• 제목/요약/키워드: 이음매 없는 튜브

검색결과 3건 처리시간 0.017초

대 직경 이음매 없는 Ti-6Al-4V 튜브의 $360^{\circ}$ 냉간 굽힘 ($360^{\circ}$ Cold Bending of Ti-6Al-4V Large-Diameter Seamless Tube)

  • 허선무;박종승
    • 한국군사과학기술학회지
    • /
    • 제3권1호
    • /
    • pp.176-182
    • /
    • 2000
  • $360^{\circ}$ bending of Ti-6Al-4V large-diameter seamless tube(62.37 mm $OD {\times} 4.40mm$ wall thickness) has been achieved at room temperature without heating. The bending process comprised two steps : the first step is $360^{\circ}$ bending by an uniquely designed rotary bender allowing spring back, which is subsequently eliminated by the second or finishing step which comprised repeated bending processes by powered three roll bender, In odor to prevent collapse of tube during bending, Cerro $Tru^{TM}$(Trade name of a non-ferrous low melting point alloy)has been employed as a filler metal. The resultant ovality(out of roundness) obtained was 1.28%, as compared with 6~8% without applying Cerro $Tru^{TM}$.

  • PDF

대 직경 이음매 없는 Ti-6Al-4V 합금 튜브의 $360^{\circ}$ 냉간 굽힘 시 벽두께 감소현상 (The Thinning Phenomena of the Wall Thickness during $360^{\circ}$ Cold Bending of Ti-6Al-4V Large-Diameter Seamless Tube)

  • 허선무;박종승
    • 한국군사과학기술학회지
    • /
    • 제3권1호
    • /
    • pp.231-236
    • /
    • 2000
  • The wall thickness of the Ti-6Al-4V Large-Diameter Seamless Tube, which is supposed to be a very important parameter in a system design, was measured during $360^{\circ}$ cold bending processes. The factors or processes affecting the wall thickness include 1) primary bending, 2)secondary or finishing step of the $360^{\circ}$ bending, 3)cleaning processes in CERO TRUTM(CT)process. But thinning effects of the wall thickness during the cleaning processes are negligible compared to those during the formers. The variations in the percentages of the change in wall thickness were found to be from -14% to +16%.

  • PDF

슬러지 연마입자를 이용한 이음매 없는 스테인리스강 튜브내면의 자기연마 (Magnetic Abrasive Polishing for Internal Face of Seamless Stainless Steel Tube Using Sludge Abrasive Grain)

  • 김희남;윤여권;김상백;최희성
    • 한국자동차공학회논문집
    • /
    • 제12권6호
    • /
    • pp.151-157
    • /
    • 2004
  • In this paper deals with behavior of the magnetic abrasive using sludge on polishing characteristics in a new internal finishing of seamless stainless steel tube applying magnetic abrasive polishing. The magnetic abrasive using sludge-abrasive grain WA and GC used to resin bond fabricated low temperature. And sludge of magnetic abrasive powder fabricated that sludge was crused into 200 mesh. The previous research have made an experiment in the static state the movement of magnetic abrasive grain is nevertheless in the dynamic state. In this paper, We could have investigated into the changes of the movement of magnetic abrasive grain. In reference to this result, we could have made the experiment which is set under the condition of the magnetic flux density, polishing velocity according to the form of magnetic brush.