• Title/Summary/Keyword: 소성정광

Search Result 9, Processing Time 0.024 seconds

Mineralogical Phase Transform of Salt-roasted Concentrate and Enhancement of Gold Leaching by Chlorine-hypochlorite Solution (소금-소성정광에 대한 광물학적 상변화와 염소-차아염소산 용액을 이용한 금 용출 향상)

  • Kim, Bong-Ju;Cho, Kang-Hee;Oh, Su-Ji;Choi, Seoung-Hwan;Choi, Nag-Choul;Park, Cheon-Young
    • Journal of the Mineralogical Society of Korea
    • /
    • v.26 no.1
    • /
    • pp.9-18
    • /
    • 2013
  • In order to optimize the gold leaching process from refractory sulfide concentrate, a chlorine-hypochlorite solution with varying concentrations and temperatures were applied to salt-roasted concentrate. The concentrate consisted of pyrite, chalcopyrite, and galena, which were turned into hematite through air-roasting at $750^{\circ}C$. Also these concentrates were changed into hematite and nantokite (CuCl)) through salt (NaCl)-roasting at $750^{\circ}C$. The results of the gold leaching experiments showed that the best gold leaching parameters were obtained when the hydrochloric acid-sodium hypochlorite mix was at a ratio of 1 : 2, the added concentration was 1.0 M concentration, the pulp density was 1.0%, and the leaching was done at a $60^{\circ}C$ leaching temperature. The leaching rate for gold was much greater in the roasted concentrate than in the raw concentrate. The leaching rate was greater in the salt-roasted concentrate than in the plain roasted concentrate too. From XRD analysis, quartz was found in the salt-roasted concentrate and in the solid residue from the chlorine-hypochlorite leaching solution at $60^{\circ}C$.

Application of Roasting Pretreatment for Gold Dissolution from the Invisible Gold Concentrate and Mineralogical Interpretation of their Digested Products (비가시성 금정광의 효율적 용해를 위한 소성전처리 적용과 분해 잔유물에 대한 광물학적 해석)

  • Kim, Bong-Ju;Cho, Kang-Hee;Oh, Su-Ji;On, Hyun-Sung;Kim, Byung-Joo;Choi, Nag-Choul;Park, Cheon-Young
    • Journal of the Mineralogical Society of Korea
    • /
    • v.26 no.1
    • /
    • pp.45-54
    • /
    • 2013
  • In order to dissolve Au, Ag, and other valuable metals from gold ore concentrate, raw gold concentrate was pre-treated by roasting and salt-roasting at $750^{\circ}C$. The roasted concentrate was treated with aqua regia digestion to dissolve the valuable metals and higher amount of Au, Ag, and valuable metals were extracted from the roasted concentrates than from the raw concentrate. Higher amount of these metals were also extracted from the salt-roasted concentrate than from the roasted concentrate. The results of the gold dissolution experiments showed that the gold dissolution was most efficient when particle size, roasting temperature, and the percentage of added salt in salt roasting were about $181{\sim}127{\mu}m$, $750^{\circ}C$, and was 20.0%, respectively. The XRD analysis suggests that quartz and pyrite were not destroyed even through roasting at $750^{\circ}C$ and decomposition with aqua regia. However, through salt roasting, pyrite was completely decomposed, whereas quartz could not be destroyed through salt-roasting at $750^{\circ}C$ and aqua regia digestion. Accordingly, it was expected that the gold contained in quartz can not be dissolved through salt-roasting and treatment with aqua regia.

The Characteristic of Te Recovery in Gold Concentrate Using Electrolysis (전기분해법을 이용한 금정광내 Te 회수 특성)

  • Kim, Bong-Ju;Cho, Kang-Hee;Jo, Ji-Yu;Choi, Nag-Choul;Park, Cheon-Young
    • Economic and Environmental Geology
    • /
    • v.47 no.6
    • /
    • pp.645-655
    • /
    • 2014
  • In order to obtain pure metallic Te from gold concentrate, roasting treatment, hypochlorite leaching, Fe removal and electrolysis experiments were carried out. The contents of Au, Ag and Te from the concentrate sample and roasted sample were much more soluble in the hypochlorite solution than in aqua regia digestion, whereas the metals Pb, Zn, Fe and Cu were easier to leach with the aqua regia than the hypochlorite. With the addition of NaOH in the hypochlorite leaching solution prior to electrolysis, the Fe removal rate achieved was only 96% in the concentrate sample, while it reached 98% in the roasted sample. The results of electrolysis for 240 min, 98% of the metallic copper was recovered from the concentrate sample, while 99% was obtained from the roasted sample due to the removal of S by roasting. The amount of anode slime was also greater in the electrolytic solution with the roasted sample than with the concentrate sample. The results on the anode slime after the magnetic separation process showed the amount of metallic pure native tellurium recovered was greater in the roasted sample than in the concentrate sample.

Optimization of Gold Leaching from the Refractory Sulfide Concentrate by HCl-NaClO-FeCl3 Solution (HCl-NaClO-FeCl3 용액을 이용한 저항성 황화광물 정광으로부터 금 용출 최적화)

  • Kim, Bong-Ju;Cho, Kang-Hee;Lee, Jong-Ju;Choi, Nag-Choul;Park, Cheon-Young
    • Economic and Environmental Geology
    • /
    • v.46 no.1
    • /
    • pp.21-28
    • /
    • 2013
  • In order to optimize gold leaching from refractory sulfide concentrate, a HCl-NaClO-$FeCl_3$ solution with varying attributes was applied to the roasted concentrate from Uil mine. The gold from Uil mine occurs in the form of invisible gold that is difficult to leach. The results of the gold leaching experiments showed that the best gold leaching parameters were $550^{\circ}C$ of roasting temperature, 2.0 M of concentration, 1.0% of pulp density, and $70^{\circ}C$ of leaching temperature. It is confirmed that the HCl-NaClO-$FeCl_3$ solution was an environmentally friendly method to leach gold and silver from the refractory sulfide concentrate as an alternative lixiviant to cyanide.

The Optimization of Silver Leaching from the Samjo Mine Concentrate by Thiourea (티오요소를 이용한 삼조광업 정광으로부터 은 용출 최적화)

  • Yang, Gwon-Seung;Kim, Bong-Ju;Choi, Nag-Choul;Park, Cheon-Young
    • Journal of the Mineralogical Society of Korea
    • /
    • v.26 no.1
    • /
    • pp.1-8
    • /
    • 2013
  • This study was carried out to test the possibility of using an environmentally friendly method of leaching silver concentrate from the Samjo mine. The Samjo mine ore contained minerals such as pyrite, chalcopyrite, galena, arsenopyrite, and sphalerite. The concentrate samples tested with the thiourea solution were roasted at $750^{\circ}C$. The results of different experimental conditions showed that the highest silver leaching rate was obtained when the concentration of thiourea was at 0.8 g with ferric sulfate at 0.425 g and the leaching temperature at $60^{\circ}C$. The Ag leaching rate obtained was 91.5% at a pulp density of 10%. However, in the XRD analysis, peaks of pyrite, galena, and hematite were still found in the leached solid residues in which the Ag leaching rate was the highest. it is expected that the unrecovered silver in the solid residue can be lost.

The Leaching of Gold-silver from Refractory Gold Concentrate by Chlorine-hypochlorite Solution (염소-차아염소산 용액에 의한 저항성 금 정광으로부터 Gold-silver 용출)

  • Cho, Kang-Hee;Kim, Bong-Ju;Oh, Su-Ji;Choi, Seoung-Hwan;Choi, Nag-Choul;Park, Cheon-Young
    • Journal of the Mineralogical Society of Korea
    • /
    • v.25 no.3
    • /
    • pp.123-130
    • /
    • 2012
  • Leaching experiments of gold and silver from roasted concentrate were carried out using a chlorine-hypochlorite solution. The leaching rate of gold was 75% at 1.5:1 ratio of chlorine and hypochlorite and increased to 81% with adding 1 M NaCl. However, at 1% pulp density and at $65^{\circ}C$, the leaching rates of Au were close to 100%. XRD analysis identified quartz in the solid residues after digestion of roasted concentrate with aqua regia or chlorine-hypochloride leaching solution. This suggests that the gold may not be leached out of the quartz in aqua regia or chlorine-hypochlorite solution. In order to leach the gold from the quartz, the concentrate will have to be pre-treated through ultra-fine grinding or treated with stronger oxidative agents.

Removal and Recovery of Arsenic from Gold Concentrate (금(金) 정광(精鑛)내의 비소(砒素)(As) 제거(除去) 및 회수(回收)에 관한 연구(硏究))

  • Yoo, Kyoungkeun;Shin, Shun-Myung;Park, Jay Hyun;Choi, Ui Kyu;Wang, Jei-Pil
    • Resources Recycling
    • /
    • v.22 no.4
    • /
    • pp.33-37
    • /
    • 2013
  • A study on the removal of arsenic from gold concentrate was conducted using thermal decomposition method at $700^{\circ}C$ as a function of reaction time. In addition, the arsenic removed from the concentrate was also collected in the bag-filter as a form of AsS. The content of arsenic in the concentrate was dramatically decreased from 12.62 wt/% to 1.40 wt.% for 1 hour and even lower than 1 wt.% after two hours. The removal efficiency of arsenic was finally achieved to be about 95% after 2 hours at a given temperature.

Decomposition and Leaching of Bastnasite by Sulfation and Recovery of Cerium Hydroxide from Leached Solution (황산화반응에 의한 불탄산염 희토류광(Bastnasite)의 분해, 침출 및 세륨수산화물의 회수)

  • Yoon, Ho-Sung;Kim, Sung-Don;Kim, Chul-Joo;Kim, Jun-Soo;Han, Choon
    • Applied Chemistry for Engineering
    • /
    • v.9 no.3
    • /
    • pp.407-412
    • /
    • 1998
  • This study was carried out to investigate the optimum leaching conditions for the sulfation and water leaching, and separation of cerium from rare earth elements in leached solution by acid-adjusting method. The optimum conditions for the sulfation and water leaching from bastnasite concentrates are that the equivalent ration of sulfuric acid to concentrates is 2.5, calcination temperature and time are $600^{\circ}C$ and 2 hrs respectively, and the pulp density in the water leaching is 9.1%. The yield of rare earth oxide is about 93% at the above condition. The process of recovery of cerium hydroxide from leached solution by acid-adjusting method was carried out as following steps. The first step is the oxidation of the solution at pH 5 by using twice the equivalent of $H_2O_2$ solution as an oxidant. The second step is the precipitation to obtain cerium complex salt and cerium hydroxide after lowering the solution to pH 2. The last step is the oxidation-precipitation by using equivalent of $H_2O_2$ solution. From these results, it was possible to prepare cerium hydroxide with the yield of 60% and the quality of 80%.

  • PDF

Decomposition of Dibenzothiophene Sulfone over KF/MgO Catalysts (KF/MgO 촉매를 이용한 Dibenzothiophene Sulfone 분해반응)

  • Kim, Hyeon-Joo;Jeong, Kwang-Eun;Jeong, Soon-Yong;Park, Young-Kwon;Jeon, Jong-Ki
    • Clean Technology
    • /
    • v.16 no.1
    • /
    • pp.12-18
    • /
    • 2010
  • The object of the present study is to apply KF/MgO catalysts to remove sulfur dioxide from dibenzothiophene sulfone, a by-product of oxidative desulfurization. Potassium fluoride was deposited via an impregnation method on MgO. The effects KF loading and calcination on the characteristics of the KF/MgO catalysts were investigated through the BET surface area, XRF, XRD, and temperature-programmed desorption of $CO_2$. The catalytic performances of the samples were investigated during the decomposition of dibenzothiophene sulfone to biphenyl and sulfur dioxide gas. KF loaded on MgO prepared by the impregnation method showed high catalytic activities for the decomposition of dibenzothiophene sulfone. The higher activity of KF/MgO just dried at 373 K, avoiding the usual activation at high temperature, than that over the calcined catalyst is ascribed to increase of the amount of basic sites. The high basicity probably may be due to the coordinately unsaturated $F^-$. The simply dried 10 % KF/MgO catalyst, without the usual activation at high temperature, showed the optimal catalytic properties.