• Title/Summary/Keyword: 섬유강화 플라스틱

Search Result 222, Processing Time 0.031 seconds

Experimental Study on the Hygrothermal Ageing Effect to the Strength of CFRP Materials for Marine Leisure Boat (열수노화 조건에서 레저선박용 탄소섬유강화플라스틱의 강도변화에 관한 실험적 연구)

  • Jeong, Han Koo;Noh, Jackyou
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.55 no.3
    • /
    • pp.205-214
    • /
    • 2018
  • This paper deals with the experimental study on the hygrothermal ageing effect to the strength of Carbon Fiber Reinforced Plastics (CFRP) materials for marine leisure boat manufactured by vacuum assisted resin infusion method. The experiments performed consist of tensile, flexural and shear tests according to American Society for Testing and Materials (ASTM) and Korean Industrial Standards (KS) test methods. Test coupons are varied from uni-directional(UD, $0^{\circ}$, $90^{\circ}$), Bi-Directional (BD), and Double-Bias (DB) carbon fiber fabrics in conjunction with epoxy resin. The results of tensile test show that tensile strength reduces significantly while not the same degree of reduction is observed for elasticity modulus with respect to the existence of hygrothermal ageing effect. This implies that the tensile strain induced from external load holds steady values but ultimate strength values change widely under hygrothermal ageing effect. In case of the flexural test, $0^{\circ}$ UD shows more strength reduction than $90^{\circ}$ UD while BD has reduced values in both flexural strength and elasticity modulus under hygrothermal ageing effect. It is learned that the bending strain induced from external load and ultimate strength values are reduced with respect to hygrothermal ageing effect. Shear test performed only on DB materials, and the results show marginal reduction in ultimate strength and moderate reduction in elasticity modulus. This means that the shear strain varies more than ultimate shear strength with respect to hygrothermal ageing effect. The experiment conducted in this paper clearly demonstrates the differences in material properties of the CFRP for the consideration of hygrothermal ageing effect. Findings obtained from this experimental study can serve as a fundamental input data for the realistic structural responses of marine leisure boat built in CFRP materials.

Estimation for Adaptability of Fiber Reinforced Plastic Composite for LNG Storage Tank (유리섬유강화 플라스틱의 LNG 저장탱크용 합판 대체 가능성 평가)

  • Kim S. B.;Cho J. M.;Cho S. H.;Kwon Y. S.
    • Journal of the Korean Institute of Gas
    • /
    • v.7 no.1 s.18
    • /
    • pp.28-32
    • /
    • 2003
  • In order to apply the properties of fiber reinforced plastic(FRP) to support panel of polyurethane foam in LNG storage tank, we estimated the mechanical properties, degree of vapour barrier, chemical stability and thermal conductivity changes as ageing. According to the results, the mechanical strength (i.g. compressive strength, bending strength, tensile strength and shear strength) are more than 30 times higher than those of plywood. The FRP-polyurethane foam(PUF) composites have lower thermal conductivity changes as ageing than plywood-PUF composites. FRP-PUF sandwich composite for LNG storage tank with these remarkable properties are compared the abilities of these structures with those of the conventional structures(plywood-PUF sandwich composite). Finally, we can obtain the effects such as superior mechanical properties and fuel saving through improved ability of vapor barrier.

  • PDF

Improvement of Flexural Structural Performance and Applied Section Shape for Sound Proof Wall Structures Using Glass Fiber Reinforced Polymer(GFRP) (GFRP를 활용한 도로 방음벽 구조물의 구조성능 및 단면형상 개선에 관한 연구)

  • Jung, Woo-Young;Choi, Hyun-Kyu
    • International Journal of Highway Engineering
    • /
    • v.11 no.4
    • /
    • pp.9-15
    • /
    • 2009
  • This research presents the structural performance and an improving technique for flexural capacity of road safety facilities based on the damage cases by wind pressure. Among road safety facilities, a support frame of soundproofing walls is considered as a prototype structure and its corresponding structural behaviors and section design are performed mainly by analytical and experimental studies. On the basis of analytical results, glass fiber reinforced polymer(GFRP) with an epoxy matrix which is high stiffness-to-weight ratio was used for applied one of strengthening techniques and their results shows that support frame strengthened by GFRP is the most effective compared to other cases proposed in this research for advancing its flexural improvement, Finally, optimum section design was performed analytically to evaluate wind-resistance capacity and its result would be very useful for developing a practical design guideline for Road safety facilities under strong wind.

  • PDF

Structural Safety Analysis of a Spherical Flight Simulator Designed with a GFRP-Foam Sandwich Composite (GFRP-폼 샌드위치 복합재료로 설계된 구체 비행 시뮬레이터의 구조 안정성 평가)

  • Hong, Chae-Young;Ji, Wooseok
    • Composites Research
    • /
    • v.32 no.5
    • /
    • pp.279-283
    • /
    • 2019
  • A flight training simulator of a fully spherical configuration is being developed to precisely and quickly control six degrees of freedom (Dof) motions especially with unlimited rotations. The full-scale simulator should be designed with a lightweight material to reduce inertial effects for fast and stable feedback controls while no structural failure is ensured during operations. In this study, a sandwich composite consisting of glass fiber reinforced plastics and a foam core is used to obtain high specific strengths and specific stiffnesses. T-type stainless steel frames are inserted to minimize the deformation of the sphere curvature. Finite element analysis is carried out to evaluate structural safety of the simulator composed of the sandwich sphere and steel frames. The analysis considers the weights of the equipment and trainee and it is assumed to be 200 kg. Gravity acceleration is also considered. The stresses and displacement acting on the simulator are calculated and the safety is assessed under two different situations.

An Experimental Study on the Mechanical Mounting between GFRP Door Impact Beam and Steel Brackets (GFRP 도어 임팩트 빔과 Steel 브래킷의 기계적 결합에 관한 실험적 연구)

  • Ha, Jung-Chan;Shin, Young-cheol;Baek, In-Seok;Lee, Seok-Soon
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.20 no.5
    • /
    • pp.103-110
    • /
    • 2021
  • The mounting performance of the GFRP(Glass fiber Reinforced Plastic) beam and the mechanical mounting of the steel bracket was studied to be mounted as a GFRP impact beam on the side door of the passenger car. Moreover, an open-hole tensile test was performed to evaluate breakage tendency based on GFRP stacking conditions. Furthermore, the tightening strength of rivets and bolts was compared using the single lap-shear tension test for the GFRP stacking pattern. Additionally, the GFRP beam and bracket mounting features were designed; moreover, the prototype and bracket were assembled. Additionally, the bracket mounting bending test and the door assembly static bending test were performed to verify the stability of the bracket mounting. In the bracket fastening bending test, no breakage occurred in the connection part between the GFRP beam and the bracket, and it showed 67% (24.4 kN) improved performance compared to steel. In the static bending test of the door assembly, the initial average reaction force increased by 25% compared to the steel, and the performance of all FMVSS-214 regulations was satisfied. The replacement of GFRP impact beams resulted in a 30% weight reduction

A Study on Fracture Property of Adhesive Interface at Tapered Double Cantilever Beam with Inhomogeneous Composite Material due to Loading Conditions of In-plane and Out-plane (면내 및 면외 하중 조건들에 따른 이종 복합 소재를 가진 경사진 이중외팔보에서의 접착계면의 파괴 특성 연구)

  • Lee, Jung-Ho;Kim, Jae-Won;Cheon, Seong-Sik;Cho, Jae-Ung
    • Composites Research
    • /
    • v.33 no.6
    • /
    • pp.401-407
    • /
    • 2020
  • At the engineering and industrial areas, the lightweight composite material has been substituted with the metals, such as steel at the structural parts. This composite material has been applied by the adhesive bonding method, as well as the joint methods with rivets, welds or bolts and nuts. The study on the strength characteristics of adhesive interface is necessarily required in order to apply the method to composite materials. CFRP specimens as the fiber reinforced plastic composites were manufactured easily and this study was carried out. The static experiments were performed under the loading conditions of in-plane and out-plane shears with the inhomogeneous composite TDCB specimens with CFRP, aluminum (Al6061), and aluminum foam (Al-foam). Through the result of this study, the durability on the inhomogeneous composite structure with adhesive interface was investigated by examining the fracture characteristic and the point in time.

Estimating Tensile Strengths of CFRP Laminates Having Various Stacking Sequences (다양한 적층을 갖는 CFRP 적층판의 인장강도 예측)

  • Park, Chan Yik;Lee, Myung-Keon;Kim, Sang-Yong;Jang, Se-Yong
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.50 no.5
    • /
    • pp.309-316
    • /
    • 2022
  • This paper presents nonlinear numerical analysis results which were compared with the tested tensile strengths of CFRP(Carbon Fiber Reinforced Plastic) laminates with 14 different stacking sequences. The composite laminate coupons were cured under an autoclave pressure using resin-impregnated unidirectional tapes. The nonlinearity of the matrix was considered for the analysis, which was obtained from lamina tests. The Hashin failure criteria and progressive failure analysis were used for the nonlinear finite element analysis. The comparison results show that the current approach is acceptable to predict the tensile strengths of the CFRP laminate coupons with various stacking sequences and no damage. However, it is not acceptable to predict the tensile strengths of the laminate specimens with a center hole.

Hydraulic Experiment on Roughness Coefficient of PE pipe (폴리에틸렌관의 조도계수에 관한 수리모형실험)

  • Dongwoo Ko;Byeong Wook Lee;Jae-Seon Yoon;Hyun-Gu Song
    • Proceedings of the Korea Water Resources Association Conference
    • /
    • 2023.05a
    • /
    • pp.288-288
    • /
    • 2023
  • 도로, 철도 등의 횡단통로, 오폐수관로, 지하배수관 등 연약지반에서 상재하중과 부등침하에 의한 파괴 위험을 줄이기 위해 구조적인 안전성과 내구성이 개선된 다양한 관로들이 활용되고 있다. 관은 매설특성에 따라 콘크리트관, 도관, 합성수지관, 덕타일 주철관, 파형강관, 유리섬유 강화 플라스틱과 폴리에스테르수지 콘크리트관 등의 종류로 구분된다(환경부, 2017). 수리설계 시 이러한 관의 단면 규모 결정 및 흐름 특성을 파악하기 위해 관수로 유량측정에 이용되는 Manning의 경험식을 이용하고 있으며, 관로의 주요 재질에 따른 다양한 조도계수가 제시되어 있다. 새로운 재질을 이용하여 제작된 관은 수리실험을 통해 조도계수를 결정하는 것이 바람직하지만, 조도계수 실험은 대규모의 실험시설과 유량공급이 요구되기 때문에 여러 한계가 있다. PE관의 경우, 미국의 ASTM 표준에 의해 저밀도 폴리에틸렌(LDPE), 선형 저밀도 폴리에틸렌(LLDPE), 고밀도 폴리에틸렌(HDPE) 등으로 분류되는데 본 연구에서는 HDPE 재질의 서로 직경이 다른 다중벽관 PE관을 대상으로 조도계수를 결정하기 위한 현장 실규모 수리실험을 수행하였다. 본 실험에서는 식생, 수로의 불규칙성, 수로노선, 침전과 세굴, 장애물, 계절적 변화, 부유물질과 소류사는 무시되며 표면조도, 관의 크기와 형상, 수위와 유량이 조도계수에 영향을 미치는 주요 인자라고 할 수 있다. 수리실험은 실물모형(Prototype)으로 한국농어촌공사 농어촌연구원의 대형수리모형실험장에서 수행되었으며. 길이 24 m, 직경 150 mm의 PE 관은 고정식 개수로, 직경 800 mm의 관은 대형유사순환수로에 각각 설치되었다. 관로의 전면에 차폐막을 설치하여 상류부 수위를 안정시킨 상태에서 실험을 수행하였고, 차폐막으로부터 하류방향으로 약 7 m(측정기준지점), 11 m, 13 m, 15 m, 17 m 떨어진 곳에서 각각 수위와 유속을 측정하였다. 실험 결과, φ150관은 직경대비 수심이 클수록 조도계수가 감소하는 경향이 나타났고, φ800관은 직경대비 수심의 변화에 따른 조도계수의 경향이 크게 드러나지 않았다. 결론적으로 PE관의 조도계수는 수심별로 변화하는 것으로 나타났으며, 특정 수심을 지나면 조도계수가 다시 감소할 것으로 판단된다.

  • PDF

One-Way Shear Strength of Donut Type Biaxial Hollow Slab Considered Hollow Shapes and Materials (중공형상 및 재료의 영향을 고려한 도넛형 이방향 중공슬래브의 일방향 전단강도)

  • Chung, Joo-Hong;Lee, Seung-Chang;Choi, Chang-Sik;Choi, Hyun-Ki
    • Journal of the Korea Concrete Institute
    • /
    • v.24 no.4
    • /
    • pp.391-398
    • /
    • 2012
  • This paper presents the shear capacities of biaxial hollow slab with donut type hollow sphere. Recently, various types of slab systems which can reduce self-weight of slabs have been studied for increasing constructions of taller and larger building structures. A biaxial hollow slab system is widely known as one of the effective slab system, which can reduce self-weight of slab. According to previous studies, the hollow slab has low shear strength, compared to solid slab. Also, the shear capacities of biaxial hollow slab are influenced by the shapes and materials of hollow spheres. However, the current code does not provide a clear computation method for the shear strength of hollow slab. To verify the shear capacities of this hollow slab, one-way shear tests were performed. Four test specimens were used for test parameters. One was conventional RC slab and others were hollow slabs. The test parameters included two different shapes and materials of plastic balls. The shape parameters were donut and non-donut forms and the material parameters were general plastic and glass fiber plastic. The results showed that the shear strengths varied depending on hollow shapes and materials used in the slab.

UV Degradation Characteristics and Applicability of Coating Agent for Conservation of FRP Artifacts (FRP 작품 보존을 위한 자외선 열화 특성 및 자외선 차단 코팅제 적용 연구)

  • Han, Ye Bin;Chung, Yong Jae
    • Journal of Conservation Science
    • /
    • v.33 no.3
    • /
    • pp.203-214
    • /
    • 2017
  • This study evaluated the degradation characteristics of FRP by ultraviolet (UV) rays and applied a UV-resistant coating to prevent the degradation of the surface of these sculptures. As a result of the degradation caused by UV rays, there were slight changes in the FRP surface and contact angle. The chromaticity sharply increased in the early phase of degradation. After applying the coating to the FRP, no significant surface changes were observed. However, it had lower changes in color as compared to the uncoated specimen, so it was verified that the control of discoloration could be possible. Some changes in the gloss and contact angle were observed depending on the extent of degradation, but the UV coating agent remained relatively stable. Analysis of the infrared light spectrum showed that there were almost no chemical changes, and it could be concluded that the coating treatment prevented degradation for a certain period. This study investigated the degradation of FRP used as materials in artwork exposed to UV rays, and it was found that there was a delay in the onset of degradation in the FRP with the UV-resistant coating when compared to the uncoated FRP.