건식 제조방식에 의해 생산된 재생 잔 골재의 품질 및 모르타르 특성에 관한 실험적 연구 (An Experimental Study on the Qualities of Recycled Fine Aggregate and Properties of Mortar Producted by the Dry Manufactured Method)

  • 윤종기;장재봉;송민섭;나철성;장종호;김무한
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 봄 학술발표회 논문집
    • /
    • pp.229-232
    • /
    • 2003
  • Recently, it is increased on the concern for the reuse of waste concrete because of the shortage of natural aggregate and the increase of waste concrete. And recycled coarse aggregate is used variously, but the existing wet method producted recycled fine aggregate has problems like the high price facilities, the long time progress of the work and recycled fine aggregate of poor. The aim of this study is to investigate the possibility of the method of dry producted high qualities recycled fine aggregate. The results of this study have shown that the possibility of the method of dry is certificated as the qualities of recycled fine aggregate satisfied the KS and the compressive strength of mortar was similar to plain.

  • PDF

재생(순환)잔골재의 부착모르타르량 측정에 관한 실험적 연구 (The experimental regarding the affix mortar quanity measurement of the recycled fine aggregate)

  • 조현대;정재동;이도헌;전명훈
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2004년도 추계 학술발표회 제16권2호
    • /
    • pp.189-192
    • /
    • 2004
  • This study bases on showing the pictures of how to keep a recycled fine aggregate well (quality control) and how to invent the measurement of mortar's quantities which largely effect on basic properties of matter: strength, durability and so on. As a result of the experiment by immersion, quantities of adhesive cement takes 7 to 8 days to stabilize by sulfuric. However, by hydrochloric acid, it takes a little quicker due to the first quick reaction, aggregate of the measurement of adhesive mortar by immersion used acid liquids are likely applicable following a suitable inspection and complementarity.

  • PDF

폐미분말을 원료로 한 저탄소형 재생시멘트의 CO2배출량 저감평가 (Evaluation of Reduction of CO2 Emission Achieved by Using Low-carbon Recycled Cement with Cementitious Waste Powder)

  • 권은희;안재철;박동천
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.250-251
    • /
    • 2014
  • With the recent movement toward sustainable development, many efforts have been made to reduce environmental loads in various domains of industry. In particular, a great deal of research and technology development has been underway on approaches to reducing industrial waste and the emission of greenhouse gases. For this reason, a quantitative analysis of the reduction in CO2 emission that could be achieved by replacing limestone material with cementitious waste powder was performed in this study. Through the analysis, it was found that CO2 emissions were reduced by up to 50 percent compared with the scenario in which OPC was used, which suggests that it is possible to reduce global CO2 emissions by approximately 5percent, or by 446.4 Tg of the 965 Tg of CO2 emissions generated by the cement industry, in the total global CO2 emissions of 19300Tg.

  • PDF

고로슬래그를 사용한 건식 및 습식 재생 잔골재 모르타르의 물리적 특성에 관한 연구 (A Study on the Physical Properties of Recycled Fine Aggregate (by Dry and Wet Type Production formula) Mortar Using Blast Furnace Slag)

  • 심종우;이세현;서치호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.501-504
    • /
    • 2006
  • Recycled aggregate mortar contains plenty of calcium hydroxide to improve the strength of blast furnace slag, although the surface mortar made of recycled aggregate deteriorates adhesion to cement paste and blast furnace slag has a low initial strength. Therefore, this study assumes that the combination with both recycled aggregate and blast furnace slag will produce a better performance. The results of the experiment show that dry mortar made of recycled aggregate provides with higher strength than wet mortar does at the 3-day and 7-day age, while lower at the 28-day age. It indicates that a large amount of cement mortar made of dry recycled aggregate has deteriorated adhesion strength. The mixes with 30% and 50% of blast furnace slag and 50% and 75% of recycled aggregate provide with much better strength at the 7-day age, although they usually have latent hydraulic property at the 28-day age. It indicates that calcium hydroxide($Ca(OH){_2}$) in recycled aggregate has affected ground granulated blast furnace slag.

  • PDF

태양광 발전을 위한 보도형 콘크리트 블록의 현장 적용과 유지관리 (Field Application and Maintenance of sidewalk concrete block for PV Power Generation)

  • 김봉균;김윤용
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제23권5호
    • /
    • pp.75-83
    • /
    • 2019
  • 파리기후협정에 따른 온실가스 자발적 감축 의무 이행을 위해 세계적으로 석탄발전과 원자력발전의 비중을 줄이고 태양광 발전을 비롯한 재생에너지의 보급에 국가적 노력을 기울이고 있다. 우리나라도 법령을 도입하여 2040년까지 재생에너지의 발전비중을 30~35%까지 늘리고자 하고 있다. 또한 국외에서는 태양광 발전을 보도 및 도로에 적용하고자 하고 노력하고 있으나 국내의 경우 관련 연구가 전무한 실정이다. 따라서 태양광발전 도로를 개발하기 위한 선행연구로서 보도 및 광장에 적용가능한 태양광 발전 콘크리트 블록을 개발하였으며 이를 현장에 시공하여 적용성을 평가하였다. 실내실험결과 압축강도는 25.5~35.7MPa이 측정되었고 휨강도는 5.1~10.5MPa이 측정되어 국내 기준은 모두 만족하는 것으로 나타났으나 단위시멘트량이 많을수록 부순잔골재의 혼입에 따라 강도가 낮게 측정되었다. 흡수율은 최대 5.7%로 나타나 국내 기준인 7%이하를 만족하였으며 동결융해시험 결과 100싸이클 후 압축강도 감소율은 최대 6.3%로 나타나 양호한 수준으로 측정되었다. 시공 후 침하량을 측정결과 최대 2.498mm가 측정되었으며 전면적에 대해 불규칙한 침하가 발생하였는데 이는 시공시 모래층의 다짐이 불량하였거나 우수에 의한 모래 유출로 인한 것으로 판단된다. 초기발전량의 경우 일사량을 고려하면 적정량이 측정되었다. 태양광 패널과 콘크리트 블록의 유지관리 기법은 추후 연구를 통하여 보다 효율적으로 확립할 필요가 있다.

고로슬래그미분말 및 하수슬러지를 활용한 저강도 콘크리트의 기초적 물성 (Fundamental Properties of Low Strength Concrete Mixture with Blast Furnace Slag and Sewage Sludge)

  • 권칠우;임남기
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제17권3호
    • /
    • pp.136-144
    • /
    • 2013
  • 본 연구에서는 각종 산업부산물 및 도시형 리싸이클링 재료 등의 재생자원을 안전하게 유효 이용할 수 있는 방안으로 BFS 및 SS를 활용한 저강도 콘크리트의 기초적 물성을 파악하기 위하여 플로우 및 블리딩, 일축압축강도, 환경오염평가를 중심으로 실험을 실시하였다. BFS 및 SS를 활용한 저강도 콘크리트의 경우 최소단위수량의 확보를 통한 유동성 개선 및 블리딩율 억제 또한, 현장 적용성을 고려한 일축압축강도의 확보에 있어 사용 잔골재의 차이에 상관없이 BFS 6000 이상을 30% 범위에서 혼입하는 것이 가장 유효한 것으로 나타났다. 특히, SS의 유효 활용 측면에서 BFS 8000을 30% 범위에서 혼합하여 사용하면 유동성 개선 및 블리딩율 억제, 일축압축강도의 확보는 물론 현장 적용에 있어 가장 최적의 배합조건으로 나타났다. 한편, SS를 활용한 시멘트 개량토를 대상으로 유해물질 함유량 및 용출시험을 실시한 결과 모두 환경 기준치 이하를 만족하는 것으로 나타나 주변 환경에 미치는 영향은 없는 것으로 확인되었다.

재생 이산화티탄을 혼입한 모르타르의 NOx 저감률 민감도 분석 (Sensitivity of NOx Removal on Recycled TiO2 in Cement Mortar)

  • 이인규;김진희;김종호;노영숙
    • 한국건설순환자원학회논문집
    • /
    • 제4권4호
    • /
    • pp.388-395
    • /
    • 2016
  • 본 논문에서는 폐수슬러지에서 제조된 재활용 이산화티탄($TiO_2$)을 혼입한 시멘트 모르타르의 NOx 저감 성능에 대해 고찰하였다. 일반적으로, 이산화티탄은 클러스터 형태로 입자가 붙어 있어, 시멘트의 응결과 경화 전에 타설체 하면에 침강하는 특징이 있다. 그 결과로 타설체의 상면과 하면에는 이산화티탄의 분포도가 서로 상당한 차이를 나타내고, 광촉매 효과도 하면에서 우수하게 나타난다. 건물이나 주택과 같은 건축구조물에서는 이를 해결하기 위해, 이산화티탄을 혼입한 프리캐스트 제품을 미리 제작 후, 조립 시에는 타설 시 상면과 하면을 뒤집어 거치하여 상대적으로 높은 이산화티탄 분포면을 대기에 노출시키는 방식을 사용한다. 그러나 콘크리트 도로포장과 같은 현장 타설의 경우, 상면과 하면을 뒤집어 거치할 수 없기 때문에 이산화티탄의 분산성은 중요하다. 이를 개선시키기 위한 본 논문의 결과로 실리카퓸, 고성능감수제, 증점제, 고로슬래그 등 전형적인 시멘트성 재료의 분산에 기여하는 재료는 이산화티탄 클러스터의 분산효과에 미미한 영향을 주었다. 급결제, 발포제, 작은 크기의 잔골재의 조합이 이산화티탄 클러스터의 분산성을 개선하였다. 분산성 개선에도 불구하고, 타설체 상면과 하면의 NOx 제거효율은 하면에 큰 효율을 지속적으로 나타내었고, 이는 표면에 분포하는 공극량에 따라 달라지는 것을 디지털 표면 이미지 분석을 통하여 확인하였다. 많은 공극분포를 갖는 표면은 상대적으로 매끄러운 표면에 비해 NO가스 흡착을 기본적으로 높이게 되고, 이를 기준으로 상대적인 NOx 제거효율이 높아지는 것으로 사료된다.