A study on the diffusion bonding of the $Al_2$O$_3$ ceramics to metal (A$_2$O$_3$세라믹과 Ni-Cr-Mo鋼과의 인서트 合金을 이용한 擴散接合에 關한 硏究)

  • 김영식;박훈종;김정일
    • Journal of Welding and Joining
    • /
    • v.10 no.3
    • /
    • pp.63-72
    • /
    • 1992
  • The joining methods of ceramics to metals which can be expected to obtain high temperature strength are mainly classified into the solid-state diffusion bonding method and the active brazing method. Between these two, the solid-state diffusion bonding method is given attentions as substituting method for active brazing method due to being capable of obtaining higher bonding strength at high temperature and accurate bonding. In this paper, the solid-state diffusion bonding of $Al_{2}$O$_{3}$ ceramics to Ni-Cr-Mo alloy steel (SNCM21) using insert metal was carried out. The insert metal employed in this study was experimentally home-made, Ag-Cu-Ti alloy. Influence of several bonding parameters of $Al_{2}$O$_{3}$SNCM21 joint was quantitatively evaluated by bonding strength test, and microstructural analyses at the interlayer were performed by SEM/EDX. From above experiments, the optimum bonding condition of the solid-state diffusion bonding of $Al_{2}$O$_{3}$/SNCM21 using Ag-Cu-Ti insert metal was determined. Futhermore, high temperature strength and thermal-shock properties of $Al_{2}$O$_{3}$/SNCM21 joint were also examined. The results obtained are as follows. 1. The maximum bonding strength was obtained at the temperature of 95% melting point of insert metal. 2. The high temperature strength of $Al_{2}$O$_{3}$/SNCM21 joint appeared to bemaximum value at test temperature 500.deg.C and the bonding strength with increasingtemperature showed parabolic curve. 3. The strength of thermal-shocked specimens was far deteriorated than those of as-bonded specimens. Especially, water-quenched specimen after heated up to 600.deg. C was directly fractured in quenching.

  • PDF

The Evaluation of Creep Degradation for the High Temperature Pipe Material by Small Punch Test (소형펀치법에 의한 고온배관재료의 크리프열화 평가)

  • Yoo, K.B.;Jang, S.H.;Song, G.W.;Ha, J.S.;Kim, J.H.
    • Proceedings of the KSME Conference
    • /
    • 2000.04a
    • /
    • pp.37-42
    • /
    • 2000
  • The boiler tubes and steam Pipes operating both at high temperature and pressure for a long period of time in a power plant are degraded by creep because of internal pressure. So, the remaining life of a component is evaluated by the creep rupture strength. Although the conventional method to evaluate the creep damage is widely used, it has some disadvantages such as requires large size specimen and long employed to evaluate the correlation between fracture toughness and evaluation time. Recently, new method so called "small lunch test' is used to evaluate degradation of creep. In this study, a conventional creep test and a small punch test are conducted using 2.25Cr-1Mo steel which is mainly used for the boiler tubes and steam pipes in power plant. The creep life, approximately 1,500 hrs, is determined by conventional method under a severe condition then specimens for a small Punch test are obtained after certain time intervals such as 1/4, 1/2 and 3/4 of final rupture time, respectively.

  • PDF

Tribological Properties of Ceramic Composite Friction Materials Reinforced by Carbon Fibers (탄소섬유가 혼합된 세라믹 복합재 제동마찰재의 마찰·마모 특성)

  • Goo, Byeong-Choon;Kim, Min-Soo
    • Tribology and Lubricants
    • /
    • v.33 no.1
    • /
    • pp.15-22
    • /
    • 2017
  • Because the running speed of vehicles is increasing and a shorter braking distance is required, high heat-resistant brake pads are needed to satisfy the requirements of customers and car makers. In the near future, hazardous materials such as Cu, Cr, Zn, and Sb will be restricted from use in friction materials. Ceramic composites reinforced by carbon fibers are good candidates for eco-friendly friction materials. In this study, we develop ceramic composite friction materials. The friction materials are composed of carbon fibers, Si, SiC, graphite, and phenol resin and are prepared by hot forming and heat treatment at high temperatures. The density, void ratio, and compressive strength are $1.59-1.66g/cm^3$, 16.6-20, and 70-90 MPa, respectively. Friction and wear tests are performed using a pin-on-plate-type reciprocating friction tester at 25, 100, and $200^{\circ}C$. The counterpart material is a CrMoV steel extracted from a KTX brake disc. Friction coefficient, wear amount, and wear mechanism are measured and examined. We determine that the friction coefficients depend on the temperature and the fluctuation of the friction coefficients is larger at higher temperatures. The amount of wear increases with the surface temperatures of the specimens. The tribological properties of the developed composites are similar to those of a Cu-based sintered friction material. Through this study, it is confirmed that ceramic composite materials can be used as friction materials.

Friction-Wear Properties of Carburized SNCM (침탄처리한 Ni-Cr-Mo강의 마찰-마모특성)

  • Baek, Seung Ho
    • Journal of the Korean Society for Heat Treatment
    • /
    • v.11 no.3
    • /
    • pp.159-167
    • /
    • 1998
  • In this study, friction-wear test was carried out on the carburized layer depth of a mechanical structure steel SNCM carburized with RX and LPG for 7hrs at $930^{\circ}C$ and also the wear properties of wear loss, wear rate, coefficient of friction, friction force and friction temperature were investigated. The wear properties for carburized layer of SNCM were tested on dry condition at the room temperature by the thrust load of 49~245N range at sliding speed of 0.2m/sec and the sliding speed of 0.2~1.0m/sec range at thrust load of 98N. Wear loss on the depth of carburizing layer was increased with increasing of thrust load and sliding speed, and with decreasing of hardness. The condition of worn surfaces were showed mild wear at less than the thrust load of 98N and sliding speed of 0.6m/sec but were showed severe wear at more than 98N and 0.6m/sec. The friction load and temperature were increased with increasing of thrust load but with increasing sliding speed was appeared minimum at 0.6m/sec. With increasing thrust load the wear rate was increased and the coefficient of friction was decreased, but with increasing sliding speed the wear rate and the coefficient of friction were decreased in 0.2~0.6m/sec and increased in 0.6~1.0m/sec, therefore 0.6m/sec in this testing is a transition velocity.

  • PDF

A Comparative Study on Arrhenius-Type Constitutive Models with Regression Methods

  • Lee, Kyunghoon;Murugesan, Mohanraj;Lee, Seung-Min;Kang, Beom-Soo
    • Transactions of Materials Processing
    • /
    • v.26 no.1
    • /
    • pp.18-27
    • /
    • 2017
  • A comparative study was performed on strain-compensated Arrhenius-type constitutive models established with two regression methods: polynomial regression and regression Kriging. For measurements at high temperatures, experimental data of 70Cr3Mo steel were adopted from previous research. An Arrhenius-type constitutive model necessitates strain compensation for material constants to account for strain effect. To associate the material constants with strain, we first evaluated them at a set of discrete strains, then capitalized on surrogate modeling to represent the material constants as a function of strain. As a result, disparate flow stress models were formed via the two different regression methods. The constructed constitutive models were examined systematically against measured flow stresses by validation methods. The predicted material constants were found to be quite accurate compared to the actual material constants. However, notable mismatches between measured and predicted flow stresses were revealed by the proposed validation techniques, which carry out validation with not the entire, but a single tensile test case.

Evaluation on the Creep Life Prediction Using Initial Strain Method (초기 연신율법을 이용한 크리프 수명예측 평가)

  • Kong, Yu-Sik;Lim, Man-Bae;Lee, Sang-Pill;Yoon, Han-Ki;Oh, Sae-Kyoo
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.6
    • /
    • pp.1069-1076
    • /
    • 2002
  • The high temperature creep behavior of heat machine systems such as aircraft engines, boilers and turbines in power plants and nuclear reactor components have been considered as an important and needful fact. There are considerable research results available for the design of high temperature tube materials in power plants. However, few studies on the Initial Strain Method (ISM) capable of securing repair, maintenance, cost loss and life loss have been made. In this method, 3 long time prediction Of high temperature creep characteristics can be dramatically induced through a short time experiment. The purpose of present study is to investigate the high temperature creep lift of Udimet 720, SCM 440-STD61 and 1Cr-0.5Mo steel using the ISM. The creep test was performed at 40$0^{\circ}C$ to $700^{\circ}C$ under a pure loading. In the prediction of creep life for each materials, the equation of ISM was superior of Larson-Miller Parameter(LMP). Especially, the long time prediction of creep life was identified to improve the reliability.

High Temperature Creep Characteristics Evaluation for Degraded Heat Resistance Steel of Power Plant by Mini-Specimen (미소시험편에 의한 재질열화된 내열강의 고온 크리프 특성 평가)

  • Lyu, Dae-Young;Baek, Seung-Se;Yu, Hyo-Sun
    • Korean Journal of Materials Research
    • /
    • v.13 no.7
    • /
    • pp.429-435
    • /
    • 2003
  • In this study the new creep test using miniaturized specimen(10${\times}$10${\times}$0.5 ㎣) was performed to evaluate the creep characteristics for degraded materials of 2.25Cr-1Mo steel. For this creep test, the artificially aged materials for 330 hrs and 1820hrs at $630^{\circ}C$ were used. The test temperatures applied for the creep deformation of miniaturized specimens was X$630^{\circ}C$ and the applied loads were between 45 kg∼80 kg. After creep test, macro- and microscopic observation were conducted by the scanning electron microscope(SEM). The creep curves depended definitely on applied load and microstructure and showed the three stages of creep behavior like uniaxial tensile creep curves. The load exponents of virgin, 330 hrs and 1820 hrs materials based on creep rate showed 14.8, 9.5 and 8.3 at $550^{\circ}C$ respectively, The 1820 hrs material showed the lowest load exponent and this behavior was also observed in the case of load exponent based on creep rupture time. In contrast to virgin material which exhibited fined dimple fractography, a lot of carbides like net structure and voids were observed on the fractography of degraded materials.

High-Temperature Design and Integrity Evaluation of Sodium-Cooled Fast Reactor Decay Heat Exchanger (소듐냉각고속로 붕괴열교환기의 고온 설계 및 건전성 평가)

  • Lee, Hyeong-Yeon;Eoh, Jae-Hyuk
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.37 no.10
    • /
    • pp.1251-1259
    • /
    • 2013
  • In this study, high temperature design and creep-fatigue damage evaluation of a decay heat exchanger (DHX) in the decay heat removal systems of a sodium-cooled fast reactor (SFR) have been performed. Detail design and 3D finite element analysis have been conducted for the DHXs to be installed in active and passive decay heat removal systems in Korean Generation IV SFR, and the DHX installed in the STELLA-1(Sodium integral effect test loop for safety simulation and assessment) at KAERI (Korea Atomic Energy Research Institute). Evaluations of creep-fatigue damage based on full 3D finite element analyses were conducted for the two Mod.9Cr-1Mo steel heat exchangers according to the elevated temperature design codes of ASME Section III Subsection NH and RCC-MR code. Code comparisons were made based on the creep-fatigue damage evaluation and issues on conservatisms of the design codes were discussed.

Evaluation of Microstructural and Mechanical Property of Medium-sized HT9 Cladding Forged Material for Sodium-cooled Fast Reactor (소듐냉각고속로 피복관용 중형 HT9 단조품 소재의 미세조직 및 기계적 특성 평가)

  • Kim, Jun-Hwan;Lee, Kang-Soo;Kim, Sung-Ho;Lee, Chan-Bock
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.10 no.1
    • /
    • pp.21-26
    • /
    • 2012
  • Microstructural and mechanical property were evaluated at the medium-sized HT9 (12Cr-1MoWV) forged steel which was considered as primary candidate for the fuel cladding in sodium-cooled fast reactor (SFR). Material was forged at $1170^{\circ}C$ after the induction melting to make round bar as 160mm diameter, 7000mm length then the radial distribution of microstructure as well as microhardness was evaluated. The results showed that overall microstructure exhibited as ferrite-martensite structure, where small amount (2~3%) of delta ferrite was formed throughout the specimen and maximum 15% of transformed ferrite was formed at the center, where it gradually decreased toward the radial direction. Sensitivity analysis of the cooling curve and Time-Temperature-Transformation (TTT) diagram revealed that formation of transformed ferrite could be avoided when the diameter was decreased down to 120mm.

Influence of Vertical Centrifugal Casting (V.C.C) Conditions and Alloying Elements on Microstructures of High Speed Steel (고속도강의 미세조직에 미치는 합금원소 및 수직원심주조 조건의 영향)

  • Kim, Sug-Won;Lee, Ui-Jong;Woo, Kee-Do;Kim, Dong-Keon
    • Journal of Korea Foundry Society
    • /
    • v.20 no.5
    • /
    • pp.323-329
    • /
    • 2000
  • The HSS consists of hard carbide and matrix of martensite, and so its characteristics of wear resistance, fracture resistance, and surface roughness are good. This study was undertaken to investigate the influence of Nb and V and manufacturing conditions on microstructural behaviors and characteristics in the HSS cylindrical specimens(90 $mm^{O.D.}$ ${\times}$ 60 $mm^{I.D.}$ ${\times}$ 50 $mm^H$) manufactured using VCC(Vertical Centrifugal Casting). In the specimen of Fe-2C-6Cr-1.5W-3Mo-4V alloy, the amount of MC carbide was increased and $M_7C_3$ carbide was decreased with the increase of V and Nb contents. The primary VC carbide was formed and followed by the rod-type eutectic MC carbide was formed in the cell boundary in 9%V added specimen. MC carbide was increased, and $M_7C_3$ carbide was decreased with the addition of Nb content. In the specimen containing more than 3%Nb, primary NbC carbide was formed within the cell of matrix. With increase in rpm, cell and carbides became fine, and amount of carbide $M_7C_3$ was decreased due to increase in cooling rate.

  • PDF