• Title/Summary/Keyword: 에폭시 섬유

Search Result 316, Processing Time 0.018 seconds

Strain Sensing of Single Lap Shear using Pencil Lead Drawn Paper Sensor (PLDPS) (연필심을 이용한 종이센서에 의한 단일 랩 전단변형률 감지능)

  • Yoo, Ji-Hoon;Shin, Pyeong-Su;Kim, Jong-Hyun;Lee, Sang-Il;Park, Joung-Man
    • Composites Research
    • /
    • v.33 no.4
    • /
    • pp.228-233
    • /
    • 2020
  • In this paper, a single lap shear test was performed using a glass fiber reinforced composite material (GFRC). Pencil lead drawn paper sensor (PLDPS) was applied for single lap shear test being performed. Bisphenol-A epoxy and amine hardener were used as adhesives combining with composite materials. To make a difference in adhesive properties, the adhesive was cured under different conditions. PLDPS was made of a 4B pencil on A4 paper. Because graphite in a pencil was an electrically conductive substance, electric resistance (ER) could be measured. A change in ER was observed by a position where a PLDPS was attached to single lap shear specimens. It was confirmed that the change in ER was different depending on two attached positions and was observed by lap shear strain as well. In case the lap shear strain was large, the change in ER of PLDPS was high. This was because the larger the extension of the adhesive part, the larger the degree of bending of the specimen and thus the larger the distance change between two electrodes.

T800/AD6005계 복합재의 습기투과에 관한 연구

  • 박명규;류백능;최영보
    • Proceedings of the Korean Society of Propulsion Engineers Conference
    • /
    • 1997.11a
    • /
    • pp.35-36
    • /
    • 1997
  • 복합재는 강도가 높고 가볍기 때문에 최근 로켓의 연소관으로 널리 사용되고 있다. 그런데 이 복합재 로켓 연소관은 제조 후 대기 환경에 장기적으로 노출되어 있기 때문에 금속 연소관과는 달리 온도 또는 습도 등의 환경에 대한 영향을 고려해야 한다. 더구나 연소관은 내부에 추진제가 충전되어 있으므로 추진제의 기계적 특성이 습도에 민감함을 생각할 때 강도뿐만 아니라 습기의 투과도 또한 매우 중요한 고려 요소가 된다. 그러나 온/습도 변화에 따른 복합재 자체의 재료 특성 변화에 대한 연구는 많이 보고되었으나 습기의 투과 정도에 관한 연구는 자료가 미흡한 실정이다. 한편, 포화 함수율은 복합재에 따라서 차이가 있으나 T300/5208의 경우 문헌을 참조하면 20-$50^{\circ}C$에서 복합재 무게의 약 1.5% 정도이며 포화에 걸리는 시간은 약 100일 정도로 나타나 있다.본 연구에서는 수분이 복합재를 통하여 투과되는 정도를 고찰하기 위하여 $20^{\circ}C$,95%RH의 온/습도를 유지하는 수조를 제작하였고, 이 수조내에 보관한 복합재 연소관의 실린더 벽면으로 투과되는 습기를 측정하기 위하여 연소관 내에 습도 센서를 투입하여 상대습도를 직접 측정하였다. 복합재 연소관이 로켓에 사용될 때는 연소관 외부에 페인트로 피막 처리하고 연소관 내부에도 추진제와의 사이에 라이너가 접착되어 있어서 수분 침투 및 온도 등의 외부 환경조건에 견디기에 더 양호한 조건이나 본 연구에서는 복합재 자체의 특성을 고찰하기 위하여 섬유를 에폭시에 함침시켜 winding한 상태 그대로의 복합재 연소관 시료를 사용하였다. 습기의 투과는 내부에 라이너/인슐레이션이 피복되거나 또는 추진제가 충전된 경우 많은 감소효과를 보였다. 순수 복합재 연소관의 경우 수조에 넣고 평형에 도달한 후로부터 약 8개월의 습기 투과 상태를 볼대 벽면을 통하여 들어가는 water vapor flux는 $20^{\circ}C$,95%RH 에서 평균적으로 9.3163$\times$$10^{-8}$g/$m^2$sec로 나타났다. 이때 습기가 투과되는 연소관이 국지점을 평판으로 가정하고 Fick's law를 이용하여 구한 습기에 대한 복합재의 확산계수는 D=2.5$\times$$10^{-6}$$mm^2$sec였으며, 이는 다른 graphite/epixy 복합재의 확산계수와 유사한 값을 나타내고 있다. 또한 추진제가 충전된 연소관을 절단하여 밀폐한 후 95%RH 습도 조건에 보관함으로써 연소관 내부의 추진제 기계적 특성에 미치는 침투된 습기의 영향도 함께 고찰하였다. 추진제에 따라 차이는 있겠으나 추진제가 충전된 연소관은 순수 복합재 연소관에 비해 습기의 투과 정도가 작으며, 본 연소관에 충전된 RDX/AP계 추진제의 경우 추진제의 습기투과에 의한 추진제 물성 변화는 미미한 것으로 나타났다.

  • PDF

이산화탄소를 이용한 방사능 오염 세척 기술개발

  • Ko, Moon-Sung;Park, Kwang-Heon;Ryu, Jung-Dong;Kim, Yang-Eun;Lee, Bum;Park, Hyun-Taek
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2000.11a
    • /
    • pp.59-59
    • /
    • 2000
  • 원자력발전소 1차계통과 격납용기 내부에서 사용되는 주요 부품들은 운전중에 발생한 방사 성 물질들의 침투와 홉착에 의해 오염되어 간다. 이 오염된 부품 및 장비, 공구, 방호복, 방호모자, 작업화 등의 세정과 정비를 위해서는 제염이 선행되어야 한다. 현재의 제염법은 2차 방사성 폐기물을 발생하는 문제점이 있다. 따라서I 2차 폐기물의 발생을 근원적으로 줄일 수 있는 새로운 제염방안이 절실히 요구되고 있는 실정이다. 본 논문에서는 이러한 문제점을 해결할 수 있는 제염법을 개발하기 위해 2가지 방법을 적용하였다. 첫째로, 원자력 발전소에 서 나오는 방사능 오염 세탁물 제염을 위한 액체 및 초임계 이산화탄소를 이용한 방사능 오염물 제염기를 개발하였다. 제염기는 반응기(16 liteer), 회수시스템 그리고 저장용기로 구성되어있다. 세정에 사용된 모든 이산화탄소는 회수되어 재사용 되어지므로 2차 폐기물의 발생을 근원적으로 없앨 수 있다. 제염성능실험결과 제염지수가 목표치보다는 낮았다. 이는 제염 기에 계면활성제와 기계적인 힘을 가한다면 높은 제염지수를 얻을 수 있을 것으로 예상된다. 둘째로, 발전소에서 나오는 오염된 공구나 장비의 세척을 위한 가변형 노즐 드라이 아이스 세척 장치를 개발하였다. 표면세정시 얼음층 형성방지를 위하여 열공급장치를 부착하였다. 유라표면에 지문을 묻혀 실험한 결과 쉽게 제거되었다. 실제 발전소에 있는 P Pump-housing의 표면을 실험한 결과 방사능의 약 40-80%가 제거되었다. 이 장치는 검출기, 제어장치, 용액상에서 세척될 수 없는 장치에 적용할 수 있는 효율적인 세척법이다. 이는 프리프레그의 표면처리 가 충과 충간의 접착강도를 증가시키고 또한 탄소섬유와 에폭시 간의 계면력을 증가시킨데 기인하는 것으로 사려된다.되었으며, duty-on 시간의 증가에 따라 $Cr_2N$ 상의 형성이 점점 많아져 80% duty-on 시간 경우에는 거의 CrN과 $Cr_2N$ 상이 공존하는 것으로 나타났다. 또한 duty-on 시간이 증가할수록 회절피크의 세기가 증가하여 결정화가 더 많이 진행되어짐을 알 수 있었다. 마찬가지로 바이어스 펄스이 주파수에 다른 결정성의 변화도 펄스의 주파수가 증가할수록 박막이 결정성이 좋아지고 $Cr_2N$ 상이 쉽게 형성되었다. 증착 진공도에 따른 결정성은 상대적으로 질소의 농도가 높은 낮은 진공도에서는 CrN 상이 주로 형성되었으며, 반대로 높은 진공도에서는 $Cr_2N$ 상이 많이 만들어졌다. 즉 $1.3{\times}10^{-2}Torr$의 증착 진공도에서는 CrN 상만이 보이는 반면 $9.0{\tiems}1-^{-2}Torr$ 진공도에서부터 $Cr_2N$ 상이 형성되기 시작하여 $5.0{\tiems}10^{-2}Torr$ 진공도에서는 두개의 상이 혼재되어 있음을 알 수 있었다. 박막의 내마모성을 조사한 결과 CrN 박막의 마찰 계수는 초기에 급격하게 증가한 후 0.5에서 0.6 사이의 값으로 큰 변화를 보이지 않았으며, $Cr_2N$ 박막도 비슷한 거동을 보였다.차 이, 목적의 차이, 그리고

  • PDF

Evaluation of Running Performance of the Composite Bogie under Different Side Beam Stiffness (사이드 빔 강성에 따른 복합소재 대차의 주행성능 평가)

  • Kim, Jung-Seok
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.4
    • /
    • pp.86-92
    • /
    • 2017
  • In this study, a running performance evaluation and roller rig test was conducted to evaluate the applicability of a composite bogie frame, which has the role of the primary suspension. The composite bogie frame was made of a GEP224 glass/epoxy prepreg. Vehicle dynamic analysis was carried out on the composite bogie with three different kinds of side beam thicknesses (50 mm, 80 mm, and 150 mm). From the results, the composite bogie with a side beam thickness of 80 mm satisfied all the dynamic design requirements. Although the composite bogie with the side beam thickness of 50mm also met the design requirements, its critical speed was just a 2% margin to the requirement. In contrast, the model of the side beam thickness of 150mm did not meet the ride comfort. In addition, a composite bogie frame with the side beam thickness of 80 mm was fabricated and installed on a complete bogie. Moreover, the roller rig test using the fully equipped bogie was performed to evaluate the critical speed. During the test, the lateral excitation was imposed on the wheelsets to realize the rail irregularity. There was no divergence of the lateral displacement of the wheelsets while increasing the speed. The measured critical speed was similar to the predicted result.

Low Velocity Impact Property of CF/Epoxy Laminate according to Interleaved Structure of Amorphous Halloysite Nanotubes (비정질 할로이사이트 나노입자의 교차적층 구조에 따른 탄소섬유/에폭시 라미네이트의 저속 충격 특성)

  • Ye-Rim Park;Sanjay Kumar;Yun-Hae Kim
    • Composites Research
    • /
    • v.36 no.4
    • /
    • pp.270-274
    • /
    • 2023
  • The stacking configuration of fiber-reinforced polymer (FRP) composites, achieved via the filament winding process, exhibits distinct variations compared to conventional FRP composite stacking arrangements. Consequently, it becomes challenging to ascertain the influence of mechanical properties based on the typical stacking structures. Thus, it becomes imperative to enhance the mechanical behavior and optimize the interleaved structures to improve overall performance. Therefore, this study aims to investigate the impact of incorporating amorphous halloysite nanotubes (A-HNTs) within different layers of five unique layer arrangements on the low-velocity impact properties of interleaved carbon fiber-reinforced polymer (CFRP) structures. The low-velocity impact characteristics of the laminate were validated using a drop weight impact test, wherein the resulting impact damage modes and extent of damage were compared and evaluated under microscopic analysis. Each interleaved structure laminate according to whether nanoparticles are added was compared at impact energies of 10 J and 15 J. In the case of 10 J, the absorption energy showed a similar tendency in each structure. However, at 15 J, the absorption energy varies from structure to structure. Among them, a structure in which nanoparticles are not added exhibits the highest absorption energy. Additionally, various impact fracture modes were observed in each structure through optical microscopy.

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.