열처리된 A3003 알루미늄합금 용접부의 미세조직 및 기계적 특성 (Microstructrue and Mechanical Properties of A3003 Aluminium Alloy Welds by Heat-treatment)

  • 이일천;송영종;국진선;윤동주;김병일
    • Journal of Welding and Joining
    • /
    • 제25권5호
    • /
    • pp.51-57
    • /
    • 2007
  • The present work was aimed to examine the variation of microstructure and mechanical properties by annealing($100{\sim}620^{\circ}C$, $2{\sim}8hr$) in A3003 Al alloy welded pipes. The A3003 Al alloy pipes with 34 mm in external diameter and 1.3 mm in thickness were manufactured by high frequency induction welding with the V shaped convergence angle $6.7^{\circ}$ and power input 50 kW. The tensile and yield strength decreased with increasing the annealing temperature remarkably, but elongation increased remarkably. Vickers hardness in welds decreased with increasing the annealing temperature remarkably. The primary intermetallic compound of $Al_{12}(Fe,\;Mn)_2Si$ was precipitated in welds as the same base metal. In a certain experimental condition, the welds line in A3003 alloys disappeared at $450^{\circ}C$ for 2 hr because of the same mechanical property and structure between welds and base metal.

고주파유도 용접된 A3003 알루미늄합금 튜브의 기계적 특성에 미치는 열처리조건의 영향 (Effects of Heat-treatment Parameters on Mechanical Properties of A3003 Al Alloy Tubes for Heat-exchangers by High Frequency Induction Welding)

  • 국진선;윤동주;김병일
    • 열처리공학회지
    • /
    • 제19권3호
    • /
    • pp.156-162
    • /
    • 2006
  • The aim of this study is to investigate the full annealing parameter for A3003 Al alloy welded tubes. The A3003 Al alloy tubes with 34 mm in external diameter and 1.3 mm in thickness for OPC drum were manufactured by high frequency induction welding with the V shaped convergence angle $6.7^{\circ}$ and power input 50 kW. The tensile and yield strength decreased with increasing the annealing temperature and time remarkably, but elongation increased remarkably. Vickers hardness in welds and base metal decreased with increasing the annealing temperature and time remarkably. In a certain experimental condition, the welds line in A3003 alloys disappeared at $520^{\circ}C$ for 4hr because of the same mechanical properties and structures between welds and base metal.

박판 A3003 Al합금의 Nd : YAG 레이저빔 용접에 관한 연구 (A Study on the Welding Behavior of A3003 Aluminium Alloy Thin Sheet by Nd : YAG Laser Beam)

  • 허인석;김병철;김도훈;김진수;이한용
    • 한국레이저가공학회지
    • /
    • 제4권1호
    • /
    • pp.29-38
    • /
    • 2001
  • This work was carried out to investigate the welding behavior of thin A3003 Al alloy sheets by Nd : YAG laser beam. Considering bead shape and mechanical properties, the laser pulse shapes selected were two kinds of 2-division and 3-division by varying power level and pulse duration. In order to obtain optimum conditions, the factorial design method and central composite design method were applied. Tensile test, optical microscopy, micro hardness test and TEM analysis were performed. Due to the annealing caused by thermal effect during laser welding, precipitates were coarsended. The HAZ was softened and failed during tensile test. The hardness of HAZ was lower than that of base metal, since the heat input relieved the work hardening effect and caused grain growth.

  • PDF

가스텅스텐아크 용접한 클래드(A4045/A3003) 알루미늄 합금의 기계적성질 및 미세조직 (Microstructure and Mechanical Properties of Clad(A4045/A3003) Al Alloy by Gas Tungsten Arc Welding)

  • 김기빈;국진선;윤동주;김병일;이일천
    • Journal of Welding and Joining
    • /
    • 제26권4호
    • /
    • pp.73-78
    • /
    • 2008
  • In this paper, research was the variation of microstructure and mechanical properties of clad(A4045/A3003) Al alloy sheet by gas tungsten arc welding. Tensile properties of the gas tungsten arc welding joint decreased because of the softened heat affected zone(HAZ). The hardness of HAZ was lower than that of base metal, because relieved the work hardening effect of the welding heat. Hardness distribution of the weld zone with the base metal appears similarly, but the hardness of HAZ decreased remarkably. The microstructure in the weld zone of A4045 clad layer was formed a coarse columner grains of Si-rich. In the case of large weld heat input, the Si of the A4045 were diffused and until A3003 weld zone they decreased the strength.

저온 브레이징용 Al-Si-Cu 합금의 Sn 첨가에 따른 융점 및 기계적 특성 변화 연구 (Effect of Tin Addition on the Melting Temperatures and Mechanical Properties of Al-Si-Cu Brazing Filler Metals)

  • 김민상;박천웅;변종민;김영도
    • 한국재료학회지
    • /
    • 제26권7호
    • /
    • pp.376-381
    • /
    • 2016
  • For the development of a low-melting point filler metal for brazing aluminum alloy, we analyzed change of melting point and wettability with addition of Sn into Al-20Cu-10Si filler metal. DSC results showed that the addition of 5 wt% Sn into the Al-20Cu-10Si filler metal caused its liquidus temperature to decrease by about 30 oC. In the wettability test, spread area of melted Al-Cu-Si-Sn alloy is increased through the addition of Sn from 1 to 5 wt%. For the measuring of the mechanical properties of the joint region, Al 3003 plate is brazed by Al-20Cu-10Si-5Sn filler metal and the mechanical property is measured by tensile test. The results showed that the tensile strength of the joint region is higher than the tensile strength of Al 3003. Thus, failure occurred in the Al 3003 plate.

Ti 첨가에 의한 심재의 결정립미세화 처리가 4343/3003/4343 알루미늄 클래드 판재의 브레이징 특성에 미치는 영향 (The Effect of Grain Refinement by Ti Addition on Brazing Characteristic of 4343/3003/4343 Aluminum Clad Sheet)

  • 신제식;문병문
    • 한국주조공학회지
    • /
    • 제30권5호
    • /
    • pp.187-195
    • /
    • 2010
  • In this study, in order to obtain a useful guide line for design and production of automotive heat exchanger components made of 4343/3003/4343 aluminum clad sheets, it was aimed to improve the understanding about the grain refinement effect on brazing characteristic of the clad sheets. Al-10Ti master alloy was used for grain refinement of 3003 core alloy, and the Ti inoculation level was systematically changed up to 0.1 wt%. The three-layer aluminum clad sheets were fabricated by hot roll bonding process. The effect of grain refinement on brazing characteristic of the clad sheets was investigated by evaluating wettability, bonding strength and sagging resistance.

무윤활 압연한 알루미늄 합금의 집합조직과 성형성 (Texture and Formability Development of Non-lubrication Rolled Al Alloy Sheet)

  • 아크라모프 사이드무로드;김인수
    • 소성∙가공
    • /
    • 제18권2호
    • /
    • pp.116-121
    • /
    • 2009
  • Formability and other mechanical properties of sheet metals are strongly dependent on the texture. It was studied to improve the formability of the Al alloy(AA3003) sheets which were rolled under the non-lubrication condition and subsequent heat treated. In the non-lubrication rolled and subsequent heat treated Al alloy sheet, the variation of the plastic strain ratios were investigated in this study. Non-lubrication rolled Al sheets showed a fine grain size and after subsequent heat treated specimens showed that the $\beta$-fiber texture component was increased. The plastic strain ratios of the non-lubrication rolled and subsequent heat treated Al alloy sheets were about two times higher than those of the original Al sheets. These could be related to the formation of $\beta$-fiber texture components through the non-lubrication rolling and subsequent heat treatment in Al sheet.

Eco-friendly Fabrication Process of Al-Ti-C Grain Refiner

  • Cho, Hoon;Kim, Bong-Hwan
    • 한국주조공학회지
    • /
    • 제30권4호
    • /
    • pp.147-150
    • /
    • 2010
  • 알루미늄 합금의 미세조직 개량을 위한 목적으로 사용되는 Al-Ti-B 합금계의 미세화제는 재활용 과정에서 붕소(B)의 농축(Agglomeration) 문제 및 Zr, Si, Cr 등을 함유하는 합금에서 미세화 효과가 급격히 감소하는 Poisoning effect 등이 지적되어 왔다. 최근에는 이를 대체할 수 있는 Al-Ti-C 합금계의 미세화제에 대한 연구가 활발한데 이는 TiC가 용탕 내에서 ${\alpha}$-Al의 핵생성처로 직접 작용하는 점에 착안한 것이다. 한편, 이들 Al-Ti-B, Al-Ti-C 계의 미세화제는 그 제조공정에서 $K_2TiF_6$를 이용함에 따라 불소함유 유해가스를 배출하여 환경 문제를 야기하고, 이를 포집/정화하기 위한 추가설비를 요구하게 된다. 따라서 대기 환경 오염 및 경제성 측면에서 유리한 미세화제의 친환경 제조기술에 대한 개발이 필요한 시점이다. 본 연구에서는 $K_2TiF_6$를 사용하지 않고 용탕 내의 자발적 반응을 이용하여 환경 및 경제적 측면에서 유리한 Al-Ti-C 미세화제를 개발하고자 하였다. A3003 합금을 대상소재로 하여 개발된 Al-Ti-C 미세화제와 상용 Al-Ti-B 미세화제의 미세화 도달시간 및 fading 발생 등을 비교하였다. 본 연구를 통하여 개발된 Al-8.6Ti-0.025C 미세화제는 상용 Al-Ti-B 미세화제 보다 적은 첨가량에도 유사한 미세화 성능을 나타내었으며 용탕 유지시간 100분까지도 fading이 발생하지 않는 것을 확인하였다.

Galvanic Corrosion Between Component Parts of Aluminum Alloys for Heat Exchanger of Automobile

  • Y. R. Yoo;D. H. Kim;G. B. Kim;S. Y. Won;S. H. Choi;Y. S. Kim
    • Corrosion Science and Technology
    • /
    • 제22권5호
    • /
    • pp.322-329
    • /
    • 2023
  • There are a variety of heat exchangers used in automobiles, such as shell and tube heat exchangers, double tube heat exchangers, and plate heat exchangers. Most of them are water-cooled to prevent engine overheating. There have been reports of corrosion damage to these heat exchangers due to continuous wetting caused by external temperature differences, road pollutants, and snow removal. In addition, galvanic corrosion, which occurs when two dissimilar materials come into contact, has been identified as a major cause. In this study, corrosion characteristics and galvanic corrosion behavior of Al alloy (AA3003, AA4045 and AA7072) used in automobile heat exchangers were analyzed. Effective clad materials for heat exchanger tubes and fins were also evaluated. It was found that AA7072 should be applied as the cladding material for fin AA3003 and that AA4045 was suitable as a cladding material for tube AA3003 because this clad materials application was the most effective clad design to delay the occurrence of pinhole in the tube. Main factors influencing galvanic corrosion dissolution were found to be galvanic corrosion potential difference and galvanic corrosion current density.

고상접합을 이용한 Al/Mg 합금의 이종 용접 (Solid State Joining Processes for Dissimilar Joints of Mg/Al Alloys)

  • 김흥주;김성욱;천창근;장웅성
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.41-41
    • /
    • 2009
  • To evaluate the applicability of dissimilar joining between Mg and Al alloys in automobile manufacturing process, solid state joining processes such as magnetic pulse welding(MPW), friction stir welding(FSW) and friction spot joining(FSJ) were attempted successfully. MPW process has been concentrated mainly on round section tube to tube and tube to bar welds. AZ31 Mg alloy has been successfully welded to pure Al A1070 as well as to Al alloy A3003. While, for friction stir welding of dissimilar sheet joints, AZ31B/A6061 with the thickness of 2mm were used and a square butt joint with a good quality was obtained at the conditions of 0.8mm/sec of travel speed and tool rotation speed of 850rpm. The maximum tensile strength of 179 MPa, which was about 80 % of the Mg base metal tensile strength, has been obtained. Finally, friction spot joining was attempted to make a dissimilar lap joint between AZ31(0.8mm) and A6061(1mm), while the joint exhibited the same level of tensile shear strength as that of similar Mg joint.

  • PDF