• Title/Summary/Keyword: ASR reaction

Search Result 68, Processing Time 0.022 seconds

Effect of Mechanical Restraint due to Steel Microfibers on Alkali-Silica Reaction in Mortars (미세 강섬유의 구속력이 모르타르의 알칼리-실리카 반응에 미치는 영향)

  • Yi, Chong-Ku
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.5
    • /
    • pp.577-584
    • /
    • 2007
  • The effect of steel microfibers (SMF) on alkali-silica reaction (ASR) was investigated using two types of reactive aggregates, crushed opal and a pyrex rod of constant diameter. Cracks are less visible in the SMF mortars compared with the unreinforced mortars. Due to crack growth resistance behavior in SMF mortar specimens, the strength loss is eliminated and the ASR products remained well confined within the ASR site. The expansion and the ASR products were characterized by microprobe analysis and inductively coupled plasma (ICP) spectroscopy. The confinement due to SMF resulted in a higher Na and Si ion concentration of the ASR liquid extracted from the reaction site. The higher concentration reduced the ASR rate and resulted in a lower reactivity of the reactive pyrex rods in SMF mortars.

Modelling of Alkali-Silica Reaction Effects on Mechanical Property Changes of Concrete

  • Kim, Jung Joong;Fan, Tai;Reda Tah, Mahmoud M.;Lim, Nam-Hyoung
    • International Journal of Railway
    • /
    • v.8 no.2
    • /
    • pp.42-45
    • /
    • 2015
  • Alkali-silica reaction (ASR) is a chemical reaction in concrete that alkalis in cement react with reactive silica in aggregate in the presence of water. When ASR takes place, it produces gels that absorb water and expand. Swelling of ASR gels can damage concrete and cause cracking and volume expansion in concrete structure. In this paper, mechanical consequences of ASR on concrete are simulated by a finite element (FE) analysis. An FE model of concrete is built. The evolution of concrete mechanical properties subjected to ASR is achieved by FE analyses. The constitutive model of concrete is attained via the FE analysis. A case study is used to demonstrate the proposed method. The simulated results using the proposed model are in good agreement with the observations of concrete with ASR reported in the literature. The results can be used for a basic research to enhance durability of concrete slab tracks and concrete railway sleepers.

The Effect of the Residual Mortar of Recycled Concrete Aggregate on Alkali Silica Reaction (순환/재생골재의 잔류 모르타르 성분이 알칼리 실리카 반응성에 미치는 영향 평가)

  • Kim, Jeonghyun;Kim, Namho;Yang, Sungchul
    • International Journal of Highway Engineering
    • /
    • v.17 no.4
    • /
    • pp.19-24
    • /
    • 2015
  • PURPOSES : The objective of this study is to evaluate the effect of the residual mortar of recycled concrete aggregate on the expansion behavior during alkali silica reaction (ASR). METHODS: In order to evaluate the net effect of residual mortar on ASR expansion behavior, two aggregate samples with the same original virgin aggregate source but different residual mortar volumes were used. ASTM C1260 test was used to evaluate the ASR expansion behavior of these two aggregates and the original virgin aggregate. RESULTS: The greater the amount of residual mortar in recycled concrete aggregates, the less is the induced ASR expansion. Depending on the amount of residual mortar in recycled concrete aggregate, the ASR expansion of recycled concrete aggregate may be less than half of that of the original virgin aggregate. CONCLUSIONS: The residual mortar of recycled concrete aggregate may lead to the under estimation of the ASR expansion behavior of the original virgin aggregate.

Effect of Waste Glass Fine Aggregate on Mechanical Properites and Alkali-Silica Reaction(ASR), After ASR Residual Mechanical Properties of High Strength Mortar (폐유리 잔골재가 고강도 모르타르의 역학적 특성 및 알칼리-실리카 반응(ASR), ASR 후, 잔류 역학적 특성에 미치는 영향)

  • Eu, Ha-Min;Kim, Gyu-Yong;Son, Min-Jae;Sasui, Sasui;Lee, Yae-Chan;Nam, Jeong-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2020.11a
    • /
    • pp.31-32
    • /
    • 2020
  • This study measured the mechanical performance and residual strength of high strength/normal strength mortar mixed with waste glass fine aggregate after alkali-silica reaction and alkali-silica reaction. As a result, the effect of improving the slip phenomenon of the waste glass fine aggregate in the high-strength mortar was not significant, but rather the amount of ASR was increased.

  • PDF

A Experimental Study on the Alkali-Silica Reaction of Crushed Stones (Part 2 : The Influence of the Alkali Content and the Kind of Added Alkali to the Alkali-Silica Reaction) (쇄석 골재의 알칼리-실리카 반응에 관한 실험적 연구( 제 2보 : 첨가알칼리량 및 종류가 알칼리-실리카 반응에 미치는 영향))

  • 이영수;윤재환;정재동;노재호;이양수;조일호
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1993.10a
    • /
    • pp.108-112
    • /
    • 1993
  • The term Alkali-Silica Reaction (ASR) is used to describe a reaction between certain siliceous aggregates and hydroxyl ions present in the pore fluid of a concrete. The ASR is affected by the content of alkali, the particle size and the content of reactive aggregate, water-cement ratio, humidity, temperature and so on. In this paper, the fluence of alkali content and kind of added alkali to the ASR was studied. As a result, the more the content of alkali was increased, the more the mortar-bar was expand and the expansion of mortar-bar was showed differently with the added alkali kinds, The reaction products by ASR were observed by SEM(Scanning Electron Microscope) and analyzed by EDXA(Energy Dispersive X-ray Analysis) also and showed a gel composed of alkali(Na+, K+), silica and calcium.

  • PDF

Characteristics of Alkali-Silica Reaction Product of Mortar Bar by ASTM C 1260 Test (ASTM C 1260 시험 콘크리트 시편의 알칼리-실리카 반응 생성물 특징)

  • Hong, Seung-Ho;Yun, Kyong-Ku
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.541-544
    • /
    • 2006
  • This study was performed to proof expansion effect of the mortar bar due to Alkali-silica Reaction (ASR) by ASTM C 1260 test. Recently, the failure case of cement concrete pavement by ASR was reported in Korea. Cement concrete structures are caused crack by ASR. The service life of cracked cement concrete structures by ASR will be shorted. In this study, crushed the slate rock producted Chungcheongnamdo Boryeong was caused 0.3% expansion at 14 days due to ASR by ASTM C 1260 test. The particular spectrum showed that the ASR gel was analyzed contents included Si, Na, K, and Ca by EDX (electron dispersive X-ray spectrometer). It was verified that the crushed aggregate was caused expansion by ASR in Korea.

  • PDF

A Case Study of Concrete Pavement Deterioration by Alkali-Silica Reaction in Korea

  • Hong, Seung-Ho;Han, Seung-Hwan;Yun, Kyong-Ku
    • International Journal of Concrete Structures and Materials
    • /
    • v.1 no.1
    • /
    • pp.75-81
    • /
    • 2007
  • The concrete pavement of the Seohae Highway in Korea has suffered from serious distress, only four to seven years after construction. Deterioration due to Alkali-Silica Reaction (ASR) has seldom been reported per se in Korea, because the aggregate used for the cement concrete has been considered safe against alkali-silica reaction so far. The purpose of this study is to examine the deterioration caused by an alkali-silica reaction of concrete pavement in Korea. The investigation methods included visual inspection and Automatic Road Analyzer (ARAN) analysis of surface cracks, coring for internal cracks, stereo microscopic analysis, scanning electronic microscope (SEM) analysis, and electron dispersive X-ray spectrometer (EDX) analysis. The results are presented as follows: the crack pattern of the concrete pavement in Korea was longitudinal cracking, map cracking or D-cracking. Local areas of damage were noticed four to five years after construction. The cracks started from edges or joints and spread out to slabs. The most intensive cracking was observed at the intersection of the transverse and longitudinal joints. Where cracking was the most intense, pieces of concrete and aggregate had spalled away from top surface and joint interface area. The progress of deterioration was very fast. The reaction product of alkali-silica gel was clearly identified by its generally colorless, white, or very pale yellow hue seen through a stereo optical microscopy. The typical locations of the reaction product were at the interface between aggregate and cement paste in a shape of a rim, within aggregate particles in the cracks, and in the large void in the cement paste. Most of the white products were found at interface or internal aggregates. SEM and EDX analysis confirmed that the white gel was a typical reaction product of ASR. The ASR gel in Korea mainly consisted of Silicate (Si) and Potassium (K) from the cement. The crack in the concrete pavement was caused by ASR. It seems that Korea is no longer safe from alkali-silica reaction.

Effect of Fineness Modulus of Reactive Aggregate on Alkali Silica Reaction

  • Jun, Ssang-Sun;Jin, Chi-Sub
    • International Journal of Concrete Structures and Materials
    • /
    • v.4 no.2
    • /
    • pp.119-125
    • /
    • 2010
  • In this study, the effects of the fineness modulus of reactive aggregate on ASR expansion and ASR products have been investigated. The reactive aggregate used was metamorphic aggregate originated from Korea. ASR tests were conducted according to accelerated mortar bar test. The morphology and chemical composition of products formed in mortar bars, 5 years after the mortar bar test had been performed, were studied by scanning electron microscopy equipped with energy dispersive spectroscopy. Test results indicated that ASR expansion of mortar bars decrease in linear proportion to the fineness modulus of reactive aggregate. SEM images indicated that mortar bars showed reactive products formed in cement paste, within air voids and within cracks through particles except for the mortar bar with the fineness modulus of 3.25. The EDS analysis of the reactive products showed presence of silica, calcium and sodium, typical of ASR product composition.

An Experimental Study on Alkali-Silica Reaction of Mortar Containing Waste Glass and By-products (폐유리 및 산업부산물을 혼입한 모르터의 ASR에 관한 실험적 연구)

  • Lee, Bong-Chun;Kwon, Hyuk-Joon;Kim, Jeong-Hwan;Lee, Jun;Park, Seung-Bum
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.93-98
    • /
    • 2001
  • Using waste glass in concrete can cause crack and strength loss by the expansion of alkali-silica reaction(ASR). In this study, ASR expansion and properties of strength were analyzed in terms of clear waste glass grading, and by-products(fly ash, blast-furnace slag) and by-products content for reduction ASR expansion due to waste glass. In this accelerated ASTM C 1260 test of waste glass, pessimum grading can be found. Also, when the by-products are used with waste glass, there is an effect on reduction of expansion and strength loss due to ASR between the alkali in the cement paste and the silica in the waste glass.

  • PDF

Mechanical Properties and ASR Behavior of Recycled Glass Fine Aggregate Mortar Mixed with Mineral Admixture (혼화재를 혼입한 순환유리잔골재 모르타르의 역학적 특성과 ASR 거동)

  • Eu, Ha-Min;Kim, Guy-Yong;Park, Jun-Young;Sasui, Sasui;Choi, Byung-Cheol;Nam, Jeong-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.05a
    • /
    • pp.195-196
    • /
    • 2023
  • In this study, the mechanical properties, alkali-silica reaction(ASR) expansion and residual mechanical properties after ASR of waste glass fine aggregate(GS) mortar according to mineral mixture were evaluated. As a result, it was found that the mineral mixture reduces the ASR expansion. However, mechanical properties and residual mechanical properties have decreased.

  • PDF