마그네슘 합금은 낮은 비중의 경량화 금속 소재이며, 주로 주조 주조재 형태로 상당한 기간 활용되어 왔으며, 최근에는 포스코에서 AZ31 합금으로 판재를 생산하면서 판재상의 마그네슘 소재의 응용이 본격화되고 있다. AZ31 마그네슘 합금 판재는 경량화가 요구되는 분야에 사용되는 것을 목표로 설계되어 상업화가 추진되고 있으며, 이의 적용을 위해서는 마그네슘 판재의 내부식성을 제어하는 표면처리 공정이 필수적이다. 마그네슘 판재를 이용하여 자동차 부품을 가공하는 경우 부품의 표면처리는 전착도장 공정 안정성 및 내구성 확보가 필수적이며, 기존의 완성차 업체에서 사용하는 전착도장 공정을 포함하여야 한다. 본 발표에서는, 판재를 이용하여 가공되는 자동차 부품의 경우 설계상 필요에 의하여 요구되는 표면처리 공정 이슈와 함께, 특히 설계에서 요구되는 이종금속을 포함하는 표면처리에 관하여 논하고자 한다.
This paper describes weldability of dissimilar metal plates with YAG laser for the use of a small-size electronic spring parts. Effects of welding conditions, combination of plates, thickness of upper plate are examined in relation to welding strength and microstructure of welded region. The obtained results are summarized as follows. Welding defects such as cavity and crack showed a tendency to easily occur in the case where 1) pulse duration is short, 2) laser power is high, 3) PBS plate with high thermal diffusivity is used for lower plate. Among these defects, the occurrence of cavity cased a drop of welding strength. This results from the reduction of welding area between upper and lower plates. In SK-5/SUS304 plates (thickness: 0.2/0.4mm/, welding strength was the highest in welding conditions: laser power is 30J/pulse, pulse duration 9ms, amount of defocus +2mm.
폭발용접은 화약의 폭발에 의한 충격 에너지를 이용하여 금속을 접합시키는 방법으로서 화약의 폭발에 의해 생기는 순간적인 높은 에너지를 이용하는 접합법이다. 1944년에 처음으로 폭발용접의 기술적, 상업적인 이점으로 인해 수요가 증가하고 있는 실정이다. 적용 예는 거대한 판재의 cladding을 포함하여 cladding nozzle, tube 와 tubeplate의 접합, pipe와 pipe의 접합등에 사용되고 있다. 종래의 용접법으로는 용접이 곤란하거나 불가능한 것으로 생각되었던 이종금속에 대해서는 적용이 가능하 고, 용접에 의한 열영향을 받지 않으며 용접 속도가 대단히 빠르다는 잇점이 있다. 또한 용접의 차이가 커서 접합이 곤란한 금속을 폭발용접하면 이음부는 충분한 강도를 가지면서 용이하게 접합할 수 있는 것이 큰 특징이다. 대부분의 금속은 폭발용접이 가능하지만 폭발의 충격에 의해서 균열이 발생되기 쉽고 주철과 같이 취약한 금속 및 Mg을 함유한 알루미늄 합금(순 알루미늄과는 접합 가능함)등은 이 용접법을 사용하기 는 곤란하다. 시공상의 특징으로는 특별한 기계 장치가 필요하지 않고 모재가 판재 혹은 파이프상이면 모재 두께에 제한 받지 않고, 어떠한 형태와도 가능하기 때문에 다품종, 소량생산이 가능하다. 한편 접합시에 화약을 사용하기 때문에 취급에 있어서 주의를 요하고 큰 폭발음 때문에 용접장소의 제한을 받는다는 것이다.
Journal of the Korean Society of Manufacturing Process Engineers
/
v.21
no.8
/
pp.99-109
/
2022
In this study, an electric resistance-heated surface friction spot-welding process was proposed and tested for the spot-welding ability of copper and aluminum dissimilar metal sheets using electric resistance heating and surface friction heating. This process has welding variables, such as the current value, energizing cycles, rotational speed, and friction time. The current value and energizing cycle can affect the resistance heat, and the rotational speed of the rotating pin and friction time influence frictional heat generation. Resistance heating before friction heating has a preheating effect on the Cu-Al contact interface and a positive effect on preventing friction heat loss during the friction stage. However, because resistance preheating can soften the copper sheet and affect the contact stress and friction coefficient, it has difficulties that may adversely affect frictional heat generation. Therefore, the optimal combination of welding variables should be determined through simulations and experiments of the spot-welding process to determine the effects of electric resistance preheating on the suggested process. Through this procedure, it is known that the proposed spot-welding process can improve the welding quality during the spot welding of Cu-Al sheets.
Journal of the Korea Academia-Industrial cooperation Society
/
v.7
no.3
/
pp.506-511
/
2006
Silver is one of the most appropriate Jewelry materials for Jewelry casting and bench working. The technique known as 'Mokumegane' is good for making silver jewelry with natural patterns, such as wood grain patterns, but the process is not easy for silversmithing because it requires complicated and heavy labour. Instead of using conventional Mokumegane technique, we propose a new modified silver-copper casting process that enables a similar surface effect with good metal bonding strength between silver and copper. Simply pouring the molten silver into pre-aligned copper granules or 0.5 mm to 1.5 mm-thick copper sheets leads to well embedded copper silver ingots. The rolled silver plates from those ingots show excellent bonding interface even after the silver plate rolled ten times. We successfully fabricated prototype rings with copper embedded silver plates. Our result implies that our newly proposed process nay be a simpler way to fabricate silver jewelry with a pseudo-Mokumegane effect.
Journal of the Computational Structural Engineering Institute of Korea
/
v.32
no.1
/
pp.1-5
/
2019
In this paper, the experimental study and finite elements analysis were conducted on homogeneous and dissimilar metals single lap-shear bonded joints to investigate the factor that affect the joint failure load. It was found that factors which have the significant effects on the failure load of the joint was stiffness of the adherends. And from experimental results, it can be confirmed that the failure load increases linearly with overlap length increases. And the failure load of dissimilar metal joints is approximately 1KN(10~17%) larger than homogeneous metal joints. In order to confirm this phenomenon, the stress distribution and strain distribution of the specimens were analyzed through the finite element analysis. The difference between homogeneous metals joints and dissimilar metals joints is that stress and strain in adhesive are concentrated at the end of the overlap zone close to aluminium which has lower rigidity than aluminium in case of dissimilar metals joints. From high rigidity of steel, the stress concentration in bonds are decreased and it cause increase of the failure strength at dissimilar metal joints.
Fabrication of a complex aluminum alloy by the ARB process using dissimilar aluminum alloys has been carried out. Two-layer stack ARB was performed for up to six cycles at ambient temperature without a lubricant according to the conventional procedure. Dissimilar aluminum sheets of AA1050 and AA5052 with thickness of 1 mm were degreased and wire-brushed for the ARB process. The sheets were then stacked together and rolled to 50% reduction such that the thickness became 1 mm again. The sheet was then cut into two pieces of identical length and the same procedure was repeated for up to six cycles. A sound complex aluminum alloy sheet was successfully fabricated by the ARB process. The tensile strength increased as the number of ARB cycles was increased, reaching 298 MPa after 5 cycles, which is about 2.2 times that of the initial material. The average grain size was $24{\mu}m$ after 1 cycle, and became $1.8{\mu}m$ after 6 cycles.
Transactions of the Korean Society of Mechanical Engineers A
/
v.33
no.4
/
pp.401-408
/
2009
This study is performed to check the three dimensional characteristics of residual stress in the dissimilar metal weld. Although two dimensional analysis has been widely used for the assessment of weld residual stress, it has limitations to understand the stress distribution of the third direction. 3-D analysis was done to understand residual stress distribution of the welded plate. A simple butt-welded plate was considered to show the stress variation on all direction. A mock-up plate weldment was fabricated with SA-508 and F316L, which are widely used in nuclear power plants. The analysis results were validated with the measured values in the mock-up.
Proceedings of the Korean Institute of Surface Engineering Conference
/
2009.05a
/
pp.104-104
/
2009
최근 국내외 휴대용 IT 관련 산업에서는 제품의 소형화에 경량화에 따른 기술 개발과 더불어 다양한 색상의 구현을 위한 연구가 활발히 진행되고 있다. 휴대용 전자 부품에 있어서 PVD 코팅은 고경도 박막을 금속 판재 및 플라스틱 기판 상에 증착하여 표면경도를 증대시켜 내구성 향상에 활용되고 있으며, 질화물 계열을 통하여 Yellow, Blue, Black, Red계 등의 색상 구현이 가능하여 현재 가장 큰 구매력의 원천으로 평가되고 있는 제품 디자인 분야에 응용이 되고 있다. 본 연구에서는 아크이온 플레이팅법과 스퍼터링법을 이용하여 고경질, 고내식 표면층 형성방법 및 다양한 칼라를 구현하는 방법에대한 연구를 수행하였다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.