The Optimization of Hydrometallurgical Process for Recovery of Zinc from Electric Arc Furnace Dust (Part I : leaching process) (습식산화법을 이용한 제강분진 내 아연회수를 위한 최적조건 도출에 관한 연구(Part I; 침출공정))

  • Moon, Dea-Hyun;Ahn, Sang-Woo;Kim, Han-lae;Kim, Ji-Tae;Chang, Soon-Woong
    • Resources Recycling
    • /
    • v.24 no.3
    • /
    • pp.27-33
    • /
    • 2015
  • EAFD (Electric Arc Furnace Dust) is considered as pernicious pollutant, assigned hazardous waste. Since this dust is a by-product of industry, it contains valuable metals such as Fe, Zn, Ni, Cu which can be turned into resources by recycling process. In this study, hydrometallurgical process was applied to recover Zn from Electric Arc Furnace Dusts. The result showed 95% Zn recovery at 3M $H_2SO_4$, Solids/Liquid ratio 1:2 and aeration of 1.8L/min for 2hr. However there was 80% Zn recovery at lower $H_2SO_4$ concentration apply for pilot scale plant.

Purification on the Leaching Solution of the Crude Zinc Oxide Recovered from the Reduction of EAF Dust (전기로제강분진으로부터 환원휘발된 조산화아연의 침출용액 정액에 관한 연구)

  • Youn Ki-Byoung
    • Resources Recycling
    • /
    • v.13 no.1
    • /
    • pp.22-27
    • /
    • 2004
  • Purification on the leaching solution of the crude zinc oxide obtained by the reduction of EAF dust has been carried out. Pb and Cd ions in the leaching solution were precipitated and removed from the solution by the addition of zinc metal powder. The purification condition for electrowinning to obtain the high purity zinc metal was investigated by analyzing the effects of Pb and Cd ion concentrations on the contents of impurities in the recovered zinc metal. The 3 N purity zinc metal was obtained at the electrolysis condition of the concentrations of Pb less than 2 ppm and Cd less than 0.1 ppm in the purified solution. For this purification, the amounts of zinc metal powder more than 8.5 g/l should be added in the crude zinc oxide leached solution.

Recovery of Gallium and Indium from Zinc Residues by Acid Leaching (산침출에 의한 아연제련잔사로부터 갈륨 및 인디움의 회수)

  • 이화영;김성규;오종기
    • Resources Recycling
    • /
    • v.2 no.2
    • /
    • pp.22-26
    • /
    • 1993
  • The flowsheet for the recovery of gallium and indium from zinc residues has been established based on the sulfuric acid treatment. In comparison with the alkali treatment, the method proposed in this work allowed the recovery of indium together with gallium. The majority of iron contained in leach liquor could be removed through the two-stage neutrallization under oxidative or reductive atmosphere. Crude gallium and indium could be obtained through the alkali and/or acid leaching of the products generated from the above treatment. In addition, cementation of indium with zinc powders could also be used for the concentration of it from weak acid solutions.

  • PDF

Effect of Ultrasound Irradiation during Cementation Process for Recovery of Iridium (이리듐 회수를 위한 시멘테이션 공정 중 초음파 조사의 영향)

  • Kim, Seunghyun;Kim, Young-Jin;Seo, Jun-Hyung;Cho, Jin-Sang;Cho, Kye-Hong;Lee, Jaeryeong
    • Resources Recycling
    • /
    • v.30 no.6
    • /
    • pp.61-67
    • /
    • 2021
  • This work investigated the cementation of iridium from iridium-containing hydrochloric acid leachate. Zinc powder was used as the reducing agent, and the effects of the stoichiometric ratio of Zn/Ir, initial Ir concentration, initial pH, reaction time, and ultrasound irradiation on iridium recovery were investigated. When only the stirrer was used for cementation, the iridium recovery increased with the addition amount of zinc, and the recovery of about 70% at 40 times the stoichiometric ratio of Zn/Ir. In contrast, when employing ultrasonic irradiation with stirring, the recovery of iridium decreased at 20 times or less the stoichiometric amount of zinc. The recovery of iridium increased at 40 times the stoichiometric ratio of Zn/Ir. This result may be due to the ionization of zinc and re-dissolution of iridium during the ultrasound irradiation treatment. When a combination of ultrasonic irradiation and stirring was used for cementation, the iridium recovery increased by more than 27% compared to that when using only the stirrer. It was possible to recover 99% of iridium under the following conditions: reaction time, 60 min; initial pH, 0.01; volume of leachate, 100 mL; 1770 ppm Ir, 40 times the stoichiometric ratio of Zn/Ir.

Recovery of Zine sulfate from zine sulfate waste water contain organic compound (유기물이 포함된 황산아연폐수로부터 황산아연의 회수)

  • Yoon, Guk-Joung;Lee, Tack-Hyuck
    • The Journal of Natural Sciences
    • /
    • v.14 no.2
    • /
    • pp.33-40
    • /
    • 2004
  • The eliminating of organic compound is essential process of the recovery of zinc sulfate from zinc sulfate waste water contained organic compound. The ozone oxidation and adsorption treatment is good for eliminating of organic compound in waste water. The zinc oxide treated an excess of sulfuric acid for zinc sulfate. We got zinc sulfate 740g from water 1kg.

  • PDF

A Study on the Cementation Reaction of Cadmium by Zinc Powders from Leaching Solution of Waste Nickel-Cadmium Batteries (폐니켈-카드뮴 전지 침출액으로부터 아연 분말을 이용한 카드뮴의 치환반응에 대한 연구)

  • Kim, Min-Jun;Park, Il-Jeong;Kim, Dae-Weon;Jung, Hang-Chul
    • Resources Recycling
    • /
    • v.28 no.1
    • /
    • pp.23-31
    • /
    • 2019
  • Cementation is one of economical and efficient recycling method precipitating the metal ion in solution by adding another active metal. In this study for optimizing cadmium recovery efficiency, it was performed as a function of the effect of pH, temperature, particle size, and input amount of zinc in 0.1 M $CdSO_4$ solution and Ni-Cd battery leaching solutions, respectively. The particle size of zinc and temperature were key factors for Cd cementation and it was confirmed that the input amount of 2.6 of Zn/Cd ratio using granular-type zinc was optimal condition for selective Cd recovery efficiency at $25^{\circ}C$.

A Study on the Separation and Recovery of Useful Metallic Elements(Zn, Pb) from the 2nd Dust in Refining of Crude-Zinc Oxide (조산화아연의 정제과정에서 발생된 2차분진으로부터 유용금속원소(Zn, Pb)의 분리회수에 관한 연구)

  • Yoon, Jae-hong;Yoon, Chi-hyun
    • Resources Recycling
    • /
    • v.30 no.1
    • /
    • pp.66-76
    • /
    • 2021
  • Electric arc furnace dust (EAFD) contains compounds, such as oxides and chlorides, including large quantities of Zn, Pb and Fe. An efficient and stable method for the extraction of metal elements from EAFD is the Rotary Kiln Process. This method is used to recover Zn in the form of crude ZnO (approximately 60%) via the addition of a reducing agent (coke, anthracite) and limestone (for basicity control) to EAFD. This process is commonly used in industry as well as in research and development. Currently, this method is used in many Korean commercial plants, producing approximately 150,000 tons of Crude ZnO per year. The majority of Zn is found in crude ZnO (approximately 76%). In addition components such as Pb, Cd, Sn, In, Fe, Cl, and F are present as oxides, chlorides, and alkaline compounds. This elements have an adverse effect on the zinc smelting process. Therefore, a refining process that eliminates these impurities is essential. In this study, we developed a process technology that efficiently separates Zn and Pb from byproducts (mainly chlorides). A bag filter was used to collect Zn and Pb generated during the dry purification process of crude ZnO. Pure components were recovered as metals or metal carbonate.

Recovery of Gallium from Zinc Smelting Residues by Alkali Leaching (아연제련잔사의 알칼리 침출에 의한 갈륨의 회수)

  • 김성규;이화영;오종기
    • Resources Recycling
    • /
    • v.9 no.3
    • /
    • pp.22-28
    • /
    • 2000
  • A study on the recovery of gallium from zinc residues is carried out by alkali leaching using NaOH. The results show that in case of alkali leaching of zinc residues, Zn, K and Si are mainly leached out and Fe and other base metals are scarcely leached out, which results in that gallium is easily recovered by solvent extraction. The leaching efficiency of gallium increases with increasing alkali concentration and solid density. Especially, alkali consumption is considerably reduced by washing the zinc residues with water before leaching in order to eleminate the soluble zinc compounds. The gallium from zinc residues is found to be leached out with a recovery of 80% or higher for 2hrs leaching with 1~1.25 M/L NaOH solution and solid density 333 g/L at $25^{\circ}C$.

  • PDF

Basic Studies on the Recovery of Zinc Metal from Wastewater by Cyclic Voltammetry (循環走査법에 의한 廢水로부터 亞鉛 回收에 관한 基礎 硏究)

  • 김진화;김동수
    • Resources Recycling
    • /
    • v.10 no.3
    • /
    • pp.29-36
    • /
    • 2001
  • Cyclic voltammetry has been applied in the basic studies for the treatment and recovery of heavy metal component contained in wastewater by electrochemical reduction. The electrochemical behaviors of zinc ion for zinc metal electrode and carbon elec-trode were characterized by voltammograms and it was showed that zinc ions were reduced to metallic form below -0.76 V vs SHE. The change in the features of crystalline form of metallic zinc upon oxidation and reduction reaction was observed by X-ray diffraction method and the Am analysis verified that zinc ions were reduced to metal on copper plate. The results of this study were regarded to be important and meaningful in the treatment of heavy metal containing wastewater and, as a result, in the obtainment of metallic product by electrochemical method.

  • PDF

Recovery of Gallium from Zinc Residues by Solvent Extraction (아연제련잔사로부터 용매추출법에 의한 갈륨의 회수)

  • 김성규;이화영;오종기
    • Resources Recycling
    • /
    • v.9 no.3
    • /
    • pp.29-36
    • /
    • 2000
  • A study on the recovery of gallium from leaching solutions is carried out by solvent extraction in order to produce gallium oxide of high purity. The results show that the extraction of gallium is found to be increase with acidities of aqueous solution up to 7.4 M/L when pure isopropyl ether is used. And the extraction of iron also increases with increasing acidity of aqueous solution. It appears that the separation of gallium from iron cannot be satisfactorily accomplished with isopropyl ether. But, in the case of extaction with D2EHPA, almost complete extraction of iron is achieved-leaving all the gallium in the aqueous solution-by maintaining the acidity of aqueous solution at 2 M/L. Accordingly, $Ga_2O_3{\cdot}H_2O$ of more than 99wt.% in purity can be produced from zinc residues through the processes comprising of alkali leaching, precipitation by neutralization and solvent extraction using isopropyl ether and D2EHPA as extractants.

  • PDF