• Title/Summary/Keyword: A5052

Search Result 145, Processing Time 0.029 seconds

Evolution of strain states during Cross-roll rolling in AA 5052 sheet using Finite Element Method (유한요소 해석을 통한 AA 5052 판재의 Cross-roll 압연시 변형율 상태의 변화)

  • Kim, S.H.;Kim, D.G.;Park, E.S.;Lee, J.S.;Huh, M.Y.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.05a
    • /
    • pp.404-407
    • /
    • 2008
  • In the present work, cross-roll rolling was carried out using a rolling mill in which the roll axis is tilted by $7.5^{\circ}$ towards the transverse direction of the rolled sample. The evolution of strain states during cross-roll rolling was investigated by three-dimensional finite element method (FEM) simulation. Parallel to cross-roll rolling, normal-rolling using a conventional rolling mill was also carried out in the same rolling condition for clarifying the effect of cross-roll rolling. It turned out that three shear rate components were all introduced to the rolled sample by the cross-roll rolling process, while only one shear rate component operated during normal-rolling.

  • PDF

Joining Ability and Mechanical Properties of Friction Stir Lap Welded A5052-H112 Alloy (A5052-H112 합금의 겹치기 마찰교반접합 건전성)

  • Ko, Young-Bong;Choi, Jun-Woong;Park, Kyeung-Chae
    • Journal of Welding and Joining
    • /
    • v.28 no.1
    • /
    • pp.34-40
    • /
    • 2010
  • In Friction Stir Lap Welding(FSLW), the movement of material within the weld was more important than the microstructure, due to the interface present between the sheets. Thus, The soundness of free defect, Effective Sheet Thickness(EST) and width of joint were most important factor of mechanical properties. Specimens by lap joint types that were 'A-type' and 'R-type' were made in this study. A-type tensile specimen was loaded at advancing side and R-type tensile specimen was loaded at retreating side. Macro-, micro-structural observation and mechanical properties of FSLW A5052-H112 alloy ware investigated under varying rotating and welding speed. The results were as follows: Material hook formed decreasing after sharply increasing was appeared at the end interface of joint area in advanced side, and material hook formed decreasing after smoothly increasing was observed at that in retreated side. Tensile load had no relation with defects. As rotating speed was higher, tensile strength was increasing and EST was decreasing regardless of joint types. joint efficiency was over 70%. In a result of fractography, fracture in A-type was partially occurred by dimple in SZ, and fracture in R-type was generally occurred by dimple in HAZ.

A Study on Electron Beam Weldmetal Cross Section Shapes and Strength of Al 5052 Thick Plate (Al 5052 함금 후판재의 전자빔 용접부 단면 형상과 강도에 관한 연구)

  • Kim, In-Ho;Lee, Gil-Young;Ju, Jeong-Min;Park, Kyoung-Tae;Chun, Byong-Sun
    • Journal of Welding and Joining
    • /
    • v.27 no.3
    • /
    • pp.73-79
    • /
    • 2009
  • This present paper investigated the mechanical properties and the microstructures of each penetration shapes classifying the conduction shape area and the keyhole shape area about electron beam welded 120(T)mm thick plated aluminum 5052 112H. As a result the penetration depth is increased linearly according to the output power, but the aspect ratio is decreased after the regular output power. In the conduction shape area, the Heat affected zone is observed relatively wider than the keyhole shape area. In the material front surface of the welded specimen, the width is decreased but the width in the material rear surface is increased. After the measuring the Micro Vikers Hardness, it showed almost similar hardness range in all parts, and after testing the tensile strength, the ultimate tensile strength is similar to the ultimate tensile strength of the base material in all the specimens, also the fracture point was generated in the base materials of all the samples. In the result of the impact test, impact absorbed energy of the Keyhole shape area is turned up very high, and also shown up the effect about four times of fracture toughness comparing the base material. In the last result of observing the fractographs, typical ductile fraction is shown in each weld metal, and in the basic material, the dimple fraction is shown. The weld metals are shown that there are no other developments of any new chemical compound during the fastness melting and solidification.

Study on Improvement of Measurement Precision in Digital Image Correlation Measurement Method by Using Subpixel Algorithms (이미지 상관법의 서브 픽셀 알고리즘을 이용한 측정 분해능 향상에 관한 연구)

  • Kim, Seung Jong;Kang, Young Jun;Choi, In Young;Hong, Kyung Min;Ryu, Won Jea
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.32 no.12
    • /
    • pp.1039-1047
    • /
    • 2015
  • Contact type sensors (e.g., displacement sensor and strain gauge) were typically used to evaluate the safety and mechanical properties in machines and construction. However, those contact type sensors have been constrained because of measurement problems such as surface roughness, temperature, humidity, and shape. The Digital Image Correlation (DIC) measurement system is a vision measurement system. This measurement system uses the taken image using a CCD camera and calculates the image correlation between the reference image and the deformed image under external force to measure the displacement and strain rates. In this paper, we discuss methods to improve the measurement precision of the digital image correlation measurement system. A tensile test was conducted to compare the precision improvement effects, by using the universal test machine and the DIC measurement system, with the use of subpixel algorithms, i.e., the Coarse Fine Search (CFS) algorithm and the Peak Finding (PF) algorithm.

Corrosion Behavior of AZ31 Magnesium Alloy during Machining (AZ31 마그네슘 합금의 절삭가공과정에서의 부식거동)

  • Kim, Jae-Hak;Kwon, Sung-Eun;Lee, Seung-Jae
    • Journal of the Korea Institute of Military Science and Technology
    • /
    • v.15 no.3
    • /
    • pp.315-321
    • /
    • 2012
  • In the study, corrosion characteristics of AZ31 magnesium alloy under various environments exposed during machining(immersion in cutting oil, 5 % cutting oil aqueous solution and distilled water & contact with dissimilar metals, SPC4 and A5052-H32) were investigated. A corrosion test was performed AZ31 magnesium alloy was immersed in each electrolyte solution after contacting with each dissimilar metals, and the results were observed by an electron microscope. In immersion tests, corrosion of AZ31 magnesium alloy showed to be in the sequence of distilled water> 5 % cutting oil aqueous solution> cutting oil> air, and in the test of contact with dissimilar metals, corrosion showed to be in the sequence of SPC4> A5052-H32> AZ31. It can be concluded that to prevent corrosion during machining, AZ31 magnesium alloy must prevent contacting water and use magnesium alloy for raw material of Jig & Fixture.

Effect of Anodizing and Dyeing Treatments on Coloring of Al-Mg (Al-Mg합금의 컬러에 미치는 양극산화 및 착색처리의 영향)

  • Bae, Sung Hwa;Lee, Hyun Woo;Son, Injoon
    • Journal of the Korean institute of surface engineering
    • /
    • v.52 no.1
    • /
    • pp.30-36
    • /
    • 2019
  • In this study, we investigated the effects of anodizing time, dyeing treatment time, and variations in coloring concentration on the color of an AA5052 alloy processed by dye-treated anodizing. The outward color of the anodized film changed to deep red according to increases in anodizing time, dyeing treatment time, and coloring concentration; accordingly, lightness $L^*$ decreased and saturation $a^*$ and $b^*$ increased. The concentration of the dye and the UV-visible absorbance showed a nearly perfect linear relationship, allowing a quantitative analysis of the absorbed dye. Because the quantity of absorbed dye increased as anodizing time, dyeing treatment time, and coloring concentration increased, the outward color of the anodized film deepened. In addition, from the GD-OES depth profile, we found that the dye was preferentially absorbed on the surface of the porous anodized film.

Influence of shaving allowance and clearance in pre-shearing process for improving shaving accuracy (셰이빙 정밀도 향상을 위한 예비전단 가공에서의 가공여유와 틈새의 영향)

  • Oh, Sol-Kil;Jo, Dae-il;Kang, Byung-Du;Kim, Jong-Ho
    • Design & Manufacturing
    • /
    • v.2 no.3
    • /
    • pp.40-44
    • /
    • 2008
  • Shaving in sheet metal forming is defined as a finish process to make the sheared surface clean which was blanked or pierced in the previous shearing stage. In this study the new shaving technique is applied to the progressive operation. The specimen is automatically fed by continuous movement of the strip. Which improve the positioning accuracy higher. For this study a square part which consist of blanking and piercing is selected for investigation and the progressive die which includes pre-piercing, pierce-shaving, half-blanking and blank-shaving etc is prepared for specimens of steel sheet(SPCC) and aluminum alloy sheet(AL5052). Experiments are carried out for several working variables such as shaving allowance, pre-shearing clearance and relative half-blanking depth. Consequently it was confirmed that the shaving by progressive die can be successfully employed to produce the clean parts requiring shaving process and optimum working conditions for shaving SPCC and AL5052 sheet metal are shaving allowance of 0.2mm(1.3% of thickness) and pre-shearing clearance of 5%.

  • PDF

Classification of Acoustic Emission Signals from Fatigue Crack Propagation in 2024 and 5052 Aluminum Alloys

  • Nam, Ki-Woo;Moon, Chang-Kwon
    • International Journal of Ocean Engineering and Technology Speciallssue:Selected Papers
    • /
    • v.4 no.1
    • /
    • pp.51-55
    • /
    • 2001
  • The characteristics of elastic waves emanating from crack initiation in 2024 and 5052 aluminum alloys subject to static and fatigue loading are investigated through laboratory experiments. The objective of the study is to determine difference in the properties of the signals generated from static and fatigue tests and also to examine if the sources of the waves could be identified from the temporal and spectral characteristics of the acoustic emission (AE) waveforms. The signals are recoded using non-resonant, flat, broadband transducers attached to the surface of the alloy specimens. The time dependence and power spectra of the signals recorded during the tests were examined and classified according to their special features. Three distinct types of signals were observed. The waveforms and their power spectra were found to be dependent on the material and the type of fracture associated with the signals. Analysis of the waveforms indicated that some signals could be attributed to plastic deformation associated with static tests. The potential application of the approach in health monitoring of aging aircraft structures using a network of surface mounted broadband sensors is discussed.

  • PDF

A Study on Electrochemical Characteristics Aluminum Multi Matrix Compound (Al-MMC) of Neutron Absorber Material

  • Lee, Jung Hwan;Lee, Yunju;Yoo, Seung Chang;Kim, Seunghyun;Kim, Ji Hyun
    • Proceedings of the Korean Radioactive Waste Society Conference
    • /
    • 2018.11a
    • /
    • pp.179-180
    • /
    • 2018
  • Al - MMC, used as a neutron absorber, shows pitting corrosion and/or galvanic corrosion in 3.5wt.% NaCl solution. If pitting corrosion penetrates the core, neutron absorption performance could be affected. Galvanic corrosion was observed between Al 5052 and Al 1070, and pitting corrosion was observed around $B_4C$.

  • PDF

Crack Propagation Behavior for Variable Load in Cantilever Beam under Bending Load (굽힘하중의 받는 외팔보의 변동하중에 대한 균열진전 거동)

  • 김엽래
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1998.03a
    • /
    • pp.178-183
    • /
    • 1998
  • This paper examines the crack growth behavior of 7075-T651 and 5052-H32 aluminum alloys for variable load within tensile load range condition. The cantilever beam type specimen with a chevron notch is used in this study. The crack growth and closure are investgated by compliance method. The applied initial stress ratio is R=0.3 and variable load are R=0.65, 0.46. Crack length, stress intensity factor range, ratio of effective stress intensity factor range and crack growth rate etc. are inspected with fracture mechanics estimate.

  • PDF