• 제목/요약/키워드: 5-axis milling

검색결과 55건 처리시간 0.022초

치과용 임플란트 적용 비귀금속 코어와 관련된 전조골세포의 변화 (Changes in pre-osteoblast cells associated with non-precious metal cores with dental implants: Pilot test)

  • 박정현;강신영;김종우;김장주;김웅철;김지환
    • 대한치과기공학회지
    • /
    • 제40권2호
    • /
    • pp.63-69
    • /
    • 2018
  • Purpose: The purpose of this study is to investigate the non-precious metal core materials used in the dental laboratory to fabricate the implant superstructure by CAD / CAM method. And to observe and compare the morphology and distribution of the osteoblasts in relation to implant osseointegration. Methods: In this study, the mandibular right first molar tooth model was selected as an international standard to produce a single core. Using this model, the impression was made with the silicone rubber, the tooth model was scanned, and a single core was designed and 5-axis milling was performed. The materials used were Cobalt-Chromium and Nickel-Chromium, and the cores for dental implant top structures were fabricated according to the procedures of the dental labs. After the fabrication, the marginal area of the core was separated and cell culture experiment was performed. The osteoblast cells used MC3T3-E1, which is currently widely used. For morphological analysis of osteoblasts, cells were posttreated and observed using CLSM (Confocal Laser Scanning Microscope) and compared. Results: The cell adhesion behavior of the specimen surface measured by CLSM was uniformly distributed in specimen A (Cobalt-Chromium) than in specimen B (Nickel-Chromium). The distribution and changes of the cells were different in the two specimens. Conclusion : It is possible to confirm that specimen A (Cobalt-Chromium) is suitable for the living body through adhesion and proliferation of osteoblasts related to implant osseointegration in the non-precious metal superstructure used after implantation. It is considered that it is preferable to use Co-Cr when fabricating the superstructure.

In vitro study of compressive fracture strength of Empress 2 crowns cemented with various luting agents

  • Kim Min-Ho;Yang Jae-Ho;Lee Sun-Hyung;Chung Hun-Young;Chang Ik-Tae
    • 대한치과보철학회지
    • /
    • 제39권3호
    • /
    • pp.260-272
    • /
    • 2001
  • All-ceramic restorations have had a more limited life expectancy than metal ceramic restorations because of their low strength. Their relatively lower strength and resistance to fracture have restricted the use of all-ceramic crowns to anterior applications where occlusal loads are lower. But there has been increasing interest in all-ceramic restorations because patients are primarily concerned with improved esthetics. Many efforts have been made to in prove the mechanical properties of dental ceramics. This study was designed to elucidate the influence of the luting agent on the strength of the Empress 2 crown (staining technique) cemented on human teeth. Seventy extracted human permanent molar teeth were chosen. Teeth were prepared for Empress 2 crowns with milling machine on a surveyor. A dental bur was placed in the mandrel that was positioned so that the long axis of the bur was perpendicular to the surveyor base. Dimensions of the Empress 2 crown preparation were $6^{\circ}$ taper on each side, $1.5{\pm}0.1mm$ shoulder margin, and 4mm crown height. The luting cements used in this study were as follow: 1. Uncemented 2. Zinc phosphate cements (Confi-Dental) 3. Conventional glass ionomer cement : Fuji 1 (GC) 4. Resin-modified glass ionomer cements : Fuji plus (GC) 5. Adhesive cements : Panavia F (Kuralay), Variolink II (Vivadent), Choice (Bisco). Fracture test using Instron. The crowns were loaded in compressive force to evaluate the effect of these cements on the breaking strength of these all-ceramic crowns. A steel ball with a diameter of 4mm was placed on the occlusal surface and load was applied to the steel ball by a cylindrical bolt with a crosshead speed of 0.5mm per minute until fracture occurred. The fractured surface was examined using Scanning Electron Microscopic Image (SEM) to discover the correlation between fracture strength and bonding capacity. Within the limitation of this in vitro study design, the results were as follows : 1. fomentations significantly increased the fracture resistance of Empress ceramic crowns compared to control. Uncemented (206.9 N): ZPC (812.9 N): Fuji 1 (879.5 N): Fuji Plus (937.7 N): Choice (1105.4 N): Variolink II (1221.1 N): Panavia F (1445.2 N). 2. Resin luting agent, treated by a silane bond enhancing agents, yielded a significant increase in fracture resistance. In some of the Panavia F group, a fracture extended into dentin. 3. According to SEM images of fractured Empress crowns, the stronger the bond at both interfaces(crown and die), the more fracture strength was acquired.

  • PDF

고온 초전도 $\textrm{YBa}_{2}\textrm{Cu}_{3}\textrm{O}_{7-x}$ 계단형 모서리 접합의 이중접합 특성 (Characteristics of Double-junction of High-$\textrm{T}_{c}$ Superconducting $\textrm{YBa}_{2}\textrm{Cu}_{3}\textrm{O}_{7-x}$ Step-edge Junctions)

  • 황준식;성건용;강광용;윤순길;이광렬
    • 한국재료학회지
    • /
    • 제9권1호
    • /
    • pp.86-91
    • /
    • 1999
  • (001) $\textrm{SrTiO}_3$(STO) 기판위에 고온초전도 $\textrm{YBa}_{2}\textrm{Cu}_{3}\textrm{O}_{7-x}$(YBCO)박막을 이용한 계단형 모서리 임계접합을 제조하였다. STO (100) 단결정 기판위에 계단형 모서리(step-edge)를 제작하기 위한 이온밀링 마스크로 plasma enhanced chemical vapor deposition방법으로 증착된 diamond-like carbon (DLC) 박막을 사용하였고, oxygen reactive ion etch 방법으로 건식식각하였다. 이렇게 제작된 계단형 모서리 기판위에 c-축 수직한 YBCO 박막과 STO박막을 pulsed laser deposition방법으로 에피텍셜하게 증착하였다. 계단의 상층과 하층에서 모두 임계가 형성되었으며 이 접합의 임계온도는 77 K 이상이었고 16K에서 $\textrm{I}_{c}\textrm{R}_{n}$products가 7.5mV, 77 K에서 0.3mV의 값을 나타내었다. 이들 전류-전압 특성은 two noisy resistively shunted Josephson junction 모델을 잘 만족하였다.

  • PDF

Evaluation of the fracture resistance of all-ceramic zirconia posts by 3 different methods

  • Jeong, Seung-Mi;Chung, Chae-Heon;Kang, Dong-Wan;Ludwig, Klaus;Kern, Matthias;Huels, Alfons
    • 대한치과보철학회지
    • /
    • 제38권6호
    • /
    • pp.757-764
    • /
    • 2000
  • Statement of the problem. All-ceramic post-and-core restorations offer a number of advantages compared with systems that use metal build-ups. In certain clinical cases, however, fractures at the joint between the post and core build-up have been reported. Purpose. The objective, therefore, is to improve the joint between the post and the core build-up. Material and methods. Three different methods were used to prepare all-ceramic post-and-core restorations; pressing IPS Empress core build-ups to CosmoPost zirconia posts, cement-ing IPS Empress core build-ups to CosmoPost zirconia posts and Celay-milling of zirconia blanks. A series of ten restorations was prepared for each of the three methods. The post-and-core complexes were tested to failure with the load applied perpendicular to the post axis. The load and deflection at fracture were recorded. Results. The highest breaking load and highest deflection were recorded for the cementing technique with values of 25.3 N and $394{\mu}m$, respectively, The corresponding values for the pressed core build-ups and the milled zirconia core build-ups were 22 N and $301{\mu}m$, and 13 N and $160{\mu}m$, respectively. All the differences are statistically significant (p=0.05). Regarding the load-dependence of the deflection, the cemented core build-ups again demonstrated the highest value with $15.5{\mu}m/N$. The difference in the values of $13.6{\mu}m/N\;and\;13{\mu}m/N$ recorded for the pressed-on and milled core build-ups, respectively, were statistically insignificant. Conclusion. In regard to the high fracture resistance of zirconia post, adhesive cementing the core build-up to the post offers a viable alternative to the conventional pressing technique. The elastic bond between the rigid high-strength zirconia post and the core build-up presents an additional advantage.

  • PDF

제작방법에 따른 임시 수복용 레진의 마모저항성에 관한 연구 (In vitro evaluation of the wear resistance of provisional resin materials fabricated by different methods)

  • 안종주;허중보;최재원
    • 대한치과보철학회지
    • /
    • 제57권2호
    • /
    • pp.110-117
    • /
    • 2019
  • 목적: 본 연구의 목적은 적층 가공(additive manufacturing)법, 절삭 가공(subtractive manufacturing)법, 전통적인 방법에 따른 임시 수복용 레진의 마모 저항성을 조사하는 것이다. 재료 및 방법: 제작방법에 따라 4개의 군으로 나누었으며, 각 군은 전용의 임시 수복용 레진을 사용하였다: S3P군, Stereolithography apparatus (SLA) 3D 프린터 및 전용의 광경화성 수지로 제작한 군; D3P군, Digital Light Processing (DLP) 3D 프린터 및 전용의 광경화성 수지로 제작한 군; MIL군, Milling machine 및 밀링용 레진 블록으로 제작한 군; CON군, 전통적인 방법 및 자가중합형 레진으로 제작한 군. 한편, 3D 프린팅된 레진 시편을 제작함에 있어 적층 각도와 층 두께를 각각 $0^{\circ}$$100{\mu}m$로 설정하였다. 구강내 환경을 재현하기 위하여 열순환 처리와 수평, 수직운동이 가능한 2축 chewing simulator를 사용하였으며, 하부에는 한쪽면이 편평하게 제작된 임시 수복용 레진을, 상부에는 끝이 3 mm 직경을 가지는 원뿔형의 steatite를 고정하여 마모시험 진행하였다(5 kg, 30,000회, 0.8 Hz, $5^{\circ}C/55^{\circ}C$). 임시 수복용 레진의 마모량은 마모 전후의 Standard Triangulated Language (STL) 파일과 전용의 CAD software를 이용하여 부피를 계산하였고, 주사전자현미경으로 마모 양상을 비교하였다. 결과: S3P군, D3P군, MIL군의 마모량은 CON군보다 유의하게 작았으며 (P < .05), S3P군, D3P군, MIL군 사이에는 통계학적으로 유의한 차이가 없었다 (P > .05). 주사전자현미경으로 마모면을 관찰한 결과, S3P군과 D3P군에서는 대합치의 운동 방향에 대해 수직적으로 갈라진 흔적이 발견되었다. MIL군에서는 전반적으로 균일한 마모면이 보인 반면, CON군에서는 대합치 운동 방향으로의 뚜렷한 마모 흔적과 다수의 기포가 관찰되었다. 결론: 본 연구의 한계 내에서, 3D 프린팅된 임시 수복용 레진은 치과용으로서 적절한 마모저항성을 보였다.