알루미늄과 유리섬유 하니컴 구조의 저속 충격 거동 (Low Velocity Impact Behavior of Aluminium and Glass-Fiber Honeycomb Structure)

  • 김진우;원천;이동우;김병선;배성인;송정일
    • Composites Research
    • /
    • 제26권2호
    • /
    • pp.116-122
    • /
    • 2013
  • 본 연구는 동일한 코어재를 가지는 알루미늄과 유리섬유의 하니컴 샌드위치 판넬의 저속 충격시 발생하는 충격 거동 및 압축 실험을 통하여 압축 강도와 압축 계수를 살펴본다. 저속 충격을 받는 하니컴의 충격 거동을 살펴보기 위하여 중량 낙하식 충격 시험을 실시하며, 충격을 가한 후 데이터 분석 및 현미경을 통하여 전형적인 충격파손모드와 손상정도를 비교 평가하였다. 동일한 충격에너지일 때 유리섬유 하니컴 샌드위치 판넬이 알루미늄 하니컴 샌드위치 판넬보다 최대 하중이 높고, 탄성 에너지가 크며, 충격 강도가 높은 것을 확인할 수 있었다.

알루미늄 하니컴 샌드위치 판넬의 저속충격거동 (Low-velocity Impact Behavior of Aluminum Honeycomb Sandwich Panel)

  • 이현석;배성인;함경춘;한경섭;송정일
    • 한국복합재료학회:학술대회논문집
    • /
    • 한국복합재료학회 2001년도 춘계학술발표대회 논문집
    • /
    • pp.78-82
    • /
    • 2001
  • Impact behaviors of Aluminum Honeycombs Sandwich Panel(AHSP) by drop weight test were investigated. Two types of specimens with 1/2" and 1/4" cell size were tested by two impactors which are weight of $5.25\textrm{kg}_{\textrm{f}}$ and $11.9\textrm{kg}_{\textrm{f}}$. Parametric studies were achieved including the impactor weight and impact sites which consist face, long-edge, short-edge, and point of the specimen. Face one of impact sites was the strongest and short-edge one of impact sites was the weakest. The damaged area of AHSP was enlarged with the increase of impactor weight that is equal to impact energy. After 3 point bending test, fracture modes of AHSP were analyzed with AE counts. Lower facesheet was fractured in the long-edge direction and then separated between facesheet and core. In the short-edge direction after core wrinkled, lower facesheet tear occurred. Impact behavior by FE analysis were increased localized damage in fast velocity because the faster velocity of the impact was, the smaller the stress of core was. Consequently, impactor weight had an effect on widely damaged area, while the impact velocity was caused on the localized damaged area.aged area.