69-72
    • /
    • 2005
  • The crystal structure of magnesium is hexagonal close-packed (HCP), so its formability is poor at room temperature. But formability is improved in high temperature with increasing of the slip planes. Purpose of this paper is to know about the mechanical properties of magnesium alloy (AZ31B), before warm and hot forming process. The mechanical properties were defined by the tension and compression tests in various temperature and strain-rate. As the temperature is increased, yield${\cdot}$ultimate strength, K-value, work hardening exponent (n) and anisotropy factor (R) are decreased. But strain rate sensitivity (m) is increased. As strain-rate increased, yield${\cdot}$ultimate strength, K-value, and work hardening exponent (n) are increased. Also, microstructures of grains fine away at high strain-rate. These results will be used in simulations and manufacturing factor for warm and hot forming process.