• 제목/요약/키워드: 자성 재료

검색결과 397건 처리시간 0.024초

등방성 Sr-페라이트 과립을 이용한 새로운 자성도자기 소지 (New Magnetic Porcelain Mmaterials using Isotropic Sr-ferrite Granules)

  • 조태식;정지욱
    • 한국전기전자재료학회논문지
    • /
    • 제17권8호
    • /
    • pp.882-887
    • /
    • 2004
  • The new magnetic porcelain materials have been studied by mixing magnetic St-ferrite powders with traditional porcelain materials before forming process. For the maintenance of magnetic characteristics after glaze firing process, the Sr-ferrite grains with the size of 1∼2 ${\mu}{\textrm}{m}$ were agglomerated as the isotropic granules with the size of 0.5∼2 mm. The high characteristics of magnetic porcelain materials were achieved at the following conditions; isotropic Sr-ferrite granules of 30 wt%, granule size of 1.4∼2 mm, and glaze firing temperature of $1250^{\circ}C$ in air The magnetic porcelain materials indicated the high magnetic properties, such as the remanent flux density of 240 G, the intrinsic coercivity of 3910 Oe, and the surface flux density of 178 G. The extraction properties of the magnetic tea cups were high compared to that of the traditional tea cups.

천연산 석영 분말의 자성처리 특성 (Characteristics on Magnetism Treatment of Quartz Powder)

  • 소대화;조용준;소현준;정종현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.1241-1244
    • /
    • 2003
  • The materials showing high structure dispersity are developed on the natural quartz base and they are obtained by mechano-chemical technology. Depending on the processing conditions and subsequent applications the materials produced by mechano-chemical reaction (MCR) show concurrently magnetic, dielectric and electrical properties. The obtained magnetic-electrical powders classified by aggregate complex of their features as segnetomagnetics, contain a dielectric material as a carrying nucleus, particularly the quartz on that surface one or more layers of different compounds are synthesized having thickness up to $10{\sim}50nm$ and showing magnetic, electrical and other properties.

  • PDF

반자장계수를 고려한 자성분말의 초투자율 측정에 관한 연구 (A Study on measuring the Initial Permeability of Magnetic Powder considered Demagnetizing factors)

  • 전홍배;허진;김철한;사공건
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 영호남학술대회 논문집
    • /
    • pp.86-90
    • /
    • 2000
  • In this study, A equipment for measuring the initial permeability of soft-ferrite powder was developed by using a differential transformer coil, and was investigated demagnetizing factors. To measure the initial permeability of magnetic ceramic powder is cumbersome since there are not any measuring equipment and method. Magnetic powder is currently used for a magnetic fluid and microwave absorber materials, and the initial permeability of the magnetic powder is very important to be evaluated a powder for some applications.

  • PDF

Cr underlayer가 Sputter 증착한 CoNiCr/Cr, CoCrTa/Cr longitudinal 자기기록매채의 미세구조와 자성특성에 미치는 영향 (Effects of Cr Underlayer on Microstructural and Magnetic Properties of Sputtered CoNiCr/Cr, CoCrTa/Cr Films)

  • 박성찬;안병태;임호빈
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1992년도 추계학술대회 논문집
    • /
    • pp.7-10
    • /
    • 1992
  • CoNiCr/Cr and CoCrTa/Cr for longitudinal magnetic recording media were. prepared on Coming 7059 glass by RF magnetron sputtering. The thickness of Cr underlayer was varied from 500 to $3000{\AA}$ and. that of magnetic layer was $700{\AA}$. Coercivity and squareness were measured using V.S.M.(vibrating sample magnetometer). The coercivity of films increased with increasing Cr thickness when the films were unannealed. The coercivity of the films annealed in a 10 mtorr vacuum increased initially with annealing time and then saturated with further increase in annealing time. The coercivity value difference between the unannealed and annealed films increased with increasing the thickness of Cr underlayer No significant change was found in squareness after anneal, regardless of Cr underlayer thickness.

  • PDF

LPE 성장법으로 성장시킨 La을 첨가한 YIG 막의 자성특성 (Magnetic Properties of La-doped YIG Films Prepared by LPE(Liquid Phase Epitaxy))

  • 김동영;한진우;김명수;이상석
    • 한국전기전자재료학회논문지
    • /
    • 제14권3호
    • /
    • pp.257-262
    • /
    • 2001
  • Single crystalline films of La doped YIG(yttrium iron garnet) were grown by the liquid phase epitaxy. The lattice constants of films obtained by DCD(double crystalline diffractometer) measurement increased with increasing La contents in films. In particular, lattice constants of films grown wiht Y/La=20 solution were nearly same as those of GGG (gadolinium gallium garnet) substrate. The saturation magnetization measured with VSM (vibrating sample magnetometer) was about 1750Gauss which is the same as that of pure YIG irrespective of La contents in films. FMR(ferromagnetic resonance) linewidth of La doped YIG was smaller than that of pure YIG. Since appropriate La doping decreases the lattice mismatch between film and substrate, the FMR linewidth was Y/La=20 in this experiment.

  • PDF

아몰퍼스 자성박막의 센싱기능에 관한 연구 (Study on the Sensing Function in Amorphous Magnetic Thin Films)

  • 김남규;진성빈;신용진;임재근;서강수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1996년도 춘계학술대회 논문집
    • /
    • pp.27-30
    • /
    • 1996
  • In this paper, we prove through the experiments the possibility that Co-amorphous magnetic films can be used as high sensibility materials. We fabricate amorphous film of Fe$\sub$4.7/Co$\sub$74.3/Si$_2$B$\sub$19/ by using sputtering method at high frequency. Then, we not only measure the magnetic Properties of the annealed samples, but also observe the magnetic domain by using an Kerr effect optical-microscope. As the result, we find that the samples have high sensibility

  • PDF

자성도자기의 특성 향상 연구 (Enhancement of magnetic characteristics of porcelain materials)

  • 조태식;정지욱;김효석
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.1
    • /
    • pp.537-540
    • /
    • 2003
  • This study was investigated to fabricate the porcelain materials with high magnetic characteristics. The high characteristics of the magnetic porcelain materials were achieved at the following conditions; powder sizes of isotropic Sr-ferrites with $1{\sim}2\;mm$ and magnetic powder infraction of 30 wt%. The magnetic tea cups with 3-mm-thick at the optimum conditions indicated the high magnetic characteristics such as the surface flux density of 178 G, the remanent flux density of 240 G, and the intrinsic coercivity of 3910 Oe.

  • PDF

잔류 자성원소 검출에 의한 금속간화합물의 기계적 합금화 공정에서의 합금화 정도 해석 (Determination of the Degree of Alloying by Detection of Residual Ferromagnetic Elements for Intermetallic Alloys Processed by Mechanical Alloying)

  • 어순철
    • 한국재료학회지
    • /
    • 제13권9호
    • /
    • pp.561-566
    • /
    • 2003
  • Mechanical alloying(MA) process using elemental powders followed by hot pressing has been applied to some intermetallic alloy system containing ferromagnetic elements, such as NiAl and $FeSi_2$. A modified thermogravimetric analysis (TGA) technique was used to investigate the degree of alloying in milled powders and hot consolidated specimens as well as heat-treated bulk specimens. It is shown that the measurement of Curie temperatures in MA intermetallic powders and consolidated specimens containing ferromagnetic components, when determined as a function of milling and heat treatment parameters, can give some insight into the progress and mechanism of alloying.

(Fe1-xCox)89Zr11 비정질 자성막에서의 자기표면탄성파 속도변화(II) (Velocity Change of Magneto Surface Acoustic Wave (MSAW) in (Fe1-xCox)89Zr11 Amorphous Films (II))

  • 김상원
    • 한국재료학회지
    • /
    • 제12권4호
    • /
    • pp.279-282
    • /
    • 2002
  • The effect of field annealing on the velocity changes of magneto surface acoustic wave (MSAW) devices has been investigated for deposited $(Fe_{1-x}Co_x)_{89}Zr_{11}$ (x = 0~1.0) amorphous films. By means of two step field annealing at $195^{\circ}C$ for 10 minute in the magnetic field of 130 Oe, the MSAW device with x=0.4 film among the devices showed the superior velocity change of 0.1 %. This gigantic value was obtained in the DC bias field of 40 Oe at the exciting frequency of 8.7 MHz. It was confirmed that such behavior was due to the variation of differential permeability caused by an optimal stress within the magnetic film.

Mn-Zn-Fe-O 금속타깃을 이용한 수직자기기록디스크의 하지연자성층용 Mn-Zn ferrite 박막제작 (Preparation for Mn-Zn Ferrite Soft Magnetic Underlayer Perpendicular Magnetic Recording Disk using Mn-Zn-Fe-O Metal Target)

  • 공석현;김경환
    • 한국전기전자재료학회논문지
    • /
    • 제19권9호
    • /
    • pp.883-887
    • /
    • 2006
  • In order to attain high-rate deposition of Mn-Zn ferrite thin film for soft magnetic underlayer in perpendicular magnetic recording media, a reactive sputtering using powder-metal targets under the mixture gas of Ar and $O_{2}$ was performed. It was succeeded that Mn-Zn ferrite films with (111) crystal orientation were deposited on Pt(111) underlayer without any annealing process. The film revealed 3.4 kG of 4 ${\pi}Ms$, 70 Oe of coercivity. The deposition rate of the new method was 16 times as high as that of the conventional method using ferrite target.