  • Ultra high strength concrete, nowadays, has been widely applied to construction of high-rise building. To improve ductility and mechanical properties, steel fiber is employed in UHSC. This study investigates practical application of expansive additives(EA) and shrinkage reducing agent(SRA), in order to secure volumetric stability and improved mechanical properties, such as autogenous shrinkage and dry shrinkage of steel-fiber-reinforced-ultra-high-strength-comet-mortar(FHSM). According to the test, individual addition of steel fiber does not affect shrinkage reduction, as expected. However FHSM, with combined addition of 5$\%$ of EA and 1$\%$ of SRA decreased 60$\%$ of autogenous shrinkage. It is considered that Proper combination of EA and SRA can secure the shrinkage resistance of FHSM.

  • PDF

혼화재 종류 및 치환율에 따른 모르터의 조기강도 특성에 관한 연구 (A study on the Early-Strength Properties of Mortar according to the Kinds and Replacement Ratio of Mineral Admixture)

  • 최세진;이성연;김성수
    • 한국건축시공학회지
    • /
    • 제7권2호통권24호
    • /
    • pp.59-65
    • /
    • 2007
  • Recently, due to the increase of high-rise buildings construction, many researches for making harden of concrete earlier and remove of forms faster are being performed to reduce construction period. In this study, we compared and analysed the early strength properties of mortar according to the kinds and replacement ratio of mineral admixture to select the kinds and replacement ratio of mineral admixture of high early strength concrete. For this purpose, mortar mixtures according to the kinds(FA, MK, ZR, BFS, DM) and replacement ratio(0, 2, 4% by volume of sand) of mineral admixture were selected. From our test data, early-age compressive strength decreased in accordance with the increase of replacement ratio of fly-ash(FA) & blast furnace slag powder(BSF) and, in case of addition admixture, early-age compressive strength of with containing 4% appeared higher compared with containing 2%.

프리믹스 시멘트를 사용한 모르터의 기초적 특성 분석 (Analysis on Basic Characteristics of Mortar with Pre-Mix Cement)

  • 김성일;장기현;이충섭;한동엽;김기훈;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2008년도 춘계 학술논문 발표대회
    • /
    • pp.93-97
    • /
    • 2008
  • The study analyzed on each kind of basic characteristics in mortar to prove an effect of pre-mix cement, ultra high strength binder. The results were as follows. in characteristics of not set mortar, fluidity time was the quickest at the time of using POBSA and was more delayed at the time of using Fly Ash than at the time of using Blast Furnace Slag as a binder. Mortar ring flow and flow con flow got smaller as fluidity time got longer, on the contrary to fluidity time. Unit capacity mass was smaller at the time of using Fly Ash than at the time of using Blast Furnace Slag. According to pre-mix, it was difficult to discover a regular tendency. In characteristics of hardening mortar, the 28th day compressive strength was better than thing mixed after measuring separately in pre-mix. According to a binder's kind, Silica Fume B, C was better than Silica Fume A.