알루미늄 합금 6061에서 와이어 진동부가에 의한 와이어 컷 방전가공에 따른 표면 거칠기 특성 (III) (Characteristics of Surface Roughness According to Wire Vibration and Wire-cut Electric Discharge Machining of Aluminum Alloy 6061 (III))

  • 류청원;최성대
    • 한국기계가공학회지
    • /
    • 제15권1호
    • /
    • pp.81-88
    • /
    • 2016
  • Recently, high-efficiency machining in the production of high-value products with complex shapes has constantly been required along with the need for hybrid machining. In this study, in addition to wire-cut Electric Discharge Machining (EDM) and vibration, we present the possibility of a hybrid process by carrying out an experiment with aluminum alloy, and the hybrid process determines the nature of the surface. The selected experimental parameters are waveform, amplitude, peak current, and two-dimensional (2D) vibration. The experimental results give the guideline for selecting reasonable machining parameters. The surface roughness was improved about 20% with increases in the amplitude of the vibration.

전자교반을 응용한 Al6061 레오로지 소재의 단조공정 (Forging Process with Al6061 Alloy Rheology Material by Electromagnetic Stirring System)

  • 강성식;오세웅;강충길
    • 소성∙가공
    • /
    • 제16권6호
    • /
    • pp.443-446
    • /
    • 2007
  • The semi-solid process has been developed near net-shape components for kinds of methods. Thixo-forming with reheating prepared billet and rheo-forming with cooled melt until semi-solid state. Material is applied electromagnetic stirring system to slurry with aluminum 6061 alloy. An experiment has variation factors which are pressure, solid-fraction, stirring current and stirring time. The mechanical properties are compared to forge sample with to apply heat treatment T6. This study is researched function a virtual pressure and fine shape zone. Optimum pressure is found to prevent defect of porosity.

근사 상사 이론을 이용한 비축대칭 등온 단조의 가공하중 예측 (Prediction of the Forming Load of Non-Axisymmetric Isothermal Forging using Approximate Similarity Theory)

  • 최철현
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 춘계학술대회논문집
    • /
    • pp.71-75
    • /
    • 1999
  • An approximate similarity theory has been applied to predict the forming load of non-axisymmetric forging of aluminum alloys through model material tests. The approximate similarity theory is applicable when strain rate sensitivity geometrical size and die velocity of model materials are different from those of real materials. Actually the forming load of yoke which is an automobile part made of aluminum alloys(Al-6061) is predicted by using this approximate similarity theory. Firstly upset forging tests are have been carried out to determine the flow curves of three model materials and aluminum alloy(Al-6061) and a suitable model material is selected for model material test of Al-6061 And then and forging tests of aluminum yokes have been performed to verify the forming load predicted from the model material which has been selected from above upset forging tests, The forming loads of aluminum yoke forging predicted by this approximate similarity theory are in good agreement with the experimental results of Al-6061 and the results of finite element analysis using DEFORM-3D.

  • PDF

Al 6061의 초정밀 절삭특성 (Ultra Precision cutting Characteristics for Al 6061)

  • 박상진
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2000년도 춘계학술대회논문집 - 한국공작기계학회
    • /
    • pp.591-596
    • /
    • 2000
  • The needs of ultra precision machined parts is increase every days. But the experimental data of nonferrous metal is insufficient. The cutting behavior in micro cutting area is different from that of traditional cutting because of the size effect. Al6061 is widely used as optical parts such as LASER reflector's mirror or multimedia instrument. Al6061 opper is machined by ultra precision machine with natural diamond tool. From the experiment and discussion on the cutting force and worked surface roughness as the variable spindle speed, feed rate and depth of cut. As a result, the cutting force increases as the increasing depth of cut, but the worked surface roughness does not increase so much. The surface roughness is good when spindle sped is above 1200rpm, and feed rate is small. The influence of depth of cut is very small.

  • PDF

알루미늄 6061 합금의 열간단조시 변형율속도 및 변형율에 따른 기계적 성질에 관한 연구 (A Study on the Mechanical Properties with the Strain rate and Strain for Aluminum 6061 Alloy in Hot Forging)

  • 김정식;이영선;김용조;이정환
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.154-158
    • /
    • 2002
  • The mechanical properties of Al 6061 excluded bar were deformed in high temperature with the variable deformation conditions and characterized by the tensile test. Three types of different strain rate were experimentally performed by using hydraulic press, crank press and hammer and two types of the nominal strain 0.5 and 0.8 were achieved. To decide optimum forging process, the relationship among the strain rate, strain and mechanical properties was explained by analyzing the microstructures of the forged and heat heated parts. The strength was deeply related with the strain rate due to the dynamic recrystallization (DRX) in hot forging, and the best forging condition was presented in Al 6061 alloy.

  • PDF

A6061-T6과 A5052-H32재의 이종 마찰교반용접시 핀 형상이 기계적 강도에 미치는 영향에 관한 연구 (A Study on the Effect that Pin Shape on Mechanical Strength in Dissimilar Friction Stir Welding A6061-T6 and A5052-H32)

  • 박희상;최원두;고준빈;이영호;신기석;김인철;최만용
    • 한국생산제조학회지
    • /
    • 제18권3호
    • /
    • pp.270-278
    • /
    • 2009
  • Friction stir welding is a relatively new solid state joining process. A6061-T6 and A5052-H32 aluminium alloy has gathered wide acceptance in the fabrication of light weight structures requiring a high strength to weight ratio and good corrosion resistance. This friction stir process uses a non-consumable tool to generate frictional heat in the abutting surfaces. The welding parameters such as tool rotational speed, welding speed, etc., and tool pin profile play a major role in deciding FSP zone formation in A6061-T6 and A5052-H32 aluminium alloy. Three different tool pin profiles have been used to fabricate the dissimilar butt joints. The formation of friction stir processed zone has been analysed macroscopically. Tensile properties of the joints have been evaluated and correlated with the friction stir processed zone formation.

  • PDF

$SiCp/A\ell$ 6061 복합재료의 피로균열진전특성에 관한 통계학적 해석 (Statistical Analysis of Fatigue Crack Growth Properties for Silicon Carbide Particles Reinforced Metal Matrix Composites)

  • 권재도;문윤배;안정주
    • 한국자동차공학회논문집
    • /
    • 제4권4호
    • /
    • pp.130-139
    • /
    • 1996
  • The silicon carbide particles reinforced aluminium 6061($SiCp/A\ell$) composites are generally known have wild range of applications from automobiles to airospaces. But, by the results of existing study for $SiCp/A\ell$ composites, there are reports that the fatigue life of $SiCp/A\ell$ composites has improved than $A\ell$matrixes and has not improved then $A\ell$ matrixes. Consequently, in order to perform the reliable life prediction for $SiCp/A\ell$, the properties of probability distribution of fatigue crack initiation life & fracture life, crack growth length in constant number of cycles, crack growth rate in constant stress intensity factor range and m & C value in Paris's fatigue crack growth law and the estimation of statistical parameters have been evaluated by the statistics method.

  • PDF

알루미늄 튜브(A3003, A6061)의 축관률에 따른 두께 변화에 관한 연구 (A study on the thickness change according to the necking ratio of aluminum tube(A3003, A6061))

  • 오종성;민경호;이춘규
    • Design & Manufacturing
    • /
    • 제15권4호
    • /
    • pp.37-42
    • /
    • 2021
  • The tube necking process increases the thickness of the material, and some of the tube necking products require cutting on the inside of the formed product as a post-process. In order to prevent over-cutting or un-cutting due to increased thickness during cutting, it is necessary to know in advance the increase in thickness after forming. Therefore, in this study, the thickness change according to the tube necking was observed. Aluminum 3003-F and 6061-O were used for the materials used in the experiment, and necking was carried out up to 50% of the outer diameter of the tube through five processes. The two materials were formed under the same conditions, and the thickness of three points was observed in each process. In addition, the thickness increase of the two materials was compared, and the trend of thickness increase according to the cumulative necking ratio was observed. As a result of the experiment, both materials had the smallest thickness at the end of the formed product. In addition, as a result of comparing the thickness measurement values of the two materials, the maximum difference was 0.1mm, indicating that there was no difference in thickness between the two materials.

경량 재료를 이용한 DCB 시험편의 열림 모드에서의 파손 특성에 관한 연구 (A Study on Fracture Characteristics in Opening Mode of a DCB Specimen Using a Lightweight Material)

  • 김재원;조재웅
    • 한국기계가공학회지
    • /
    • 제20권1호
    • /
    • pp.42-47
    • /
    • 2021
  • Recently, many structures using lightweight materials have been developed. This study was conducted by using Al6061-T6 and carbon fiber reinforced plastic (CFRP), two common lightweight materials. In addition, the failure characteristics of an interface bonded between a single material and a heterogeneous bonding material were analyzed. The specimens bonded with CFRP and Al6061-T6 were utilized by the combination of the heterogeneous bonding material. The specimens had a double cantilevered shape and the bonding between the materials was achieved by applying a structural adhesive. The experiments were conducted in opening mode: the lower part of the samples was fixed, while their upper part was subjected to a forced displacement of 3 mm/min by using a tensile tester. Under the tested amount of strength, energy release rate, and considering the specimens' fracture characteristics in opening mode, the specimen "CFRP-Al" presented the maximum stress, followed by "Al" and "CFRP". We can hence conclude that the inhomogeneous material "CFRP-Al" is useful for the construction of lightweight structures bonded with structural adhesive.

MICROSTRUCTURAL CHARACTERISTICS OF HOT FORGED AL 6061 ALLOY

  • Kwon Y.-N.;Lee Y.-S.;Lee J.-H.
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 The 8th Asian Symposium on Precision Forging ASPF
    • /
    • pp.55-58
    • /
    • 2003
  • Many researches have been already done on the issues of high temperature deformation and the microstructural evolution. The information has been very useful for the plasticity industry, especially successful for the extrusion. However, the parts made with forging usually have a complex shape. It is difficult to control the distribution of the variables like strain, strain rate and temperature rise due to the working heat during a hot-forging process. Consequently, the microstructural variation could be occurred depending on the plastic deformation history that the forged part would get during a hot forging. In the present study, the microstructural characteristic of a hot-forged 6061 aluminum alloy has been discussed on the aspect of grain size evolution. A forging of 6061 aluminum alloy has been carried out for a complex shape with a dimensional variation. Also, finite element analysis has been done to understand how the deformation variables such as strain, strain rate give an influence on the microstructure of a hot forged aluminum product.

  • PDF