P/M법과 유도가열 공정을 이용한 발포용 6061 Al 합금 프리커서 제조 (Fabrication of Al 6061 Foamable Precursor by Powder Metallurgical and Induction Heating Method)

  • 윤성원;강충길
    • 소성∙가공
    • /
    • 제12권5호
    • /
    • pp.457-464
    • /
    • 2003
  • In the powder compact melting technique, proper precursor fabrication is very important because density distribution after foaming and foamability are determined during precursor fabrication process. The fabrication of the precursor has to be performed very carefully because any residual porosity or other defects will lead to poor results in further processing. In order to evaluate the effect of the compaction parameters on the kinetics of the foaming process, a series of experiments were performed. In this study, aluminium foams with a closed cell structure were fabricated by using both the powder compact method and the induction heating process. A proper induction coil was designed to obtain a uniform temperature distribution over the entire cross sectional area of precursor. To establish the foamable precursor fabrication conditions, effects of process parameters such as the titanium hydride content (0.3∼1.5 wt.%), pressing pressure of the foamable precursor (50∼150kN) on the pore morphology were investigated.

Microstructure and Mechanical Properties of AA6061/AA5052/AA1050 Alloy Fabricated by Cold Roll-Bonding and Subsequently Annealed

  • Seong-Hee Lee;Sang-Hyeon Jo;Jae-Yeol Jeon
    • 한국재료학회지
    • /
    • 제33권11호
    • /
    • pp.439-446
    • /
    • 2023
  • Changes in the microstructure and mechanical properties of as-roll-bonded AA6061/AA5052/AA1050 three-layered sheet with increasing annealing temperature were investigated in detail. The commercial AA6061, AA5052 and AA1050 sheets with 2 mm thickness were roll-bonded by multi-pass rolling at ambient temperature. The roll-bonded Al sheets were then annealed for 1 h at various temperatures from 200 to 400 ℃. The specimens annealed up to 250 ℃ showed a typical deformation structure where the grains are elongated in the rolling direction in all regions. However, after annealing at 300 ℃, while AA6061 and AA1050 regions still retained the deformation structure, but AA5052 region changed into complete recrystallization. For all the annealed materials, the fraction of high angle grain boundaries was lower than that of low angle grain boundaries. In addition, while the rolling texture of the {110}<112> and {123}<634> components strongly developed in the AA6061 and AA1050 regions, in the AA5052 region the recrystallization texture of the {100}<001> component developed. After annealing at 350 ℃ the recrystallization texture developed in all regions. The as-rolled material exhibited a relatively high tensile strength of 282 MPa and elongation of 18 %. However, the tensile strength decreased and the elongation increased gradually with the increase in annealing temperature. The changes in mechanical properties with increasing annealing temperature were compared with those of other three-layered Al sheets fabricated in previous studies.

분무성형법에 의해 제조된 $Al-SiC)_p$ 금속기 복합재료의 미세조직과 성질에 관한 연구 (A Study on the Microstructures and Properties of $Al-SiC)_p$ Metal Matrix Composites Fabricated by Spray Forming Process)

  • 김춘근
    • 한국분말재료학회지
    • /
    • 제1권1호
    • /
    • pp.42-51
    • /
    • 1994
  • 6061Al-SiCP metal matrix composite materials(MMCs) were fabricated by injecting SiCP particles directly into the atomized spray. The main attraction of this technique is the rapid fabrication of semi-finished, composite products in a combined atomization, particulate injection(10 $\mu\textrm{m}$, 40 $\mu\textrm{m}$, SiCP) and deposition operation. Conclusions obtained are as follows; The microstructure of the unreinforced spray formed 6061Al alloy consisted of relatively fine(50 $\mu\textrm{m}$) equiaxed grains. By comparision, the microstructure of the I/M materials was segregated and consisted of relatively coarse(150 $\mu\textrm{m}$) grains. The probability of clustering of SiCP particles in co-sprayed metal matrix composites increased it ceramic particle size(SiCP) was reduced and the volume fraction was held constant. Analysis of overspray powders collected from the spray atomization and deposition experiments indicated that morphology of powders were nearly spherical and degree of powders sphercity was deviated due to composite with SiCp particles. Interfacial bonding between matrix and ceramics was improved by heat treatment and addition of alloying elements(Mg). Maximum hardness values [Hv: 165 kg/mm2 for Al-10 $\mu\textrm{m}$ SiCp Hv--159 kg/mm2 for Al-40 $\mu\textrm{m}$SiCp] were obtained through the solution heat treatment at $530^{\circ}C$ for 2 hrs and aging at $178^{\circ}C$, and there by the resistance were improved.

  • PDF

자동차 휠용 6061 Al합금의 단조 및 T6 열처리 전후의 미세조직과 기계적 특성 평가 (Evaluation of Mechanical Property and Microstructure of Forged and T6-treated 6061 Aluminum Alloy Wheel)

  • 이지혜;정헌수;염종택;김정한;박노광;이용태;이동근
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.354-359
    • /
    • 2007
  • Effects of forging and mechanical properties of 6061 aluminum alloy wheel for automobiles were investigated in the present study. Microstructural and tensile characteristics of automobile wheel after hot forging process using dynamic screw press were analyzed to evaluate effect of metal flow on mechanical properties. The results showed advanced mechanical properties of 6061 alloy wheel because of $Mg_2Si$ precipitation by T6, elongated grain by forging, and work hardening by dense metal flow, etc. Hot compression tests were conducted in order to characterize high temperature compression deformation behaviors and microstructural variation in the range of $300{\sim}450^{\circ}C$, in the strain rate range of $10^{-3}{\sim}10^1\;sec^{-1}$. As strain rate increased, maximum compression stress increased but it was shown the reverse linear relation between temperature and maximum stress irrelevant to strain rate variation. On the other hand, temperature and yield stress didn't have any linear relation and its relation showed big deviation by a function of strain rate and test temperature.

자동차 휠용 6061 Al합금의 고온변형거동에 따른 단조성형조건 설계 (Forging Process Design by High Temperature Deformation Behavior of the 6061 Aluminum Alloy)

  • 이동근;이지혜;김정한;박노광;이용태;정헌수
    • 대한금속재료학회지
    • /
    • 제46권7호
    • /
    • pp.449-457
    • /
    • 2008
  • Compression deformation behaviors at high temperature as a function of temperature and strain rate were investigated in the 6061 aluminum alloy, which is used for automobile wheel. Compression tests were carried out in the range of temperatures $300{\sim}475^{\circ}C$ and strain rate $10^{-3}{\sim}10^{-1}sec^{-1}$. By analyzing these results, strain rate sensitivity, deformation temperature sensitivity, the efficiency of power dissipation, Ziegler's instability criterion, etc were calculated, which were plastic deformation instability parameters as suggested by Ziegler, Malas, etc. Furthermore, deformation processing map was drawn by introducing dynamic materials model (DMM) and Ziegler's Continuum Criteria. This processing map was evaluated by relating the deformation instability conditions and the real microstructures. As a result, the optimum forging condition for the automobile wheel with the 6061 aluminum alloy was designed at temperature $450^{\circ}C$, strain rate $1.0{\times}10^{-1}sec^{-1}$. It was also confirmed by DEFORM finite element analysis tool with simulation process.

해수 내 다양한 알루미늄 선박용 재료의 캐비테이션 진폭에 따른 캐비테이션-침식 손상 연구 (Investigation on Cavitation-Erosion Damage with the Cavitation Amplitude of Al Alloy Materials in Seawater)

  • 양예진;김성종
    • Corrosion Science and Technology
    • /
    • 제19권5호
    • /
    • pp.250-258
    • /
    • 2020
  • Recently, 5000 series and 6000 series Al alloys have been used as hull materials for small and medium-sized ships because of their excellent weldability, corrosion resistance, and durability in marine environments. Al ships can navigate at high speed due to their light weight. However, cavitation-erosion problems cause reducing durability of Al ship at high speed. In this investigation, 5052-O, 5083-H321, and 6061-T6 Al alloy materials were used to evaluate the damage characteristics with amplitude (cavitation strength). As a result of the electrochemical experiments, the corrosion current density and corrosion potential of 6061-T6 in seawater were 8.52 × 10-7 A/㎠ and -0.771 V, respectively, presenting the best corrosion resistance. The cavitation-erosion experiment showed that 5052-O had the lowest hardness value and cavitation-erosion resistance. 5052-O also had a very short incubation period. As the experiment progressed for 5052-O, pitting formed and grew in a short time, and was observed as severe cavitation-erosion damage that eliminated in large quantities. Among the three specimens, 5083-H321 presented the highest hardness value and the damage rate was the smallest after the initiation of pitting.

Weld formation mechanism during friction stir spot welding of 6061 Al

  • Sato, Yutaka S.;Fujimoto, Mitsuo;Abe, Natsumi;Kokawa, Hiroyuki
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2009년 추계학술발표대회
    • /
    • pp.239-242
    • /
    • 2009
  • Friction stir spot welding (FSSW), developed based on principle of friction stir welding, has been paid attention as a new solid-state spot welding process. Since FSSW can produce high-quality weld in Al alloys more easily than resistance spot welding, this process has been already used for construction of Al components in the automotive industries. Despite the large industrial interests in FSSW, fundamental knowledge on welding phenomena of this process has not been fully understood. In this study, FSSW phenomena, such as the consolidation mechanism, the microstructural evolution and the material flow, were examined in Al alloy 6061. This study clarified that the elliptical zone found in the vicinity of the pin hole on the cross section was characterized by the initially lapped surface of two sheets. Moreover, the following material flow was proposed; capture of the upper material with the threads on the pin surface, spiral flow along the tool rotation, and then release at the tip of the pin.

  • PDF

공작기계의 4차 산업혁명에서 5축 절삭가공기 교육 중 AC축을 제어하는 2NC 헤드 가공상의 유한요소 해석으로 응력 및 변형에 관한 연구 (A Study on Stress and Deformation through Finite Element Analysis of 2NC Head Processing Controlling AC Axis during 5-Axis Cutting Machine Training in the 4th Industrial Revolution of Machine Tool System)

  • 이지웅
    • 실천공학교육논문지
    • /
    • 제13권2호
    • /
    • pp.327-332
    • /
    • 2021
  • 교육용으로 사용되는 피삭재(소재)는 SM20C, Al6061, 아크릴 등의 소재를 사용한다. SM20C 소재는 탄소강으로서 자격증 시험 및 기능경기대회에서 많이 사용되지만 산업현장에서도 많이 사용된다. Al6061 소재는 탄소강에 비하여 경도가 낮아지고 전성(연성)이 강한 소재이기에 공구의 구성인선이 많이 발생하는 소재 라고 한다. 아크릴 소재를 이용하여 학생들에게 실습지도 하면 어느 부분에서 과다 절삭으로 인하여 진동이 발생하고 공구의 파손이 발생하는 소재이다. 이러한 과정에서 5축장비인 2NC헤드에게 가해지는 충격이 정밀도 제어에는 어느정도 영향을 줄 수 있는지 알아본다. 5축장비의 가장 취약한 부분은 AC축을 제어하는 헤드가 가장 약한 부분이라 할 수 있다. 이 부분의 정밀도 및 누적 공차가 발생할 경우 모든 제품의 정밀도가 떨어지는 현상이 발생한다. 따라서 2NC헤드의 핵심적인 부분, 스핀들 하우징은 Al7075 T6(미국 알코아사) 소재를 사용하고 전체 바디는 FCD450 (구상흑연주철) 사용하여 진행하였다. 이 두가지 소재에서 작용되는 진동 및 절삭 과정에서 힘을 극한조건에서 유한요소 해석으로 적용되는 값을 밝혀 내고자 해석을 진행하였다. 이러한 해석 데이터를 활용하여 학생들이 5축절삭 보다 5축 가공기의 구조를 보고 이해하는데 도움이 되기를 기대한다.

5축 절삭가공기 교육 중 2NC 헤드의 고강도 알루미늄을 적용한 스핀들 하우징의 극한 조건의 진동해석에 관한 연구 (A Study on the Vibration Analysis of Spindle Housing with High Strength Aluminum of 2NC Head in Five-axis Cutting Machine Training)

  • 이지웅
    • 실천공학교육논문지
    • /
    • 제14권1호
    • /
    • pp.119-125
    • /
    • 2022
  • 교육용으로 사용되는 피삭재(소재)는 SM20C, Al6061, 아크릴 등의 소재를 사용한다. SM20C 소재는 탄소강으로서 자격증 시험 및 기능경기대회에서 많이 사용되지만 산업현장에서도 많이 사용된다. Al6061 소재는 탄소강에 비하여 경도가 낮아지고 전성(연성)이 강한 소재이기에 공구의 구성인선이 많이 발생하는 소재라고 한다. 아크릴 소재를 이용하여 학생들에게 실습지도 하면 어느 부분에서 과다 절삭으로 인하여 진동이 발생하고 공구의 파손이 발생하는 소재이다. 이러한 과정에서 5축장비인 2NC헤드에게 가해지는 충격이 정밀도 제어에는 어느정도 영향을 줄 수 있는지 알아본다. 5축장비의 가장 취약한 부분은 AC축을 제어하는 헤드가 가장 약한 부분이라 할 수 있다. 이 부분의 정밀도 및 누적 공차가 발생할 경우 모든 제품의 정밀도가 떨어지는 현상이 발생한다. 따라서 2NC헤드의 핵심적인 부분, 스핀들 하우징은 Al7075 T6(미국 알코아사) 소재를 사용하여 진행하였다. 이 소재에서 작용되는 진동 및 절삭 과정에서 힘을 극한조건에서 유한요소 해석으로 적용되는 값을 밝혀 내고자 해석을 진행하였다. 이러한 해석 데이터를 활용하여 학생들이 5축절삭 보다 5축가공기의 구조를 보고 이해하는데 도움이 되기를 기대한다.

Al6061의 엔드밀 절삭가공에서 초음파 진동이 가공 표면에 미치는 영향 (Effects of Ultrasonic Vibration on Machined Surface of Aluminium 6061 in Endmill Cutting Process)

  • 정명원;곽태수;김명규;김건희
    • 한국기계가공학회지
    • /
    • 제13권3호
    • /
    • pp.96-102
    • /
    • 2014
  • This study focused on the effects of ultrasonic vibration on a machined surface of Al6061 material in the endmill cutting process. It is known that ultrasonic vibration greatly increases the efficiency of the machining process when cutting or grinding. An ultrasonic vibration table was developed for application to ultrasonic vibration endmill machining experiments.Inthisstudy,the surface roughness and actual depth of the cut measured confirm the effects of ultrasonic vibration. As a result of the experiments, the actual depth of the cut increased during endmill machining when using ultrasonic vibration. The surface roughness was improved with increases in the amplitude of the vibration and the depth of the cut.