• Title/Summary/Keyword: 잔존물

Search Result 464, Processing Time 0.021 seconds

An Experimental Study on the Evaluation of Residual Tensile Load-carrying Capacity of Corroded Steel Plates of Temporary Structure (가시설 부식 강재의 잔존 인장 내하성능 평가에 관한 실험적 연구)

  • Kim, In-Tae;Chang, Hong-Ju;Cheung, Ji-Young
    • Journal of Korean Society of Steel Construction
    • /
    • v.22 no.5
    • /
    • pp.399-409
    • /
    • 2010
  • Steel structures are threatened to reduce load-carrying capacity as the cross section is decreased by corrosion. However, there has been no method in definitely evaluating residual load-carrying capacity and the effect of corrosion to the load-carrying capacity of steel. This study evaluated tensile residual load-carrying capacity of corroded steel plates by using tensile tests of specimens, which were selected from the web of temporary structure's main beam. After the surface shapes were measured and tensile tests were examined, the rust of 21 corroded specimens was, first of all, removed using a chemical method. From the tensile test result, which of reference specimens that was picked off at the flange of the same main 13-mm-thick beam and corroded specimens were based, surface geometry and correlation with the reduction of corroded thickness and strain, yield strength or tensile strength was established as constant numbers. Effective thickness of corroded steel with irregular cross sections could be calculated using average residual thickness and standard deviation. The irregular cross sections could be the evaluated tensile strength that is equalized to non-corroded uniform steel's regardless of corrosion. Also, reasonable measuring intervals of residual thickness could be proposed by using this result to apply for executive work.

PHYSICAL PROPERTIES OF VAR10US BRANDS OF ELASTOMERIC CHAINS (수종의 합성 고무탄성재의 성질에 관한 연구)

  • Kim, Kyung-Ho;Hwang, Chung-Ju;Sung, Sang-Jin
    • The korean journal of orthodontics
    • /
    • v.27 no.6 s.65
    • /
    • pp.943-954
    • /
    • 1997
  • Forces needed for orthodontic tooth movement are obtained from various appliances such as orthodontic wires or elastic rubber. Orthodontic elastic rubber is widely used clinically, but permanent deformation and force decay may occur from the environmental changes, time of clinical use and the extent of the stretch, making the Prediction of force being applied difficult. The Present study examined and compared the changes in residual force between three brands of elastomeric chains (Ormco Generation II Power Chains ; brand A, RMO : Energy-Chain ; brand B, Unitek : AlastiK ; brand C) under various environmental conditions, amount of initial force, types of elastomer and the rate of extension. The characteristic physical properies of the elastomeric chains were as follows. 1. In all three brands, the residual force ratio was largest when the chains were stored in air, with no difference between water and saliva. 2. In all three brands, after 24 hours, there was no statistical difference in residual force ratio according to the initial force level. 3. In Brand A and B, the presence of filament had no correlation with the residual force ratio. In Brand C force decay was more severe when the chain contained filament. 4. In each brand, rate of extension had no effect on residual force ratio. 5. Brand B showed relatively higher residual force ratio compared to other brands.

  • PDF

Estimation of Shear Strength of Discontinuous (bedding) Cut Sedimentary Rock Slope by Using Back Analysis (역해석을 통한 퇴적암 절취비탈면 불연속면(층리)의 전단강도 추정)

  • Kim, Chang-Ho;Kim, Bong-Yong;Park, Tae-Wan;Kim, Tae-Hyung
    • Journal of the Korean Geosynthetics Society
    • /
    • v.17 no.1
    • /
    • pp.139-152
    • /
    • 2018
  • This study is an analysis of slope failure examples of cut sedimentary hills during construction road in Kyoungsang Basin, especially Yangsan Fault system (Ilkwang-Dongrae fault). This area involved a lot of hillslope failures compared to other areas during road construction. The exposed failure slopes were first face-mapped, and then back analyzed based on the limit equilibrium method to assess the shear strength parameters of discontinuity (bedding). The results of this analysis indicate that the shear strength parameters of discontinuity (bedding) are significantly smaller than those used in the design stage and presented in the existing works. The filling in the bedding and emerging groundwater may be decreasing strength parameters. Especially, the clay in the bedding plays a key role in the effect of the shear strength. The study also suggests that the bedding angle and the internal friction angle are proportional to each other. Using this relationship and knowing the bedding angle, the friction can easily be estimated.

Microencapsulation of aronia extract and stability of encapsulated anthocyanins during sulgidduk cooking (아로니아 추출물의 미세캡슐 제조 및 설기떡의 안토시아닌 안정성 연구)

  • Choi, Yeji;Koh, Eunmi
    • Korean Journal of Food Science and Technology
    • /
    • v.54 no.2
    • /
    • pp.163-170
    • /
    • 2022
  • Aronia (Aronia melanocarpa cv. Viking) contains high amounts of anthocyanins, which are susceptible to heat. This study was conducted to identify an efficient coating material for encapsulating aronia extract to enhance the stability of anthocyanins during cooking. Maltodextrin, maltodextrin+gum Arabic, and maltodextrin+carboxymethyl cellulose were chosen as the coating materials, mixed with aronia extract at a ratio of 2:1, and freeze-dried after homogenization. The encapsulated aronia extract was then used as a sulgidduk ingredient. Sulgidduk prepared with the encapsulated aronia had significantly higher values for redness, anthocyanin retention, total phenolic content, and antioxidant activity compared to sulgidduk prepared with non-encapsulated aronia. In addition, the sensory evaluation revealed that sulgidduk prepared with encapsulated aronia produced better color and taste. These results indicate that the encapsulation of aronia extract improved the stability of the anthocyanins in aronia, and encapsulated aronia can be used as a functional colorant in the food industry.

An Experimental Study of Spalling Characteristics of High-Strength Reinforced Concrete Columns with PP Fibers (PP 섬유를 함유한 고강도 철근콘크리트 기둥의 폭열 특성에 관한 실험적 연구)

  • Sin, Sung-Woo;Yu, Suk-Hyeong
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.2
    • /
    • pp.83-90
    • /
    • 2006
  • A spalling is defined as the damages of concrete exposed to high temperature during the fire by causing cracks and localized bursting of small pieces of concrete. It is reported that spalling is caused by the vapor pressure and polypropylene(PP) fiber has an important role in protecting from spalling. The characteristics of fire resistance of high-strength reinforced concrete columns with various concrete strength and various contents of PP fiber were investigated in this study. In results, the ratio of unstressed residual strength of columns increases as the concrete strength increases and the ratio of unstressed residual strength of columns exposed to fire decreases as the content of PP fiber increases from 0% to 0.2%.

A Preliminary Study on the Reused Channel-Type Lining Board with Corrosion-Damage (부식 강재 복공판의 재사용성 평가에 관한 기초적 연구)

  • Kim, In-Tae;Kim, Dong-Woo;Choi, Hyoung-Suk;Cheung, Jin-Hwan
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.13 no.4 s.56
    • /
    • pp.170-179
    • /
    • 2009
  • Channel-type lining board(CLB) is a welded steel structure used in the field of open cut subway excavation and building basement construction. Lining board is generally installed at the underground environment which is exposed to corrosion factors such as humidity, temperature and corrosive gases. This study evaluates reusability of the corroded lining board by experimental and analytical method. Static loading tests were performed to know serviceability of corroded CLB after checking thickness loss of the used CLB parts. Strain of the plates and middle point deflection was measured simultaneously. According to experimental test results and comparison with numerical analysis, the thickness loss of the plates by corrosion makes more vertical displacements and stresses in members under the DB vehicle load considering impact factor. As a result, this paper is proposed a way to evaluate used and corroded CLB by checking the plates thickness and it makes construction engineers easy to know optimal time to replace their old CLBs with new one.

SP시험법에 의한 재료의 파괴강도 평가

  • 정세희;정희돈
    • Journal of the KSME
    • /
    • v.28 no.4
    • /
    • pp.387-393
    • /
    • 1988
  • 본 SP시험법은 사용되는 시편이 미소하다는 장점 때문에 재질의 평가나 더불어 비파괴검사의 일환으로서 이용할 수 있음을 서명해 왔다. 현존하고 있는 거대구조물들의 잔존수명평가가 요 구되는 있는 지금, 정량적인 경년변화측정방법으로서 SP시험법은 높은 가능성을 내포하고 있는 시험법으로 여겨지며, 이 방법을 현장에 정착시키기 위해선 산. 학. 연의 공동연구체제가 필요 하다고 할 수 있다.

  • PDF

Analytical Evaluation of Residual Strength for Steel Frame in case of Column Member Loss (기둥손실에 따른 철골프레임 잔존내력의 해석적 평가)

  • Park, Hwon-Mo;Yeshewawork, D.;Kim, Hyun-Soo;Choi, Jae-Hyouk
    • Journal of the Computational Structural Engineering Institute of Korea
    • /
    • v.24 no.6
    • /
    • pp.675-683
    • /
    • 2011
  • When impacts by falling objects are applied to the structures, vertical resisting member(column or column group) results in progressive collapse. By knowing clearly load-deformation relationship of a structural frame, to prevent progressive collapse by absorbing potential energy of falling objects though column groups are lost by the impact of falling object accidently. If residual strength in vertical direction exceeds vertical load, which the sum of the weight of falling objects and usual supportive vertical load as the result of absorbing released location energy, it does not result in progressive collapse. On the other hand, in case when weight of falling objects is included in usual supportive vertical load. In this paper, 1-story 4-spans model is analyzed by non-linear FEM and to examine the level of deterioration, limit analysis of 1-story 4-spans plane frame was carried out.

비파괴시험에 의한 균열크기의 측정

  • 박은수
    • Journal of the KSME
    • /
    • v.28 no.4
    • /
    • pp.343-348
    • /
    • 1988
  • 몇 가지 균열검출법 및 크기의 측정법에 대하여 개요, 문제점, 정량적 측정에 유의해야 할 점을 살펴보았다. 아직 어느 방법도 모든 균열에 적용할 만큼 완전한 방법은 없지만 적용범위와 유 의사항을 이해하고 측정대상에 맞는 방법을 올바로 적용한다면 목적에 부합하는 결과를 얻을 것으로 본다. 기기나 구조물의 파괴원인을 정확히 규명하고 잔존수명을 정확히 예측하여 파괴를 방지하려면 재료의 강도특성이나 파괴역학적 해석법의 연구에 못지 않게 비파괴적 균열검출법과 정량적 측정법에 관한 연구도 깊이 이루어져야 하리라 믿는다. 그러나 아직 우리나라에서는 이 점에 미흡함이 많다. 더 나은 측정방법을 고안해 내고, 측정장치를 개발하여 균열에 대한 정보 의 정확성을 높여 구조물의 안전성 평가의 신뢰성을 향상시킬 수 있는 연구가 활발히 진행되 어야 할 것이다.