This study was to investigate the effect of the new surface treatment method of zirconia on the shear bond strength with resin cement. The zirconia specimens were classified according to the surface treatment. CON: non-treatment, HF: 10 minutes exposure to 9% HF, ZS15: Apply 15% ZrO2 slurry, ZS30: Apply 30% ZrO2 slurry, ZS50: Apply 50% ZrO2 slurry. The resin cement was layered on the surface treated zirconia, and the shear bond strength between the zirconia and the resin cement was measured after thermo-cycling. The statistical methods for shear bond strength were Kruskal-Wallis test, Mann-Whitney U test, and Bonferroni correction(α=.05/10=.005). ZS15, ZS30, and ZS50 groups treated with zirconia slurry showed higher shear bond strength than CON and HF groups(p<.05/10=.005). Within the limits of this study, the surface treatment using zirconia slurry increased the shear bond strength with resin cement. The new surface treatment method complements and improves the limitations of the adhesion of zirconia, so that various clinical applications of zirconia can be expected.
Proceedings of the Membrane Society of Korea Conference
/
1996.10a
/
pp.59-59
/
1996
막분리에 의한 폐윤활유 재생공정을 개발하기 위한 기초 연구로써 폐윤활유 분리/재생용으로 적합한 복층(multilayer)세라믹 복합막의 제조와 합성막의 폐유 분리 효율등이 연구되었다. 결함이 없고 두께가 균일한 지르코니아 복합막 (기공크기 0.07 $\mu$m 이하)은 압출 성형법으로 제조한 튜브형 $\alpha$-알루미나 담체 (외경 7.8 mm, 두께 0.6 mm, 기공크기 0.7 $\mu$m)내부표면에 역침지 인상법(reverse dip-drawing technique)에 의하여 지르코니아 슬러리를 코팅 한 후 950$\circ$C에서 1시간 열처리하여 제조 되었다. 또한 지르코니아 복합막 위에 니타니아 졸-겔 코팅을 한 후 450$\circ$C에서 2시간 열처리하여 기공크기가 15 nm정도인 3층 복합막을 제조 하였다. SEM, Bubble Point Test, Mercury Porosimeter 그리고 분획 분자량 측정등에 의하여 복합막의 코팅층 두께, 결함유무 및 막의 기공크기등을 분석하였다.
Zirconia/alumina mixture powder was spray-dried various degree of dispersion, type of dispersants and powder content in the slurry. The quality of the granule was determined by observation of the granule shapes after spray drying and fracture of intergranular boundaries during pressing. Defect-free granules were obtained from the powders that formed weak flocs in the slurry. The granules, spray-dried from the slurry containing 32.5 vol% powder mixture and PVP as binder, were fractured completely during shaping and the sintered specimens showed a density of 99.7% and a flexural strength of 850 MPa.
경제적이고 단순성의 공정특성을 갖는 닥터 블레이드법을 이용하여 평판형 고체산화물 연료전지의 고체전해질용 이트리아 안정화 지르코니아 박막을 제조하였다. 슬러리의 최적 제조조건과 그린 필름의 최적 소성조건을 얻었으며, 이 제조 조건에서 제조된 전해질의 결정구조, 미세구조 그리고 전기적 성질을 각각 X-선 회절, 주사전자현미경 그리고 교류 임피던스 분석기를 이용하여 조사하였다. 동량의 8mol% 이트리아를 첨가한 경우, 닥터 블레이드법에 의해 제조된 이트리아 안정화 지르크니아 박막은 금형가압성형법에 의해 제조된 이트리아 안정화 지르코니아 펠렛과 거의 비슷한 전기전도도를 나타내었다. 닥터 블레이드법에 의해 제조된 이트리아 안정화 지르크니아 박막의 경우, 8mol%이트리아를 첨가한 경우의 전도도가 3mol%이트리아를 첨가한 경우 보다 993K 이상과 523K 8mol% 이트리아를 첨가한 경우의 전도도가 3mol%이트리아를 첨가한 경우의 전도도가 3mol%이트리아를 첨가한 경우 보다 993K이상과 523K이하의 온도에서는 더 높고, 523-933K사이의 온도구간에서는 낮게 나타났다. 게다가, 모든 시편에 있어서 전체 전도도에 대한 벌크 전도도의 기여도에 대한 기여도보다 더 크게 나타났다.
세라믹 분리막은 알루미나($Al_2O_3$), 지르코니아($ZrO_2$), Carbon, 실리콘 카바이드, 스테인레스 등의 무기재료를 이용하여 제조된 분리막이다. 압출성형공정으로 제조된 지지체는 1700$^{\circ}C$ 이상의 소결공정을 거치므로 지지체 상단에 슬러리 코팅공정으로 형성된 얇은 막에게 안정된 분리기능을 수행할 수 있도록 커다란 물리적 강도를 제공한다. 따라서, 세라믹 분리막은 다공성 세라믹 구조를 갖는 특징적인 두 개 또는 세 개의 균일한 층으로 구성된 복합막이라 할 수 있다.
The preparation method of yttria-stabilized zirconia(YSZ) thin film for an anode support type solid oxide fuel cell(SOFC) by electrophoretic deposition(EPD) and dip-coating was studied. And the difference in both preparation method was investigated through basic understanding of processing parameters which may significantly affect weight microstruxcture and defect of film. In dip-coating the thickness of film increased with time until 30 s and then the weight of film decreased with time due to particle falling off from the coagulated film. In EPD although the weight of film increased with time and applied constant-current sagging of the film was observed when the applied current was less that 0.035 mA/$cm^2$ and more than 120 s. Since YSZ thin film by EPD on porous substrate was dense smooth and homogeneous it was expected to be suitable for the electrolyte of an anode support type SOFC.
Transactions of the Korean hydrogen and new energy society
/
v.17
no.2
/
pp.204-211
/
2006
The electrolyte in the solid oxide fuel cell must be dense enough to avoid gas leakage and thin enough to reduce the ohmic resistance. In order to manufacture the thin and dense electrolyte layer, 8 mol% $Y_2O_3$ stabilized-$ZrO_2$ (8YSZ) electrolyte layers were coated on the porous tubular substrate by the novel vacuum slurry dip-coating process. The effects of the slurry concentration, presintering temperature, and vacuum pressure on the thickness and the gas permeability of the coated electrolyte layers have been examined in the vacuum slurry coating process. The vacuum-coated electrolyte layers showed very low gas permeabilities and had thin thicknesses. The single cell with the vacuum-coated electrolyte layer indicated a good performance of $495\;mW/cm^2$, 0.7 V at $700^{\circ}C$. The experimental results show that the vacuum dip-coating process is an effective method to fabricate dense thin film on the porous tubular substrate.
Kim, Ji-Hyeon;Yang, Tae-Yeong;Lee, Yun-Bok;Yun, Seok-Yeong;Park, Heung-Chae
Korean Journal of Materials Research
/
v.11
no.6
/
pp.519-526
/
2001
The effects of methyl isobutyl ketone(MIBK)/ethanol(EtOH) solvent mixtures on the dispension, particle size distribution and rheology of $Al_2$O$_3$/ZrO$_2$ nonaqueous suspensions were investigated by measuring sedimentation density and viscosity. The sedimentation density of $Al_2$O$_3$ and ZrO$_2$ particles increased in MIBK-rich($\geq$60 vol%) solvents with 'Hypermer' KD-1 as a dispersant. The ball-milled suspensions in 80MIBK/20EtOH(vol%) solvent exhibited the narrow and unimodal particle size distribution. Although all Suspensions exhibited the Pseduo-Plastic flow(Shear thinning) the shear thinning behavior was somewhat different depending on the mixture ratio of $Al_2$O$_3$/ZrO$_2$ and MIBK/EtOH. Under a given shear rate( <300 s$^{-1}$ for $Al_2$O$_3$; <3000 s$^{-1}$ for ZrO$_2$) the strongest shear thinning appeared in the $Al_2$O$_3$ and ZrO$_2$ suspensions with pure MIBK solvent. The shear thinning was nearly independable on the mixture ratio of $Al_2$O$_3$/ZrO$_2$ in case of using the identical solvent(80MIBK/20EtOH, vol%).
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.