비대칭 압연 패스 회수에 따른 AA1050 Al 판재의 집합조직과 소성변형비 변화 (Texture and Plastic Strain Ratio Changes with the Number of Passes of Asymmetric Rolling in AA1050 Al Alloy Sheet)

  • 남수권;정해봉;김인수
    • 소성∙가공
    • /
    • 제19권8호
    • /
    • pp.502-507
    • /
    • 2010
  • The physical and mechanical properties and formability of sheet metals depend on preferred crystallographic orientations (texture). In this research work, the texture development and formability (plastic strain ratios) of AA1050 Al alloy sheets after 3 and 10 passes of asymmetric rolling and subsequent heat treatment were investigated. The plastic strain ratios of 10 passes asymmetrically rolled and subsequent heat treated samples are 1.3 times higher than those of the initial AA1050 Al alloy sheets. The ${\Delta}r$ of 10 passes of asymmetrically rolled and subsequent heat treated samples is 1/30 times lower than those of the initial AA1050 Al alloy sheets. The plastic strain ratios of 10 passes of asymmetrically rolled and subsequent heat treated Al sheets are higher than those of 3 passes ones. These results could be attributed to the formation of $\gamma$-fiber, ND//<111>, and the other texture components by means of asymmetric rolling in Al sheets.

비대칭 압연한 AA 1050 합금의 조직 변화 (Texture of Asymmetrically Rolled AA 1050 Aluminum alloy)

  • 사이드무로드 아크라모프;김인수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.326-327
    • /
    • 2007
  • A study on the texture and the formability after asymmetric rolled and subsequent heat-treated AA 1050 aluminum alloy sheets have been carried out. The specimens after the asymmetric rolling showed a very fine grain size, a decrease of <100>//ND, and an increase of <111>//ND textures. The change of plastic strain ratios has been investigated and it was found that they were higher than those of the initial Al sheet.

  • PDF

마찰 압연한 AA 1050 합금의 조직 변화 (Texture of Frictionally Rolled AA 1050 Aluminum alloy)

  • 사이드무로드 아크라모프;김인수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.328-329
    • /
    • 2007
  • A study on the texture and the formability after frictional rolled and subsequent heat-treated AA 1050 aluminum alloy sheets have been carried out. The specimens after the frictional rolling showed a very fine grain size, a decrease of <100>//ND, and an increase of <111>//ND textures. The change of plastic strain ratios has been investigated and it was found that they were higher than those of the initial Al sheet.

  • PDF

Microstructure and Mechanical Properties of AA6061/AA5052/AA1050 Alloy Fabricated by Cold Roll-Bonding and Subsequently Annealed

  • Seong-Hee Lee;Sang-Hyeon Jo;Jae-Yeol Jeon
    • 한국재료학회지
    • /
    • 제33권11호
    • /
    • pp.439-446
    • /
    • 2023
  • Changes in the microstructure and mechanical properties of as-roll-bonded AA6061/AA5052/AA1050 three-layered sheet with increasing annealing temperature were investigated in detail. The commercial AA6061, AA5052 and AA1050 sheets with 2 mm thickness were roll-bonded by multi-pass rolling at ambient temperature. The roll-bonded Al sheets were then annealed for 1 h at various temperatures from 200 to 400 ℃. The specimens annealed up to 250 ℃ showed a typical deformation structure where the grains are elongated in the rolling direction in all regions. However, after annealing at 300 ℃, while AA6061 and AA1050 regions still retained the deformation structure, but AA5052 region changed into complete recrystallization. For all the annealed materials, the fraction of high angle grain boundaries was lower than that of low angle grain boundaries. In addition, while the rolling texture of the {110}<112> and {123}<634> components strongly developed in the AA6061 and AA1050 regions, in the AA5052 region the recrystallization texture of the {100}<001> component developed. After annealing at 350 ℃ the recrystallization texture developed in all regions. The as-rolled material exhibited a relatively high tensile strength of 282 MPa and elongation of 18 %. However, the tensile strength decreased and the elongation increased gradually with the increase in annealing temperature. The changes in mechanical properties with increasing annealing temperature were compared with those of other three-layered Al sheets fabricated in previous studies.

ECAP한 Al 판재의 판재성형성 (Formability of ECAPed Al Alloy Sheet)

  • ;김인수;이민구;박병현
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 춘계학술대회 논문집
    • /
    • pp.285-287
    • /
    • 2006
  • Ultra-fine grained and high hardened Al sheet was obtained by Equal channel angular pressing (ECAP). During this process the microstructure, the hardness and the texture of AA 1050 Al alloy sheet are changed by a severe shear deformation. The plastic strain ratio after the ECAP and subsequent heat-treatment condition has been investigated in this study. It was found that the average r-value of the ECAPed and subsequent heat-treated specimen was 1.7 times higher than those of the initial Al sheet. This could be attributed to the various texture formations through the ECAP and subsequent heat-treatment of AA 1050 Aluminum alloy sheet.

  • PDF

ECAP 한 알루미늄 판재의 성형성 연구 (Formability of ECAPed Al Alloy Sheet)

  • 사이드무로드아크라모프;김인수;이민구;박병현
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2006년도 제5회 박판성형 SYMPOSIUM
    • /
    • pp.88-91
    • /
    • 2006
  • Ultra-fine grained and high hardened Al sheet was obtained by Equal Channel Angular Pressing (ECAP). During this process the microstructure, the hardness and the texture of AA 1050 Al alloy sheet are changed by a severe shear deformation. The plastic strain ratio after the ECAP and subsequent heat-treatment condition was investigated in this study. It was found that the average r-value of the equal channel angular pressed and subsequent heat-treated specimen was 1.7 times higher than that of the initial Al sheet. This could be attributed to the various texture formations through the ECAP and subsequent heat-treatment of AA 1050 Aluminum alloy sheets.

  • PDF

ECAP로 심한 전단 소성변형한 후 열처리한 AA 1050 알루미늄 합금 판재의 집합조직과 소성변형비 (Texture and Plastic Strain Ratio of the Severe Shear Deformed with ECAP and Heat-treated AA 1050 Aluminum Alloy Sheet)

  • ;이민구;박병현;김인수
    • 소성∙가공
    • /
    • 제14권6호
    • /
    • pp.553-558
    • /
    • 2005
  • A study on the microstructure, the texture and the formability of the samples after ECAPed and subsequent heat-treated AA 1050 aluminum alloy sheet have been carried out. The specimens after the ECAP showed a very fine grain size, a decrease of <100> // ND, and an increase of <111> // ND textures. The $\{111\}<112>,\;\{123\}<634>,\;\{110\}<001>,\;\{112\}<111>,\;\{110\}<111>,\;and\;\{013\}<231>$ texture components were increased in the specimens after the ECAP and subsequent heat-treatment at $400^{\circ}C$ for 1 hour. One of the most important properties in sheet metals is formability. The r-value or plastic strain ratio has was as a parameter that expressed the formability of sheet metals. The change of the plastic strain ratios after the ECAP and subsequent heat-treatment conditions were investigated and it was found that they were two times higher than those of the initial Al sheets. This could be attributed to the formation above texture components through the ECAP and subsequent heat-treatment of AA 1050 Aluminum alloy sheet.

에어로졸 증착법에 의한 YSZ 코팅된 AA1050 알루미늄 합금의 전기화학적 부식 특성 (Electrochemical Corrosion Properties of YSZ Coated AA1050 Aluminium Alloys Prepared by Aerosol Deposition)

  • 유현삼;임태섭;류정호;박동수;홍성현
    • 한국세라믹학회지
    • /
    • 제48권5호
    • /
    • pp.439-446
    • /
    • 2011
  • Yttria stabilized zirconia (YSZ) coating was formed on AA1050 Al alloys by aerosol deposition (AD), and its electrochemical corrosion properties were investigated in 3.5 wt% NaCl and 0.5M $H_2SO_4$ solutions. The crack-free, dense, and ~5 ${\mu}m$ thick YSZ coating was successfully obtained by AD. The as-deposited coating was composed of cubic-YSZ nanocrystallites of ~10 nm size. The potentiodynamic test indicated that the YSZ coated Al alloy had much lower corrosion current densities (2 nA/$cm^2$) by comparison to uncoated sample and exhibited a passive behavior in anodic branch. Particularly, a pitting breakdown potential could not be identified in $H_2SO_4$. EIS tests revealed that the impedance of YSZ coated sample was ${\sim}10^6{\Omega}cm^2$ in NaCl and ${\sim}10^7{\Omega}cm^2$ in $H_2SO_4$, which was about 3 or 4 orders of magnitude higher than that of uncoated sample. Consequently, the corrosion resistance of Al alloy had been significantly enhanced by the YSZ coating.

ECAP 한 후 열처리한 알루미늄 AA 1050 합금 판재의 집합조직과 소성변형비 변화 (Plastic Strain Ratio and Texture of the ECAPed and Heat-treated Aluminum AA 1050 Sheet)

  • ;이민구;박병현;김인수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.369-372
    • /
    • 2005
  • A study on the microstructure, the texture and the formability of the samples after ECAPed and subsequent heat-treated AA 1050 aluminum alloy sheet have been carried out. The specimens after the ECAP showed a very fine grain size, a decrease of <100> // ND. The <110>// ND textures appears in the specimens after the ECAP and subsequent heat-treatment at $400^{\circ}C$ for 1 hour. One of the most important properties in sheet metals is formability. The r-value or plastic strain ratio has was as a parameter that expressed the formability of sheet metals. The change of the plastic Strain ratios after the ECAP and subsequent heat-treatment conditions were investigated and it was found that they were two times higher than those of the initial Al sheets. This could be attributed to the formation above texture components through the ECAP and subsequent heat-treatment of AA 1050 Aluminum alloy sheet.

  • PDF

비대칭 압연 알루미늄의 소성변형비 (Plastic Strain Ratios of Asymmetry Rolled Aluminum Sheets)

  • 사이드무로드 아크라모프;김인수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.425-426
    • /
    • 2007
  • The physical and mechanical properties of the sheets metals are closely related to the presence of preferred crystallographic orientations which were produced by the manufacturing process. To obtain the aluminum alloys sheets with good Al sheet formability, the plastic strain ratio (or r-value) of AA1050 Al sheets after asymmetric rolling and subsequent heat treatment was studied. The AA1050 aluminum alloy sheets after asymmetric rolling with high reduction ratio and following heat treatment had the higher plastic strain ratio.

  • PDF