Preceramic Polymer Technology for High Temperature Ceramic Composite and its Application (초고온복합소재용 프리세라믹폴리머 합성 및 응용기술)

  • Lee, Yoonjoo;Kim, Younghee;Bae, Seong Gun;Lee, Hyeon Myoung;Cho, Kwang Youn;Kwon, Woo Teck;Kim, Soo Ryong;Riu, Doh Hyung;Shin, Dong Geun
    • Composites Research
    • /
    • v.30 no.2
    • /
    • pp.102-107
    • /
    • 2017
  • The preceramic polymer can realize a variety of complex ceramic structures that can not be obtained by conventional ceramic processes. Polycarbosilane, which is a typical preceramic polymer, can control the molecular structure, molecular weight and molecular weight distribution for preparing complex morphology and microstructure of SiC ceramics, including SiC fiber. In this paper, synthesis and molecular structure control technique of polycarbosilane is explained. The silicon carbide fiber prepared by melt spinning, stabilization and heat treatment, and ceramic fiber composites technology made by PIP process are also discussed. In addition, we introduce an example of the development of a complex silicon carbide material such as a silicon carbide hollow fiber having a nanoporous structure.

Influence of Oxidation Inhibitor on Carbon-Carbon Composites: 5. Studies on Anti-oxidation Properties of the Composites (산화억제제 첨가에 의한 탄소/탄소 복합재료의 물성에 관한 연구: 5. 탄소/탄소 복합재료의 내산화성 연구)

  • 박수진;서민강;조민석;이재락
    • Polymer(Korea)
    • /
    • v.24 no.2
    • /
    • pp.237-244
    • /
    • 2000
  • Phenolic resin used as a precursor of carbonized matrix for carbon-carbon composites was modified by addition of molybdenum disilicide (MoSi$_2$) in various concentrations of 0, 4, 12 and 20% by weight to improve the anti-oxidation properties of the composites. The green body was manufactured by a prepreg method and was submitted to carbonization up to 110$0^{\circ}C$. In this work, the oxidation behavior of carbon-carbon composites with MoSi$_2$ as an oxidation inhibitor was investigated at the temperature range of 600-100$0^{\circ}C$ in an air environment. The carbon-carbon composites with MoSi$_2$ showed a significantly improved oxidation resistance due to both the reduction of the porosity formation and the formation of mobile diffusion barrier for oxygen when compared to those without MoSi$_2$. Carbon active sites should be blocked, decreasing the oxidation rate of carbon. This is probably due to the effect of the inherent MoSi$_2$ properties, resulted from a formation of the protective layer against oxygen attack in the composites studied.