증기 터빈축 강재의 장시간 크리프 수명 예측법 개선 (Improvement of long-time creep life prediction of steam turbine rotor steel)

  • 오세규;정순억;전태언
    • 한국해양공학회지
    • /
    • 제10권1호
    • /
    • pp.47-52
    • /
    • 1996
  • This paper deals with a study on improvement of long-time creep life prediction of steam turbine rotor steels by using initial strain method as a new approach at high temperatures of 500 to 70$0^{\circ}C$ . The main result shows that the inital strain method could be reliably utilized to predict and evaluate the long-time creep life as creep rupture strength and that the predicting equation for long-time creep life under a certain creep stress at a certain high temperature could be empirically derived out from each initial instantaneous strain measured.

  • PDF

보일러 管材料의 크리프破斷特性에 미치는 고온부식의 影響 (The Effects of Hot Corrosion on the Creep Rupture Properties of Boiler Tube Material)

  • 오세욱;박인석;강상훈
    • 대한기계학회논문집
    • /
    • 제13권2호
    • /
    • pp.236-242
    • /
    • 1989
  • 본 연구에서는 주로 보일러의 과열기 및 재열기등의 관재료로 널리 사용되고 있는 304 스테인레스강에 대하여 실제 고온부식현상을 재현한 부식환경하인 630.deg. C, 690.deg. C 및 750.deg. C 3가지 온도범위에서 크리프시험을 실시하고 고온부식이 크리프파단 특성에 미치는 영향을 부식조건이 없는 고온대기중의 실험결과와 비교 검토하였다.

STS304강의 단시간 크리프 파단특성 평가 (Characteristics of Short-Term Creep Rupture in STS304 Steels)

  • 김선진;공유식
    • 한국해양공학회지
    • /
    • 제21권4호
    • /
    • pp.28-33
    • /
    • 2007
  • The objective of this paper is to investigate the relationship between the short-term creep rupture time and the creep rupture properties at three different elevated temperatures in STS304 stainless steel. Uniaxial constant stress creep rupture tests were performed on the steel to observe the creep rupture behaviors at the elevated temperatures of 600, 650 and 700, according to the testing matrix. It is very important to predict creep life in practical creep design problems. As one of the series of studies on the statistical modelling of probabilistic creep rupture time and the development of creep life prediction techniques, the relationship between applied stress and creep rupture behaviors, such as creep strain rate and rupture time, were investigated. In addition, the Monkman-Grant relationship was observed between the steady-state creep rate and the creep rupture time. The creep rupture surfaces observed by SEM showed up dimple phenomenon at all conditions.

10%Cr Martensite계 내열주강 용접부의 Creep파단 특성 및 미세 조직 (Creep Characteristics and Micro-structure for 10%CrMoVNbN Cast Steel Welded Joints)

  • 지병하;양병일;이경운;권희경
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.146-148
    • /
    • 2004
  • 최근 전세계적으로 활발히 진행되고있는 화력발전소용 내열강의 연구는 화력발전소의 열효율 향상을 위한 주증기 조건의 고온ㆍ고압화를 실현하기 위해 고온 크리프 파단강도 개선에 모든 연구력이 집중되고있다. (중략)

  • PDF

마찰용접된 니켈기 초내열합금 Alloy718의 고온 크리프 파단 특성 (High Temperature Creep Rupture Characteristics of Ni-Based Alloy718 Jointed by Friction Welding)

  • 권상우;공유식;김선진
    • 한국해양공학회지
    • /
    • 제22권6호
    • /
    • pp.58-63
    • /
    • 2008
  • The short-term high temperature creep rupture behavior of Ni-based Alloy718 steels jointed by friction welding wasinvestigated at the elevated temperatures of 550 to $700^{\circ}C$ under constant stress conditions. The creep rupture characteristics such as creep stress, rupture time, steady state creep rate, and initial strain were evaluated. Creep stress has a quantitative correlation between creep rupture time and steady state creep rate. The stress exponents (n, m) of the experimental data at 550, 600, 650 and $700^{\circ}C$ were derived as 26.1, -22.4, 22.5, -18.5, 17.4, -14.3 and 6.9, -8.1, respectively. The stress exponents decreased with increasing creep temperature. The creep life prediction was derived by the Larson-Miller parameter (LMP) method and the result equation obtained is as follows: T(logtr+20)=-0.00148${\sigma}^2$-3.089${\sigma}$+23232. Finally, the results were compared with those of the base metal for Alloy718.

2상 스테인리스강(STS 329J1)의 크리프 특성 (Creep Behaviours of Duplex Stainless Steel)

  • 황경충;권종완;윤종호
    • 한국공작기계학회논문집
    • /
    • 제14권2호
    • /
    • pp.42-47
    • /
    • 2005
  • Micro duplex stainless steel is used to denote a fine scale two-phase micro structure consisting austenite and firrite. The development of this structure was done by proper thermo-mechanical processing. The objective of present investigation is to study creep characteristics of this alloy. Since we have little design data about the W behaviors of the alloy. An apparatus has been designed and built fir conducting creep tests under constant load conditions. A series of creep tests on them have been performed to get the basic design data and life prediction of micro duplex stainless steel products and we have gotten the 1311owing results. First the stress exponents decrease as the test temperatures increase. Secondly, the creep activation energy Gradually decreases as the stresses become higher. Thirdly, the constant of Larson-Miller Parameters on this alloy is estimated as about 5. Last, the fiactographs at the creep rupture show both the ductile and brittle fracture modes according to the creep conditions.

안경테소재 합금(Ti-6AI-4V)의 크리프 특성 (Creep Behaviours of Glasses Rim Material Alloy)

  • 황경충;윤종호
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2003년도 추계학술대회
    • /
    • pp.248-253
    • /
    • 2003
  • Titanium alloy has widely been used as glasses rim material because it has high specific strength and also is light, harmless to men. But, we have little design data about the creep behaviors of the alloy. Therefore, in this study, an apparatus has been designed and built for conducting creep tests under constant load conditions. A series of creep tests on them have been performed to get the basic design data and life prediction of titanium products and we have gotten the following results. First, the stress exponents decrease as the test temperatures increase. Secondly, the creep activation energy gradually decreases as the stresses become bigger. Thirdly, the constant of Larson-Miller parameters on this alloy is estimated about 13. And last, the fractographs at the creep rupture show both the ductile and the brittle fracture according to the creep conditions.

  • PDF

티타늄합금(Ti-6Al-4V)의 0.3Tm에서 크리프 특성 (Creep Characteristics of Titanium Alloy(Ti-6Al-4V) at 0.3Tm)

  • 윤종호;황경충;우현구
    • 한국자동차공학회논문집
    • /
    • 제13권3호
    • /
    • pp.117-122
    • /
    • 2005
  • Titanium alloy has widely been used as material for glasses frame parts because it has high specific strength. It is also light and harmless to human body. However, we have little design data about the mechanical properties such as the creep behaviors of the alloy. Therefore, in this study, creep tests under four constant stress conditions have been conducted with four different temperature conditions. A series of creep tests had been performed to get the basic design data and life prediction of titanium products and we have gotten the following results. First, the stress exponents decrease as the test temperatures increased. Secondly, the creep activation energy gradually decrease as the stresses became bigger. Thirdly, the constant of Larson-Miller parameter on this alloy was estimated as about 2.5. Finally, the fractographs at the creep rupture showed the ductile fracture due to the intergranullar rupture and some dimples.

Sn-3.5Ag-xCu무연 솔더의 크리프 성질 연구 (The Creep Properties of Pb-free Sn-3.5Ag-$\chi$Cu Solder Alloys)

  • 주대권;유진
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2001년도 추계 기술심포지움
    • /
    • pp.141-145
    • /
    • 2001
  • Sn-3.5Ag 무연 솔더에 Cu를 첨가한 3원계 합금을 만든 후 압연과 열처리한 후 크리프 특성을 연구하였다. 모든 솔더 합금에서 1차 크리프는 거의 관찰되지 않았으며, 2차와 3차 크리프가 대부분을 차지하였고, 최소 크리프 변형율은 Cu 함량이 0.75 wt %에서 최소이었고, 응력 지수는 약 4이었으며, 파단 시간 또한 0.75 wt% Cu에서 가장 길었다. 크리프 기구는 격자 확산에 의한 전위의 상승과 전위 활주에 의한 고온 크리프임을 앞 수 있었으며, Cu의 첨가는 1 wt% 가지 연성에 큰 영향을 주지 않았으나, 1.5 wt% 첨가했을 경우 연성은 크게 감소하였다.