Physical and Chemical Effects of Extracellular Matrix on the Growth of Cardiomyocytes (HL-1) (세포외 기질 물질의 물리·화학적 영향에 따른 심근세포(HL-1)의 성장 연구)

  • Hong, Yoon-Mi;Choi, Seong-Kyun;Kim, Sun-Min
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.35 no.11
    • /
    • pp.1229-1235
    • /
    • 2011
  • The extracellular matrix (ECM) is a key factor affecting cell growth and adhesion to the culture surface, and it is also important for maintaining the innate characteristics of cells. Here, we describe the effects of the ECM on cardiomyocyte (HL-1 cell line) growth, viability, phenotype, and contractile ability. Five different ECM materials were investigated to analyze their effects on the cell growth. The physical morphology of the ECM-coated surfaces was scanned with an atomic force microscope (AFM), and the attachment, growth, proliferation, viability, and phenotype of the cells were analyzed using fluorescence immunostaining and an inverted phase contrast microscope.

Racemic and enantiomeric effect of tartaric acid on the hydrophilicity of polysulfone membrane

  • Sharma, Nilay;Purkait, Mihir Kumar
    • Membrane and Water Treatment
    • /
    • v.7 no.3
    • /
    • pp.257-275
    • /
    • 2016
  • The enantiomeric and racemic effects of tartaric acid (TA) on the properties of polysulfone (PSn) ultrafiltration membranes were studied in terms of morphology and hydrophilicity (HPCT) of membrane. Asymmetric membranes were prepared by direct blending of polyvinyl pyrrolidone (PVP) with D-TA and DL-TA in membrane casting solution. FTIR analysis was done for the confirmation of the reaction of PVP and TA in blended membranes and plain PSn membranes. Scanning electron microscope (SEM), field emission scanning electron microscope (FESEM) and atomic force microscopy (AFM) were used for analyzing the morphology and structure of the resulting membranes. The membranes were characterized in terms of pure water flux (PWF), hydraulic permeability and HPCT. PWF increased from $52L/m^2h$ to $79.9L/m^2h$ for plain and D-TA containing PSn membrane, respectively. Water contact angle also found to be decreased from $68^{\circ}$ to $55^{\circ}$. In Additionally, permeation and rejection behavior of prepared membranes was studied by bovine serum albumin (BSA) solution. A considerable increase in BSA flux (from $19.1L/m^2h$ for plain membrane to $32.1L/m^2h$ for D-TA containing membrane) was observed. FESEM images affirm that the pore size of the membranes decreases and the membrane permeability increases from 0.16 to 0.32 by the addition of D-TA in the membrane. D-TA increases the HPCT whereas; DL-TA decreases the HPCT of PSn membrane. PVP (average molecular weight of 40000 Da) with D-TA (1 wt%) gave best performance among all the membranes for each parameter.

이종밴드갭을 갖는 $TiO_2/Cr_2O_3$/Cr 다층박막의 친수성

  • Park, Seon-Ho;Lee, Gi-Seon;Mun, Chang-Jun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.373-373
    • /
    • 2010
  • 광촉매능을 갖는 $TiO_2$는 국내외적으로 많은 연구가 진행되고 있다. 빛의 조사로 발생하는 다양한 물리 화학적 촉매특성이 환경정화 뿐만 아니라 및 에너지 흡수차단 기능도 갖고 있어 최근 주목을 받고 있다. 응용분야로 초친수성 유리제품, 필터, 살균기능의 의료용 부품소재, 고효율 수소생산 및 태양전지 등에 활용성이 커서 친환경에너지 소재로 각광을 받고 있다. 본 연구에서는 초친수성 자동차의 사이드미러 개발을 위해 유리표면에 초친수성 $TiO_2$를 코팅하 고 그의 특성을 평가하였다. 특히, 이종밴드갭을 갖는 복합구조 $TiO_2/Cr_2O_3$/Cr 박막을 스퍼터링법으로 증착하여 중간층인 $Cr_2O_3$의 역할을 고찰하였다. 제조된 박막의 결정구조는 thin film형 X-선회절기(XRD)를 사용하여 분석하였으며, 박막의 표면 미세구조는 FE-SEM(Field Emission Scanning Electron Microscope)와 AFM(Atomic Force Microscope)으로, 화학구조는 XPS(X-ray Photoelectron Spectroscope)로 분석하였다. 친수성 평가는 실온 분위기에서 접촉각 측정기(Topcon-UVR2)를 사용하여 평가 하였으며 이때 조사되는 UV는 파장이 365nm이다. $Cr_2O_3$(비정질)/Cr박막위에 제조된 $TiO_2$ 박막은 균일한 anatase-$TiO_2$가 성장했으나, Cr, $Cr_2O_3$(결정질)박막위에 제조 된 $TiO_2$ 박막은 anatase상과 rulile상이 혼합된 형태로 성장하였다. $TiO_2$/Cr, $TiO_2/Cr_2O_3$(비정질)/Cr, $TiO_2/Cr_2O_3$(결정질)/Cr박막은 UV조사 1시간 만에 $10^{\circ}$ 이하의 초친수성을 나타내었다. 이종 밴드갭을 갖는 $TiO_2/Cr_2O_3$(비정질)/Cr박막은 40시간까지 친수성을 유지하는 결과를 나타냈다.

  • PDF

Machining Characteristics of SiC reinforced Composite by multiple diamond-coated drills (다이아몬드 피복공구에 의한 SiC 강화 복합재료의 절삭특성)

  • M. Chen;Lee, Y. M.;S. H. Yang;S. I. Jang
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.533-537
    • /
    • 2003
  • Compared to sintered polycrystalline diamond (PCD), the deposited thin film diamond has a great advantage on the fabrication of cutting tools with complex geometries such as drills. Because of high performance in high speed machining non-ferrous difficult-to-cut materials in the field of automobiles industry, aeronautics and astronautics industry, diamond-coated drills find large potentialities in commercial applications. However, the poor adhesion of the diamond film on the substrate and high surface roughness of the drill flute adversely affect the tool lift and machining quality and they become the main technical barriers for the successful development and commercialization of diamond-coated drills. In this paper, diamond thin films were deposited on the commercial WC-Co based drills by the electron aided hot filament chemical vapor deposition (EACVD). A new multiple coating technology based on changing gas pressure in different process stages was developed. The large triangular faceted diamond grains may have great contribution to the adhesive strength between the film and the substrate, and the overlapping ball like blocks consisted of nanometer sized diamond crystals may contribute much to the very low roughness of diamond film. Adhesive strength and quality of diamond film were evaluated by scanning electron microscope (SEM), atomic force microscope (AFM), Raman spectrum and drilling experiments. The ring-block tribological experiments were also conducted and the results revealed that the friction coefficient increased with the surface roughness of the diamond film. From a practical viewpoint, the cutting performances of diamond-coated drills were studied by drilling the SiC particles reinforced aluminum-matrix composite. The good adhesive strength and low surface roughness of flute were proved to be beneficial to the good chip evacuation and the decrease of thrust and consequently led to a prolonged tool lift and an improved machining quality. The wear mechanism of diamond-coated drills is the abrasive mechanical attrition.

  • PDF

Effect of post-treatment routes on the performance of PVDF-TEOS hollow fiber membranes

  • Shadia R. Tewfik;Mohamed H. Sorour;Hayam F. Shaalan;Heba A. Hani;Abdelghani G. Abulnour;Marwa M. El Sayed;Yomna O. Mostafa;Mahmoud A. Eltoukhy
    • Membrane and Water Treatment
    • /
    • v.14 no.2
    • /
    • pp.85-93
    • /
    • 2023
  • Membrane separation is widely used for several applications such as water treatment, membrane reactors and climate change. Cross-linked organic-inorganic hybrid polyvinylidene fluoride (PVDF) / Tetraethyl orthosilicate (TEOS) was adopted for the preparation of optimized hollow membrane (HFM) for membrane distillation or other low pressure separators for mechanical properties and permeability under varying pretreatment schemes. HFMs were prepared on semi-pilot membrane fabrication system. Novel adopted post-treatment schemes involved soaking in glycerol, magnesium sulphate (MgSO4), sodium hypochlorite (NaOCl), and isopropanol for different durations. All fibers were characterized for morphology using a scanning electron microscope (SEM), surface roughness using atomic force microscope (AFM), elemental composition by examining Energy Dispersive Spectroscopy (EDS), water contact angle (CA°) and porosity. The performance of the fibers was evaluated for pure water permeation flux (PWF). Post-treatment with MgSO4 gave the highest both tensile modulus and flux. Assessment of properties and performance revealed comparable results with other organic-inorganic separators, HF or flat. In spite of few reported data on post treatment using MgSO4 in presence of TEOS, this proves the potential of low cost treatment without negative impact on other membrane properties. The flux is also comparable with hypochlorite which manifests substantial precaution requirements in actual industrial use.The relatively high values of flux/bar for sample treated with TEOS, post treated with MgSO4 and hypochlorite are 88 and 82 LMH/bar respectively.

Characteristics of Rhenium-Iridium coating thin film on tungsten carbide by multi-target sputter

  • Cheon, Min-Woo;Kim, Tae-Gon;Park, Yong-Pil
    • Journal of Ceramic Processing Research
    • /
    • v.13 no.spc2
    • /
    • pp.328-331
    • /
    • 2012
  • With the recent development of super-precision optical instruments, camera modules for devices, such as portable terminals and digital camera lenses, are increasingly being used. Since an optical lens is usually produced by high-temperature compression molding methods using tungsten carbide (WC) alloy molding cores, it is necessary to develop and study technology for super-precision processing of molding cores and coatings for the core surface. In this study, Rhenium-Iridium (Re-Ir) thin films were deposited onto a WC molding core using a sputtering system. The Re-Ir thin films were prepared by a multi-target sputtering technique, using iridium, rhenium, and chromium as the sources. Argon and nitrogen were introduced through an inlet into the chamber to be the plasma and reactive gases. The Re-Ir thin films were prepared with targets having a composition ratio of 30 : 70, and the Re-Ir thin films were formed with a 240 nm thickness. Re-Ir thin films on WC molding core were analyzed by scanning electron microscope (SEM), atomic force microscope (AFM), and Ra (the arithmetical average surface roughness). Also, adhesion strength and coefficient friction of Re-Ir thin films were examined. The Re-Ir coating technique has received intensive attention in the coating processes field because of promising features, such as hardness, high elasticity, abrasion resistance and mechanical stability that result from the process. Re-Ir coating technique has also been applied widely in industrial and biomedical applications. In this study, WC molding core was manufactured, using high-performance precision machining and the effects of the Re-Ir coating on the surface roughness.

Optimization of chemical mechanical polishing for bulk AlN single crystal surface (화학적 기계적 연마 공정을 통한 bulk AlN 단결정의 표면 가공)

  • Lee, Jung Hun;Park, Cheol Woo;Park, Jae Hwa;Kang, Hyo Sang;Kang, Suk Hyun;Lee, Hee Ae;Lee, Joo Hyung;In, Jun Hyeong;Kang, Seung Min;Shim, Kwang Bo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.28 no.1
    • /
    • pp.51-56
    • /
    • 2018
  • To evaluate surface characteristics of AlN single crystal grown by physical vapor transport (PVT) method, chemical mechanical polishing (CMP) were performed with diamond slurry and $SiO_2$ slurry after mechanical polishing (MP), then the surface morphology and analysis of polishing characteristics of the slurry types were analyzed. To estimate how pH of slurry effects polishing process, pH of $SiO_2$ slurry was controlled, the results from estimating the effect of zeta potential and MRR (material removal rate) were compared in accordance with each pH via zeta potential analyzer. Eventually, surface roughness RMS (0.2 nm) could be derived with atomic force microscope (AFM).

Preparation and Current-Voltage Characteristics of Well-Aligned NPD (4,4' bis[N-(1-napthyl)-N-phenyl-amino] biphenyl) Thin Films (분자배열된 4,4' bis[N-(1-napthyl)-N-phenyl-amino] biphenyl 증착박막 제조와 전기적 특성)

  • Oh, Sung;Kang, Do-Soon;Choe, Youngson
    • Applied Chemistry for Engineering
    • /
    • v.17 no.6
    • /
    • pp.591-596
    • /
    • 2006
  • Topology and molecular ordering of NPD(4,4'-bis-[N-(1-naphthyl)-N-phenyl-amino]biphenyl) thin films deposited under magnetic field with post-deposition annealing were investigated. NPD was deposited onto ITO glass substrates via thermal evaporation process in vacuum. It is of great importance for highly oriented organic/metal films to have improved device performances such as higher current density and luminance efficiency. AFM (Atomic Force Microscope) and XRD (X-Ray Diffraction) analyses were used to characterize the topology and structure of oriented NPD films. The multi-source meter was used to observe the current-voltage characteristics of the ITO (Indium-Tin Oxide) / NPD (4,4'bis[N-(1-napthyl)-N-phenyl-amino]-biphenyl) / Al (Aluminum) device. While NPD thin films deposited under magnetic field were not molecularly well aligned according to the XRD results, the films after post-deposition annealing at $130^{\circ}C$ were well-oriented. AFM images show that NPD thin films deposited under magnetic field had a smoother surface than those deposited without magnetic field. The current-voltage performance of NPD thin films was improved due to the enhanced electron mobility in the well-aligned NPD films.

A Study on Selenization of Cu-In-Ga Precursors by Cracked Selenium (Cracked Selenium을 이용한 CIGS 박막 셀렌화 공정에 관한 연구)

  • Kim, Minyoung;Kim, Girim;Kim, Jongwan;Son, Kyeongtae;Lee, Jongkwan;Lim, Donggun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.26 no.7
    • /
    • pp.503-509
    • /
    • 2013
  • In this study, $Cu(In_{1-x},Ga_x)Se_2$ (CIGS) thin films were prepared on the Mo coated soda-lime glass by the DC magnetron sputtering and a subsequent selenization process. For the selenization process, selenization rapid thermal process(RTP) with cracker cell, which was helpful to smaller an atomic of Se, was adopted. To make CIGS layer, they were then annealed with the cracked Se. Based on this selenization method, we made several CIGS thin film and investigated the effects of In deposition time, and selenization time. Through x-ray diffraction (XRD), scanning electron microscope (SEM), energy dispersive spectroscopy (EDS), and atomic force microscopy (AFM), it is found that the Mo/In/CuGa structure and the high sputtering power shows the dominant chalcopyrite structure and have a uniform distribution of the grain size. The CIGS films with the In deposition time of 5 min has the best structure due to the smooth surface. And CIGS films with the selenization time of 50 min show good crystalline growth without any voids.

Influence of Oxygen Annealing on Temperature Dependent Electrical Characteristics of Ga2O3/4H-SiC Heterojunction Diodes (산소 후열처리가 Ga2O3/4H-SiC 이종접합 다이오드의 온도에 따른 전기적 특성에 미치는 영향 분석)

  • Chung, Seung Hwan;Lee, Hyung Jin;Lee, Hee Jae;Byun, Dong Wook;Koo, Sang Mo
    • Journal of the Semiconductor & Display Technology
    • /
    • v.21 no.4
    • /
    • pp.138-143
    • /
    • 2022
  • We analyzed the influence of post-annealing on Ga2O3/n-type 4H-SiC heterojunction diode. Gallium oxide (Ga2O3) thin films were deposited by radio frequency (RF) sputtering. Post-deposition annealing at 950℃ in an Oxygen atmosphere was performed. The material properties of Ga2O3 and the electrical properties of the diodes were investigated. Atomic Force Microscopy (AFM), X-Ray Diffraction and Scanning Electron Microscope (SEM) images show a significant increase in the roughness and crystallinity of the O2-annealed films. After Oxygen annealing X-ray Photoelectron Spectroscopy (XPS) shows that the atomic ratio of oxygen increases which is related to a decrease in oxygen vacancy within the Ga2O3 film. The O2-annealed diodes exhibited higher on-current and lower leakage current. Moreover, the ideality factor, barrier height, and thermal activation energy were derived from the current-voltage curve by increasing the temperature from 298 - 434K.