• Title/Summary/Keyword: A6061

Search Result 387, Processing Time 0.025 seconds

Metal Flow and Interface Bonding of Copper Clad Aluminum Rods by the Direct Extrusion (직접압출에 의한 Cu-Al 층상 복합재료 봉의 금속유동과 계면접합)

  • Yun, Yeo-Kwon;Kim, Hee-Nam
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.18 no.6
    • /
    • pp.166-173
    • /
    • 2001
  • Composite materials consists of two or more different material layers. The usefulness of clad metal rods forms the possibilities of combination of properties of different metals. Copper clad aluminum composite materials are being used for economic and structural purpose. In this study, composite billet consists of commercially pure copper and aluminum(A6061) and experimental conditions consist of the combinations of clad thickness, extrusion ratio, and semi-cone angle of die. In order to investigate the influence of these parameters on the hot direct extrudability of the copper clad aluminum composite material rods, the experimental study have been performed with various extrusion temperatures, extrusion ratios, semi-cone angles of die, and composition rate of Cu:Al.

  • PDF

Characteristics of Elastic Waves Generated by Fatigue Crack Penetration and Growth in an Aluminum Plate

  • Ahn, Seok-Hwan;Nam, Ki-Woo
    • Journal of Mechanical Science and Technology
    • /
    • v.17 no.11
    • /
    • pp.1599-1607
    • /
    • 2003
  • The characteristics of elastic waves emanated from crack initiation in 6061 aluminum alloy subjected to fatigue loading are investigated through experiments. The objective of the study is to determine the differences in the properties of the signals generated from fatigue test and also to examine if the sources of the waves could be identified from the temporal and spectral characteristics of the acoustic emission (AE) waveforms. The signals are recorded using nonresonant, flat, broadband transducers attached to the surface of the alloy specimens. The time dependence and power spectra of the signals recorded during the tests were examined and classified according to their special features. Six distinct types of signals were observed. The waveforms and their power spectra were found to be dependent on the crack propagation stage and the type of fracture associated with the signals. The potential application of the approach in health monitoring of structural components using a network of surface mounted broadband sensors is discussed.

Friction Welding of Sintered Hard Tool Materials to Metals and Its Quality Evaluation by AE (마찰용접에 의한 초경공구재와 금속간의 압접기술개발과 AE에 의한 품질평가)

  • 오세규;전태언;박일동;오명석;이주석
    • Journal of Ocean Engineering and Technology
    • /
    • v.10 no.1
    • /
    • pp.36-46
    • /
    • 1996
  • This paper deals with determinig the proper friction welding condition and analyzing various mechanical properties of friction welded joints of sintered carbide tool materials(K20, P25, and SKDX5 for the blade part of drill or press punch) to alloy steel (SKH4, SCM440 for the shank part of drill or press punch), the alloy steel to aluminum(A6061 for the interlayer material between the blade part and the shank) and sintered carbide tool materials to alumminum. And also acoustic emission test will be carried out during fiction welding to evaluate the weld quality.

  • PDF

Dynamic deformation behavior of aluminum alloys under high strain rate compressive/tensile loading (상용 알루미늄 합금의 고속 인장/압축 변형거동 규명)

  • Lee, O.S.;Kim, G.H.;Kim, M.S.;Hwang, S.W.
    • Proceedings of the KSME Conference
    • /
    • 2000.11a
    • /
    • pp.268-273
    • /
    • 2000
  • Mechanical properties of the materials used for transportations and industrial machinery under high strain rate loading conditions are required to provide appropriate safety assessment to these mechanical structures. The Split Hopkinson Pressure Bar(SHPB) technique, a special experimental apparatus, can be used to obtain the material behavior under high strain rate loading condition. In this paper, dynamic deformation behaviors of the aluminum alloys, Al2024-T4, Al6061-T6 and Al7075-T6, under high strain rate compressive and tensile loading are determined using SHPB technique.

  • PDF

Measurements of Micro-Defects in the Aluminum Thixoformed Part using Computed Tomography(CT) Technology (CT를 이용한 알루미늄 반응고 성형품의 미세 결함 측정)

  • Lee, S.Y.;Kim, C.H.
    • Transactions of Materials Processing
    • /
    • v.18 no.5
    • /
    • pp.422-427
    • /
    • 2009
  • Computed tomography(CT) has been applied to measure micro-defects in the aluminum knuckle parts manufactured by the thixoforming process. 6061 aluminum alloys were used to form knuckle samples in the semi-solid temperature after the SIMA processing of billets. Tensile specimens were cut from the different locations in a thixoformed knuckle. The size and the distribution of forming defects in tensile specimens were analyzed using CT scanning and image analysis technology before tensile tests. It has been qualitatively shown that the stress-strain curves were significantly affected by the size and the distribution of forming defects although the defect sizes lie in the range of micro-meters.

The preparation of Al-Si alloy welding rod by the horizontal continuous casting process with the heating mold (가열주형 수평식연속주조법에 의한 Al-Si 합금 용접봉 제조)

  • 김원태;김명한;이보영
    • Journal of Welding and Joining
    • /
    • v.12 no.3
    • /
    • pp.101-108
    • /
    • 1994
  • The horizontal continuous casting process with the heating mold was adopted for fabricating defect-free 4043 Al alloy rods of 3.2m dia. with mirror surfaces. These rods were drawn into 2.4mm dia. rods for GTAW welding. The GTAW welding tests were carried out by use of these welding rods with 6061 Al alloy as a base metal. After welding, the X-ray tests, tensile strength tests, bending tests, and microstructural analysis of welded zone and HAZ were carried out. The results represented that the welding rods with good surfaces and welding properties could be made by the horizontal continuous casting, and followed by the drawing process.

  • PDF

Solid State Diffusion Brazing of the Aluminum Alloy Castings According to the Heat Treatment Conditions (열처리온도 및 시간에 따른 알루미늄 주조재의 고상확산 접합 특성)

  • Sun, J.H.;Shin, S.Y.;Hong, J.W.
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.21 no.6
    • /
    • pp.300-306
    • /
    • 2008
  • Solid state diffusion brazing of aluminum castings (AC4C) and wrought alloys (Al6061) was conducted in order to improve thermal conductivity and temperature uniformity of the aluminum heater which was generally fabricated by casting method. Tensile strength and thermal conductivity are raised with increasing brazing temperature, obtaining 122.5 MPa and $206W/m{\cdot}K$ at $540^{\circ}C$ 5hrs brazing conditions, respectively. The diffusion brazed heater, shows maximum temperature difference of $4^{\circ}C$, exhibits a enhanced temperature uniformity compared with the cast heater having the maximum temperature difference of $11^{\circ}C$.

Characteristics of Bending Strength on Coating Condition of Metal Surface Polyurethan Coating Material (금속표면에 폴리우레탄코팅한 소재의 코팅조건 변화에 따른 굽힘강도 특성)

  • 이강길
    • Journal of Ocean Engineering and Technology
    • /
    • v.15 no.2
    • /
    • pp.124-129
    • /
    • 2001
  • The research on anticorrosive of valve for ship, waterworks, and drainage system is very important. The purpose of this paper is to develop the metal/polyurethan adhesive technique at insider of the value to prevent corrosion in the value. It is performed to the bending strength test by using metal /polyurethan in the metals (SB41, Al6061). It is investigated to the effects of bending strength on curing temperature, preheating time and curing time, and to the fracture mechanism of metal/polyurethan adhensived specimen. As a results, we find that the bending strength is the highest at curing temperature of 11$0^{\circ}C$ and the curing time is 60 minutes in metal/polyurethan adhesive specimen.

  • PDF

Deposition of Diamond Like Carbon Thin Films by PECVD (PECVD법에 의한 DLC 박막의 증착)

  • 김상호;김동원
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.2
    • /
    • pp.122-128
    • /
    • 2002
  • This study was conducted to synthesize the diamond like carbon films by plasma enhanced chemical vapor deposition (PECVD). The effects of gas composition on growth and mechanical properties of the films were investigated. A little amount of hydrogen or oxygen were added to base gas mixture of methane and argon. Methane dissociation and diamond like carbon nucleation were enhanced by installing negatively bias grid near substrate. The deposited films were indentified as hard diamond like carbon films by micro-Raman spectroscopy. The surface and fractured cross section of the films which were observed by scanning electron microscopy showed that film growth is very slow as about 0.3$\mu\textrm{m}$/hour, and relatively uniform with hydrogen addition. Vickers hardness of tungsten carbide (WC) cutting tool increased from about 1000 to 1600~1800 by deposition of DLC film, that of commercial TiN coated tool was about 1270. In cutting test of aluminum 6061 alloy, DLC coated cutting tool showed 1/3 or lower crater and flank wear than TiN coated or non-coated WC cutting tools.

Enhanced Properties of Aluminum Oxide Layers with Post Heat Treatment (후열처리에 의한 알루미늄 산화층의 특성 향상)

  • Jeon, Yoonnam;Kim, Sangjun;Park, Jihyun;Jeong, Nagyeom
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.5
    • /
    • pp.275-281
    • /
    • 2019
  • Anodization is widely used to enhance the properties of aluminum, such as hardness, electric resistance, abrasion resistance, corrosion resistance etc. But these properties can be enhanced with additional process. According to the partial crystallization of oxide layer with post heat treatment, enhanced hardness can be expected with partial crystallization. In this study, post heat treatments were applied to the anodized aluminum alloys of Al6061 to achieve the partial crystallization, and crystallizations were evaluated with the reduced breakdown voltages. Interestingly, remarkable enhanced hardness (21~29%), abrasion resistance (26~62%), and reduced breakdown voltage (24~44%) were observed for the sulfuric acid anodized samples when we annealed the anodized samples with 1hour post heat treatment at $360^{\circ}C$. For the Al5052 alloys, a lot of cracks were observed when we applied the post heat treatment.