Basic Mix Proportions of Antiwashout Underwater Polymer Cement Mortar as a Repair Material (보수재료로서 수중불분리 폴리머 시멘트 모르타르의 기초적 배합)

  • Jo, Young-Kug
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.05a
    • /
    • pp.193-194
    • /
    • 2019
  • The purpose of this study is to design the basic mix proportions of antiwashout underwater polymer cement mortar as a repair material. The antiwashout underwater polymer cement mortars are prepared with various mix proportions using three type polymer dispersions without or with antifoamer. From the test results, the whole antiwashout underwater polymer cement mortars can be cast underwater without segregation like plain mortar. It is apparent that the flexural strength of antiwashout underwater SBR cement mortars with antifoamer at polymer- cement ratios of 5% and 10% is higher than that of plain mortar irregardless of a little low compressive strength.

  • PDF

Durability Properties of Ultra Rapid Hardening Mortar Produced with Alumina-based Binder for Repairing Sewage Treatment Pipes (하수관거 보수용 알루미나계 결합재 초속경 모르타르의 내구 특성)

  • Eun-Ho, Kim;Byung-Jae, Lee;Sun-Mok, Lee;Yun-Yong, Kim
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.4
    • /
    • pp.482-488
    • /
    • 2022
  • In this study, the durability of ultra rapid hardening mortar for sewage pipe was evaluated by type of mortar binder. As a result of analyzing the internal structure for each type of mortar, it was confirmed that Al2(OH)3 was generated in the internal structure of the CAC-based mortar, and its corrosion resistance was superior to that of other types of mortar. As a result of the compressive strength test, OPC had the tsmallest strength, followed by CAC100 > CAC100P > CAC80. This trend was similar to the previous study results. Chloride ion penetration resistance and freeze-thaw test showed similar trends. That is, CAC and C12A7 were better than OPC, and CSA was worse than OPC. This is mostly beacuse of cracks caused by expansion of CSA-based mortar. CAC100P mix showed the best chemical resistance. It is thought that this is because the alumina gel formed inside the mortar and the polymer combine to make the internal structure more dense.