마찰교반접합한 알루미늄 합금과 스테인리스 강 이종접합부 계면 조직 및 접합부 강도 (Interface Analysis and Mechanical Properties of Friction Stir Welded Dissimilar joints between Stainless steel and AI alloy)

  • 이원배;이창용;연윤모;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.189-191
    • /
    • 2005
  • Dissimilar joining of AI 6013-T4 alloys and austenite stainless steel was carried out using friction stir welding technique. Microstructures near the weld zone and mechanical properties of the joint have been investigated. Microstructures in the stainless steel side and AI alloy were depended on the thermo-mechanical condition which they received. TEM micrographs revealed that the interface region was composed of the mixed layers of elongated stainless steel and ultra-fine grained AI alloy and intermetallic compound layer which was identified as the $Al_{4}Fe$ with hexagonal close packed structure. Mechanical properties were lower than those of 6013 AI alloy base metal, because tool inserting location was deviated to AI alloy from the butt line, which resulted in the lack of the stirring.

  • PDF

차량 밸브용 내열강재 이종 마찰용접부의 피로특성 평가 (An Evaluation of Fatigue Properties on Dissimilar Friction Weld of Heat-Resisting Steels Used in Vehicle Valves)

  • 이동길;이상열;정재강
    • 한국자동차공학회논문집
    • /
    • 제10권2호
    • /
    • pp.186-192
    • /
    • 2002
  • The fatigue crack propagation characteristics were investigated on dissimilar friction weld of two kind of heat-resisting steels (STR3 and STR35) commonly used in valve materials for vehicles. A small circular artificial defect was machined to induce fatigue crack at bonded line, heat affected zone and base metal of the weld on the surface of the specimens. From the results of the experiment, the fatigue limits of the materials STR3 and STR35 were obtained to be 429.0MPa and 409.4MPa respectably. The STR35 base metal and 1.0mm HAZ specimens showed 190% and 82% higher fatigue life than STR3 base metal. And the fatigue life of 1.0mm HAZ specimen was shown 99% on STR3 and 29% on STR35 higher than that of their base metal. But the fatigue life of weld interface specimen was shown 18% on STR3 and 72% on STR35 lower than that of their base metal because of the weld interface separation.

탄소강-스테인리스강 용접부의 피로균열진전 특성에 관한 연구 (A Study on the Fatigue Crack Growth Characteristics for the Weldment of Carbon steel-Stainless steel)

  • 권재도;김우현;김길수;박중철;배용탁;김중형
    • Journal of Welding and Joining
    • /
    • 제16권4호
    • /
    • pp.47-54
    • /
    • 1998
  • Various equipments in plants are welded with two different materials and it is required to investigate the effects of fatigue crack propagation on the neighborhood of a welded portion. The characteristics of fatigue crack growth in the base metal of carbon and stainless steel, in the carbon and stainless steel sides located in the neighborhood of welded portion (carbon/stainless steel), respectively and welded portion, are investigated. The results show that the crack growth in the welded portion (carbon/stainless steel) is an average value of the crack growths in the carbon and stainless steel respectively located in the neighborhood of the welded portion. It is found that the crack growth in the welded portion is not significantly different from those in the carbon and stainless steel sides. Hence it can be concluded that the structure welded with two different materials wold not impede the integrity based on the fatigue crack growth.

  • PDF

이종마찰용접 강봉재의 기계적특성과 비파괴 평가 (The Mechanical Properties and the Nondestructive Evaluation of Dissimilar Friction Welded Steel Bars)

  • 정원택;공유식;김선진
    • 동력기계공학회지
    • /
    • 제10권1호
    • /
    • pp.77-82
    • /
    • 2006
  • In this study, dissimilar friction welding were produced using 15mm diameter solid bar in chrome molybedenum steel(SCM440) to carbon steel(S45C) to investigate their mechanical properties and the relationship between the weld parameters and the nondestructive coefficients, such as AE counts and ultrasonic attenuation coefficient. The main friction welding parameters were selected to endure good quality welds on the basis of visual examination, tensile tests, Vickers hardness surveys of the bond of area and heat affected zone. The specimens were tested as-welded and post weld heat treated(PWHT). The tensile strength of the friction welded steel bars was increased up to 100% of the S45C base metal under the condition of all heating time. The ductility of PWHT specimens is higher than as-welded.

  • PDF

이종 마찰용접 강봉재의 후열처리에 따른 기계적 특성 (Mechanical Properties of Dissimilar Friction Welded Steel Bars in Relation to Post Weld Heat Treatment)

  • 공유식;김선진
    • 대한기계학회논문집A
    • /
    • 제30권4호
    • /
    • pp.402-408
    • /
    • 2006
  • Dissimilar friction welding were produced using 15(mm) diameter solid bar in chrome molybedenum steel(KS SCM440) to carbon steel(KS S45C) to investigate their mechanical properties. The main friction welding parameters were selected to endure good quality welds on the basis of visual examination, tensile tests, Vickers hardness surveys of the bond of area and H.A.Z and microstructure investigations. The specimens were tested as-welded and post-weld heat treated(PWHT). The tensile strength of the friction welded steel bars was increased up to 100% of the S45C base metal under the condition of all heating time. Optimal welding conditions were n=2,000(rpm), $P_1=60(MPa),\;P_2=100(MPa),\;t_1=4(s),\;t_2=5(s)$ when the total upset length is 5.4 and 5.7(mm), respectively. The peak of hardness distribution of the friction welded joints can be eliminated by PWHT. Two different kinds of materials are strongly mixed to show a well-combined structure of macro-particles without any molten material and particle growth or any defects.

레일강의 균열발생·천이 및 피로균열진전거동 (Behavior of the Crack Initiation, Transition and Fatigue Crack Growth of Rail Steel)

  • 이종선;강기원;최린;김정규
    • 한국강구조학회 논문집
    • /
    • 제11권1호통권38호
    • /
    • pp.33-42
    • /
    • 1999
  • 궤도용 차량의 안전성 확보를 위한 연구의 일환으로서 레일강의 균열 발생 조건과 모재와 용접부에 대한 정적파괴거동 및 단일모드 하중하의 피로균열진전거동을 검토하였다. 레일에서 횡방향 균열의 원점은 표면하층균열이며 이는 최대전단응력에 의해 발생하였다. 또한 표면하층균열의 크기가 증가함에 따라 균열의 진전은 전단모드에서 혼합모드로 천이될 가능성이 증가하였다. 용접부의 평면변형률 파괴인성은 조직의 조대화와 경도의 상승으로 인하여 모재에 비하여 약 10% 저하하였다. 용접부의 제 2단계 영역의 피로 균열진전속도는 낮은 ${\Delta}K$ 영역에서 모재에 비하여 저하하였으나 높은 ${\Delta}K$영역에서는 이의 차이가 소멸되었으며 이러한 경향은 R=0.1의 낮은 응력비에서 현저하였다. 이는 용접부의 미시조직이 모재에 비하여 성장하였기 때문이라고 판단된다.

  • PDF

FCAW 이종접합에서 용접자세에 따른 기계적 시험 특성 평가 (Evaluation of Mechanical Test Characteristics according to Welding Position in FCAW Heterojunction)

  • 조병준;이성준
    • 한국산학기술학회논문지
    • /
    • 제20권8호
    • /
    • pp.649-656
    • /
    • 2019
  • 조선소, 교량 구조물, 건설기계, 플랜트 산업 등 다양한 분야에서 폭 넓게 활용되고 있는 이산화탄소 아크용접(FCAW: Flux Cored Arc Welding)은 피복 아크 용접(SMAW: Shielded Metal Arc Welding)의 단점을 보완하기 위한 대안으로 1950년대 초 개발되었다. FCAW는 모든 자세에서 용접이 가능하고 작업여건 변수가 많은 현장에서 우수한 품질을 얻을 수 있는 장점이 있어 탄소강과 합금강의 중판, 후판 용접에 많이 사용되고 있다. 본 연구에서는 FCAW를 이용하여 SS400(일반구조용 압연강재)와 SM490A(용접구조용 압연강재)를 이종용접한 후 용접부의 기계적 특성(인장시험, 굽힘시험, 경도시험, 충격시험, 매크로시험)을 분석하고 다음과 같은 결론을 도출하였다. 인장시험 결과, 모든 용접자세에서 KS 규격 인장강도 범위($400{\sim}510N/mm^2$)를 만족하였다. 굽힘시험 결과, 대부분의 시편에서 굽힘시 표면의 터짐 현상이나 기타 결점이 나타나지 않았고, 소성변형 후에도 충분한 인성을 발휘하는 것을 확인할 수 있었다. 경도시험 결과, 모든 결과 값이 KS B 0893의 규격치 350Hv보다 낮게 나타나 양호한 것으로 판단된다. 충격시험 결과, 모든 결과가 KS 기준 수치인 27J 보다 큰 것으로 나타났다. 매크로시험 결과 용접부의 형상별로 균일한 조직 상태를 나타냈으며, 용접부 전단면에 걸쳐 내부 결함, 기포 또는 불순물 등이 발견되지 않아 라미네이션의 우려가 없는 것으로 나타났다.

레이저 이종용접에서의 입열량 변화에 대한 용접특성 (Welding Characteristics on Heat input Changing of Laser Dissimilar Metals Welding)

  • 모양우;신병헌;신호준;유영태
    • 한국공작기계학회논문집
    • /
    • 제15권2호
    • /
    • pp.51-58
    • /
    • 2006
  • Laser welding of dissimilar metals has been widely used to improve a wear resistance and a corrosion resistance of the industrial parts. The objective of this research works is to investigate the influence of the process parameters, such as the welding for SM45C and STS304 with CW Nd:YAG lasers. The bead-on-plate welding tests are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the dissimilar welding, the welding quality of the cut section, stain-stress behavior and the hardness of the welded part are investigated. From the results of the investigation, it has been shown that the optimal welding condition without defects in the vicinity of the welded area and with a good welding qualify is 1600W of the laser power, 0.85m/min of welding speed and $4{\ell}/min$ of pressure for shielding gas.

레이저 이종용접에서의 입열량 변화에 대한 용접특성 비교 (Comparison of Welding Characteristics on Heat input Changing of Laser Dissimilar Metals Welding)

  • 신호준;유영태;신병헌;안동규
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 추계학술대회 논문집
    • /
    • pp.997-1003
    • /
    • 2005
  • Laser welding of dissimilar metals has been widely used to improve a wear resistance and a corrosion resistance of the industrial parts. The objective of this research works is to investigate the influence of the process parameters, such as the welding for SM45C and STS304 with CW Nd:YAG lasers. The bead-on-plate welding tests are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the dissimilar welding, the welding qualify of the cut section, stain-stress behavior and the hardness of the welded part are investigated. From the results of the investigation, it has been shown that the optimal welding condition without defects in the vicinity of the welded area and with a good welding quality is 1600W of the laser power, 0.85m/min of welding speed and 4m/min of pressure for shielding gas.

  • PDF