Syntheses of Rayon-like Polyester (Rayon-like 폴리에스터의 합성(合成))

  • Ahn, Young-Moo;Park, Young-Gi
    • Journal of Fashion Business
    • /
    • v.11 no.5
    • /
    • pp.155-164
    • /
    • 2007
  • Viscose rayon has advantages such as vivid luster, good dyeability, low static electricity, good absorbance and good spinnability but also has flaws such as easy crease and decrease of physical properties when it gets wetting, and it requires dry cleaning. Therefore in order to synthesize the polymer to solve the problems of rayon while keeping the advantages of it, this study made the high specific gravity polyester for ultra drape property and high contraction polyester for rayon-like fiber having volume, soft and warm sense. The polyester with high specific gravity, 1.47 was made by adding 7 wt% of $BaSO_4$ as additive. High contraction polyester was made by copolymerization by using IPA 5 mole% to increase the amorphous region as comonomer and also using Newpol BPE-20(NPE) 1.5 wt% not to decrease the properties.

Optimum Condition of Spinning for Rayon-like Yarn (Rayon-like 섬유의 최적 방사 조건)

  • Ahn, Young-Moo
    • Journal of Fashion Business
    • /
    • v.12 no.1
    • /
    • pp.120-128
    • /
    • 2008
  • Rayon fiber as clothing material has silk-like property which relates to other synthetic fibers. It has many advantages that is required to women's clothes. However rayon has many shortcomings. Therefore this research is to spin rayon-like polyester which has high contraction property to be synthesized by previous research to solve those shortcomings and to maintain advantages of rayon. The contraction ratio of regular polyester is 30% and the contraction ratio of this synthesized polyester is over 60%. The spinning temperature of regular polyester ranges from $285^{\circ}C$ to $300^{\circ}C$. However, this copolymer is set range from $270^{\circ}C$ to $290^{\circ}C$, which is $10^{\circ}C$ less than regular polyester due to decreasing melting temperature. The spinning velocity effects the tensile strength and elongation of yarn magnificently. The high velocity of spinning makes yarn highly oriented, increases the tensile strength and decreases the elongation. This research defines the condition as following; draw ratio 2.734, First roller temperature $85^{\circ}C$, Slit heater temperature $175^{\circ}C$.