• Title/Summary/Keyword: 세라믹계 도장

Search Result 3, Processing Time 0.018 seconds

A Study on the Slip Behavior of Coated High Tension Bolted Joints (도장처리한 고장력볼트 연결부의 미끄러짐 특성에 관한 연구)

  • Kyung, Kab Soo;Lee, Seung Yong;Kim, Ki Hyun
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.28 no.5A
    • /
    • pp.691-697
    • /
    • 2008
  • Coating the high tension bolted frictional joint has been generally allowed for anti-corrosion purpose. However in case of painting on paying surface of the high tension bolt, the influence on a slip strength of the joint depending on precision of painting has remained controversial. The study thus was intended to identify the slip behavior on high tension bolted frictional joint when applying ceramic painting, which has been currently developed. A slip test was conducted on a high tension bolted frictional joint specimen on which ceramic painting has been applied and a slip load and slip coefficient were measured. Based on result, the safety and usability of ceramic painting-applied high tension bolted frictional joint was evaluated. As a result, a difference to some extent by specimen in terms of load-displacement when a slip occurred was observed but an average slip coefficient appeared to have exceeded 0.4, which is the design frictional coefficient set forth in the specification. To secure the safety and usability of ceramic painting-applied high tension bolted frictional joint, it's necessary to establish the standard for painting as well as to revise the relevant specification.

Suggestion of Deterioration Curve for New-type Coating on Atmospheric Environment by Acceleration Corrosion Test (부식촉진 실험을 통한 대기환경에서 신설 도장계의 노화곡선 제안)

  • Jeong, Young-Soo;Kim, Min-Jeong;Jeon, Seok-Hyeon;Ahn, Jin-Hee;Kim, In-Tae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.2
    • /
    • pp.75-83
    • /
    • 2019
  • In this study, to propose the deterioration curves of urethane, ceramic, polysiloxane and fluorocarbon coating for the steel bridge, an accelerated corrosion tests were carried out. The each coating system wes applied on the top of the specimens, and circular initial defects were introduced with different diameters with 0.5, 1.0, 3.0, 5.0 mm. An accelerated corrosion test condition was used to simulate severe corrosive environment depending on ISO 20340. The deterioration curve of each coating type was evaluated based on deteriorated area from the circular defects. In order to evaluate the coating service life of installed steel bridge using deterioration curve, the acceleration coefficient was calculated at correlation between ISO 20340 and corrosivity categories by ISO 9223 based on field corrosion rate. From test results, the propagation rate of coating deterioration area was different to diameter of circular defects. In case of urethane coating, the coating service lifes of 3% deterioration area was evaluated in 31.8, 15.8, 9.9 and 3.9 years with C2, C3, C4 and C5 category.

Durability Characteristics of Concrete with Nano Level Ceramic Based Coating (나노합성 세라믹계 도장재를 도포한 콘크리트의 내구성능)

  • Kim, Seong-Soo;Lee, Jeong-Bae;Han, Seung-Woo
    • Journal of the Korea Concrete Institute
    • /
    • v.19 no.5
    • /
    • pp.639-646
    • /
    • 2007
  • This study performed several tests for the durability of the concrete coated with nano synthesis ceramics which do not contain volatile organic compounds harmful to environment. The tests were adhesion test on dry and humid concrete, SEM test, MIP analysis, carbonation, chloride diffusion by electronic facilitation, freezing-thawing resistance, alkaline resistance, and brine resistance test. In the adhesion test on dry and humid concrete, nano synthesis ceramics coating produced the highest results among all the coatings tested. Nano synthesis ceramics adhered solidly on the concrete surface. The adhesive strength seemed to result from the hydrogen bond between nano synthesis ceramics which are inorganic and generated by hydrolysis and re-condensation reaction and the concrete's hydrates such as calcium silicate aluminate or calcium silicate hydrate. SEM test and MIP analysis results show surface structure with finest crevices pore in the nano synthesis ceramics coating applied concretes. In the carbonation, chloride diffusion, and freezing-thawing resistance tests, the concretes with nano synthesis ceramics coating indicated the best results. Based on these test results, further progress in application of nano synthesis ceramics coatings to various concrete structures including costal structures and sewerage arrangements can be expected.