• Title/Summary/Keyword: A6061-T6

Search Result 145, Processing Time 0.027 seconds

Microstructure and Mechanical Properties of AA6061/AA5052/AA6061 Complex Sheet Fabricated by Cold-Roll Bonding Process (냉간압연접합법에 의해 제조된 AA6061/AA5052/AA6061 복합판재의 미세조직 및 기계적 성질)

  • Hwang, Ju-Yeon;Lee, Seong-Hee
    • Korean Journal of Materials Research
    • /
    • v.29 no.6
    • /
    • pp.392-397
    • /
    • 2019
  • A cold roll-bonding process is applied to fabricate an AA6061/AA5052/AA6061 three-layer clad sheet. Two AA6061 and one AA5052 sheets of 2 mm thickness, 40 mm width, and 300 mm length are stacked, with the AA5052 sheet located in the center. After surface treatment such as degreasing and wire brushing, sample is reduced to a thickness of 1.5 mm by multi-pass cold rolling. The rolling is performed at ambient temperature without lubricant using a 2-high mill with a roll diameter of 400 mm at rolling speed of 6.0 m/sec. The roll bonded AA6061/AA5052/AA6061 complex sheet is then hardened by natural aging(T4) and artificial aging(T6) treatments. The microstructures of the as-roll bonded and age-hardened Al complex sheets are revealed by optical microscopy; the mechanical properties are investigated by tensile testing and hardness testing. After rolling, the roll-bonded AA6061/AA5052/AA6061 sheets show a typical deformation structure in which grains are elongated in the rolling direction. However, after T4 and T6 aging treatment, there is a recrystallization structure consisting of coarse equiaxed grains in both AA5052 and AA6061 sheets. The as roll-bonded specimen shows a sandwich structure in which an AA5052 sheet is inserted into two AA6061 sheets with higher hardness. However, after T4 and T6 aging treatment, there is a different sandwich structure in which the hardness of the upper and lower layers of the AA6061 sheets is higher than that of the center of the AA5052 sheet. The strength values of the T4 and T6 age-treated specimens are found to increase by 1.3 and 1.4 times, respectively, compared to that value of the starting material.

Microstructure and Mechanical Properties of Cold Roll-Bonded Layered AA6061/AA5052/AA6061/AA5052 Aluminum Alloy Sheet (냉간압연접합된 층상 AA6061/AA5052/AA6061/AA5052 알루미늄합금판재의 미세조직 및 기계적 성질)

  • Jo, Sang-Hyeon;Park, Bo-Bae;Lee, Seong-Hee
    • Korean Journal of Materials Research
    • /
    • v.32 no.3
    • /
    • pp.161-167
    • /
    • 2022
  • A cold roll-bonding process is applied to fabricate an AA6061/AA5052/AA6061/AA5052 layered sheet. Two AA6061 and one AA5052 sheets of 2mm thickness, 40mm width and 300mm length are alternately stacked, then reduced to a thickness of 2.0 mm by multi-pass cold rolling after surface treatment such as degreasing and wire brushing. The rolling is performed at ambient temperature without lubricant using a 2-high mill with a roll diameter of 400 mm at a rolling speed of 6.0 m/sec. The roll-bonded AA6061/AA5052/AA6061/AA5052 layered sheet is then hardened by natural aging (T4) and artificial aging (T6) treatments. The microstructure of the as-roll bonded and the age-hardened Al sheets was revealed by SEM observation; the mechanical properties were investigated by tensile testing and hardness testing. After T4 and T6 aging treatment, the specimens had a recrystallization structure consisting of coarse equiaxed grains in both AA5052 and AA6061 regions. The as-roll-bonded specimen showed a clad structure in which the hardness of AA5052 regions was higher than that of AA6061 regions. However, after T4 and T6 aging treatment, specimens exhibited different structures, with hardness of AA6061 regions higher than that of AA5052 regions. Strengths of T6 and T4 age-treated specimens were found to increase by 1.55 and 1.36 times, respectively, compared to the value of the starting material.

The failure analysis of patch bonded repair on Al 6061-T6 alloy structures with cracked bolt hole (볼트 균열 홀을 갖는 알루미늄 6061-T6 합금의 패치 본딩 보수/보강 부위에 대한 파괴역학적 해석에 관한 연구)

  • Yoon, Young-Ki;Kim, Guk-Gi;Park, Jong-Jun;Yoon, Hi-Seak
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.148-152
    • /
    • 2000
  • The aluminum alloy 6061-T6 has been successfully used in structural applications especially the pressure vessel of the Advanced Neutron Source research reactor. And aluminum alloys, including 6061-T6, have a face-centered-cubic crystals structure. Under normal circumstances face-centered-cubic crystal structures do not exhibit cleavage fractures even at very lo9w temperatures. In aluminum-based structures, plates frequently find use as connecting links. Mechanical fasteners are often utilized in instances where ease of application, familiarity with fabrication processes, and severe dynamic loading are of concern. Plates frequently find use as connecting elements in structures built from aluminum alloys. Many structural elements employ mechanical fasteners. Twenty and twenty aluminum alloy 6061-T6 plates, representing four different bolt patterns, were mechanically deformed. And variable materials such as A1 6061-T6, Al 2024-T3, Carbon/Epoxy, Glass/Epoxy Composite and Woven fiber composite, are used as patch materials. From this experiment, it has been shown that the strength of patch-repaired specimens is different with the patch materials.

  • PDF

Analysis of Microstructure and Mechanical Properties According to Heat Treatment Conditions in GMAW for Al 6061-T6 Alloy (Al 6061-T6 합금의 MIG 용접 후 열처리조건에 따른 미세조직 및 기계적 물성 분석)

  • Kim, Chan Kyu;Cho, Young Tae;Jung, Yoon Gyo;Kang, Shin Hyun
    • Journal of Welding and Joining
    • /
    • v.34 no.4
    • /
    • pp.34-39
    • /
    • 2016
  • Recently, aluminum alloy has used various industry, such as automobile, shipbuilding and aircraft because of characteristics of low density and high corrosion resistance. Al 6061-T6 is heat treatment materials so it has high strength and mostly used for assembly by mechanical fastening such as a bolting and riveting. In GMA (Gas Metal Arc) welding of alloy, some defects which are hot cracking, porosity, low-mechanical properties and large heat affected zone is generated, because of high heat conductivity. It reduces mechanical properties. In this study, the major factor effected on properties are analyzed after welding in Al 6061-T6 in GMAW, then optimize heat treatment conditions. Plate of Al 6061-T6 with a thickness of 12 mm is welded in V groove and applied welding method is butt joint. Mechanical properties and microstructure are analyzed according to heat treatment condition. Tensile strength, microstructure and Hardness are evaluated. Result of research appears that Al 6061-T6 applied heat treatment show outstanding mechanical properties.

Microstructure and Mechanical Properties of AA1050/AA6061/AA1050 Layered Sheet Aging-Treated after Cold Roll-Bonding (냉간접합압연 후 시효처리된 AA1050/AA6061/AA1050 층상판재의 미세조직 및 기계적 성질)

  • Sang-Hyeon Jo;Seong-Hee Lee
    • Korean Journal of Materials Research
    • /
    • v.33 no.12
    • /
    • pp.565-571
    • /
    • 2023
  • AA1050/AA6061/AA1050 layered sheet was fabricated by cold roll-bonding process and subsequently T4 and T6 aging-treated. Two commercial AA1050 sheets of 1 mm thickness and one AA6061 sheet of 2 mm thickness were stacked up so that an AA6061 sheet was located between two AA1050 sheets. After surface treatments such as degreasing and wire brushing, they were then roll-bonded to a thickness of 2 mm by cold rolling. The roll-bonded Al sheets were then processed by natural aging (T4) and artificial aging (T6) treatments. The as roll-bonded Al sheets showed a typical deformation structure, where the grains are elongated in the rolling direction. However, after the T4 and T6 aging treatments, the Al sheets had a recrystallized structure consisting of coarse grains in both the AA5052 and AA6061 regions with different grain sizes in each. In addition, the sheets showed an inhomogeneous hardness distribution in the thickness direction, with higher hardness in AA6061 than in AA1050 after the T4 and T6 age treatments. The tensile strength of the T6-treated specimen was higher than that of the T4-treated one. However, the strength-ductility balance was much better in the T4-treated specimen than the T6-treated one. The tensile properties of the Al sheets fabricated in the present study were compared with those in a previous study.

Effect on Anodizing Oxide Film for Aluminum 6061-T6 Alloy on Corrosion and Stress Corrosion Cracking in Seawater (알루미늄 6061-T6 합금에 대한 양극산화층이 해수 내 부식 및 응력부식균열에 미치는 영향)

  • Shin, Dong-Ho;Hwang, Hyun-kyu;Jung, Kwang-Hu;Kim, Seong-Jong
    • Journal of the Korean institute of surface engineering
    • /
    • v.53 no.5
    • /
    • pp.219-226
    • /
    • 2020
  • This paper investigated the characteristics of anodized aluminum 6061-T6 alloy for corrosion and stress corrosion cracking(SCC) under natural seawater. The hard anodizing oxide film formed on the 6061-T6 was a uniform thickness of about 25 ㎛. The corrosion characteristics were performed with a potentiodynamic polarization test. SCC was characterized by a slow strain rate tensile test under 0.005mm/min rate. As a result, the anodizing film showed no significant effect on SCC in the slow strain rate test. However, the corrosion current density of base metal was measured to be approximately 13 times higher than that of the anodized specimen. Therefore, the anodizing film significantly improved the corrosion resistance of 6061-T6 alloy in natural seawater.

Evaluation of Electrochemical Characteristic and Investigation on Optimum Condition in Friction Stir Welding for 6061-T6 Al Alloy (6061-T6 합금의 최적 마찰교반 용접 조건 규명 및 전기화학적 특성 평가)

  • Kim, Seong-Jong;Jang, Seok-Ki
    • Journal of the Korean institute of surface engineering
    • /
    • v.41 no.6
    • /
    • pp.341-350
    • /
    • 2008
  • In friction stir welding for 6061-T6 with various traveling speed and rotation speed conditions, the best mechanical characteristics presented in traveling speed of 507 mm/min and rotation speed of 1100RPM. The maximum tensile strength and yield strength increased with the increasing of traveling speed. The result of the electrochemical characteristic evaluation in friction stir welding at optimum conditions for 6061-T6 Al alloy presented a good characteristics compare to base metal.

Erosion Corrosion Characteristics of Al5052-O and Al6061-T6 Aluminum Alloys with Flow Rate of Seawater (해수 유속 변화에 따른 Al5052-O와 Al6061-T6 알루미늄 합금의 침식부식 특성)

  • Kim, Young-Bok;Kim, Seong-Jong
    • Corrosion Science and Technology
    • /
    • v.18 no.6
    • /
    • pp.292-299
    • /
    • 2019
  • The hull material of a high-speed ship may cause erosion damage from fluid impact. When physical erosion and electrochemical corrosion combine, erosion corrosion damage occurs. The aluminum ship is vulnerable to erosion corrosion because it can be operated at high speed. Thus, in this study, Al5052-O and Al6061-T6 aluminum alloys for the marine environment were selected as experimental materials. The erosion corrosion resistance of Al5052-O and Al6061-T6 aluminum alloys in seawater was investigated by an erosion test and potentiodynamic polarization test at the various flow rate (0 m/s, 5 m/s, 10 m/s, 15 m/s, 20 m/s). Erosion corrosion characteristics were evaluated by surface analysis, 3D analysis, SEM analysis, and the Tafel extrapolation method. The results of surface damage analysis after the erosion test showed that Al6061-T6 presented better erosion resistance than Al5052-O. The results of the potentiodynamic polarization test at the various flow rate, corrosion current density by Tafel extrapolation presented lower values of Al6061-T6 than Al5052-O. Al5052-O showed more surface damage than Al6061-T6 at all flow rates. Consequently, Al6061-T6 presented better erosion corrosion resistance than Al5052-O. The results of this study are valuable data for selecting hull material for an aluminum alloy vessel.

A Study on Deformation Behaviors of Al 6061, 7075 Tube at Different Heat Treatments for Warm Hydroforming (온간액압성형공정 적용을 위한 알루미늄 6061, 7075 튜브의 열처리조건에 따른 변형특성연구)

  • Yi, Hyae-Kyung;Moon, Young Hoon
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.20 no.1
    • /
    • pp.1-10
    • /
    • 2007
  • The deformation behaviors of full annealed and T6 treated 6061, 7075 aluminum tubes are investigated at various temperature performing uniaxial tensile test. Full annealed Al 6061 and Al7075 tubes, and T6 treated Al7075 tube don't show sharp local necking with an elongation of 50% at $300^{\circ}C$. So it is expected that influenced by elevated tempterature. At $300^{\circ}C$ and strain rate of 0.001/s, many micro-cracks are observed in T6 treated Al 6061 tube, which is believed to be responsible for the decrease of total elongation.

Ultrasonic linear and nonlinear properties of fatigued aluminium 6061-T6 with voids (기공을 포함한 피로손상 알루미늄 6061-T6의 초음파 특성평가)

  • Kang, To;Song, Sung-Jin;Na, Jeong K.;Park, Jin-Ho
    • Journal of the Korean Institute of Gas
    • /
    • v.19 no.5
    • /
    • pp.41-46
    • /
    • 2015
  • It is known that in aluminum 6061-T6, which is composed of $Mg_2Si$ and ${\beta}-Al_5FeSi$, void nucleation grows around ${\beta}-Al_5FeSi$ of Al606-T6. In this work, growth of voids was checked by scanning a 6061-T6 specimen with SEM observation. The effects of dislocation damping, coherency strain and voids on ultrasonic attenuation and nonlinearity parameters were experimentally measured. It was observed that a nonlinearity parameter increases until 75 percent of fatigue life and decreases after that. From the results, the authors inferred that dislocation damping and coherency damping increase nonlinearity parameters and void nucleation decreases them as ultrasonic scattering increases with void. The application of nonlinearity parameters in estimating degradation of materials with complex microstructures through fatigue process, therefore, should be carefully considered.