Tribological Characteristics of Si-Diamond-Like Carbon Films in a Condition with Carbon Nanotube Ink Lubricant (Carbon Nanotube 잉크 환경에서의 Si-Diamond-Like Carbon 박막의 내마모 특성)

  • Jang, Kil-Chan;Kim, Tae-Gyu
    • Korean Journal of Materials Research
    • /
    • v.21 no.3
    • /
    • pp.149-155
    • /
    • 2011
  • We investigated tribological characteristics of diamond-like carbon (DLC) in a condition with carbon nanotube (CNT) content of 1wt% in aqueous solution. Si-DLC films were deposited by radio frequency plasma enhanced chemical vapor deposition (RF-PECVD) process on Al6061 aluminum alloy. In this study, the deposition of DLC films was carried out in vacuum with a chamber pressure of 10-5 to 10-3 Torr achieved by mechanical pump followed by turbo molecular pump. The surface adsorbed oxygen on the Aluminum substrates was removed by passing Ar gas for 10 minutes. The RF power was maintained at 500W throughout the experiment. A buffer layer of HMDSO was deposited on the substrate to improve the adhesion of DLC coating. At this point CH4 gas was introduced in the chamber using gas flow controller and DLC coating was deposited on the buffer layer along with HMDSO for 50 min. The thickness of 1 ${\mu}m$ was obtained for DLC films on aluminum substrates The tribological properties of as synthesized DLC films were analyzed by wear test in the presence of dry air, water and lubricant such as CNT ink.

Measurement of Cutting Force in Diamond Turning Process (다이아몬드 터닝의 절삭력 측정용 tool holder를 이용한 미세절삭력 특성 연구)

  • 정상화;김상석;도철진;홍권희;김건희
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2001.04a
    • /
    • pp.938-941
    • /
    • 2001
  • A tool holder system has been designed and builted to measure cutting forces in diamond turning. This system design includes a 3-component piezo-electric tranducer. Initial experiments with tool holder system included verification of its predicted dynamic characteristics as well as a detailed study of cutting parameters. In this research, tool holder system is modeled by considering the element dividing, material properties, and boundary conditions using MSC/PATRAN. Mode and frequency analysis of structure is simulated by MSC/NASTRAN, for the purpose of developing the effective design. In addition, tool holder system is verified by vibration test using accelerometer. Many cutting experiments have been conducted on 6061-T6 aluminum. Tests have involved investigation of velocity effects, and the effects of depth and feedrate on tool force. Cutting velocity has been determined to have negligible effects between 4 and 21㎧.(6) Forces generally increase with increasing depth of cut. Increasing feedrate does not necessarily lead to higher forces. Results suggest that a sample model may not be sufficient to describe the forces produced in the diamond turning process.

  • PDF

Analyzing Friction Coefficient and Wettability of Micro-Dimple Fabricated Using Elliptical Vibration Texturing Method (이중 주파수 타원형 진동 궤적법 기반 마이크로 딤플의 마찰계수 및 습윤성 분석)

  • Park, Gun Chul;Ko, Tae Jo;Kurniawan, Rendi;Ali, Saood
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.19 no.5
    • /
    • pp.38-44
    • /
    • 2020
  • Surface texturing of micro-dimples has been used in many manufacturing industries to reduce friction between two sliding contacted surfaces. Surface texturing decreases the frictional force owing to minimizing of the sliding contact area. In this paper, micro-dimples have been fabricated on an Al6061-T6 surface using a two-frequency elliptical vibration texturing (TFEVT) method. A high-frequency of 18 kHz and low-frequency of 250 Hz were applied to an elliptically-vibrated tool holder. The Stribeck curve was plotted to analyze the friction coefficient trends. Furthermore, the representative wetting index, such as the water contact angle (WCA), was measured by considering the friction coefficient. WCA is associated with micro-dimple density and associated parameters. Consequently, the dimpled surfaces with a low friction coefficient exhibited a relatively high WCA in the feed direction. According to the Stribeck curve, the dimpled surfaces demonstrate superior friction performance for mixed-film lubrication compared to the non-textured surface.

The Velocity Analysis of Woven Glass Fiber Composites Using Cross-correlation Properties (상호상관성를 이용한 망상형 유리섬유 복합체의 속도분석 연구)

  • Lee, Y.H.;Lee, S.H.
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.13 no.4
    • /
    • pp.18-24
    • /
    • 1994
  • This paper discusses experimental results obtained by the potentiality of cross-correlation function as a tool for analyzing propagation of wave in an aluminum and a woven glass fiber composite. Each propagated wave has its own characteristic time delay, and examination of the cross-correlation of input and output signal give the most proper wave velocity and significant path. Using the above distinctive features, we observed the propagation velocity for the aluminum alloy and a woven glass fiber composite more acurately and easily then the common methods. The fiber locations of this composite also determined by the basis of these results.

  • PDF

Electrochemical Evaluation of Corrosion Properties of Aluminum Alloy as a Sacrificial Anode for Offshore Structure Protection (해양구조물의 방식을 위한 알루미늄 합금의 희생양극적 부식 특성의 전기화학적 평가)

  • Rhee, Jin-Ho;Lee, Jae-Ho
    • Journal of the Korean institute of surface engineering
    • /
    • v.48 no.2
    • /
    • pp.68-72
    • /
    • 2015
  • The corrosion behavior of metals and alloys for the safety of offshore structures in seawater was investigated for the application of sacrificial anodes. The experiments were focused on the polarization behaviors and the surface morphology of each metal after experiments. Pure Zn, pure Al (Al1050), Al alloys (Al5052, Al6061), Mg alloys (AZ31, AZ91D) and steel (SCM440) were assessed in 3.5% sodium chloride solution by means of potentiodynamic polarization to verify the galvanic corrosion potential ($E_{couple}$). Potentiostat plots were plotted to compare the surface and corrosion current density ($i_{couple}$) of metals as sacrificial anodes in seawater to protect steel alloy as a cathode. Al alloys showed the best performance as a sacrificial anode, on the other hand, Mg alloys showed overprotection behavior. The surface morphologies of sacrificial anodes were observed by FESEM and compared.

Improvement of Cutting Performance of DLC Coated WC against Al Alloy (DLC박막을 코팅한 초경공구의 Al합금에 대한 절삭성능 향상)

  • Lee, K.Y.
    • Journal of Power System Engineering
    • /
    • v.12 no.3
    • /
    • pp.66-71
    • /
    • 2008
  • Diamond-like-carbon (DLC) coatings could be good candidates as solid lubricants for cutting tools in dry machining of aluminum alloy. In this work, DLC thin films were produced as a friction reduction coating for WC-Co insert tip using the plasma immersion ion beam deposition (PIIED) technique. DLC coatings were also coated on $Al_2O_3$ specimens and high temperature wear tested up to $400^{\circ}C$ in dry air to observe the survivability of the DLC coating in simulated severe cutting conditions using a pin-on-disc tribotester with Hertzian contact stress of 1.3GPa. It showed reduced friction coefficients of minimum 0.02 up to $400^{\circ}C$. And cutting performance of DLC coated WC-Co insert tips to Al 6061 alloy were conducted in a high speed machining center. The main problems of built-up edge formation in aluminum machining are drastically reduced with improved surface roughness. The improvements were mainly related to the low friction coefficient of DLC to Al alloy and the anti-adhesion of Al alloy to WE due to the inertness of DLC.

  • PDF

Repair of Mold by Cold Spray Deposition and Mechanical Machining (저온 분사 적층과 절삭가공을 이용한 금형보수 사례연구)

  • Kang Hyuk-Jin;Jung Woo-Gyun;Chu Won-Sik;Ahn Sung-Hoon
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.23 no.7 s.184
    • /
    • pp.101-107
    • /
    • 2006
  • Cold gas dynamic spray or cold spray is a novel manufacturing method for coatings. Cold spray is a high rate and direct material deposition process that utilizes the kinetic energy of particles sprayed at high velocity (300-1,200m/s). In this research, a technique to repair the damaged mold by cold spray deposition and mechanical machining was proposed. An aluminum 6061 mold with three-dimensional surface was fabricated, intentionally damaged and material-added by cold spray, and its original geometry was re-obtained successfully by Computer Numerical Control (CNC) machining. To investigate deformation of material caused by cold spray, deposition was conducted on thin aluminum plates ($100mm{\times}100mm{\times}3mm$). The average deformation of the plates was $205{\sim}290{\mu}m$ by Coordinate Measurement Machine (CMM). In addition, the cross section of deposited layer was analyzed by scanning electron microscopy (SEM). To compare variation of hardness, Vickers hardness was measured by micro-hardness tester.

A Characteristics of Thick and Hard Al-Cu Alloy by Overlaying Welding Process (오버레이 용접법에 의한 Al-Cu 합금 경화후막의 특성)

  • 박정식;양변모;박경재
    • Journal of Welding and Joining
    • /
    • v.14 no.4
    • /
    • pp.53-61
    • /
    • 1996
  • It was attempted to improve the wear resistance of Al alloy under the load condition by making a formation of the thicker surface hardening alloy layers. The thicker surface hardening alloy layers were formed on 6061 Al alloys overlayed by MIG and TIG welding process with Cu powders feeding. The characteristics of hardening and wear resistance have been investigated in relation to the microstructures of alloyed layers, with a selection of optimum alloying conditions for formation of overlaying layer. The results obtained were summarized as follows With increasing feeding rate of Cu powders by MIG welding, the hardness and specific wear of the overlay weld alloys were increased. It is considered that these high hardness and specific wear of overlay weld alloys were due to the formation of Θ($Al_2Cu$) phases. With increasing feeding rate of Cu powders by TIG welding, the hardness and specific wear of the overlay weld alloys were increased in feeding rates 12 and 18g/min. However, the hardness and specific wear were decreased in the powder feeding rate 38g/min. It is considered that considered that decrease of hardness and specific wear in the powder feeding rate 38g/min due to formation of ${\gamma}$($Al_4Cu_9$) phases.

  • PDF

Optical Image Split-encryption Based on Object Plane for Completely Removing the Silhouette Problem

  • Li, Weina;Phan, Anh-Hoang;Jeon, Seok-Hee;Kim, Nam
    • Journal of the Optical Society of Korea
    • /
    • v.17 no.5
    • /
    • pp.384-391
    • /
    • 2013
  • We propose a split-encryption scheme on converting original images to multiple ciphertexts. This conversion introduces one random phase-only function (POF) to influence phase distribution of the preliminary ciphertexts. In the encryption process, the original image is mathematically split into two POFs. Then, they are modulated on a spatial light modulator one after another. And subsequently two final ciphertexts are generated by utilizing two-step phase-shifting interferometry. In the decryption process, a high-quality reconstructed image with relative error $RE=7.6061{\times}10^{-31}$ can be achieved only when the summation of the two ciphertexts is Fresnel-transformed to the reconstructed plane. During the verification process, any silhouette information was invisible in the two reconstructed images from different single ciphertexts. Both of the two single REs are more than 0.6, which is better than in previous research. Moreover, this proposed scheme works well with gray images.

Spreading and Deposition Characteristics of a Water Droplet Impacting on Hydrophobic Textured Surfaces (소수성 텍스쳐 표면에 충돌한 단일 액적의 퍼짐 및 고착 특성)

  • Lee, Jae-Bong;Moon, Joo-Hyun;Lee, Seong-Hyuk
    • Journal of ILASS-Korea
    • /
    • v.17 no.1
    • /
    • pp.14-19
    • /
    • 2012
  • The present study conducts experimental investigation on spreading and deposition characteristics of a $4.3{\mu}l$ de-ionized (DI) water droplet impacting upon aluminum (Al 6061) flat and textured surfaces. The micro-textured surface consisted the micro-hole arrays (hole diameter: $125{\mu}m$, hole depth: $125{\mu}m$) fabricated by the conventional micro-computer numerical control (${\mu}$-CNC) milling machine process. We examined the surface effect of texture area fraction ${\varphi}_s$ ranging from 0 to 0.57 and impact velocity of droplet ranging from 0.40 m/s to 1.45 m/s on spreading and deposition characteristics from captured images. We used a high-speed camera to capture sequential images for investigate spreading characteristics and the image sensor to capture image of final equilibrium deposition droplet for analyze spreading diameter and contact angle. We found that the deposition droplet on textured surfaces have different wetting states. When the impact velocity is low, the non-wetting state partially exists, whereas over 0.64 m/s of impact velocity, totally wetting state is more prominent due to the increase kinetic energy of impinging droplet.