Fabrication of BSCCO High Tc Superconducting Precursor (BSCCO 초전도 전구체의 합성)

  • Lee, Sang-Heon;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 2005.07c
    • /
    • pp.1964-1965
    • /
    • 2005
  • A high Tc superconducting with a nominal composition of $Bi_2Sr_2Ca_2Cu_3O_Y$ was prepared by the citarte method. The solid precursor produced by the dehydration of the gel at $120^{\circ}C$ for 12h is not in the amorphous state as expected but in a crystalline state. X-ray diffraction peaks of nearly the same angular position as the peaks of high Tc phase were observed in the precursor. After pyrolysis at $400^{\circ}C$ and calcination at $840^{\circ}C$ for 4h, the (001)peak of the high Tc phase was cleary observed. Experimental results suggest that the intermediate phase formed before the formation of the superconducting phase may be the most important factro in determining whether it is easy to form the high Tc phase or not, because the nucleation barriers of the two superconducting phase may be altered by the variation of the crystal structures of those intermediate phase.

  • PDF

Fabrication of BSCCO High Tc Superconducting Precursor (BSCCO 초전도 전구체의 합성)

  • Lee, Sang-Heon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.290-291
    • /
    • 2005
  • A high Tc superconducting with a nominal composition of $Bi_2Sr_2Ca_2Cu_3O_Y$ was prepared by the citarte method. The solid precursor produced by the dehydration of the gel at $120^{\circ}C$ for 12h is not in the amorphous state as expected but in a crystalline state. X-ray diffraction peaks of nearly the same angular position as the peaks of high Tc phase were observed in the precursor. After pyrolysis at $400^{\circ}C$ and calcination at $840^{\circ}C$ for 4h. the (001)peak of the high Tc phase was cleary observed. Experimental results suggest that the intermediate phase formed before the formation of the superconducting phase may be the most important factor in determining whether it is easy to form the high Tc phase or not. because the nucleation barriers of the two superconducting phase may be altered by the variation of the crystal structures of those intermediate phase.

  • PDF

Fabrication of High Tc Superconductor Using Thermal Pyrolysis (열분해법에 의한 고온 초전도 합성)

  • Lee, Sang-Heon
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.85-86
    • /
    • 2006
  • A high Tc superconducting with a nominal composition of $Bi_2Sr_2Ca_2Cu_3O_y$ was prepared by the citarte method. The solid precursor produced by the dehydration of the gel at $120^{\circ}C$ for 12h is not in the amorphous state as expected but in a crystalline state. X-ray diffraction peaks of nearly the same angular position as the peaks of high Tc phase were observed in the precursor. After pyrolysis at $400^{\circ}C$ and calcination at $840^{\circ}C$ for 4h, the (001)peak of the high Tc phase was cleary observed. Experimental results suggest that the intermediate phase formed before the formation of the superconducting phase may be the most important factro in determining whether it is easy to form the high Tc phase or not, because the nucleation barriers of the two superconducting phase may be altered by the variation of the crystal structures of those intermediate phase.

  • PDF

A Study on DC-Link Current Ripple of Multi-Phase/Multi-Stage Boost Converter (다상/다단 부스트 컨버터의 DC-Link 리플 전류 분석)

  • Seung-Min Kim;Dong-Hee Kim
    • The Transactions of the Korean Institute of Power Electronics
    • /
    • v.28 no.1
    • /
    • pp.59-67
    • /
    • 2023
  • This paper explores the variation of DC-Link current ripple analysis in terms of duty cycle and phase angle of Multi-phase/Multi-stage boost converter. A 2-Stage/1-Stage boost converter DC-Link current is used to determine the difference between the 1st stage diode current and the 2nd stage inductor current. Each stage boost converter diode and inductor current is subordinate to the phase angle and duty cycle. The magnitude of the ripple current is variable according to phase angle and duty cycle. The analysis results are verified by variation of DC-Link current ripple using a 1kW typical 2-stage/1-stage boost converter.

Oxygen Deficiency, Hydrogen Doping, and Stress Effects on Metal-Insulator Transition in Single-Crystalline Vanadium Dioxide Nanobeams

  • Hong, Ung-Gi;Jang, Seong-Jin;Park, Jong-Bae;Bae, Tae-Seong
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.424.1-424.1
    • /
    • 2014
  • Vanadium dioxide (VO2) is a strongly correlated oxide exhibiting a first-order metal-insulator transition (MIT) that is accompanied by a structural phase transition from a low temperature monoclinic phase to a high-temperature rutile phase. VO2 has attracted significant attention because of a variety of possible applications based on its ultrafast MIT. Interestingly, the transition nature of VO2 is significantly affected by stress due to doping and/or interaction with a substrate and/or surface tension as well as defects. Accordingly, there have been considerable efforts to understand the influences of such factors on the phase transition and the fundamental mechanisms behind the MIT behavior. Here, we present the influences of oxygen deficiency, hydrogen doping, and substrate-induced stress on MIT phenomena in single-crystalline VO2 nanobeams. Specifically, the work function and the electrical resistance of the VO2 nanobeams change with the compositional variation due to the oxygen-deficiency-related defects. In addition, the VO2 nanobeams during exposure to hydrogen gas exhibit the reduction of transition temperature and the complex phase inhomogenieties arising from both substrate-induced stress and the formation of the hydrogen doping-induced metallic rutile phase.

  • PDF

Latent Heat Storage Characteristics of Some Paraffins(CnH2n+2) for Thermal Environment Control of Greenhouse (그린하우스 열환경 조절을 위한 파라핀계 화합물(CnH2n+2)의 잠열 축열 특성)

  • 송현갑;유영선
    • Journal of Biosystems Engineering
    • /
    • v.21 no.1
    • /
    • pp.84-93
    • /
    • 1996
  • Several paraffins(CnH2n +2) can be used as the thermal energy storage medium because of their large amount of latent heat and their flexibility of phase change temperature. But they have not been used in the thermal energy storage system because their long term stability have not been verified. Paraffins(CnH2n+2) which the values of n are 23, 24, 26 and 28 were selected for this experimental research. And this research was peformed to apply them to the practical systems. The results were summarized as follows. (1) The increase of phase change cycles had no effect on their phase change temperatures. (2) According as the values of n increased from 23 to 28, the specific heats of paraffins(CnH2n+2) increased, and were in the range of 0.47 0.75 ㎉/$kg^circ C$. (3) Thermal conductivities of them were in the range of 0.14 0.17 W/$m^circ C$. and specific gravities of them were in the range of 765800 kg/m3. (4) The density of paraffins was in the range of 765 800 kg/$m^circ C$ , and the density of solid phase was larger than that of liquid phase. (5) When the number of phase change cycles was 1, 500 cycles, the latent heat of paraffins was 90% of the initial value.

  • PDF

Physical Property and Phase Transformation in a Commercial Dental Casting High Gold Alloy (시판치과주조용 고금합금의 물리적 성질 및 상변태)

  • Lee, Hee-Kyung;Park, Myoung-Ho;Lee, Hwa-Sik
    • Journal of Technologic Dentistry
    • /
    • v.28 no.1
    • /
    • pp.27-41
    • /
    • 2006
  • The physical property and phase transformation in a commercial dental casting high gold alloy was investigated as a function of ageing temperature and time using microvickers hardness tester, X-ray diffraction, optical and electron microscopy and EPMA analyser. 1. With increasing ageing time, the hardness of solution-treated gold alloys increased slowly at the initial stage of ageing treatment at an ageing temperature of $300{\sim}400^{\circ}C$, and it reached a maximum value of hardness at the medium stage. Finally, it decreased gradually during further ageing. The maximum value of hardness at was similar with that of the conventional materials and suitable for using as the crown & bridge. 2. During isothermal ageing at a temperature range of $300{\sim}400^{\circ}C$, three phases consisting of the Au-rich ${\alpha}_1$phase with a face-centered cubic structure, the Pt3Zn ${\alpha}_2$phase with an ordered AuCu3(L12) type(f.c.c.) and the Pt-rich ${\alpha}_3$phase with face-centered cubic structure in solution-treated gold alloys were transformed into different three phases consisting of the ${\alpha}_1$phase, the ${\alpha}_3$phase and the PtZn $\beta$phase with an ordered AuCu I(L10) type. 3. The hardening of gold alloys was attributed to the lattice strains of the matrix resulting from the transformation of the ${\alpha}_2$phase to the $\beta$phase. 4. The softening of gold alloys during over-ageing was attributed to the coarsening of the nodules consisting of the $\beta$phase and ${\alpha}_1$matrix.

  • PDF

Wideband 6-port Phase Correlator Using Caxial Cable Impedance Transformer and Wireline Coupler (동축선 임피던스 변환기와 Wireline Coupler를 이용한 광대역 6-단자 위상 상관기)

  • Park, Ung-hee
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.26 no.8
    • /
    • pp.1188-1195
    • /
    • 2022
  • The 6-port phase correlator consists of one in-phase power divider and three 3-dB 90-degree phase difference power dividers, and is mainly used in a demodulation circuit that determines the phase of an input signal. This paper proposes the wideband 6-port phase correlator that consists of an in-phase power divider using a wideband 2:1 impedance transformer with three 37.5-Ω coaxial cables, and a 3-dB 90-degree phase difference power divide using Wireline. The proposed wideband phase correlator fabricated at a center frequency of 1000MHz has the value of the input reflection coefficient(S11 and S22) -14dB or less in the frequency range of 640~1270MHz. Also, the signal transmission characteristic(Si1), from the in-phase power divider input port to four output ports, has the amplitude of -6.5±0.6dB and the phase error of within ±3.4°, and the signal transmission characteristic(Si2), from the 90 degree phase difference power divider input port to four output ports, has the amplitude of -6.1±0.6dB and the phase error of within ±6.2°.

Design and Fabrication of Broadband Phase Shifter Based on Vector Modulator (벡터 모듈레이터형 광대역 위상 변위기의 설계 및 제작)

  • 류정기;오승엽
    • The Journal of Korean Institute of Electromagnetic Engineering and Science
    • /
    • v.14 no.7
    • /
    • pp.734-740
    • /
    • 2003
  • In this paper, A Vector Modulator based a wideband analog phase shifter is realized with four P-I-N diode attenuators, an asymmetric coupled line coupler, a symmetric coupled line coupler, and a power combiner. Simple configuration to have advantages in cost, size, power, and the number of passive circuits is presented. The phase variation due to phase and amplitude error of a P-I-N diode attenuator is derived and used to optimize the overall circuit. The phase shifter shows a total phase shift of 360$^{\circ}$, a 8.2$^{\circ}$maximum phase error, and a 16${\pm}$2.5 dB insertion loss over the wide frequency range of 1 GHz to 3 GHz.

5-Bit Digital Phase Shifter for 12 GHz Band Active Phased Array Antenna System (12 GHz대 능동 위상 배열 안테나 시스템을 위한 5-비트 디지털 위상 변위기)

  • 김경식;최익권
    • The Journal of Korean Institute of Electromagnetic Engineering and Science
    • /
    • v.13 no.3
    • /
    • pp.308-315
    • /
    • 2002
  • In this paper, the 5-bit digital phase shiftier with 10 InGaAs HEMTs is designed and fabricated for U.S. mobile DBS receiving active phased array antenna system in 12 GHz band. 11.25 $^{\circ}$, 22.5$^{\circ}$ and 45$^{\circ}$ phase bits are designed in leaded-line type. 90$^{\circ}$ and 180$^{\circ}$ phase bits are designed in reflection type combined with ring hybrid. The return loss more than 17.5 ㏈, insertion louts less than 7.8 ㏈, and maximum phase error of $\pm$6$^{\circ}$for 32 phase responses are measured in 12.2 GHz~ 12.7 GHz band.