  • Stainless steels stabilized with Ti or Nb are largely used in offshore and shipbuilding industries due to its excellent corrosion resistance. In this study, carbide stabilizers, Ti and Nb, were added to stainless steel 304 specimens with different concentrations(Ti: 0.26%, 0.71%, Nb: 0.29%, 0.46%, 0.71%), and their mechanical and electrochemical characteristics were evaluated. Micro-Vickers hardness testing was employed to characterize the mechanical characteristics with alloying elements. Electrochemical evaluation techniques including Tafel analysis, cyclic polarization experiment, galvanostatic experiment were utilized to compare the corrosion characteristics of the specimens. The result of hardness tests revealed that Nb containing specimens showed increasing hardness with increasing alloying contents while adding Ti had little effect on increase in hardness. In the case of electrochemical measurements, the electrochemical characteristics of the specimens were enhanced with increasing Nb contents while they were deteriorated with increasing Ti contents. As a result, different stabilizers and their contents may produce significant differences in electrochemical characteristics, and there such effect must be taken account of in development of stainless steels for marine environment.

A Study on Quantitative Thickness Evaluation Using Film Density Variation in Film Radiography (Film Radiography에서 농도차를 이용한 정량적 두께 평가에 관한 연구)

  • Lee, Sung-Sik;Lee, Jeong-Ki;Kim, Young-H.
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.19 no.5
    • /
    • pp.356-362
    • /
    • 1999
  • Based on the assumption that film density increases exponentially with exposure in the industrial radiographic film. an equation representing the characteristic curves of industrial radiographic films and a new density-thickness relation are suggested. The accuracy and reliability of the suggested relation has been tested using radiographs of a carbon steel step wedge with known thickness variation by polychromatic X-ray and ${\gamma}$-ray ($Ir^{192}$). The experimental results were well agreed to the proposed relation in the range of film densities from 1.0 to 3.5 and it was more accurate than the conventional relation. It is also found that ${\gamma}$-ray is more effective in this purpose than polychromatic X-ray, which results in variation of effective linear absorption coefficient due to beam hardening effect as thickness increases. Therefore using the equation and experimentally determined parameters the quantitative evaluation of thickness variation is possible and it can be used to evaluate the depth of local corrosion of pressure vessels in plants.

  • PDF

Performance Based Evaluation of Concrete Carbonation from Climate Change Effect on Curing Conditions of Wind Speed and Sunlight Exposure Time (기후변화의 풍속과 일조시간 양생조건에 따른 콘크리트 탄산화 성능중심평가)

  • Kim, Tae-Kyun;Shin, Jae-Ho;Choi, Seung-Jai;Kim, Jang-Ho Jay
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.19 no.5
    • /
    • pp.45-55
    • /
    • 2015
  • Currently, extreme weather events such as super typhoon, extreme snowfall, and heat wave are frequently occurring all over the world by natural and human caused factors. After industrial growth in the 1970s, earth's temperature has risen sharply. due to greenhouse effect. Global warming can be attributed to gases emitted from using fossil fuel such as average carbon dioxide, perfluorocarbons, nitrous oxide, and methane. Especially, carbon dioxide has the highest composition of about 90%. in the fossile fuel usage emitted gas. Concrete has excellent durability as a building material climate change. However, due to various of physical and chemical environmental effect such as conditions during its curing process, the performance degradation may occur. Carbon dioxide in the atmosphere causes steel corrosion and durability decreases by lowering the alkalinity of concrete. Therefore, in this study, concrete durability performance with respect to carbonation from curing conditions change due to wind speed and sunshine exposure time. Concrete carbonation experiment are performed. using wind speed (0, 2, 4, 6) m/s and sunlight exposure time (2, 4, 6, 8) hrs. Also, performance based evaluation through the satisfaction curve based on the carbonation depth and carbonation rate test results are performed.

Experimental Study on Flexural Behavior of RC Beams Strengthened with Prestressed CFRP Plate (CFRP판으로 프리스트레싱 보강한 RC 보의 휨거동에 관한 실험적 연구)

  • Han, Sang-Hoon;Hong, Ki-Nam;Kim, Hyung-Jin;Woo, Sang-Kyun
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.26 no.2A
    • /
    • pp.301-310
    • /
    • 2006
  • Carbon fiber reinforced polymer (CRFP) materials are well suited to the rehabilitation of civil engineering structures due to their corrosion resistance, high strength to weight ratio and high stiffness to weight ratio. Their application in the field of the rehabilitation of concrete structures is increased due to the vast number of bridges and buildings in need of strengthening. However, RC members, strengthened with externally bonded CFRP plates, happened to collapse before reaching the expected design failure load. Therefore, it is necessary to develop the new strengthening method to overcome the problems of previous bonded strengthening method. This problems can be solved by prestressing the CFRP plate before bonding to the concrete. In this study, a total of 21 specimens of 3.3 m length were tested by the four point bending method after strengthening them with externally bonded CFRP plates. The CFRP plates were bonded without prestress and with various prestress levels ranging from 0.4% to 0.8% of CFRP plate strain. All specimen with end anchorage failed by a plate fracture regardless of the prestress levels while the specimen without end anchorage failed by the separation of the plate from the beam due to premature debonding. The cracking loads was proportionally related to the prestress levels, but the maximum loads of specimens strengthened with prestressed CFRP plates were insignificantly affected by the prestress levels.

Distribution of Agalmatolite Mines in South Korea and Their Utilization (한국의 납석 광산 분포 현황 및 활용 방안)

  • Seong-Seung Kang;Taeyoo Na;Jeongdu Noh
    • The Journal of Engineering Geology
    • /
    • v.33 no.4
    • /
    • pp.543-553
    • /
    • 2023
  • The current status of domestic a agalmatolite mines in South Korea was investigated with a view to establishing a stable supply of agalmatolite and managing its demand. Most mined agalmatolite deposits were formed through hydrothermal alteration of Mesozoic volcanic rocks. The physical characteristics of pyrophyllite, the main constituent mineral of agalmatolite, are as follows: specific gravity 2.65~2.90, hardness 1~2, density 1.60~1.80 g/cm3, refractoriness ≥29, and color white, gray, grayish white, grayish green, yellow, or yellowish green. Among the chemical components of domestic agalmatolite, SiO2 and Al2O3 contents are respectively 58.2~67.2 and 23.1~28.8 wt.% for pyrophyllite, 49.2~72.6 and 16.5~31.0 wt.% for pyrophyllite + dickite, 45.1 and 23.3 wt.% for pyrophyllite + illite, 43.1~82.3 and 11.4~35.8 wt.% for illite, and 37.6~69.0 and 19.6~35.3 wt.% for dickite. Domestic agalmatolite mines are concentrated mainly in the southwest and southeast of the Korean Peninsula, with some occurring in the northeast. Twenty-one mines currently produce agalmatolite in South Korea, with reserves in the order of Jeonnam (45.6%) > Chungbuk (30.8%) > Gyeongnam (13.0%) > Gangwon (4.8%), and Gyeongbuk (4.8%). The top 10 agalmatolite-producing mines are in the order of the Central Resources Mine (37.9%) > Wando Mine (25.6%) > Naju Ceramic Mine (13.4%) > Cheongseok-Sajiwon Mine (5.4%) > Gyeongju Mine (5.0%) > Baekam Mine (5.0%) > Minkyung-Nohwado Mine (3.3%) > Bugok Mine (2.3%) > Jinhae Pylphin Mine (2.2%) > Bohae Mine. Agalmatolite has low thermal conductivity, thermal expansion, thermal deformation, and expansion coefficients, low bulk density, high heat and corrosion resistance, and high sterilization and insecticidal efficiency. Accordingly, it is used in fields such as refractory, ceramic, cement additive, sterilization, and insecticide manufacturing and in filling materials. Its scope of use is expanding to high-tech industries, such as water treatment ceramic membranes, diesel exhaust gas-reduction ceramic filters, glass fibers, and LCD panels.