• Title/Summary/Keyword: 임시 수복재 및 충전재

Search Result 3, Processing Time 0.017 seconds

Effect of Provisional Restorative and Filling Materials on Bond Strength of Adhesive Resin Cement between Lithium Disilicate Glass-Ceramic and Dentin (Lithium Disilicate Glass-ceramic과 상아질 간의 접착성 레진 시멘트의 결합강도에 대한 임시 수복재와 임시 충전재의 영향)

  • Oh, Sang-Chun;Sim, Hun-Bo
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.29 no.4
    • /
    • pp.359-365
    • /
    • 2013
  • The aim of this study was to evaluate the effect of temporary restorative and filling material on bonding strength between lithium disilicate glass-ceramic and dentin. 60 extracted human molars were cross-sectioned at occlusal third and were embedded into self-cure acrylic resin. Then the teeth were randomly divided into four groups of 15 each. Lithium disilicate glass-ceramic is cemented to dentin as follows: after no any application of the provisional materials (Group A), after application of ALIKETM (GC America Inc.)(Group B), after application of Luxatemp$^{(R)}$ Automix plus (DMG, Germany)(Group C), after application of Fermit$^{(R)}$ (Ivoclar Vivadent, Leichtenstein)(Group D). After the specimens were stored in distilled water for 24 hours, the shear bond strength of the specimens were measured using UTM (Zwick 1456 41, Zwick, Germany) at a crosshead speed of 1mm/min. The data were analysed by one-way ANOVA and Tukey HSD tests. There were no statistically significant differences of bond strength among the groups. Fracture type was showed mixed type of adhesive and cohesive fracture in most of specimens. Within the limitation of this study, bond strength of adhesive resin cement between lithium disilicate glass-ceramic and dentin was not affected by provisional restorative and filling materials.

An Experimental Study on Microleakage in Light-activated Temporary Filling Materials (광중합형 임시충전재의 미세누출에 관한 실험연구)

  • Hwang, Su-Hyun;Yu, Ji-Su;Kim, Sun-Ju
    • Journal of dental hygiene science
    • /
    • v.11 no.4
    • /
    • pp.333-337
    • /
    • 2011
  • The purpose of this experiment was to examine possibility of microleakage by water, temperature change, and bite force inside the mouth during the period of using light-activated temporary filling materials. 2 kinds of light-activated temporary filling materials were used in order to measure weight and compressive strength and to evaluate microleakage between filling material and cavity wall according to frequency of thermal circulation. First, Light-activated temporary filling material was increased the weight, which was measured according to the period of using. As for the result of comparing between products, the weight of Quicks was indicated to be higher. Second, Compressive strength of Spacer had significant difference depending on period of using. However, significant difference wasn't shown in the compressive strength of Quicks. In Spacer that showed significant difference, the compressive strength increased greatly in the difference of 3 days. Third. As for micro-leakage according to frequency of thermal circulation, the microleakage was indicated to be the highest in the group that carried out 7,000 times. The group with operation of 1,000 times and the group with operation of 3,000 times were indicated the statistically lower micro-leakage than the group with operation of 7,000 times. This study brought about a rise in micro-leakage depending on the passage in the period of using. However, it is obvious fact that micro-leakage increases according to the passage of time after restoration.

Influence of air abrasion and different dentin sealing techniques on microtensile bond strength to dentin (상아질의 봉쇄 시기와 표면처리 방법이 미세인장 결합강도에 미치는 영향)

  • Kang, Dong-Ho;Han, Chong-Hyun;Park, Jung-Won;Kim, Sun-Jai
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.1
    • /
    • pp.8-15
    • /
    • 2010
  • Purpose: The purpose of this study was to evaluate the effect of various methods of dentin bonding agent application and air abrasion pretreatment on microtensile bond strength between dentin and resin, using a self-etching adhesive system. Material and methods: Thirty freshly extracted human molars were obtained and divided into 6 groups of 5 teeth. A 2-step self etching adhesive system (Clearfil SE Bond) was used for all groups. The control specimens were prepared using a direct immediate bonding technique. The delayed dentin sealing specimens were prepared using an indirect approach without dentin prebonding. The immediate dentin sealing specimens were prepared using dentin prebonding immediately following preparation. Immediate dentin sealing teeth and delayed dentin sealing teeth had provisional restorations using Fermit for two weeks. Then all specimens of each group were divided into two groups of three, depending on air abrasion pretreatment. Composite "crowns" were incrementally built on and specimens were stored in water for 24 hours. All teeth were prepared for a microtensile bond strength test. Bond strength data were analyzed with a one-way ANOVA test, and post hoc comparison was done using the Scheffe's test. Results: The mean microtensile bond strengths of all groups were not statistically different from each other. Conclusion: When preparing teeth for indirect restorations, IDS and DDS with Clearfil SE bond, have no difference on the microtensile bond strength between dentin and resin. Air abrasion pretreatment did not affect the microtensile bond strength when using IDS and DDS with Clearfil SE bond.