We studied the specular spin valve (SSV) having the spin filter layer (SFL) in contact with the ultrathin free layer composed of Ta3/NiFe2/IrMn7/CoFel/(NOLl)/CoFe2/Cu1.8/CoFe( $t_{F}$)/Cu( $t_{SF}$ )/(NOL2)/Ta3.5 (in nm) by the magnetron sputtering system. For this antiferromagnetic I $r_{22}$M $n_{78}$-pinned spin filter specular spin valve (SFSSV) films, an optimal magnetoresistance (MR) ratio of 11.9% was obtained when both the free layer thickness ( $t_{F}$) and the SFL thickness ( $t_{SF}$ ) were 1.5 nm, and the MR ratio higher than 11% was maintained even when the $t_{F}$ was reduced to 1.0 nm. It was due to increase of specular electron by the nano-oxide layer (NOL) and of current shunting through the SFL. Moreover, the interlayer coupling field ( $H_{int}$) between free layer and pinned layer could be explained by considering the RKKY and magnetostatic coupling. The coercivity of the free layer ( $H_{cf}$ ) was significantly reduced as compared to the traditional spin valve (TSV), and was remained as low as 4 Oe when the $t_{F}$ varied from 1 nm to 4 urn. It was found that the SFL made it possible to reduce the free layer thickness and enhance the MR ratio without degrading the soft magnetic property of the free layer.
The MR ratios and the exchange biasing field and interlayer coupling field were investigated in $Ni_{91}Fe_{19}/Co_{90}Fe_{10}/Cu/Co_{90}Fe_{10}/NiO$ spin-valve sandwiches grown on antiferromagnetic NiO films as a function of the NiO thickness, the thickness of Cu and pinning layer $Co_{90}Fe_{10}$. The spin-valve sandwiches were deposited on the Corning glass 7059 by means of the 3-gun dc and 1-gun rf magnetron sputtering at a 5 mtorrpartial Ar pressure and room temperature. The deposition field was 50 Oe. The MR curve was measured by the four-terminal method with applied magnetic soft bilayer [NiFe/CoFe] (90$\AA$) decreased dramatically to less than 10 Oe when the NiFe/CoFe bilayer used an NiFe bilayer thicker that 20$\AA$. So NiFe layer improved the softmagnetic properties in the NiFe/CoFe bilayer. The GMR ratio and the magnetic field sensitivity of the spin-valve film $Ni_{91}Fe_{19}(40{\AA})/Co_{90}Fe_{10}(50{\AA}) /Cu(30{\AA})/Co_{90}Fe_{10}(35{\AA})/NiO(800{\AA})$ was 6.3% and about 0.5 (%/Oe), respectively. The MR ratio had 5.3% below an annealing temperature of 20$0^{\circ}C$ which slowly decreased to 3% above 30$0^{\circ}C$. The large blocking temperature of the spin-valve film was taken (as being) due to the good stability of the NiO films. Thus, the spin-valve films with a free NiFe/CoFe layer clearly had a high large GMR output and showed a effective magnetic field sensitivity for a suitable spin-valve head material.
Interlayer coupling field, coercivity, magnetoresitance ratio, and magnetic sensitivity depending on the thickness of free CoFe layer for the CoFe/Cu/CoFe/IrMn multilayer are investigated. In case of CoFe layer of $30\;{\AA}$ thickness for the CoFe(t)/Cu($25\;{\AA}$)/CoFe($60\;{\AA}$)/IrMn($80\;{\AA}$) multilayer with ferromagnet/non-magnet/ferromagnet structure induced by IrMn layer, the lowest coercivity and the highest magnetic sensitivity, which is contained soft magnetic property, are observed. On the other side, in case of CoFe layer of $90\;{\AA}$ thickness, there are the highest coercivity and the lowest magnetic sensitivity. The fabricated CoFe($30\;{\AA}$)/Cu($25\;{\AA}$)/CoFe($60\;{\AA}$)]/IrMn($80\;{\AA}$) spin valve device with $2{\times}8{\mu}m^2$ patterning size are measured by two probe method, which is selected the sensing current as the longitudinal direction and the easy axis as the transversal direction. The measuring magntoresistance ratio and magnetic sensitivity of GMR-SV device having the soft magnetic property are 3.0% and 0.3%/Oe, respectively.
Spin dynamics of magnetic tunnel junctions with free and fixed reference layers is investigated by ferromagnetic resonance micromagnetic simulations. First, in magnetic tunnel junctions with an exchange biased synthetic ferrimagnetic reference layer, a magnetization direction of each layer and the tunneling magnetoresistance are calculated for a DC magnetic field. To investigate the spin exciting modes in magnetic tunnel junctions, we simulate the ferromagnetic resonance frequency spectra with small RF magnetic fields. Exciting modes of the tunneling magnetoresistance calculated by an included angle between free and reference layers is interpreted from those of each layer. Spin exciting modes are different according to a signs of the DC magnetic field. In a negative magnetic field, FMR frequency spectra of free and reference layers are well elucidated by the modified Kittel's equation. However, in a positive magnetic field, there is no simple analytic solution related to FMR frequency spectra due to the coupled modes. Since ferromagnetic layers in magnetic tunnel junctions are interactive each other, careful considerations of the reference and fixed layer as well as the free layer are required for understanding on the spin dynamics of magnetic tunnel junctions with an exchange biased synthetic ferrimagnetic reference layer.
Proceedings of the Korean Magnestics Society Conference
/
2012.11a
/
pp.146-148
/
2012
미크론 자성비드 검출용 바이오센서에 활용하는 GMR-SV 박막을 이온빔 스퍼터링 증착법으로 glass/Ta(5.8 nm)/NiFe(5 nm)/Cu(t nm)/NiFe(3 nm)/FeMn(12 nm)/Ta(5.8 nm)의 구조를 갖도록 증착하였다. 비자성체 Cu의 두께가 3.0 nm에서 2.2 nm까지 얇아질수록 교환결합력은 증가하였으며 자기저항비는 다소 낮았다. 비자성체의 두께가 얇으면 반강자성체의 층간 교환작용이 강자성체의 고정층 뿐만 아니라 자유층의 스핀배열에도 영향을 주고 있음을 확인할 수 있었다. 또한 리소그래피 공정 과정을 거쳐 GMR-SV 소자를 제작하여 미트론 자기비드를 검출하였다. 여기서 자기비드를 떨어뜨리기 전과 후의 자기저항비, 교환결합력, 보자력은 각각 0.9%, 3 Oe, 2 Oe의 값을 나타내었다. 이것으로 미크론단위의 바이오센서로서 활용할 수 있는 가능성을 보여주었다.
A spin valve structure of Ta/NiFe/CoFe/Cu/CoFe/Ru/CoFe/FeMn/Ta which has a synthetic antiferromagnet (CoFe/Ru/CoFe), was fabricated by using a magnetron sputtering system. The thickness and composition of magnetic free and pinned layers affect the magnetic properties such as exchange interaction strength of each layer and so on. Even though Rutherford Backscattering Spectrometry (RBS) has advantages of quantitative and non-destructive analysis, it is almost impossible to determine the thickness and composition of magnetic thin films using lBS because of its poor mass resolution for a higher atom number (Z>20). In this study, quantitative analysis of the element composition and thickness for the spin valve sample was performed by combining both Proton Induced X-ray Emission Spectrometry (PIXE), which is one of element specific analysis techniques, and grazing-exit RBS with a highly improved depth resolution and absolute quantitative analysis. For the quantitative analysis, standardization of PIXE was carried out with NiFe, CoFe, and FeMn layers, which are one of constituent layers of spin valve films. Through PIXE standardization and the aid of PHE experimental results of the spin valve sample, ire overlapped signal in a grazing-exit RBS spectrum were successfully resolved and the thickness of the Ru layer was determined with a resolution of ∼1 .
Proceedings of the Korean Society of Precision Engineering Conference
/
2003.06a
/
pp.979-982
/
2003
In this study, because of change in electromagnetic force, deformation of the free surface motion of a magnetic fluid is changed. Deformation of the free surface motion of a magnetic fluid for the change in electromagnetic force is discussed and carried out theoretically and experimentally on the basis of Rosensweig Ferrohydrodynamic Bernoulli Equation. Objective of this study explicates free surface motion by electromagnetic force and planes to designed controller. To control free surface of magnetic fluid, it embody designed two-dimensional free surface form of magnetic fluid. By using this characteristics, they applied to oscillator for surface control, flow control, boundary layer control. Strength of magnetic field and height of free surface of magnetic fluid measure as a hall-effect sensor. As performing height control of magnetic fluid, the result will be presented possibility of free surface deformation control.
Proceedings of the Korean Magnestics Society Conference
/
2002.12a
/
pp.164-165
/
2002
기록저장 장치의 고 기록밀도에 따라서 급성장을 하고 있는 자기 기록매체에 대하여 자장 센서의 크기의 감소는 외부 누설자계의 영향으로 많은 노이즈와 함께 안정한 스핀 작동을 구현할 수 없게 된다. 이를 해결하기 위해 반강자성적 결합을 하고 있는 합성형 반강자성적 다층막을 고정층에 삽입하여 고정층과 자유층간의 정자기적 영향을 억제하는 방법과 함께 높은 GMR비를 얻음으로서 노이즈보다 높은 신호출력을 얻는 방법이 있다. (중략)
Kim, K.Y.;Shin, K.H.;Kim, H.J.;Jang, S.H.;Kang, T.
Journal of the Korean Magnetics Society
/
v.10
no.5
/
pp.203-209
/
2000
Top synthetic spin valves with structure Ta/NiFe/CoFe/Cu/CoFe(P 1)/Ru/CoFe(P2)/FeMn/Ta on Si (100) substrate with natural oxide were prepared by dc magnetron sputtering system. We have changed only the thickness in free layers and the thickness difference (Pl-P2) in two ferromagnetic layers separated by Ru, and investigated the effect of magnetic film thickness on interlayer coupling field in spin valve with synthetic antiferromagnet. According to the decrease of free layer thickness, interlayer coupling field was increased due to the magnetostatic coupling(orange peel coupling). In case of t$\_$P1/>t$\^$P2/, interlayer coupling field agreed well with the modified Neel model suggested in conventional spin valve structures by Kools et al. However, in case of t$\_$P1/>t$\^$P2/, it was found that the interlayer coupling field was not explained by the Modified Neel Model and was confirmed the necessity of further remodeling. The dependence of Cu thickness on the interlayer coupling field was investigated and 10 Oe of interlayer coupling field was obtained when the Cu thickness is 32 $\AA$.
To obtain low switching field ($H_{SW}$) we introduced amorphous ferromagnetic $Co_{70.5}Fe_{4,5}Si_{15}B_{10}$ single and synthetic antiferromagnet (SAF) free layers in magnetic tunnel junctions (MTJs). The switching characteristics for MTJs with structures $Si/SiO_2/Ta$ 45/Ru 9.5/IrMn 10/CoFe 7/AlOx/CoFeSiB 7 or CoFeSiB (t)/Ru 1.0/CoFeSiB (7-t)/Ru 60 (in nm) were investigated and compared to MTJs with $Co_{75}Fe_{25}$ and $Ni_{80}Fe_{20}$ free layers. CoFeSiB showed a lower saturation magnetization of $560 emu/cm^3$ and a higher anisotropy constant of $2800\;erg/cm^3$ than CoFe and NiFe, respectively. An exchange coupling energy ($J_{ex}$) of $-0.003erg/cm^2$ was observed by inserting a 1.0 nm Ru layer in between CoFeSiB layers. In the CoFeSiB single and SAF free layer MTJs, it was frond that the size dependence of the $H_{SW}$ originated from the lower $J_{ex}$ experimentally and by micromagnetic simulation based on the Landau-Lisfschitz-Gilbert equation. The CoFeSiB SAF structures showed lower $H_{SW}$ than that of NiFe, CoFe and CoFeSiB single structures. The CoFeSiB SAF structures were proved to be beneficial far the switching characteristics such as reducing the coercivity and increasing the sensitivity in micrometer to submicrometer-sized elements.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.